초록
The influence of the concentration of precursor solution and the number of solution coatings on the densification of the $Pb(Zr_xTi_{1-x})O_3$ (PZT) thick films was studied. PZT powder and PZT precursor solution were prepared by3 sol-gel method and PZT thick films were fabricated by the screen-printing method on the alumina substrates. The composition of powder and precursor solution were PZT(70/30) and PZT(30/70), respectively. The PZT precursor solution was spin-coated on the PZT thick films. A concentration of a coating solution was 0.5 to 2.0 mol/L[M] and the number of coating was repeated from 0 to 6. The XRD patterns of all PZT thick films shelved typical perovskite polycrystalline structure. The porosity of the thick films was decreased with increasing the number of coatings and 6-time coated films with 1.5 M showed the dense microstructure and thickness of about $60{\mu}m$. The relative dielectric constant of the PZT thick film was increased with increasing the number of solution coatings and the thick films with 1.5 M, 6-time coated showed the 698. The remanent polarization the 1.5 M and 6-time coated PZT thick films was $38.3{\mu}C/cm^2$.