• 제목/요약/키워드: $(Ba,Sr,Ca)TiO_{3}$

검색결과 99건 처리시간 0.032초

Dielectric and Pyroelectric Properties of Dy-doped BSCT Thick Films by Screen-printing Method

  • Noh, Hyun-Ji;Lee, Sung-Gap;Nam, Sung-Pill
    • Journal of Electrical Engineering and Technology
    • /
    • 제4권4호
    • /
    • pp.527-530
    • /
    • 2009
  • $(Ba_{0.57}Sr_{0.33}Ca_{0.10})TiO_3$(=BSCT) powders, prepared by the sol-gel method, were doped using $MnCO_3$ as the acceptor and $Dy_2O_3$ as the donor. This powder was mixed with an organic vehicle. BSCT thick films were fabricated by the screen-printing techniques on the alumina substrate. The structural and dielectric properties of BSCT thick films were investigated with variation of the $Dy_2O_3$ amount. As a result of the differential thermal analysis (DTA), the exothermic peak was observed at around $670^{\circ}C$ due to the formation of the polycrystalline perovskite phase. All the BSCT thick films showed the XRD patterns of a typical polycrystalline perovskite structure. The average grain size of BSCT thick films decreased with an increasing amount of $Dy_2O_3$. The relative dielectric constant and dielectric loss of the BSCT thick film doped $Dy_2O_3$ 0.1mol% were 4637.4 and 1.6% at 1kHz, respectively.

Screen-printing법으로 제작한 BSCT 후막의 구조적 특성 (The Structural properties of BSCT thick films fabricated by screen-printing method)

  • 허영식;이성갑;박상만;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.545-548
    • /
    • 2002
  • $(Ba_{0.6-x}Sr_{0.4}Ca_x)TiO_3$(BSCT) (x=0.10, 0.15, 0.20) powders were prepared by the sol-gel method and BSCT thick films were fabricated by the screen-printing method. The structural properties as a faction of the composition ratio were studied. As a result of the differential thermal analysis (DTA), exothermic perk was observed at around $860^{\circ}C$ dne to the formation of the polycrystalline perovskite phase. The BSCT thick films sintered at $1350^{\circ}C$ for 2h showed the average grain size of $2{\sim}7{\mu}m$. The average thickness of BSCT thick films, obtained by 3 times of screen-printing, was approximately $85{\mu}m$.

  • PDF

거제도 화산암의 암석학적 연구 (Petrology of the Volcanic Rocks in Geoje Island, South Korea)

  • 윤성효;이준동;이상원;고정선;서윤지
    • 암석학회지
    • /
    • 제6권1호
    • /
    • pp.1-18
    • /
    • 1997
  • 이 연구에서는 한반도 남해안 도서지역중 거제도 일대의 화산암류를 대상으로 암석 기재, 암석화학적 특성을 알아보고, 화산암류의 조구적 위치 및 성인에 대하여 고찰하고자 한다. 본 역의 화산암류는 백악기의 퇴적암층을 기반으로 피복하여 주로 안산암질 화성쇄설암과 용암류가 교호로 누적된 산상 즉, 최하부는 두터운 화산각력암, 응회각력암 및 라필리응회암 누층으로 구성되고, 상부로 감에 따라 상대적으로 안산암 용암류가 라필리응회암과 응회암을 협재하며 빈번하게 노출되고 최상부에는 데사이트-유문암질 용결회류응회암류가 분포한다. 본 역의 화산암류는 주성분 화학조성으로 볼 때, 현무암에서 현무암질안산암, 안산암, 데사이트 그리고 유문암에 이르는 넓은 성분 조성을 하며 전형적인 BAR조합을 나타낸다. 본 역의 화산암류는 칼크-알칼리암계열에 속하며, SiO2에 대한 K2O 성분에서 medium-K의 조성을 나타내고, La, Th 및 Nb 상관도에서 조산대안산암(orogenic andesite)의 영역에 도시된다. 미량원소 함량을 MORB값으로 표준화한 spider diagram에서 Sr, K, Rb, Ba, Th 등이 다른 원소에 비하여 상대적으로 높은 값을 가지는 반면, Nb, P, Ti, Cr의 함량이 낮은, 지판의 침강 섭입에 관련된 대륙연번부/도호의 조구적환경에 관련된 암석들에 나타나는 특징을 잘 나타낸다. 희토류원소를 chondrite로 표준화한 그림에서는 전체적으로 LREEs가 HREEs에 비하여 부화되어 있으며, 현무암에서 현무암질안산암, 안산암, 데사이트 및 유문암으로 감에따라 Eu의 '-'이상이 점진적으로 커지며, 변화패튼이 대체로 평행한 배영을 보여주므로 본 역의 암석들은 동원마그마에서 유래하였음을 알 수 있다. 지구조위치 판별도에서 본 역의 화산암류는 지판이 침강 섭입하는 지판경계부에서 생성된 마그마로부터 유래한 화산암의 조구적 위치 즉 정상적인 대륙연변호(normal continental margin arc)의 영역에 해당한다. 거제도지역의 화산암류는 약 10% 정도의 맨틀물질의 부분용융으로 형성된 현무암질 시원마그마가 생성되어 지각으로 상승하는 과정에서 분별되어 칼크-알칼리 안산암질 마그마가 형성되었으며, 이 마그마로부터 계속 분별결정작용, 동화작용 및 마그마 혼합 등의 과정을 거치면서 다양한 화산암류를 형성한 것으로 해석된다.

