• 제목/요약/키워드: $(Na,K)NbO_3$ ceramics

검색결과 161건 처리시간 0.027초

ZnO와 MnO2를 동시에 첨가한 (K0.5Na0.5)NbO3 세라믹스의 압전 특성에 대한 연구 (Piezoelectric Properties of Lead-Free (K0.5Na0.5)NbO3 Ceramics Added with ZnO and MnO2)

  • 홍영환;박영석;정광휘;조성열;이재신
    • 한국전기전자재료학회논문지
    • /
    • 제29권4호
    • /
    • pp.210-214
    • /
    • 2016
  • We investigated the sintering behavior and piezoelectric properties of lead-free $(K_{0.5}Na_{0.5})NbO_3$ ceramics co-doped with excess 0.01 mol ZnO and x mol $MnO_2$, where x was varied from 0 to 0.03. Excess $MnO_2$ addition was found to retard the grain growth and densification during sintering. However, 0.005 mol $MnO_2$ addition improved the piezoelectric properties of 0.01 mol ZnO added $(K_{0.5}Na_{0.5})NbO_3$ ceramics. The planar mode piezoelectric coupling coefficient, electromechanical quality factor, and piezoelectric constant $d_{33}$ of 0.01 mol ZnO and 0.005 mol $MnO_2$ added specimen were 0.40, 304, and 214 pC/N, respectively.

MnO2 as an Effective Sintering Aid for Enhancing Piezoelectric Properties of (K,Na)NbO3 Ceramics

  • Jeong, Seong-Kyu;Hong, In-Ki;Do, Nam-Binh;Tran, Vu Diem Ngoc;Cho, Seong-Youl;Taib, Weon Pil;Lee, Jae-Shin
    • 한국분말재료학회지
    • /
    • 제17권5호
    • /
    • pp.399-403
    • /
    • 2010
  • The effects of $MnO_2$ doping on the crystal structure, ferroelectric, and piezoelectric properties of (K,Na)$NbO_3$ (KNN) ceramics have been investigated. $MnO_2$ was found to be effective in enhancing the densification and grain growth during sintering. X-ray diffraction analysis indicated that Mn ions substituted B-site Nb ions up to 2 mol%, however, further doping induced unwanted secondary phases. In comparison with undoped KNN ceramics, the well developed microstructure and the substitution to B-sites in 2 mol% Mn-doped KNN ceramics resulted in significant improvements in both piezoelectric coupling coefficient and electromechanical quality factor.

하소온도 변화에 따른 (Na,K)$NbO_3$계 무연 압전세라믹스의 특성에 관한 연구 (A Study on the Characteristics of (Na,K)$NbO_3$-system Pb-free Piezoelectric Ceramics with Calcination Temperature)

  • 류성림;정광현;이상호;류주현;박창엽;홍재일;이덕출
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.305-306
    • /
    • 2005
  • In this paper, in order to develop Pb-free piezoelectric ceramics, $(Li_{0.04}Na_{0.44}K_{0.52})(Nb_{0.86}Ta_{0.10}Sb_{0.04})O_3$ ceramics were fabricated with the variation of calcination temperature and sintering temperature. Specimens couldn't be sintered below $111^{\circ}C$ and showed the largest density at calcination temperature of $800^{\circ}C$. Specimens manufactured with the variation of calcination temperature showed pseudo-tetragonal phase, and showed the optimal values of kp=0.45, ${\varepsilon}r$=1336 and $d_{33}$=254 at calcination temperature of $800^{\circ}C$ and sintering temperature of $1110^{\circ}C$.

  • PDF

K5.4Cu1.3Ta10O29 첨가에 따른 0.97[(K0.5Na0.5)(Nb0.97Sb0.03)O3]-0.03[(Bi0.5K0.5)TiO3] 세라믹스의 압전 및 유전 특성 (Piezoelectric and Dielectric Properties of 0.97[(K0.5Na0.5)(Nb0.97Sb0.03)O3]-0.03[(Bi0.5K0.5)TiO3] Ceramics Modified with K5.4Cu1.3Ta10O29)

  • 이갑수;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제24권9호
    • /
    • pp.728-732
    • /
    • 2011
  • In this study, piezoelectric and dielectric properties of Lead-free $0.97[(K_{0.5}Na_{0.5})(Nb_{0.97}Sb_{0.03})O_3]+0.03[(Bi_{0.5}K_{0.5})TiO_3]$ (abbreviated as 0.97NKNS-0.03BKT)ceramics synthesized by conventional solid-state reaction process were investigated as a function of $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition. The results indicated that the $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition significantly improved the sinterability, grain growth and piezoelctric properties of 0.97NKNS-0.03BKT ceramics. The optimum values as planar piezoelectric coupling coefficient ($k_p$= 0.355), piezoelectric constant ($d_{33}$= 207 pC/N) and mechanical quality factor ($Q_m$= 128) were obtained when 0.009KCT was added. The electromechanical coupling factor($k_p$) was slightly decreased according to the increasing temperature.

