• Title/Summary/Keyword: transition temperature

Search Result 2,885, Processing Time 0.036 seconds

Effects of the strain on the threshold current density in InGaAs/InGaAsP multiple quantum well lasers (InGaAs/InGaAsP 다중양자우물 레이저에서 변형이 문턱전류밀도에 미치는 효과)

  • 김동철;유건호;주흥로;김형문;김태환
    • Korean Journal of Optics and Photonics
    • /
    • v.9 no.2
    • /
    • pp.111-116
    • /
    • 1998
  • Thirteen InGaAs/InGaAsP separate-confinement heterostructure multiple quantum well lasers were designed such that the strain in the active layer from 0.9% compressive strain to 1.4% tensile, and their threshold current density was caluculated to see the effects of strain on the threshold current density. The well width was adjusted such that the bandgap of the quantum well is 1.55 ${\mu}{\textrm}{m}$, For the calculation of the band structure and transition matrix element needed for the gain calculation, a block diagonalized 8$\times$8 second-order $\to{k}.\to{p}$ Hamiltonian was used to incorporate the conduction band nonparabolicity and the valence band mixing. The threshold current density shows discontinuity at 0.4% tensile strain where the first heavy-hole subband and the first light-hole subband cross and at 0.5% tensile strain where the second conduction subband begins to exist. The threshold current density at room temperature has a maximum around these 0.4-0.5% tensile strains, and as strain varies in either direction it decreases first and then increases a little after a local minimum. This calculated trend is consistent with the other reported experimental results. We discussed the results of this calculation in comparison with other theoretical or experimental papers on the effect of strain.

  • PDF

Interfacial disruption effect on multilayer-films/GaN : Comparative study of Pd/Ni and Ni/Pd films

  • 김종호;강희재;김차연;전용석;서재명
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2000.02a
    • /
    • pp.113-113
    • /
    • 2000
  • 직접천이형 wide band gap(3.4eV) 반도체중의 하나인 GaN를 청색 및 자외선 laser diode, 고출력 전자장비 등으로 응용하기 위해서는 낮은 접합저항을 갖는 Ohmic contact이 선행되어야 한다. 그러나 만족할만한 p-type GaN의 Ohmic contact은 아직 실현되고 있지 못하며, 이는 GaN와 접합 금속과의 구체적인 반응의 연구를 필요로 한다. 본 연구에서 앞서 Pt, Pt, Ni등의 late transition metal을 p-GaN에 접합시킨 결과 이들은 접합 당시 비교적 평탄하나 후열 처리과정에서 비교적 낮은 온도에서 기판과 열팽창계수의 차이로 인하여 평탄성을 잃어버리면서 barrier height가 증가한다는 사실을 확인하였다. 따라서 본 연구에서는 이러한 열적 불안정성을 극복하기 위하여 Ni과 Pd를 차례로 증착하고 가열하면서 interfacial reaction, film morphology, Fermi level의 움직임을 monchromatic XPS(x-ray photoelectron spectroscopy) 와 SAM(scanning Auger microscopy) 그리고 ex-situ AFM을 이용하여 밝히고자 하였다. 특히 후열처리에 의한 계면 반응에 수반되는 구성 금속원소 간의 합금현상과 금속 층의 평탄성이 밀접한 관계가 있다는 것을 확인하였다. 이러한 합금과정에서 나타나는 금속원소들의 중심 준위의 이동을 체계적으로 규명하기 위해서 Pd1-xNix와 Pd1-xGax 합금들의 표준시료를 arc melting method로 만들어 농도에 따른 금속원소들의 중심 준위의 이동을 측정하여, Pd/Ni/p-GaN 및 Ni/Pd/p-GaN 계에서 열처리 온도에 따른 interfacial reaction을 확인하였다. 그 결과 두 계가 상온에서 nitride 및 alloy를 형성하지 않고 고르게 증착되고, 열처리 온도를 40$0^{\circ}C$에서 $650^{\circ}C$까지 증가시킴에 따라 계면반응의 부산물인 metallic Ga은 증가하고 있으마 nitride는 여전히 형성되지 않는 것을 확인하였다. 증착당시 Ni이 계면에 있는 Pd/Ni/p-GaN의 경우에는 52$0^{\circ}C$까지의 열처리에 의하여 Ni과 Pd가 골고루 섞이고 그 평탄성도 유지되고 barier height의 변화도 없었다. 더 높은 $650^{\circ}C$ 가열에 의해서는 surface free energy가 작은 Ga의 활발한 편석 현상으로 인해 표면은 Ga이 풍부한 Pd-Ga의 합금층으로 덮이고, 동시에 작은 pinhole들이 발생하며 barrier height도 0.3eV 가량 증가하게 된다. 반면에 증착당시 Pd이 계면에 있는 Ni/Pd/p-GaN의 경우에는 40$0^{\circ}C$의 가열까지는 두 금속이 그들 계면에서부터 섞이나, 52$0^{\circ}C$의 가열에 의해 이미 barrier height가 0.2eV 가량 증가하기 시작하였다. 더 높은 $650^{\circ}C$가열에 의해서는 커다란 pinhole, 0.5eV 가량의 barrier height 증가, Pd clustering이 동시에 관찰되었다. 따라서 Ni과 Pd의 일함수는 물론 thermal expansion coefficient가 거의 같으며 surface free energy도 거의 일치한다는 점을 감안하면, 이렇게 뚜렷한 열적 안정성의 차이는 GaN와 contact metal과의 반응시작 온도(disruption onset temperature)의 차이에 기인함을 알 수 있었다. 즉 계면에서의 반응에 의해 편석되는 Ga에 의해 박막의 strain이 이완되면, pinhole 등의 박막결함이 줄어 들고, 이는 계면의 N의 out-diffusion을 방지하여 p-type GaN의 barrier height 증가를 막게 된다.

