Ammoniacal Leaching for Recovery of Valuable Metals from Spent Lithium-ion Battery Materials (폐리튬이온전지로부터 유가금속을 회수하기 위한 암모니아 침출법)

  • Ku, Heesuk;Jung, Yeojin;Kang, Ga-hee;Kim, Songlee;Kim, Sookyung;Yang, Donghyo;Rhee, Kangin;Sohn, Jeongsoo;Kwon, Kyungjung
    • Resources Recycling
    • /
    • v.24 no.3
    • /
    • pp.44-50
    • /
    • 2015
  • Recycling technologies would be required in consideration of increasing demand in lithium ion batteries (LIBs). In this study, the leaching behavior of Ni, Co and Mn is investigated with ammoniacal medium for spent cathode active materials, which are separated from a commercial LIB pack in hybrid electric vehicles. The leaching behavior of each metal is analyzed in the presence of reducing agent and pH buffering agent. The existence of reducing agent is necessary to increase the leaching efficiency of Ni and Co. The leaching of Mn is insignificant even with the existence of reducing agent in contrast to Ni and Co. The most conspicuous difference between acid and ammoniacal leaching would be the selective leaching behavior between Ni/Co and Mn. The ammoniacal leaching can reduce the cost of basic reagent that makes the pH of leachate higher for the precipitation of leached metals in the acid leaching.

Leaching of Vanadium and Tungsten from Spent SCR Catalysts for De-NOx by Soda Roasting and Water Leaching Method (소다배소(焙燒) 및 수침출법(水浸出法)에 의한 탈질용(脫窒用) 폐(廢) SCR 촉매(觸媒)로부터 바나듐과 텅스텐 침출(浸出))

  • Kim, Hye-Rim;Lee, Jin-Young;Kim, Joon-Soo
    • Resources Recycling
    • /
    • v.21 no.6
    • /
    • pp.65-73
    • /
    • 2012
  • Selective catalytic reduction(SCR) catalysts are obtained from de-NOx system of thermoelectric power plant. A process was developed for valuable metals such as vanadium and tungsten recovery from spent SCR catalyst by using soda roasting followed by water leaching. Spent SCR catalyst having $V_2O_5$(1.23 mass %) and $WO_3$(7.73 mass %). For getting soluble metal forms of the targeted metals like vanadium and tungsten soda roasting process was implemented. In soda roasting process, sodium carbonate added 5 equivalent ratio at roasted temperature $850^{\circ}C$ with 120 min roasted time for $544{\mu}m$ particle size of spent SCR catalyst. After soda roasting process moved to water leaching for roasted spent catalyst. Before leaching process the roasted spent catalyst was grinded up to $-45{\mu}m$ size. The leaching time is 30 min at $40^{\circ}C$ temperature, 10 % pulp density. The final leaching efficiency obtained 46 % of vanadium and 92 % of tungsten from present process.