• Title/Summary/Keyword: titanium coating

Search Result 348, Processing Time 0.032 seconds

HISTOLOGICAL COMPARISONS OF TITANIUM PLASMA SPRAYED IMPLANT AND HYDROXYAPATITE COATED IMPLANT TO BONE INTERFACE IN PERIODONTALLY INVOLVED EXTRACTION SOCKETS IN DOGS (성견 치주질환 이환 발치와에 즉시 임플란트 매식술시 Titanium plasma sprayed 임프란트와 Hydroxyapatite coated 임프란트의 계면조직에 관한 연구)

  • Kim, Jin-Sook;Kim, Chong-Kwan
    • Journal of Periodontal and Implant Science
    • /
    • v.23 no.3
    • /
    • pp.400-410
    • /
    • 1993
  • Dental implants have been widely used in the treatment of esthetic and functional problems of the mouth due to alveolar bone loss, after tooth extraction. The success of implantation strongly depends on osseointegration. For osseointegration, implant material, methodology, and design have been investigated. For materials, two popular materials at present are titanium and hydroxyapatite. For methods, immediate implantation is being used recently. The purpose of this study is to evaluate osseointegration between the unthreaded cylindrical TPS implant and the HA-coated implant by a histomorphometric analysis. For this analysis, experimental periodontits was induced on the 3, 4 premolars of adult dogs by the ligation of orthodontic threads. Thereafter, each tooth was extracted. TPS. Implants and HA-coated implants were immediately inserted in the extraction socket. In control group, TPS implants were immediately inserted, and In experimental group, HA implants were immediately inserted. The dogs were sacrificed after 12 weeks, then the specimens were prepared for LM and histomorphometric analysis. The conclusion of this study is as follows l. In both control and experimental group, no inflammatory cells were observed. 2. The results of the histomorphometric analysis showed that the total osseointegration was 48.5% in control group, and 68.8% in expermental group. The experimental group was higher than the control group, and the difference was not statistically significant (p<0.05). 3. The results of the histomorphometric analysis showed that the osseointegration in the hole was 40.6% in control group, and 70.2% in experimental group. The experimental group was higher than the control group, and the difference was statistically significant (p<0.05). In both control and experinental group, no inflammatory cells were observed. 4. The results of the histomorphometric analysis showed that the osseointegration in the lower part was 52.1% in control group, and 73.3% in experimental group. The experimental group was higher than the control group, and the difference was statistically significant (p<0.05). 5. In experimental group, the bone to HA interface seemed to be mixed of bone and HA. We could not distinguish HA from the bone. The HA coating was detached from the titanium surface.

  • PDF

Surface Coating and Corrosion Characteristics of Bipolar Plates of PEMFC Application (PEMFC용 분리판 표면코팅 및 부식성 평가)

  • Kang, Kyung-Min;Kim, Dong-Mook;Choi, Jeong-Sik;Cha, In-Soo;Yun, Young-Hoon
    • Journal of Hydrogen and New Energy
    • /
    • v.22 no.2
    • /
    • pp.199-205
    • /
    • 2011
  • Stainless steel 304 and 316 plates were deposited with the multi-layered coatings of titanium film (0.1 um) and gold film (1-2 um) by an electron beam evaporation method. The XRD patterns of the stainless steel plates modified with the multi-layered coatings showed the crystalline phases of the external gold film and the stainless steel substrate. Surface microstructural morphologies of the stainless steel bipolar plates modified with multi-layered coatings were observed by AFM and FE-SEM images. The external gold films formed on the stainless steel plates showed micro structure of grains of about 100 nm diameter. The grain size of the external surface of the stainless steel plates increased with the gold film thickness. The electrical resistance and water contact angle of the stainless steel bipolar plates covered with multi-layered coatings were examined with the thickness of the external gold film.

