• 제목/요약/키워드: tensile bond

검색결과 554건 처리시간 0.031초

애크릴릭 및 실리콘 계열 연성 의치상 이장재의 결합력에 관한 연구 (A Study for Bond Strengths of Acrylic and Silicone Based Soft Lining Materials)

  • 남은주;임주환
    • 구강회복응용과학지
    • /
    • 제16권1호
    • /
    • pp.27-36
    • /
    • 2000
  • One of the methods to improve the softness and comfortness of denture base is the use of soft denture liners. In this study, specimens were made by 2 kinds of acrylic based soft lining materials and 2 kinds of silicone based soft lining materials, and bonded to acrylic resin(Lucitone $199^{(R)}$). Then they were tested the differences of tensile bond strengths according to the materials, thickness, surface treatment and failure mode. 1. Tensile bond strength according to soft lining materials was increased in order of Coe-$soft^{(R)}$, $Mollosil^{(R)}$, $Trusoft^{(R)}$, Ufi-Gel $C^{(R)}$. The differences between groups were statistically significant at level of 0.05. 2. Tensile bond strength according to thickness of soft lining materials was increased in order of 3mm, 2mm, 1mm. The differences between groups were not statistically significant. 3. Tensile bond strength of treated surface showed higher bond strength than nontreated surface. The difference between groups was not statistically significant. 4. The failure mode of Coe-$soft^{(R)}$, $Trusoft^{(R)}$, $Mollosil^{(R)}$ were mainly cohesive failure, and that of Ufi-Gel $C^{(R)}$ were mainly adhesive failure.

  • PDF

교면용 양면 시트방수재 상부 포장층 재료에 따른 부착방법 변경시 인장접착강도 확인 (Tensile Bond Strength Westing When Changing Adhesion Method of Double-sided Waterproof Sheet Used on Surface Layer of Bridge-deck)

  • 안기원;김천학;오상근
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2019년도 춘계 학술논문 발표대회
    • /
    • pp.217-218
    • /
    • 2019
  • In this study, to overcome the limitation of material application as the surface layer of bridge decks (asphalt concrete, concrete), a newly developed waterproof sheet is proposed to be usable for both asphalt concrete and concrete. Subsequent tensile bond strength was tested, and the test results showed that the tensile bond strengths were similar to depending on the type of the surface layer material for bridge decks, confirming the applicability of the proposed material.

  • PDF

산처리(酸處理)된 Enamel표면(表面)에 대(對)한 Composite resin의 인장접착강도(引張接着强度)에 관(關)한 연구(硏究) (STUDY OF THE TENSILE BOND STRENGTH OF COMPOSITES RESINS APPLIED TO ACID-ECHED ENAMEL)

  • 이영근;민병순;최호영;박상진
    • Restorative Dentistry and Endodontics
    • /
    • 제12권2호
    • /
    • pp.45-53
    • /
    • 1987
  • The purpose of this study was to evaluate the tensile bond strength between composite resin and the human enamel. Three composite resin systems, two chemical (Clearfil Posterior, and Clearfil Posterior-3) and one light cure (Photo Clearfil-A), used with and without an intermediate resin (clearfil bonding agent), were evaluated under different amounts of load (10g, 200g and 200g for a moment) for in vitro tensile bond strength to acid-eched human enamel. Clinically intact buccal or lingual surfaces of 144 freshly extracted human permanent molars, embedded in acrylic were flattened with No #600 carborundum discs. Samples were randomly assigned to the different materials and treatments using a table of random numbers. Eight samples were thus prepared for each group(Table 2) these surfaces were etched with an acid etchant (Kurarey Co. Japan) in a mode of etching for 30 seconds, washing for 15 seconds, and drying for 30-seconds. During the polymerization of composite resin on the acid-etched enamel surfaces with and without bonding agent 10-gram, 200 gram and temporary 200 gram of load were applied. The specimens were stored in 50% relation humidity at $37^{\circ}C$ for 24 hours before testing. An universal Testing machine (Intesco model No. 2010, Tokyo, Japan) was used to apply tensile loads in the vertical directed (fig 5), and the force required for separation was recorded with a cross head speed of 0.25 mm/min and 20 kg in full scale. The results were as follow: 1. The tensile bond strength was much greater in applying a bonding agent than in not doing that. 2. The tensile bond strength of chemical cure composite resin was higher than that of light cure composite resin with applying on bonding agent on the acid-etched enamel. 3. In case of not applying a bonding agents on the acid-etching enamel, the highest tensile bond strength under 200 gram of load was measured in light cure composite resin. 4. The tensile bond strength under 200-gram of load has no relation with applying the bonding agent. 5. Under the load of 10-gram, There was significant difference in tensile bond strength as applying the bonding agent.

