Effect of Bark and Drying Waste Liquor of Larix kaempferi Used as An Additive on The Fuel Characteristics of Wood Pellet Fabricated with Rigida Pine and Quercus mongolica Sawdust (첨가제로서 낙엽송의 수피 및 건조폐액이 리기다소나무 및 신갈나무 펠릿의 연료적 특성에 미치는 영향)

  • Yang, In;Chae, Hyun-Gyu;Han, Gyu-Seong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.45 no.3
    • /
    • pp.258-267
    • /
    • 2017
  • In this study, pitch pine (Pinus rigida, PIR) and Mongolian oak (Quercus mongolica, QUM) pellets were fabricated with bark or/and drying waste liquor (DWL) of larch (Larix kaempferi, LAK) as an additive. Based on the results of fuel characteristics of the pellets, optimal conditions for producing the high-quality pellets were provided. In the analysis of chemical composition, bark contained holocelluose and lignin of 90% and over. DWL had 0.1% solid assumed to sugars which are generated from the oven-drying of LAK logs. QUM showed high ash content (2.2%) by containing of bark in the sawdust. Bark and DWL of LAK had high ash content of 4% and over. Calorific values of all specimens and additives were higher than that of the $1^{st}$-grade standard of wood pellets designated by NIFOS (18.0 MJ/kg). PIR and QUM pellets were fabricated with additive of 2 wt% based on the solid weight of oven-dried sawdust using a piston-type flat-die pelletizer, and thus ash content and calorific value of the pellets did not affect by the use of additive. Durability of the pellets increased with the use of additive. Durabilties of pellets, which were fabricated with bark as an additive and DWL as a controller of moisture content for sawdust, did not differ from those of pellets without additives and were lower than those of pellets either with bark or DWL. However, use of both bark and DWL for the production of wood pellets might be favorable because it can make a profit from the collection process of DWL. Based on the results of fuel characteristics of the pellets, QUM and PIR pellets were produced by a flat-die pelletizer. Moisture content (MC), bulk density and durability of the pellets improved with the use of additive. Particularly, sawdust MC of 10% and the addition of bark or DWL for PIR as well as sawdust MC of 12% and the addition of bark for QUM might be optimal conditions for the production of high-quality pellets. Except for the ash content of QUM pellets, other properties of PIR and QUM pellets exceeded the $1^{st}$-grade wood pellets standards of NIFOS.

Studies on the feeding value of the waste wood of Leniinus eddodes (표고 재배(栽培) 폐재(廢材)의 사료화(飼料化)에 관(關)한 연구(硏究))

  • Kim, Bub-Whoe;Lee, Teck-Won;Min, Du-Sik;Kim, Nae-Soo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.6 no.1
    • /
    • pp.8-14
    • /
    • 1978
  • In order to determine the feeding value of t:1e waste wood of Lentinus eddodes, the waste wood was milled and treated with $Ca(OH)_2$ and cellulase, then raw waste wood and the treated waste wood were fed to broiler chicken and Korean native goates. The results obtained were as follows; 1. The chemical composition of the waste wood was c. protein 2.26%. c. fat 2.57%. c. fiber 44.60 and c. ash 5.58%. No differences were detected between the raw waste wood and $Ca(OH)_2$ or cellulase treated waste wood in chemical composition. 2. In amino acid composition. no cystine and methionine was showed, but trace amount of Vitamin A, $B_1$, and $B_2$, and cholin chloride were detected. 3. Trichoderma viride SANK. No. 16374 was used to decompose the cellulose. 4. In broiler performance, when waste wood meal was subsituted for 5% wheat bran, no adverse effect was showed on weight gain, feed in take and feed efficiency. But $Ca(OH)_2$ and cellulase treated waste wood meal could be subsituted for 8% wheat bran. 5. In Korean native goat performance, feeding waste wood meal subsituted by 50% various bran (25% defatted rice bran and 25% barley bran) had no adverse effect on growth and feed efficiency. 6. Considering the above results, though the waste wood meal could be replaced to part of various bran, there was a bottle-neck to process the waste wood. The waste wood of Lentinus edodes was little feeding value on bed of ruminant.

