Abstract
In this study, the influence of heat treatment and Ca contents on the electrochemical behavior was investigated. Mg-Ca alloys, i.e., Mg-0.22wt%Ca, Mg-0.56wt%Ca, Mg-1.31wt%Ca are prepared by ingot metallurgy. As-cast Mg-Ca alloys exhibited better electrochemical properties than pure Mg. Especially, Mg-0.22wt%Ca alloy improves its anode efficiency up to 62% and lowers the OCP up to -1.72VSCE. Microstructure and XRD patterns of Mg-Ca alloys show that additive Ca element is mainly solid-solutioned. While, the others show the microstructure and XRD pattern with large $Mg_2Ca$ at grain boundary. To assess the effect of heat treatment on the as-cast Mg-alloy, the specimens were heat treated at $200^{\circ}C$ for 2 hours under $CO_2$ gas atmosphere. Although corrosion properties of Mg-Ca alloys are somewhat deteriorated by heat treatment at $200^{\circ}C$ Mg-0.22wt%Ca alloy with uniformly distributed nano-sized $Mg_2Ca$ phase in ${\alpha}$-Mg matrix show still better corrosion properties than pure Mg specimen.