  • PDF

한반도 동남부 제3기 연일, 어일분지에 나타나는 현무암질암의 암석학적 연구 (Petrology of the Tertiary Basaltic Rocks in the Yeonil and Eoil Basins, Southeastern Korea)

  • 심성호;박병준;김태형;장윤득;김정훈;김정진
    • 암석학회지
    • /
    • 제20권1호
    • /
    • pp.1-21
    • /
    • 2011
  • 한반도 남동부에 자리잡고 있는 제3기 분지 중에서 장기, 어일 분지에 대한 암석학적인 기재 및 지화학적 자료를 바탕으로 과거 조구조적 위치와 현무암질암을 생성한 기원마그마의 특성을 고찰하였다. 어일 현무암질 암내 사장석 반정에서는 여러 형태의 누대구조와 융식구조 및 체구조가 나타나며 반정의 성분변화에서 핵부분은 $An_{63.46-98.38}\;Ab_{1.62-32.96}\;Or_{0-3.58}$의 영역 (anorthite-labradorite)에 도시되고, 최외각은 $An_{40.89-82.44}\;Ab_{17.10-46.43}\;Or_{0-12.68}$의 영역 (bytownite-labradorite)에 해당한다. 주원소 분석결과, 이들 암석들은 현무암질 안산암 영역에 점시되며, 비알칼리암(sub-alkaline)계열에 해당한다. TAS도에 현무암과 현무암질 안산암의 영역에 점시되며, 비알칼리암(sub-alkaline)계열에 해당한다. $SiO_2$ 값이 커질수록 $Na_2O$$K_2O$는 증가하며 $TiO_2$, $FeO^*$, CaO, MgO, $P_2O_5$는 감소하는 경향을 보여준다. $K_2O-SiO_2$도표에서도 중-K계열의 칼크알칼리계열에 해당함을 보여준다. 미량원소 및 희토류 원소의 경향은 분화가 진행됨에 따라 Co, Ni, V, Zn, Sc 등과 같은 호정성 원소는 감소하고, Ba, Rb 등의 불호정성 원소들은 증가하는 특징을 보여준다. 0.81~1.00의 $Eu/Eu^*$값은 사장석 분별작용이 일부 암석에서는 거의 일어나지 않았거나 사장석의 분별이 약했다는 것을 시사한다. 동위원소 분석결과 $^{87}Sr/^{86}Sr$은 0.704090~0.704717, $^{143}Nd/^{144}Nd$은 0.512705~0.512822로서 Nd에 비해 Sr의 변화폭이 크지만 0.0007 내외의 변화폭을 보인다. 이러한 동위원소의 변화는 연구지역 현무암이 해양판의 섭입에 의해 결핍맨틀과 부화맨틀이 혼합되어 형성된 마그마에 기원함을 추정할 수 있게 한다. 동위원소비는 맨틀 경향에 잘 따르며 결핍맨틀(DMM)과 부화맨틀(EM)의 섞임 현상에 의한 맨틀조성을 갖는 마그마에 기원을 두고 있다.