  • PDF

FRP 복합체의 콘크리트에 대한 접착강도 시험방법 변수 연구 (Parametric Study on Test Method for Pull-off Strength of FRP Composite Material used in Strengthening RC Members)

  • 최기선;유영찬;이한승;김긍환
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 춘계학술발표회 논문집(I)
    • /
    • pp.222-225
    • /
    • 2006
  • Pull-off test is widely used to evaluate bond performance between concrete and FRP composite. However, reliability of experiment result declines due to many difference between test methods of each national standards. This study analyzed problems of various existing test methods for pull-off test and suggested standardized test method. In addition, since tensile strength of concrete is smaller than bond strength of epoxy resin, maximum bond strength of epoxy resin shall be limited within tensile strength of concrete. Alternative testing method, therefore, which decrease FRP adhesion areas than concrete adhesion areas is suggested to widen test range of bond strength in pull-off test. In the experimental results, bond performance can be estimated up to two times of tensile strength of concrete by reducing FRP adhesion areas by 1/3.

  • PDF

수중코팅제와 콘크리트 모재 간의 인장 부착 특성 (Tensile Bond Characteristics between Underwater Coating Materials and Concrete Substrate)

  • 김민욱;정연웅;강성훈;문주혁;이진학
    • 한국해안·해양공학회논문집
    • /
    • 제30권6호
    • /
    • pp.298-305
    • /
    • 2018
  • 본 연구에서는 해양 항만 콘크리트 구조물의 보수작업을 위한 수중코팅제의 부착 특성을 조사하기 위하여 실험적 연구를 수행하였다. 고려된 실험변수는 코팅제의 종류, 코팅대상 모재의 표면 거칠기, 도포 작업환경(육상 혹은 수중)으로 부착 강도는 Pull-off 방식으로 측정하였다. 코팅제의 부착 강도는 각 수중코팅제의 도포 작업 완료 24시간 후에 ASTM C1583 규정에 따라 측정하였다. 또한, 콘크리트 모재와 코팅제 간의 부착파괴 거동(코팅제, 계면, 콘크리트 모재)을 육안으로 관찰하였으며 측정된 부착 강도 수치에 근거하여 각 실험요인의 비교분석을 수행하였다. 실험결과, 수중에서 도포한 코팅제의 부착 강도가 육상의 경우에 비해 감소하는 경향을 보였으며 수중환경에서는 부착 강도에 미치는 모재 표면 거칠기의 영향이 육상의 경우에 비하여 미비하였다. 마지막으로 수중코팅제의 선정, 사용 시에 유의할 점에 대하여 설명하였다.

인장 보강재 및 거푸집으로 활용한 FRP 판과 타설 콘크리트 사이의 부착에 관한 실험적 연구 (Bond Slip Behavior of Cast-In-Place Concrete and FRP Plank Using Formwork and Tensile Reinforcement)

  • 유승운
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.309-312
    • /
    • 2006
  • An experimental study for bond slip behavior of concrete and a FRP plank was used as the both formwork and the tensile reinforcement for a concrete structural member is described. For the FRP plank and the concrete to act as a composite structural member a satisfactory bond at the interface between the smooth surface of the FRP and the concrete must be developed. This study focuses on investigation of the bond slip behavior of sand coated interface between FRP and cast-in-place concrete experimentally.