  • PDF

Optical transition dynamics in ZnO/ZnMgO multiple quantum well structures with different well widths grown on ZnO substrates

  • Li, Song-Mei;Kwon, Bong-Joon;Kwack, Ho-Sang;Jin, Li-Hua;Cho, Yong-Hoon;Park, Young-Sin;Han, Myung-Soo;Park, Young-Sik
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.121-121
    • /
    • 2010
  • ZnO is a promising material for the application of high efficiency light emitting diodes with short wavelength region for its large bandgap energy of 3.37 eV which is similar to GaN (3.39 eV) at room temperature. The large exciton binding energy of 60 meV in ZnO provide provides higher efficiency of emission for optoelectronic device applications. Several ZnO/ZnMgO multiple quantum well (MQW) structures have been grown on various substrates such as sapphire, GaN, Si, and so on. However, the achievement of high quality ZnO/ZnMgO MQW structures has been somehow limited by the use of lattice-mismatched substrates. Therefore, we propose the optical properties of ZnO/ZnMgO multiple quantum well (MQW) structures with different well widths grown on lattice-matched ZnO substrates by molecular beam epitaxy. Photoluminescence (PL) spectra show MQW emissions at 3.387 and 3.369 eV for the ZnO/ZnMgO MQW samples with well widths of 2 and 5 nm, respectively, due to the quantum confinement effect. Time-resolved PL results show an efficient photo-generated carrier transfer from the barrier to the MQWs, which leads to an increased intensity ratio of the well to barrier emissions for the ZnO/ZnMgO MQW sample with the wider width. From the power-dependent PL spectra, we observed no PL peak shift of MQW emission in both samples, indicating a negligible built-in electric field effect in the ZnO/$Zn_{0.9}Mg_{0.1}O$ MQWs grown on lattice-matched ZnO substrates.

  • PDF

A Study on Physicochemical Properties of Epoxy Coatings for Liner Plate in Nuclear Power Plant (원자력발전소 격납건물 철재면 에폭시 도장시편의 물리화학적 특성 평가)

  • Lee, Jae-Rock;Seo, Min-Kang;Lee, Sang-Kook;Lee, Chul-Woo;Park, Soo-Jin
    • Applied Chemistry for Engineering
    • /
    • v.16 no.6
    • /
    • pp.809-814
    • /
    • 2005
  • In this work, the thermal properties of epoxy coating system on the liner plate in the containment structure of nuclear power plants had been examined by irradiation and design basis accident (DBA) conditions. The effect of immersion in hot water on adhesion strength of the coating system had been also studied. The glass transition temperature ($T_g$) and thermal stability of ET-5290/carbon steel A 32 epoxy coating systems were measured by DSC and TGA analyses, respectively. Contact angle measurements were used to determine the effect of immersion on the surface energetics of epoxy coating system, with a viewpoint of surface free energy. Adhesion tests were also executed to evaluate the adhesion strength at interfaces between carbon steel plate and epoxy resins. As a result, it was found that the irradiation led to an improvement of internal crosslinked structure in cured epoxy systems, resulting in significantly increasing the thermal stability, as well as the $T_g$. Also, the immersion in hot water made a role in the post-curing of epoxy resins and increased the mechanical interlocking of the network system, resulting in increasing the adhesion strength of the epoxy coating system.