경남 밀양지역 납석광상과 안산암질 모암의 지구화학적 연구 (A Geochemical Study on Pyrophyllite Deposits and Andesitic Wall-Rocks in the Milyang Area, Kyeongnam Province)

  • 오대균;전효택;민경원
    • 자원환경지질
    • /
    • 제25권1호
    • /
    • pp.27-39
    • /
    • 1992
  • Several pyrophyllite deposits occur around the Milyang area where Cretaceous andesitic rocks and spatially related granitic rocks are widely distributed. Pyrophyllite ores consist mainly of pyrophyllite, and quartz with small amount of sericite, pyrite, dumortierite, and diaspore. The andesitic rocks and spatially related granitic rocks in this area suggest that they could be formed from the same series of a calc-alkaline magma series. The contents of $SiO_2$, $Al_2O_3$, LOI(loss on ignition) are enriched, and $K_2O$, $Na_2O$, CaO, MgO, $Fe_2O_3$ are depleted in altered andesitic rocks and ores. Enrichment of As, Cr, Sr, V, Sb and depletion of Ba, Cs, Ni, Rb, U, Y, Co, Sc, Zn are characteristic during mineralization. The pyrophyllite ores can be discriminated from the altered-and unaltered wall-rocks by an increasing of $(La/Lu)_{cn}$ from 4.18~22.13 to 8.98~55.05. In R-mode cluster analysis, Yb-Lu-Y, La-Ce-Hf-Th-U-Zr, $TiO_2-V-Al_2O_3$, Sm-Eu, $CaO-Na_2O-MnO$, Cu-Zn-Ag, $K_2O-Rb$ are closely correlated. In the discriminant analysis of multi-element data, $P_2O_5$, As, Cr and $Fe_2O_3$, Sr are helpful to identify the ores from the unaltered-and altered wall-rocks. In the factor analysis, the factors of alteration of andesitic rocks and ore mineralization were extracted. In the change of ions per unit volume, $SiO_2$, $Al^{3+}$ and LOI are enriched and $Na^+$, $K^+$, $Ca^{2+}$, $Mg^{2+}$, $Mn^{2+}$ and $Fe^{3+}$ are depleted during the alteration processes. The Milyang and the Sungjin pyrophyllite deposits could be mineralized by hydrothermal alteration in a geochemical condition of low activity ratio of alkaline ions to hydrogen ion with reference to spatially related granitic rocks.

  • PDF

초고주파 소자로의 응용을 위한 BST계 후막의 전기적 특성에 관한 연구 (Electrical properties of BST system thick films for microwave devices applications)

  • 이성갑;박춘배;한병성;박복기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 제5회 영호남 학술대회 논문집
    • /
    • pp.31-34
    • /
    • 2003
  • ($Ba_{0.6-x}Sr_{0.4}Ca_x)TiO_3$ (BSCT) (x=0.10, 0.15, 0.20) powder, prepared by the sol-gel method, were mixed with organic vehicle and the BSCT thick films were fabricated by the screen-printing techniques on alumina substrates using the BSCT paste. The structural and the electrical properties were investigated for various composition ratio and sintering temperature. BSCT thick film thickness, obtained by four printings, was approximately 110 ~ 120 ${\mu}m$. The Curie temperature and dielectric constant at room temperature were decreased with increasing Ca content. The relative dielectric constant, dielectric loss and tunability of the BSCT(50/40/10) specimen, which was sintered at $1420^{\circ}C$ and measured at 1MHz, were about 910, 0.46% and 9.28% at 5kV/cm, respectively.

  • PDF

소결온도에 따른 BSCT 후막의 구조적, 유전적 특성 (Structural and Dielectric Properties of BSCT Thick films with Various Sintering Temperature)

  • 이성갑;이영희;이상헌
    • 한국전기전자재료학회논문지
    • /
    • 제16권4호
    • /
    • pp.304-310
    • /
    • 2003
  • (Ba$\sub$0.6-x/Sr$\sub$0.4/Ca$\sub$x/)TiO$_3$(BSCT) (x=0.10, 0.15, 0.20) powder, prepared by the sol-Bel method, were mixed with organic binder and then BSCT thick films were fabricated by the screen printing techniques on alumina substrates using the BSCT paste. The structural and the dielectric Properties were investigated for various composition ratio and sintering temperature. The second phase appeared in BSCT(40/40/20) thick film sintered at 1450$^{\circ}C$. BSCT thick film thickness, obtained by four printings, was approximately 110∼120$\mu\textrm{m}$. The Curie temperature and dielectric constant at room temperature were decreased with increasing Ca content. The relative dielectric constant, dielectric loss and tunability of the BSCT(50/40/10) specimen, which was sintered at 1420$^{\circ}C$ and measured at 1MHz, were about 910, 0.46% and 9.28% at 5㎸/cm, respectively.