  • PDF

Evaluation of the Basic Properties for the Korean Major Domestic Wood Species I. Korean Red Pine (Pinus densiflora) in Pyeongchang-gun, Gangwon-do

  • Yonggun PARK;Chul-ki KIM;Hanseob JEONG;Hyun Mi LEE;Kwang-Mo KIM;In-Hwan LEE;Min-Ji KIM;Gyu Bin KWON;Nayoung YOON;Namhee LEE
    • Journal of the Korean Wood Science and Technology
    • /
    • v.52 no.1
    • /
    • pp.87-100
    • /
    • 2024
  • Wood has different properties depending on the species or growth area. Therefore, in order to use wood efficiently, it is necessary to have a proper understanding of the characteristics of wood depending on the species and the appropriate use for them. In particular, in order to effectively use more than 1,000 species of woody plants in South Korea as wood, it is necessary to evaluate the characteristics of various Korean domestic woods and make a database of them. In this study, the anatomical properties (length and width of tracheid, cell wall thickness), physical properties (specific gravity and shrinkage), mechanical properties (bending strength, compressive strength, tensile strength, shear strength, hardness), and chemical composition (ash, extract, lignin, total sugar content) of Korean red pine which was grown in Pyeongchang-gun, Gangwon-do, South Korea were evaluated.

Improvement in The Fuel Characteristics of Empty Fruit Bunch by Leaching and Wet Torrefaction (용탈처리와 습식 반탄화에 의한 Empty Fruit Bunch의 연료적 특성 향상)

  • Gong, Sung-Ho;Lee, Hyoung-Woo;Lee, Jae-Won
    • Journal of the Korean Wood Science and Technology
    • /
    • v.44 no.3
    • /
    • pp.360-369
    • /
    • 2016
  • In this study, sequential leaching and wet torrefaction were performed to improve the fuel characteristics of empty fruit bunch (EFB). Leaching was carried out at $25{\sim}90^{\circ}C$ for 5~30 min. The highest ash removal efficiency of 55.99% was achieved when leaching was performed at $90^{\circ}C$ for 10 min. The ash removal efficiency was dependent more on leaching temperature than time. Wet torrefaction was carried out at $180{\sim}200^{\circ}C$ for 5~40 min, following the leaching. Most of the inorganic compounds were removed at removal efficiencies of 41.05~63.58% during sequential leaching and wet torrefaction, while silica remained in the biomass. Chloride, calcium, magnesium, and phosphorus showed more than 80% removal efficiencies. The calorific value of EFB increased to 7.96% (4730 kcal/kg) in comparison to the raw material (4390 kcal/kg) when wet torrefaction was performed at $200^{\circ}C$ for 40 min following leaching.

Studies on the Wood Properties of Lesser-Known Species Grown in Indonesia(IV) -The Fundamental Wood Properties of Tamiang, Bangelem and Kamasulan- (인도네시아산 미이용 수종의 목재성질(IV) - Tamiang, Bangelem 및 Kamasulan 목재의 기초성질 -)

  • 정성호;정두진;박병수;이도식;조성택;이동협;홍인표;전수경
    • Journal of the Korea Furniture Society
    • /
    • v.11 no.2
    • /
    • pp.25-35
    • /
    • 2000
  • This study was carried out to investigate the wood properties for development the proper uses of lesser-known tree species. The tested species are Tamiang(Hydnocarpus woodii) Bangelem (Strombosia zeylanica) and Kamasulan(Anisophyllea ferruginea) grown in Indonesia. fundamental wood properties such as anatomical, physical and chemical properties and characteristics related to wood processing were examined. The results are summarized as follows : These species are diffuse porous, interlocked grained and coarse textured wood. Exceptionally, texture of Tamiang is fine. The heartwoods of these species are not distinguished clearly to the sapwoods. These species have high specific gravity, high shrinkage, and excellent strength properties. However, Tamiang has moderate specific gravity. Sawing characteristics are poor for these species except Tamiang. Sawing characteristics is moderate for Tamiang. Drying characteristics are moderate for Tamiang and Bangelem, and Poor for Kamasulan. The surfacing characteristics by planer are moderate f3r all these species. Bending property and durability are poor. Ash content is low in Bangelem.

  • PDF

A Study on Anatomical and Physical Properties of Exotic Species (First Report; Pinus banksiana) (외래수종의(外來樹種) 해부학적(解剖學的) 및 물리적(物理的) 성질(性質)에 관(關)한 연구(硏究) 제1보(第1報) (Pinus banksiana))

  • Shim, Chong-Supp;Jo, Jae-Myeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.10 no.3
    • /
    • pp.45-45
    • /
    • 1982
  • There are many important exotic species in Korea, such as white pine, pitch pine, jack pine, oak, ash, etc. Some of them are already being used for various construction purposes, in spite of their history imported to and cultivated in Korea being very young. No study was carried out on the various properties of these exotic species, which arc needed for their proper use at present.

