The study investigated the behavior of plain and fibered Ultra-High Performance Concrete (UHPC) beams under varying loading conditions using integrated analysis of the flexure and acoustic emission tests. The loading rate of testing is -0.25 -2 mm/min. It is observed that on increasing loading rate, flexural strength increases, and toughness decreases. The acoustic emission testing revealed that higher loading rates accelerate crack propagation. Fiber effect and matrix cracking are identified as significant contributors to the release of acoustic emission energy, with fiber rupture/failure and matrix cracking showing rate-dependent behavior. Crack classification analysis indicated that the rise angle (RA) value decreased under quasi-static loading. The average frequency (AF) value increased with the loading rate, but this trend reversed under rate-dependent conditions. K-means analysis identified distinct clusters of crack types with unique frequency and duration characteristics at different loading rates. Furthermore, the historic index and signal strength decreased with increasing loading rate after peak capacity, while the severity index increased in the post-peak zone, indicating more severe damage. The sudden rise in the historic index and cumulative signal strength indicates the possibility of several occurrences, such as the emergence of a significant crack, shifts in cracking modes, abrupt failure, or notable fiber debonding/pull-out. Moreover, there is a distinct rise in the number of AE knees corresponding to the increase in loading rate. The crack mapping from acoustic emission testing aligned with observed failure patterns, validating its use in structural health monitoring.
Arash K. Pour;Amir Shirkhani;Ehsan Noroozinejad Farsangi
Structural Engineering and Mechanics
/
v.91
no.2
/
pp.177-195
/
2024
This research plans to investigate the simultaneous impact of bamboo fibers (BF) and steel fibers (SF) on the mechanical and spalling characteristics of ultra-high-performance concrete (UHPC) exposed to high temperatures (HT). To this aim, 25 mixtures were made and assessed. BF was added at five contents of 0, 2.5, 5, 7.5 and 10 kg/m3. Additionally, SF was used at five weight contents: 0%, 1%, 2%, 3% and 4%. Specimens were exposed to temperatures ranging between 25℃ and 800℃. Thus, com-pressive, tensile, and flexural strengths, elastic moduli, mass loss, and permeability were measured. Experiments revealed that the simultaneous use of low BF and SF contents could totally prevent spalling of UHPC, but the use of either SF or BF alone could not prevent spalling at high levels of fibers. Besides, the synergetic positive impact of BF and SF on the spalling resistance of UHPC was by reason of the rise of BF' permeability and the bridging role of SF at HT. Moreover, it was concluded that the use of SF could moderate the adverse influence of BF on the compressive resistance of UHPC.
Seonhyeok Kim;Taegeon Kil;Sangmin Shin;Daeik Jang;H.N. Yoon;Jin-Ho Bae;Joonho Seo;Beomjoo Yang
Computers and Concrete
/
v.32
no.5
/
pp.487-498
/
2023
The present study investigated the flexural behavior of reinforced concrete (RC) beams strengthened with an ultrahigh performance concrete (UHPC) panel having various thicknesses. Two fabrication methods were introduced in this study; one was the direct casting of UHPC onto the bottom surface of the RC beams (I-series), and the other was the attachment of a prefabricated UHPC panel using an adhesive (E-series). UHPC panels having thicknesses of 10, 30, 50, and 70 mm were applied to RC beams, and these specimens were subjected to four-point loading to assess the effect of the UHPC thickness on the flexural strengthening of RC beams. The test results indicated that the peak strength and initial stiffness were vastly enhanced with an increase in the thickness of the UHPC panel, showing an improved energy dissipation capacity. In particular, the peak strength of the E-series specimens was higher than that of I-series specimens, showing high compatibility between the RC beam and the UHPC panel. The experimental test results were comparatively explored with a discussion of numerical analysis. Numerical analysis results showed that the predictions are in fair agreement with experimental results.
Journal of the Korea institute for structural maintenance and inspection
/
v.12
no.5
/
pp.81-90
/
2008
This paper concerns the flexural capacity of reinforced concrete beams with ultra-high performance cementitious composites(UHPCC). It was investigated if the existing equations to estimate the flexural capacity of reinforced fiberous concrete beams are applicable with the experiments including lightly reinforced concrete beams. The reinforcing effect when the steel fiber reinforced concrete was used in beams was also estimated. The results showed that the equation to predict the flexural capacity of reinforced steel fiber concrete by ACI 544 committee didn't have a good agreement with the test results and underestimated the flexural capacity in especially lightly reinforced beams with under 1.5% reinforcement ratio. the enhancement of flexural capacity was quite considerable in lightly reinforced beams when the steel fiber reinforced concrete was used. A equation to predict the reinforcing effect of steel fiber in reinforced steel fiber beams was developed. the equation was proposed as a function of both the characteristics of steel fiber and reinforcement ratio.