운산 금 광상의 엽리상 석영맥에서 산출되는 백색운모와 녹니석의 산상 및 화학조성 (Occurrence and Chemical Composition of White Mica and Chlorite from Laminated Quartz Vein of Unsan Au Deposit)

  • 유봉철
    • 광물과 암석
    • /
    • 제34권1호
    • /
    • pp.1-14
    • /
    • 2021
  • 운산 금 광상은 한반도의 3대(대유동 광상, 광양 광상) 금 광상중의 하나였다. 이 광상의 지질은 선캠브리아기의 변성퇴적암류와 중생대의 반상화강암으로 구성된다. 이 광상은 선캠브리아기의 변성퇴적암류와 중생대의 반상화강암내에 발달된 단층대를 따라 충진한 함 금 석영맥 광상으로 조산형 금 광상에 해당된다. 이 광상의 석영맥은 광물조합에 따라 1) 방연석-석영맥형, 2) 자류철석-석영맥형, 3) 황철석-석영맥형, 4) 페크마틱 석영맥형, 5) 백운모-석영맥형 및 6) 단순석영맥형으로 분류된다. 연구된 석영맥은 황철석-석영맥형이며 견운모화작용, 녹니석화작용 및 규화작용이 관찰된다. 백색운모는 유색대에서 백색석영, 황철석, 녹니석, 금홍석, 모나자이트, 저어콘, 인회석, 칼리장석 및 방해석 등과 함께 세립질 내지 중립질 입단으로 산출된다. 이 백색운모의 화학조성은 (K0.98-0.86Na0.02-0.00Ca0.01-0.00Ba0.01-0.00 Sr0.00)1.00-0.88(Al1.70-1.57Mg0.22-0.09Fe0.23-0.10Mn0.00Ti0.04-0.02Cr0.01-0.00V0.00Ni0.00)2.06-1.95 (Si3.38-3.17Al0.83-0.62)4.00O10(OH2.00-1.91F0.09-0.00)2.00로써 이론적인 이중팔면체형 운모류 값보다 Si가 높고 K, Na, Ca는 낮다. 이 광상의 엽리상 석영맥에서 산출되는 백색운모의 화학조성 변화는 팬자이틱(phengitic) 또는 Tschermark 치환[(Al3+)VI+(Al3+)IV <-> (Fe2+ 또는 Mg2+)VI+(Si4+)IV] 및 직접적인 (Fe3+)VI <-> (Al3+)VI 치환에 의해 일어났음을 알 수 있다. 엽리상 석영맥에서 산출되는 녹니석의 화학조성은 (Mg1.11-0.80Fe3.69-3.14Mn0.01-0.00Zn0.01-0.00K0.07-0.01Na0.01-0.00Ca0.04-0.01Al1.66-1.09)5.75-5.69 (Si3.49-2.96Al1.04-0.51)4.00O10 (OH)8로써 이론적인 녹니석보다 Si 함량이 높다. 이 녹니석의 화학조성 변화는 팬자이틱(phengitic) 또는 Tschermark 치환(Al3+,VI+Al3+,IV <-> (Fe2+ 또는 Mg2+)VI+(Si4+)IV) 및 팔면체적 Fe2+ <-> Mg2+ (Mn2+) 치환에 의해 일어났음을 알 수 있다. 따라서 운산 광상의 엽리상 석영맥 및 변질광물은 조산운동 시 연성전단(ductile shear) 시기에 형성되었음을 알 수 있다.

$Pr_{2}O_{3}$ 첨가량에 따른 BSCT 세라믹의 미세구조 특성 (Microstructure properties with variation of doped amount $Pr_{2}O_{3}$ of BSCT ceramics)