Study on the Preparation and Characteristics of $(Pb_{1-x}Sr_x)TiO_3$ Thin Films by the Sol-gel Process (졸-겔법을 이용한 $(Pb_{1-x}Sr_x)TiO_3$ 박막의 제조 및 특성에 관한 연구)

  • 선계혁;윤희한;황규석;김병훈
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.11
    • /
    • pp.1195-1202
    • /
    • 1996
  • To prepare the dielectric thin films of (Pb1-xSrx)TiO3 (x=0.1, 0.2, 0.3, 0.35, 0.5) by the sol-gel process titanium (IV) isopropoxide (Ti[OCH(CH3)2]4) and Pb Sr, acetate were used therefore the thin films were fabricated by dip-coating method. Stability of the sol decreased with addition of Sr content thin films could be fabricated up to 35mol% Over this range precipitation of sol occured thin films couldn't be obtained. Transmittance of thin films at visible range decreased with the increase of heat-treatment temperature but exhibited transmit-tance above 60% in all case. Moreover transmittance of thin films at visible range slightly increased with of addition of Sr,. When thin film containing 30 mol% srontium was heated at 600℃ the best perovskite phase was obtained. The dielectric constant (ε) was 280 and dielectric loss factor (tan δ) was 0.021 and curie tempera-ture (Tc) decreased with the increase of addition of Sr.

  • PDF

Evaluation of Elastic Properties for Nanoscale Coating Layers Using Ultrasonic Atomic Force Microscopy (초음파원자현미경을 이용한 나노스케일 박막 코팅층에 대한 탄성특성 평가)

  • Kwak, Dong Ryul;Cho, Seung Bum;Park, Ik Keun
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.24 no.5
    • /
    • pp.475-480
    • /
    • 2015
  • Ultrasonic atomic force microscopy (Ultrasonic-AFM) has been used to investigate the elastic property of the ultra-thin coating layer in a thin-film system. The modified Hertzian theory was applied to predict the contact resonance frequency through accurate theoretical analysis of the dynamic characteristics of the cantilever. We coat 200 nm thick Aluminum and Titanium thin films on the substrate using the DC Magnetron sputtering method. The amplitude and phase of the contact resonance frequency of a vibrating cantilever varies in response to the local stiffness constant. Ultrasonic-AFM images were obtained using the variations in the elastic property of the materials. The morphology of the surface was clearly observed in the Ultrasonic-AFM images, but was barely visible in the topography. This research demonstrates that Ultrasonic-AFM is a promising technique for visualizing the distribution of local stiffness in the nano-scale thin coatings.

Effect of $Li_4Ti_5O_{12}$ coating layer on capacity retention of $LiMn_2O_4$ as cathode materials of lithium ion secondary batteries for HEV application (HEV용 리튬 이차전지 양극물질 $LiMn_2O_4$$Li_4Ti_5O_{12}$ 코팅에 따른 영향)

  • Wai, Yin-Loo;Choi, Byung-Hyun;Jee, Mi-Jung;Lee, Dae-Jin;Shin, Jae-Su;Song, Kwang-Ho
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2007.11a
    • /
    • pp.125-128
    • /
    • 2007
  • In these recent years, low cost and stable battery electrode materials have been studied for HV/HEV application. Spinel cathode material $LiMn_2O_4$ is widely studied as a promising cathode material of lithium ion secondary batteries because of it is low cost, easily to be prepared and capable to be operated in high voltage range. In this study, $LiMn_2O_4$ was undergoing surface modification with spinel lithium titanium oxide by sol-gel method in order to enhance its capacity retention. Properties of both unmodified and surface-modified $LiMn_2O_4$ were characterized by XRD, SEM, particle size analyzer while their cycling performance was tested with charge and discharge tester.

  • PDF

Evaluation Method for Improvement of Indoor Air Quality Using Mass Balance (물질수지를 이용한 실내공기질 개선정도 평가)