비납계 (Bi1/2Na1/2)TiO3-Ba(Cu1/3Nb2/3)O3 세라믹의 압전 및 변위 특성 (Piezoelectric and Strain Properties of Lead-free (Bi1/2Na1/2)TiO3-Ba(Cu1/3Nb2/3)O3 Ceramics)

  • 류정호;정대용
    • 한국재료학회지
    • /
    • 제21권11호
    • /
    • pp.628-633
    • /
    • 2011
  • Studies on lead-free piezoelectrics have been attractive as means of meeting environmental requirements. We synthesized lead-free piezoelectric $(Bi_{1/2}Na_{1/2})TiO_3-Ba(Cu_{1/3}Nb_{2/3})O_3$ (BNT-BCN) ceramics, and their dielectric, piezoelectric, and strain behavior were characterized. As BCN with a tetragonal phase was incorporated into the rhombohedral BNT lattice, the lattice constant increased. A small amount of BCN increased the density and dielectric constant forming the complete solid solution with BNT. However, BCN above 10 mol% was precipitated into a separate phase, and which was detected with XRD. In addition, EDX measurement revealed that Cu in BCN was not distributed homogeneously but was accumulated in a certain area. A lower density with a large amount of BCN was attributed to the nonsinterable property of BCN with large tetragonaliy. The dielectric constant vs the temperature change and the strain vs the electric field indicated that the ferroelectric property of BNT was diminished and paraelectric behavior was enhanced with the BCN addition. BNT-7.5BCN showed a 0.11% unimorph strain with a 9.0 kV/mm electric field with little hysteresis.

KNbO3 치환이 (Li,Na,K)(Nb,Sb,Ta)O3계 세라믹스의 유전 및 압전 특성에 미치는 영향 (Effects of KNbO3-Substitution on the Dielectric and Piezoelectric Properties of (Li,Na,K)(Nb,Sb,Ta)O3 System Ceramics)

  • 노정래;류주현;이상돈
    • 한국전기전자재료학회논문지
    • /
    • 제26권3호
    • /
    • pp.204-208
    • /
    • 2013
  • In this study, $KNbO_3$-substituted (Li,Na,K)(Nb,Sb,Ta)$O_3$ ceramics were investigated to develop Pb-free composition ceramics for multilayer actuator and energy harvester applications. The X-ray diffraction analysis indicated that all samples were pure perovskite phase and no secondary phase was found. A tetragonality as a function of $KNbO_3$ substitution showed the maximum value at 1.5 mol% $KNbO_3$ and then decreased. The SEM image analysis showed the maximum grain size of $3.14{\mu}m$ at 1.5mol% $KNbO_3$. In the composition ceramics with 1.5 mol% $KNbO_3$ sintered at $1,100^{\circ}C$, excellent properties of density= 4.75 $g/cm^3$, electromechanical coupling factor ($k_p$)= 0.50 and piezoelectric constant($d_{33}$)= 290 pC/N were obtained, respectively, suitable for piezoelectric actuator and energy harvester applications.

Structural and piezoelectric properties of lead-free (1-x)$(Na_{0.5}\;K_{0.5})NbO_3$-xBa($Ti_{0.9}$, $Sn_{0.1}$)$O_3$ ceramics

  • 차유정;남산;김창일;정영훈;이영진;백종후
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 춘계학술발표대회
    • /
    • pp.33.1-33.1
    • /
    • 2009
  • Lead-free (1-x)$(Na_{0.5}K_{0.5})NbO_3$-xBa($Ti_{0.9}Sn_{0.1})O_3$ [NKN-BTS-100x] ceramics doped with 1 mol% $MnO_2$ have been prepared by the conventional solid state method and their structural and piezoelectric properties were investigated. The NKN-BTS-100x ceramics exhibited a dense and homogeneous microstructure when they were sintered at $1030-1150^{\circ}C$. Grain growth was observed for the specimen sintered at relatively low temperature of $1050^{\circ}C$. A tetragonal/orthorhombic morphotropic phase boundary (MPB) in the perovskite structure was also appeared for the NKN-BTS-100x ceramics (0.04$1050^{\circ}C$. The enhanced piezoelectric properties in the NKN-BTS ceramics with a MPB composition were obtained. Especially, for the NKN-BTS-6 ceramics, a high dielectric constant (${\varepsilon}^T_3/\varepsilon_0=1,400$), piezoelectric constant ($d_{33}=237$) and electromechanical coupling factor ($k_p=0.42$) were obtained.