Proceedings of the Korea Concrete Institute Conference
/
2004.11a
/
pp.573-576
/
2004
High performance SFRC composed of mira-sized ultra fine particles is characterized by high strength, high ductility and excellent durability. therefore many researches about materials based on new composition like this are performed recently. many researchers have reported that adding steel fiber to concrete improved its tensile and flexural strength significantly. the main objective of this research is to examine the effect of adding steel fiber on the tensile strength of high performance SFRC. variables considered in this study are w/c ratio and fiber volume fraction.
Seo, Seung-Hoon;Kwon, Shi-Won;Oh, Sang-Keun;Kim, Byoung-Il
Proceedings of the Korean Institute of Building Construction Conference
/
2019.05a
/
pp.63-64
/
2019
Due to the rapid deterioration of the domestic atmosphere, people are suffering from inconveniences such as wearing fine dust masks all the time during outdoor activities. In this study, light transmitting concrete, LEFC(Light Emotion Friendly Concrete), using TiO2 photocatalyst was produced. Since the characteristics of LEFC where acrylic rods are inserted require self-consolidating performance, the purpose was to utilize UHPC(Ultra High Performance Concrete) materials to obtain high-flowability. Further, the compressive strength and flexural strength were evaluated to prevent the reduction of epidemiological performance by utilizing UHPC materials. As such, a basic study was carried out to develop LEFC materials using photocatalyst that can purify the air and stimulate human sensibility.
The analytical model was constituted to evaluate the flexural strength of UHPFRC(ultra high performance fiber reinforced concrete) member. The analytical approach was attemped to study the effect of the joint and the result compared with the experimental study to verify the analytical model. The calculated value tends to underestimate about 23%~25% in comparison with the experimental result of the jointed test member because the bond stress between precast UHPFRC and cast-in-place UHPFRC surface is not considered in the analytical model. But in the case of the continuous test member, the analytical model provides reasonable results for the flexural strength of UHPFRC member.
The paper presents the studies carried out on low velocity impact of Ultra high performance concrete (UHPC) panels of size $350{\times}350{\times}10mm^3$ and $350{\times}350{\times}15mm^3$. The panels are cast with 2 and 2.5% micro steel fibre and compared with UHPC without fiber. The panels are subjected to low velocity impact, by a drop-weight hemispherical impactor, at three different energy levels of 10, 15 and 20 J. The impact force obtained from the experiments are compared with numerically obtained results using finite element method, theoretically by energy balance approach and empirically by nonlinear multi-genetic programming. The predictions by these models are found to be in good coherence with the experimental results.
초고성능 콘크리트(Ultra High Performance Concrete, UHPC)는 종래의 보통 콘크리트와 다른 새로운 재료로써 높은 강도와 향상된 연성을 그 특징으로 한다. 이러한 새로운 재료의 활용을 위하여 본 연구는 초고성능 콘크리트의 부착 성능을 평가하고자 하였다. 수정된 RILEM 방법을 사용하여 초고성능 콘크리트와 이형철근의 pull-out 실험을 수행하였으며 보통 콘크리트와 비교하여 5~10배에 달하는 부착강도를 확인하였다. 또한 항복강도 400MPa급 철근에 대하여 철근 직경 2배 이상의 부착 길이에서 철근의 파단 강도에 해당하는 부착 성능을 나타내었으며 400MPa급 철근과 700MPa급 고장력 철근의 실험 결과 비교로부터 초고성능 콘크리트에서 고장력 철근 활용의 효율성을 확인하였다.
Proceedings of the Korean Institute of Building Construction Conference
/
2023.11a
/
pp.149-150
/
2023
This study proposes the most suitable strength prediction model equation for UHPC by calculating the apparent activation energy of UHPC according to the curing temperature and deriving the integrated temperature and compressive strength prediction equation. The results are summarized as follows. The apparent activation energy was calculated using the Arrhenius function, which was calculated as 21.09 KJ/mol. A model equation suitable for UHPC was calculated, and when the Flowman model equation was used, it was confirmed that it was suitable for the properties of UHPC using a condensation promoting super plasticizing agent.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.