Synthesis and Properties of Nonlinear Optical Polymer Derived from α-Methyl Styrene/Maleic Anhydride by Polymer Reaction (고분자 반응을 이용한 Maleic anhydride계 비선형 광학 고분자의 합성 및 전기광학 특성)

  • Park, Lee Soon;Keum, Chang Dae;Song, Jae Won;Kim, Kwang Taek;Kim, Gi Heon;Kang, Shin Won
    • Applied Chemistry for Engineering
    • /
    • v.9 no.5
    • /
    • pp.704-709
    • /
    • 1998
  • Non-linear optical polymer based on poly (${\alpha}$-methylstyrene-co-maleic anhydride) (MSMA) substrate polymer was prepared by polymer reaction method and its thermal and electro-optic properties were examined. In the polymer reaction between MSMA substrate polymer and 2-[4-(4-nitrophenylazo)-N-ethylphenylamino]ethanol (DR1) chromophore, the degree of substitution of DR1 into MSMA was higher with the 4-dimethylaminopyridine (DMAP) as catalyst and 3-dicyclohexyl carbodiimide (DCC) as dehydrating agent (sample, MSMA-DC) than the one with just 4-dimethylaminopyridine as catalyst (sample, MSMA-D). The synthesized NLO polymer (MSMA-DC) exhibited electro-optic coefficient of 18 pm/V (632.8 nm) and glass transition temperature ($T_g$) of about $175^{\circ}C$.

  • PDF

Effect of High Pressure Freezing and Thawing Process on the Physical Properties of Pork (초고압 동결 및 해동방법이 돈육의 물리적 특성에 미치는 효과)

  • Shim, Kook-Bo;Hong, Geun-Pyo;Choi, Mi-Jung;Min, Sang-Gi
    • Food Science of Animal Resources
    • /
    • v.29 no.6
    • /
    • pp.736-742
    • /
    • 2009
  • This study was conducted to investigate the effect of various high pressure freezing and thawing treatments on the physical properties of pork. To compare the effects of the freezing and thawing process on meat quality, atmospheric freezing followed by running water thawing (AFRT), pressure shift freezing followed by running water thawing (SFRT), and pressure shift freezing and pressure assisted thawing (SFAT) were conducted at pressure of 250 MPa and cooling temperature of $-22^{\circ}C$. SAFT and SFRT showed a shorter phase transition time and total thawing time than AFRT. The pH value of treated samples increased significantly (p<0.05) compared to unfrozen meat. In addition, SFAT and SFRT showed a higher pHvalue than AFRT. Although the water holding capacity was significantly decreased (p<0.05) for SFAT and SFRT, SFRT reduced drip loss. In regards to color, SFAT and SFRT resulted in a significant increase in color parameters (p<0.05) relative to AFRT, while SFAT produced a higher L*-value. High pressure treatment significantly increased shear force (p<0.05) compared to AFRT, and, where SFRT showed the highest shear force. Therefore, these combined results indicated that the hydrostatic pressure treatment improved the functional properties of pork and increased the freezing and thawing rate.

Effects of Freezing-Thawing Conditions on Physicochemicnl and Histological Properties of Plaice, Paralichthys olivaceus Muscle (동결-해동 조건이 넙치육의 물리$\cdot$화학적 및 조직학적 변화에 미치는 영향)

  • CHO Young-Je;CHO Min-Sung;LEE Nam-Gul;CHOI Young-Jun;KIM Tae-Jin
    • Korean Journal of Fisheries and Aquatic Sciences
    • /
    • v.31 no.4
    • /
    • pp.463-470
    • /
    • 1998
  • To improve muscle quality and prolong freshness of sashimi, the effects of freezing-thawing condition on physicochemical and rheological properties of plaice muscle were investigated. Muscle tested were frozen with quick freezing (liquid nitrogen gas) or slow freezing ($-15^{\circ}C$ air). Transition time of zone of ice crystal formation was within 10 minute for quick freezing and 110 minute for slow freezing. Time required for thawing to $0^{\circ}C$ in muscle temperature by various thawing methods was shortest with $25^{\circ}C$ tap water, followed by $15^{\circ}C$ tap water, $10^{\circ}C$ tap water, $25^{\circ}C$ air, $5^{\circ}C$ tap water and $0^{\circ}C$ cold water. Breaking strength of muscle was higher in quickly frozen sample than in slowly frozen sample. According to sashimi term, changes in breaking strength of muscle did not show any difference in quickly frozen sample, while showed significant difference in slowly frozen sample. The remaining content of ATP was not effected by freezing speed, and ATP content was apt to higher in quickly thawed sample than in slowly thawed sample. IMP was the majority of ATP and it's related compounds of sample after freezing and thawing. Collagen matrix was weakened markedly in slowly frozen sample than in quickly frozen sample.