  • PDF

An Experimental Study on the Geopolymer for Wood Wool Ceramic Board (목모 패널용 Geopolymer Binder 개발에 관한 실험적 연구)

  • Park Dong Cheol;Lee Sea Hyun;Song Tae Hyeob;Shim Jong Woo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.11a
    • /
    • pp.711-714
    • /
    • 2005
  • This paper focused on development of geopolymer for wood wool ceramic board. Geopolymer can substitude ordinary portland cement and its accelerator of wood wool cement board as inorganic polymer. In this study, what we would obtain geopolymer's properties such as initial setting time(KS L 5108), flow(KS L 5102) and compressive strength of 3days aged(KS L 5105), was less than 1 hour, more than $110\%$, more than 40Mpa. Geopolymer have three essential materials called filler, hardener and geopolymer liquor. So, We applied filler by quartz, hardener by blast furnace slag powder, metakaoline and fly ash, geopolymer liquor by NaOH, KOH and sodium silicate solution. As result of this experiment, what we could obtain best fitted geopolymer's properties such as initial setting time, flow and compressive strength of 3days aged, was 45min, $116\%$ and 43.6Mpa. This result can be applicable to commercial wood wool ceramic board.

  • PDF

Wood pelletizing using pine root waste biomass - different pelletizing properties between trunk and root biomass of Pinus densiflora (소나무 뿌리 폐기물을 이용한 목질 펠릿 제조 - 목부와 뿌리로 제조한 펠릿의 특성 비교)

  • Shin, Soo-Jeong;Han, Gyu-Seong;Myeong, Soo-Jeong;Cho, Jung-Sik;Yeon, Ik-Jun
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2008.10a
    • /
    • pp.71-73
    • /
    • 2008
  • Different biosolid fuel (wood pellet) properties between trunk and root of pine (Pinus densiflora) biomass were investigated. Trunk has more organic solvent extracts and Klason lignin content which has higher heating values than root biomass component. In root biomass, polysaccharides content was higher than trunk biomass. Based on Higher Heating Value (HHD) analysis and ash content, trunk biomass showed better solid fuel characteristics than root biomass. But pine root biomass had lower HHD than trunk biomass, its HHD values were higher than other hardwood or annual plant lignocellulosic biomass.

  • PDF

Porosity Development on Activation of Char from Dry and Wet Babbool Wood

  • Manocha, Satish;Chauhan, Vanraj B.;Manocha, L.M.
    • Carbon letters
    • /
    • v.3 no.3
    • /
    • pp.133-141
    • /
    • 2002
  • It is well known that the porosity and adsorption capacity in a carbon depends on the nature of precursor, pyrolysis and activation conditions and the ash content. The studies on carbon prepared from the dry and wet babbool wood were under taken to ascertain the effect of initial state of precursor on the development of porosity in the resulting activated carbon. The characterization and adsorption studies carried out shows the presence of mainly mesoporosity in the carbon prepared from dry wood while more of microporosity was observed in the activated carbon prepared from wet wood. The results on porosity in both the cases have been compared and correlated with their processing conditions.

  • PDF

Development of Carbonization Technology and Application of Unutilized Wood Wastes(I) -Carbonization and It's Properties of Thinned Trees- (미이용 목질폐잔재의 탄화 이용개발(I) -수종의 간벌재 탄화와 탄화물의 특성-)

  • Kim, Byung-Ro;Kong, Seog-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.2
    • /
    • pp.70-77
    • /
    • 1999
  • Objective of this research is to obtain fundamental data of carbonized wood wastes for soil condition, de-ordorization, absorption of water, carrier for microbial activity, and purifying agent for water quality of river. The carbonization technique and the properties of carbonized wood wastes(thinned trees) are analyzed. Proximate analysis shows the thinned wood contains 0.22-0.73% ash, 77-80% volatile matter, and 10-14% fixed carbon. The charcoal yield decreases and the shrinkage rate increases as the carbonization temperature and time increase. The charcoal yields of Larix leptolepis, Pinus rigida and Pinus densiflora are high, whereas those of Pinus koraiensis and Quercus variabilis are low. The shrinkage rate by carbonization has same trend as water removal of wood. The specific gravity after the carbonization decreases about 50% comparing to green wood. The charcoal has 0.89-4.08% ash, 6.31-13.79% volatile matter, and 73.9-83.5% fixed carbon. As the carbonization temperature and time increase, pH of charcoal increases. When the carbonization temperature is $400^{\circ}C$, pH is about 7.5. When the temperature is between 600 to $800^{\circ}C$, pH is about 10 with small difference. The water-retention capacity is not affected by the carbonization temperature and time. The water-retention capacity within 24hr is about 2.5 - 3times of sample weight, and the equivalent moisture content becomes 2-10% after 24 hr.

  • PDF