Abstract

Because of the supply-demand problem of aggregate, recently, the construction sites using 100% crushed sand are increasing and the use of low quality aggregate such as farmland sand is increasing too. When the low quality aggregate is used, the various quality defect of concrete such as the strength reduction, the increase of shrinkage and bleeding can be occurred. Therefore, in this study, the performance improvement PC admixture was developed to minimize the quality defect of plain concrete of basement parking area, when the low quality aggregate was used at the plain concrete of basement parking area. The slump loss to elapsed time test, the compressive strength test, the bleeding test and the drying shrinkage test were carried out.

최근 국내에서 천연골재의 고갈, 수급 불균형 등의 이유로 부순모래를 100% 사용하거나, 내륙 지역의 경우 개답사, 마사토 등과 같은 저품질의 골재를 사용하는 경우가 증가하고 있으며, 높은 흡수율과 점성의 증가로 인하여 작업성 확보를 위해 배합수 량이 증가되는 실정이다. 배합수의 증가로 강도 저하, 건조수축 증가, 블리딩 증가 등에 인한 다양한 품질하자를 유발하게 된다. 특히 지하주차장 무근콘크리트의 경우 표면부와 저면의 수축차의 증가로 인한 컬링이 발생하게 되고, 컬링이 발생한 후에 차량이 통과하게 되면 무근 콘크리트에 균열이 발생하게 된다. 지하 최하층의 경우 배수판 사이를 흐르는 지하수의 유입으로 누수현상도 발생하게 되며, 차량 통행에 따른 소음도 발생할 수 있다. 또한 블리딩 증가로 인한 표면 강도 저하로 박리, 박락 등의 하자가 다발적으로 발생하여 매년 민원과 소송이 증가하고 있다. 따라서 본 연구에서는 이러한 문제를 해결하기 위해서 저품질의 골재가 사용되었을 경우 지하주차장 무근콘크리트의 품질하자를 최소화시키기 위한 성능개선형 PC 혼화제를 개발하였으며, 슬럼프 경시변화, 압축강도, 블리딩, 건조수축 길이변화 시험을 실시하여 일반 준PC 혼화제를 사용한 콘크리트와 비교하였다. 그 결과 경시에 의한 슬럼프의 저하를 최소화시킬 수 있음을 확인할 수 있었으며, 추가적인 가수가 필요 없거나 최소화시킬 수 있으므로 일반 준PC 혼화제를 사용한 콘크리트보다 고품질을 확보할 수 있을 것으로 기대된다. 특히 건조수축량이 20% 정도 감소하여 건조수축균열 및 컬링 제어에 효과적일 것으로 판단된다.

Keywords

References

  1. Jo MK, Song YL, Park YJ, Lee HK, Han MC, HAN CG. Basic and strength properties of aggregates from various locations in sud-korea. Proceedings of The Korea Institute of Building Construction. 2015 Nov 14; Yonsei University, Seoul, Korea. Seoul (Korea): The Korea Institute of Building Construction; 2015. p. 145-46.
  2. Shin JH, Choi HU, Yoo BH, Son HJ, Lee DG, Han HS. Basic research on improved quality of concrete using low-quality aggregates. Proceedings of the Korea Concrete Institute. 2017 May 10-12; Phoenix Island, Jeju, Korea. Seoul (Korea): Korea Concrete Institute; 2017. p. 483-84.
  3. Moon BY, Lee SJ, Park YJ, Jo MK, Han MC, Han CG. Mixture proportion and compressive of the concrete according to changes of type of fine aggregate and unit binder weight. Proceedings of The Korea Institute of Building Construction, 2015 Nov 14; Yonsei University, Seoul, Korea. Seoul (Korea): The Korea Institute of Building Construction; 2015. p. 19-20.
  4. Cement Concrete and Aggregates Australia. Curling of concrete slabs. 2006. p. 1-6.
  5. Mailvaganam N, Springfield J, Repette W, Taylor D. Curling of concrete slabs on grade. Construction Technology Undate. National Research Council of Canada. 2000 Dec;44(6):1-6.
  6. Lee DG, Han HS, Jung YW. Chemical Admixture Technology for Reducing Shrinkage of Concrete, Magazine of the Korea Concrete Institute. 2016 Nov;28(6):31-6.
  7. Korean Standards Association. Method of test for slump of concrete. KS F 2402. 2007.
  8. Korean Standards Association. Standard test method for compressive strength of concrete. KS F 2405. 2010.
  9. Korean Standards Association. Standard test method for bleeding of concrete. KS F 2414. 2015.
  10. Korean Standards Association. Testing method for length change of mortar and concrete. KS F 2424. 2015.