  • Kim, Young-Hee;Kim, Moon-Hyeon;Yang, Won-Ho
    • Journal of Environmental Science International
    • /
    • v.15 no.10
    • /
    • pp.913-918
    • /
    • 2006
  • Despite the wide distribution of air pollutants, the concentrations of indoor air pollutants may be the dominant risk factor in personal exposure due to the fact that most people spend an average of 80% of their time in enclosed buildings. Researches for improvement of indoor air quality have been developed such as installation of air cleaning device, ventilation system, titanium dioxide$(TiO_2)$ coating and so on. However, it is difficult to evaluate the magnitude of improvement of indoor air quality in field study because indoor air quality can be affected by source generation, outdoor air level, ventilation, decay by reaction, temperature, humidity, mixing condition and so on. In this study, evaluation of reduction of formaldehyde and nitrogen dioxide emission rate in indoor environments by $TiO_2$ coating material was carried out using mass balance model in indoor environment. we proposed the evaluation method of magnitude of improvement in indoor air quality, considering outdoor level and ventilation. Since simple indoor concentration measurements could not properly evaluate the indoor air quality, outdoor level and ventilation should be considered when evaluate the indoor net quality.

Bone Ingrowth and Enhancement of Bone Bonding Strength at Interface between Bone and HA Coated Stainless Steel (HA 코팅된 스테인레스강과 뼈의 계면에서의 경조직 성장 및 결합력 향상)

  • Kim, C.S.;Kim, S.Y.;Kim, D.H.;Khang, G.
    • Proceedings of the KOSOMBE Conference
    • /
    • v.1996 no.05
    • /
    • pp.133-136
    • /
    • 1996
  • We investigated how hydroxyapatite (HA) coating onto a porous super stainless steel (S.S.S, 22Cr-20Ni-6Mo-0.25N) affects bone ingrowth in a dog transcortical femoral model. Implants were histologically evaluated after 4 and 48 weeks of implantation, and the bone bonding strength at the bone/implant interface was examined by employing the pull-out test. The direct osseous tissue bonding onto the HA-coated S.S.S was observed, but the uncoated stainless steels had thin fibrous tissue layers. The mean interface strength of the HA-coated S.S.S was 1.5 and 2.5 times greater than those of the S.S.S and the 316L SS after one year of implantation, respectively. In preliminary studies, no toxic responce was observed from a cytotoxicity test of the S.S.S, having similar corrosion resistance to titanium. Our results suggest that early osteoconductive nature of HA coating may induce long term osteointegration for a bioinert substrate.

  • PDF

INFLUENCE OF TUNGSTEN CARBIDE/CARBON COATING ON THE PRELOAD OF IMPLANT ABUTMENT SCREWS (임플랜트 지대주 나사의 텅스텐 카바이드/탄소 코팅이 전하중에 미치는 영향에 관한 연구)

  • Choi Jin-Uk;Jeong Chang-Mo;Jeon Young-Chan;Lim Jang-Seop;Jeong Hee-Chan;Eom Tae-Gwan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.44 no.2
    • /
    • pp.229-242
    • /
    • 2006
  • Statement of problem: In order to increase preload with reducing the friction coefficient, abutment screws coated with pure gold and Teflon as dry lubricant coatings have been introduced. But the reported data indicate that if screw repeated tightening and loosening cycle, an efficiency of increasing preload was decreased by screw surface wearing off. Purpose: This study was to evaluate the influence of tungsten carbide/carbon coating, which has superior hardness and frictional wear resistance, on the preload of abutment screws and the stability of coating surface after repeated closures. Material and method: The rotational values of abutment screws and the compressive forces between abutment and fixture were measured in implant systems with three different joint connections, one external butt joint and two internal cones. Moreover the stability and the alteration of coating surface were examined by comparison of the compressive force and the removable torque values during 10 consecutive trials, observation with scanning electron microscope and analyzed the elemental composition with energy dispersive x-ray spectroscopy Results and conclusion: 1. Application of coating resulted in significant increase of compressive force in all implant systems(P<.05). The increasing rate of compressive force by coating in external butt joint was gloater than those in internal cones (P<.05). 2. Coated screw showed the significant additional rotation compared to non-coated screw in all implant systems (P<.05). There were no significant differences in the increasing rate of rotation among implant systems (P>.05). 3. Removable torque values were greater with non-coated screw than that with coated screw (P<.05). 4. Coated screw showed insignificant variations in the compressive forces during 10 consecutive trials(P>.05) 5. After repeated trials, the surface layer of coated screw was maintained relatively well. However surface wearing and irregular titanium fragments were found in non-coated screw.