  • PDF

Radiological Safety Assessment for KAERI Incineration Plant on the Basis of Trial Burn Results (시험소각결과에 기준한 한국원자력연구소 소각시설의 방사학적 안전성 평가)

  • Yang, Hee-Chul;Kim, Bong-Hwan;Kim, Chang-Hee;Park, Won-Man;Jeong, Myung-Soo
    • Journal of Radiation Protection and Research
    • /
    • v.23 no.2
    • /
    • pp.109-114
    • /
    • 1998
  • Radiological safety for the conventional operation of Demonstration-Scale Incineration Plant (DSIP) was assessed on the basis of the results of trial burns using the simulated and real radioactive wastes. Radiation dose assessments for routine releases on an annual basis as well a several severe accidental releases on a short-term basis (2h) revealed that there would be no significant environmental impact when low-level waste Is incinerated in DSIP. For semivolatile radioactive cesium species, expected emission concentrations slightly exceeded 10% of maximum permissible concentration. Removal characteristics of the bag filter for condensed-phase cesium species was investigated by the trial burns of simulated waste with inactive cesium tracer. In the off-gas before passing through bag filter, distributions of condensed cesium species in the transition size ranging between the diffusional and inertial region are less than 5%. The overall collection efficiency of the bag filter for cesium species was higher than 99.9%, showing enough decontamination capability as a primary filter for the low-temperature dry off-gas system in radwaste incineration plant.

  • PDF

On the Properties of TLCP/PBT Blends Prepared by In Situ Polymerization in PBT Solution (In situ 중합에 의해서 제조된 TLCP/PBT 블렌드의 특성 연구)

  • Choi, Jae-Kon;Park, Il-Soo;Kim, Sun;Choi, Yoo-Sung;Lee, Eung-Jae;Jo, Byung-Wook
    • Elastomers and Composites
    • /
    • v.39 no.3
    • /
    • pp.217-227
    • /
    • 2004
  • A new thermotropic liquid crystalline polymer(TLCP) containing a triad aromatic ester type mesogenic unit and butylene terephthalate unit(BT) in the main chain was synthesized by polycondensation reaction. The TLCP synthesized showed nematic mesophasic behavior and its transition temperature from solid to mesophase was $260^{\circ}C$. The TLCP/PBT blends were prepared by in-situ polymerization in PBT solution and characterized by differential scanning calorimeter(DSC), thermogavimetric analyzer(TGA), scanning electron microscope(SEM), x-ray diffractometer(XRD), and dynamic mechanical thermal analyze, (DMTA). The blends showed well dispersed TLCP phases with domain sizes $0.05{\sim}0.2{\mu}m$ in the PBT matrix. As the increasing TLCP content from 5 to 20 wt%, ${\Delta}Hm$ values of pure PBT in the blend were increased because TLCP acts as a nucleating agent in the PBT matrix. The mechanical properties of the blends depended on the TLCP contents because the TLCP acted effectively as a reinforcing material in the PBT matrix. The blends showed good interfacial adhesion between the TLCP phase and PBT matrix.The blends prepared by in-situ polymerization showed higher mechanical properties and well dispersed TLCP domains than those of the blends prepared by melt blending.

Linewidth Reduction of a Yellow Laser by a Super-cavity and the Measurement of the Cavity Finesse (초공진기를 이용한 노란색 레이저의 선폭 축소 및 초공진기의 예리도 측정)

  • Lee, Won-Kyu;Park, Chang-Yong;Park, Sang-Eon;Ryu, Han-Young;Yu, Dai-Hyuk;Mun, Jong-Chul;Suh, Ho-Suhng
    • Korean Journal of Optics and Photonics
    • /
    • v.21 no.3
    • /
    • pp.123-128
    • /
    • 2010
  • Sum frequency generation was utilized to obtain a yellow laser with the wavelength of 578.4 nm for a probe laser of an Yb lattice clock. The output of an Nd:YAG laser with wavelength of 1319 nm and that of an Yb-fiber laser with wavelength of 1030 nm were passed through a waveguided periodically-poled lithium niobate (WG-PPLN) for sum frequency generation. It is required that the probe laser has a linewidth of the order of 1 Hz to fully resolve the Yb lattice clock transition. Thus, the linewidth of the probe laser was reduced by stabilizing the frequency to a super-cavity. This was made of ULE with a low thermal expansion coefficient, and was mounted on an active vibration-isolation table at the optimal point for the reduced sensitivity to vibration. Also, this was installed in a vacuum chamber, and the temperature was stabilized to 1 mK level. This system was installed in an acoustic enclosure to block acoustic noise. The finesse of the super-cavity was measured to be 380 000 from the photon life time of the cavity.