Abstract

The composite of porous silicon (Si) and amorphous carbon (C) is prepared by pyrolysis of a nano-porous Si + pitch mixture. The nano-porous Si is prepared by mechanical milling of magnesium powder with silicon monoxide (SiO) followed by removal of MgO with hydrochloric acid (etching process). The Brunauer-Emmett-Teller (BET) surface area of porous Si ($64.52m^2g^{-1}$) is much higher than that before etching Si/MgO ($4.28m^2g^{-1}$) which indicates pores are formed in Si after the etching process. Cycling stability is examined for the nano-porous Si + C composite and the result is compared with the composite of nonporous Si + C. The capacity retention of the former composite is 59.6% after 50 charge/discharge cycles while the latter shows only 28.0%. The pores of Si formed after the etching process is believed to accommodate large volumetric change of Si during charging and discharging process.

Keywords

References

  1. T. D. Besenhard, J. Yang and M. Winter: J. Power Sources, 68 (1997) 87. https://doi.org/10.1016/S0378-7753(96)02547-5
  2. C. J. Wen and R. A. Huggins: J. Solid State Chem., 37 (1976) 271.
  3. A. M. Wilson and J. R. Dahn: J. Electrochem. Soc., 142 (1995) 326. https://doi.org/10.1149/1.2043994
  4. H. Li, X. Huang, L. Chen, Z. Wu and Y. Liang: Electrochem. Solid-State Lett., 2 (1999) 547. https://doi.org/10.1149/1.1390899
  5. I.-S. Kim, P. N. Kumta and G. E. Blomgren: Electrochem. Solid-State Lett., 3 (2000) 493.
  6. I.-S. Kim, G. E. Blomgren and P. N. Kumta: J. Power Sources, 130 (2004) 275. https://doi.org/10.1016/j.jpowsour.2003.12.014
  7. M. Yoshio, H. Wang, K. Fukuda, T. Umeno, N. Dimov and Z. Ogumi: J. Electrochem. Soc., 149 (2002) A1598. https://doi.org/10.1149/1.1518988
  8. N. Dimov, S. Kugino and M. Yoshio: Electrochim. Acta, 48 (2003) 1579. https://doi.org/10.1016/S0013-4686(03)00030-6
  9. J. Yang, B. F. Wang, K. Wang, Y. Liu, J. Y. Xie and Z. S. Wen: Electrochem. Solid-State Lett., 6 (2003) A154. https://doi.org/10.1149/1.1585251
  10. H. Dong, X. P. Ai and H. X. Yang: Electrochem. Commun., 5 (2003) 952. https://doi.org/10.1016/j.elecom.2003.09.004
  11. H. Y. Lee and S. M. Lee: J. Power Sources, 112 (2002) 649. https://doi.org/10.1016/S0378-7753(02)00461-5
  12. Y. Liu, K. Hanai, T. Matsumura, N. Imanishi, A. Hirano and Y. Takeda: Electrochem. Solid-State Lett., 7 (2004) A492. https://doi.org/10.1149/1.1818021
  13. M. S. Park, Y. J. Lee, S. Rajendran, M. S. Song, H. S. Kim and J. Y. Lee: Electrochim. Acta, 50 (2005) 5561. https://doi.org/10.1016/j.electacta.2005.04.042
  14. H. Y. Lee, Y. L. Kim, M. K. Hong and S. M. Lee: J. Power Sources, 141 (2005) 159. https://doi.org/10.1016/j.jpowsour.2004.08.023
  15. J. Yang, Y. Takeda, N. Imanishi, C. Capiglia, J. Y. Xie and O. Yamamoto: Solid State Ionics, 152/153 (2002) 125. https://doi.org/10.1016/S0167-2738(02)00362-4
  16. X. Yang, J. McBreen, W. Yoon, M. Yoshio, H. Wang, K. Fukuda and T. Umeno: Electrochem. Commun., 4 (2002) 893. https://doi.org/10.1016/S1388-2481(02)00483-6
  17. N. Dimov, S. Kugino and M. Yoshio: J. Power Sources, 136 (2004) 108. https://doi.org/10.1016/j.jpowsour.2004.05.012
  18. G. X. Wang, J. Yao and H. K. Liu: Electrochem. Solid- State Lett., 7 (2004) A250. https://doi.org/10.1149/1.1764411
  19. T. Kim, S. Park and S. M. Oh: Electrochem. Commun., 8 (2006) 1461. https://doi.org/10.1016/j.elecom.2006.06.020
  20. J. H. Kim, H. Kim and H. J. Sohn: Electrochem. Commun., 7 (2005) 557. https://doi.org/10.1016/j.elecom.2005.03.013
  21. B. C. Kim, H. Uono, T. Sato, T. Fuse, T. Ishihara and M. Senna: Solid State Ionics, 172 (2004) 33. https://doi.org/10.1016/j.ssi.2004.02.028
  22. T. Morita and N. Takami: J. Electrochem. Soc., 153 (2006) A425. https://doi.org/10.1149/1.2142295
  23. B. C. Kim, H. Uono, T. Satou, T. Fuse, T. Ishihara, M. Ue and M. Senna: J. Electrochem. Soc., 152 (2005) A523. https://doi.org/10.1149/1.1856990