패턴 된 기판 위에 형성된 메조포러스 $TiO_2$막 형성 기구 및 미세구조 연구

  • An, Heung-Bae;Nam, U-Hyeon;Lee, Jeong-Yong;Kim, Yeong-Heon
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.469-469
    • /
    • 2011
  • 고효율 염료감응형 태양전지(DSSC, Dye-Sensitized Solar Cell)의 구현을 위해서 유용한 방법중 하나는 정렬된 기공 (pore)을 $TiO_2$막 내에 형성시키는 것이다. 메조포러스 (mesoporous) $TiO_2$막은 dip coating이나 spin coating과 같은 방법으로 주로 증착되고 있으며, P123이나 F127과 같은 amphiphilic triblock copolymer를 메조포러스 구조를 만들기 위한 뼈대로 사용하고 있다. 또한, 이렇게 생성된 구조에서 amphiphilic triblock copolymer는 열처리 공정을 통하여 쉽게 제거될 수 있다. 고효율 태양전지를 구현하는 또 다른 방법으로는 패턴 된 기판을 사용하는 것이다. 패턴 된 기판은 빛의 반사를 억제하여 흡수율을 높이는 역할을 한다. 그러나 패턴 된 기판 위에서 메조포러스 $TiO_2$막의 형성에 관한 연구는 부족한 실정이다. 본 연구에서는 spin coating 방법으로 패턴 된 Si (111) 기판 위에 메조포러스 $TiO_2$를 성장하고 그 미세구조를 분석하였다. 패턴 된 기판은 nanosphere lithography(NSL) 법으로 mask를 증착한 후 건식 식각 (dry etching) 공정을 통해서 제작되었으며, 마스크와 불순물 등 은 초음파 세척 등으로 제거되었다. 메조포러스 $TiO_2$막은 1-propanol, P123, titanium isopropoxide와 HCl을 섞어 만든 용액으로 1 cm${\times}$1 cm 기판 위에 3000 rpm과 4000 rpm으로 각각 증착하였으며, 5일 동안 4도에서 에이징한 후 350도에서 3시간 열처리하였다. 이렇게 형성한 메조포러스 막의 형상과 미세구조적 특성이 주사전자현미경(SEM, scanning electron microscope), X-선 회절(XRD, X-ray diffraction) 등을 이용하여 연구되었다. 특히, 증착 조건에 따른 메조포러스 $TiO_2$박막의 형성 기구에 관한 고찰이 진행되었다. 나아가, $TiO_2$박막과 패턴 사이에 형성되는 계면 구조에 관한 연구를 투과전자현미경을 이용하여 진행하였다.

  • PDF

Effect of Intermediate Layer Coated Diamond Particles on Performance of Diamond Tool (다이아몬드 입자에 형성된 중간층이 다이아몬드 공구 성능에 미치는 영향)

  • Son, Kyung-Sik;Lee, Jung-Hoon;Choi, Yong-Je;Jung, Uoo-Chang;Chung, Won-Sub
    • Journal of Surface Science and Engineering
    • /
    • v.46 no.5
    • /
    • pp.216-222
    • /
    • 2013
  • In order to improve the performance of electrodeposited diamond-nickel composite, surface modification of diamond particles was carried out using powder immersion reaction assisted coating (PIRAC). Titanium and chromium were selected as coating elements, which are known as carbide former. With respect to the powder elements, various phases were formed on diamond; metallic Ti and TiC for Ti powder, $Cr_3C_2$ for Cr powder, and TiC and $Cr_3C_2$ for Ti-Cr mixed powder. Surface modified diamond particle showed higher specific surface area, especially Ti coating induced considerable increase of specific surface area. The increase of specific surface area suggests increase of surface roughness, and that was confirmed by surface observation using FE-SEM. In addition, wear properties of diamond-nickel composite including surface modified diamonds were improved, and Ti coated diamond showed the highest performance. The wear property of diamond-nickel composite is dependent on adhesion strength between diamond particle and nickel layer. Therefore, surface modification of diamond particle by PIRAC increasing surface roughness is effective to improve the properties of diamond-nickel composite.