  • 노현지;이성갑;박상만;윤상은;김지은;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2007년도 제38회 하계학술대회
    • /
    • pp.1283-1284
    • /
    • 2007
  • The barium strontium calcium titanate((Ba,Sr,Ca)$TiO_3$) powders prepared by the sol-gel method and $MnCO_3$ as acceptor were mixed oxide method. The microstructure was investigated with variation of $Pr_{2}O_{3}$ amount. The BSCT powder and $Pr_{2}O_{3}$ were mixed with organic vehicle(Ferro. B75001). BSCT thick films were fabricated by the screen-printing method on alumina substrates. The bottom electrode was Pt and upper electrode was Ag, respectively. All BSCT thick films were sintered at $1420^{\circ}C$, for 2h. The result of the differential thermal analysis(DTA), exothermic peak at around $654^{\circ}C$ due to the formation of the polycrystalline perovskite phase. In the X-ray diffraction(XRD) patterns, all BSCT thick films showed the typical perovskite polycrystalline structure and no pyrochlore phase was dbserved. The microstructure investigated by scanning electron microscope(SEM). Pore and grain size of BSCT thick films were decreased with increasing amount of $Pr_{2}O_{3}$ dopant. And the average grain size and thickness of BSCT thick films doped with 0.1 mol% $Pr_{2}O_{3}$ was $3.09{\mu}m$, $60{\mu}m$, respectively. The relative dielectric constant decreased and dielectric loss decreased with increasing amount of $Pr_{2}O_{3}$ dopant, the values of the BSCT thick films no doped with $Pr_{2}O_{3}$ were 7443 and 4 % at 1 kHz, respectively.

  • PDF

광주지역 하상퇴적물에 대한 지질집단별 지구화학적 연구 (Geochemical Study on Geological Groups of Stream Sediments in the Gwangju Area)

  • 김종균;박영석
    • 자원환경지질
    • /
    • 제38권4호
    • /
    • pp.481-492
    • /
    • 2005
  • 이 연구에서는 광주지역 하상퇴적물에 대한 지질집단별 지구화학적 특성에 대해 규명 하고자 한다. 이를 위해 물이 흐르고 있는 1차 수계를 대상으로 하상퇴적물시료 104개를 채취하였고, 실험실에서 자연건조 시켰다. 화학분석을 위한 시료는 알루미나 몰타르를 이용하여 200메쉬 이하로 분쇄하였고, XRF ICP-AES, NAA분석을 실시하였다. 연구지역 하상퇴적물에 대해, 지질집단별 지구화학적 특성 비교와 기존 암석에 대한 연구에서 얻어진 암석화학적인 특성과의 비교를 위해, 선캠브리아기 화강편마암 지역, 쥬라기 화강암 지역, 백악기 화순안산암 지역으로 분리하였다 광주지역 하상퇴적물의 주성분원소 함량은 $SiO_2\;51.89\~70.63\;wt.\%,\;Al_2O-3\;12.91\~21.95\;wt.\%,\;Fe_2O_3\;3.22\~9.89\;wt.\%,\;K_2O\;1.85\~4.49\;wt.\%,\;MgO\;0.68\~2.90\;wt.\%,\;Na_2O\;0.48\~2.34\;wt.\%,\;CaO\;0.42\~6.72\;wt.\%,\;TiO_2\;0.53\~l.32\;wt.\%,\;P_2O_5\;0.06~0.51\;wt.\%\;and\;MnO\;0.05\~0.69\;wt.\%.$이다. 하상퇴적물과 암석에 대한 AMF 삼각도에서, 암석은 칼크-알칼리계열에 도시되는데 비하여, 하상퇴적물은 솔레아이트 계열과 칼크-알칼리계열의 경계부위에 도시된다. 이는 $Fe_2O_3$ 함량이 암석에서보다 하상퇴적물에 더 많이 함유되어 있는 것과 관련이 있는 것으로 보인다. $SiO_2$에 대한 $K_2O+Na_2O$의 비교그림에서, 하상퇴적물은 암석에서와 같이 subalkaline 계열에 점시된다. 하상퇴적물의 미량성분원소 및 희토류 원소 함량은 $Ba 590\~2170ppm$, Be$1\~2.4$ppm, Cu $13\~179ppm$, Nb $20\~34ppm$, Ni$10\~50ppm$, Pb $17\~30$ppm, Sr $70\~1025$ ppm, V$42\~135$ ppm, Zr$45\~171$ ppm, Li$19\~77$ppm, Co$4.3\~19.3$ppm, Cr$28\~131$ppm, Cs$3.1\~17.6$ ppm, Hf $5\~27.6$ ppm, Rb $388\~202$ ppm, Sb$0.2\~l.2$ ppm, Sc$6.4\~17$ ppm, Zn $47\~389$ ppm, Pa $8.8\~68.8$ ppm, Ce$62\~272$ppm, Eu$1\~2.7$ppm and Yb$0.9\~6$ppm의 범위를 보인다.