  • PDF

Ag2O 첨가에 따른 0.98(Na0.5K0.5)NbO3-0.02Li(Sb0.17Ta0.83)O3 세라믹스의 압전특성 (Piezoelectric Properties of Ag2O-doped 0.98(Na0.5K0.5)NbO3-0.02Li(Sb0.17Ta0.83)O3 Ceramics)

  • 김현주;이승환;이성갑;이영희
    • 한국전기전자재료학회논문지
    • /
    • 제25권1호
    • /
    • pp.29-32
    • /
    • 2012
  • Lead-free $0.98(Na_{0.5},K_{0.5})NbO_3-0.02Li(Sb_{0.17}Ti_{0.83})O_3$ (hereafter 0.98NKN-0.02LST) ceramics doped with $Ag_2O$ were prepared using a conventional mixed oxide method. The specimen showed superior structural and electrical properties when 1 mol% $Ag_2O$ was doped. For the 0.98NKN-0.02LST+1.0mol%$Ag_2O$ ceramics sintered at $1,100^{\circ}C$, piezoelectric constant ($d_{33}$) of sample showed the optimum values of 207 pC/N. The 0.98NKN-0.02LST+1.0 mol%$Ag_2O$ ceramics are a promising candidate for lead-free piezoelectric materials.

$La_2O_3$ 첨가에 따른 (Ka,K)$NbO_3$ 세라믹스의 미세구조 및 압전 특성

  • 서병호;성금현;노정래;이상호;류주현;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 춘계학술회의 초록집
    • /
    • pp.12-12
    • /
    • 2010
  • The piezoelecric properties of $(K_{0.5}Na_{0.5})(Nb_{0.96}Sb_{0.04})O_3$+$1.2mol%K_4CuNb_8O_{23}$+$xmol%La_2O_3$ lead-free piezoelecric ceramics were investigated as a function x. These ceramics were fabricated by conventional ceramics processing. Piezoelectric constant ($d_{33}$) and piezoelectric charge coefficient ($g_{33}$) of x=0.2 mol% composition exhibited good properties of 160.3pC/N and 37.4($10^{-3}Vm/N$), respectively.

  • PDF

(1-x)$(Na_{0.5}K_{0.5})NbO_3-xLiNbO_3$ 무연 압전세라믹스의 첨가물질에 따른 전기적 특성 평가

  • 우덕현;류성림;윤만순;권순용
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.260-260
    • /
    • 2007
  • 강유전성 세라믹스 재료로써는 PZT계열의 세라믹재료가 널리 쓰이고 있다. 이는 우수한 유전 및 압전특성을 가지고 있으나, PbO을 다량 함유하고 있어 $1000^{\circ}C$이상에서 PbO가 급격하게 휘발되는 성질에 따라서 조성의 변동이 생겨 재현성이 어려우며 이를 방지하기 위하여 과잉 PbO를 첨가시키기 때문에 PbO휘발로 인한 강한 독성이 인체에 유해하다. 최근에는 Pb의 환경문제가 대두됨에 따라 이를 대체할 다른 물질의 개발이 활발하게 연구되고 있다. 대표적인 비납계 강유전 세라믹스인 $(Na_{0.5}K_{0.5})NbO_3$ ($d_{33}$ = 120 pC/N, Kp = 39%, Qm = 210, 이하 NKN라 표기) 조성은 $KNbO_3,\;NaNbO_3$ 상태도에 따라 순수한 NKN 세라믹스는 $1140^{\circ}C$에서 안정상을 가지나, 높은 온도로 인하여$Na_2O$$K_2O$가 쉽게 휘발됨에 따라 화학량 비의 변화가 생겨 이차 상을 형성하기도 한다. 따라서 본 연구에서는 $LiNbO_3$의 새로운 고용체를 추가시켜 기본 NKN조성에 압전성 및 고온에서의 상안정성을 향상시키고자 하였다. 최적 조성을 설계하기 위하여 (1-x)$(Na_{0.5}K_{0.5})NbO_3-xLiNbO_3$, x=(0,0.02,0.04,0.06,0.08)의 범위에서 조성을 변화시키면서 실험하였다. 시편 제작은 일반적인 세라믹스 소결 공정을 적용하였는데, $850^{\circ}C$에서 5시간 하소 후 $1080^{\circ}C$에서 2시간 소결하였다. 하소 및 소결 후에는 XRD분석을 통해 perovskite구조를 확인하였고, 미세구조 확인을 위해 주사전자현미경 (SEM)으로 관찰하였다. 압전특성을 평가하기 위해 압전 $d_{33}$-meter를 사용하였으며, impedance analyzer (HP 4194A)를 이용하여 전기적 특성을 측정하였다.