  • PDF

반복주조된 치과용 합금의 피착면 처리방법에 따른 접착성 수지와의 접착강도에 관한 실험적 연구 (AN EXPERIMENT STUDY ON THE BOND STRENGTH OF ADHESIVE RESINS TO SUEEXSSIVELY RECAST ALLOYS FOR REISN-BONDED RESTORATIONS)

  • 정금태;양재호;이선형;정헌영
    • 대한치과보철학회지
    • /
    • 제28권2호
    • /
    • pp.53-76
    • /
    • 1990
  • The purpose of this study was to evaluate the tensile bond strength of adhesive resins to successively recast Rexillium III and Degudent-U. Recasting was done 4times successively. Specimen $A_1$, were cast by new metal, and $A_2$ by surpus of $A_1$, $A_3$ by surplus of, $A_2$ $A_4$ by surplus of $A_3$, $A_5$ by surplus of $A_4$ plus 50% new metal. The types of surface treatment for resinbonded restoration in this experiment were electrolytic etching by OXY-ETCH(Oxy dental products, Inc., Hillside, New Jersey, U.S,A.), aluminum oxide blasting, anodic oxidation by EZ-OXISOR( Towagiken Co., Kyoto, Japan), electrotinplating by Kura Ace(Kuralay Co., Kyoto, Japan). Three kinds of cementing resin used in this study were Comspan(K.P. Cauil Co, Milford Delaware, U.S.A.), Super Bond C&B(Sun-Medical Co. Ltd., Kyoto,Japan), Panavia EX(Kuralay Co., Ltd., Osaka, Japan). Tensile bond strength was measured by Instron Universal testing machineModel 1125) and all the specimen were observed with SEM(JEOL, JSM-T2000) and mode of bond failure were recorded. The obtained results were as follows : 1. In electrolytic etched group, tensile bond strength was decreassed when recast alloy was used, and tensile bond strength of Compan and panavia EX were not significantly different(P>0.05). 2. In remaining group treated by aluminum oxide blasting, EZ-OXIOR, Kura Ace, tensile bond strength were not changed when recast alloy were used, and tensile bond strength of SuperBond(C&B and Panavia EX were not significantly different(P>0.05). 3. IN SEM evaluation, electrolytic etched group and electrotinplated group exhibited different image when recast alloy was used, and remaining groups treated by aluminum oxide blasting, EZ-OXISOR exhibited the same. 4. IN observation of bond failure, electrolytic etched group exhibited adhesive failure and remaing groups treated by aluminium oxid blasting, EZ-OXISOR, Kura Ace exhibited adhesive and cohesive failure.

  • PDF

TENSILE BOND STRENGTH BETWEEN ELASTOMERIC IMPRESSION MATERIALS AND TRAY RESINS DEPENDING ON THE THICKNESS OF THE TRAY ADHESIVE

  • Kim, Tae-Won;Moon, Hong-Seok;Lee, Keun-Woo;Chung, Moon-Kyu
    • 대한치과보철학회지
    • /
    • 제44권6호
    • /
    • pp.699-711
    • /
    • 2006
  • Statement of problem. Elastomeric impression materials have been widely used to obtain an accurate impression. However there have not been enough studies on the influence of the thickness of the tray adhesives on the bonding strength between the trays and the elastomeric impression materials. Purpose. In order to understand the relationship between the thickness of the tray adhesive and the tensile bond strength and to suggest the thickness at which the bonding strength is strongest, tensile bond strength related to the thickness of adhesives of 3 different elastomeric impression materials were tested. Materials and methods. 3 impression materials, $Permlastic^{(R)}$. Regular Set(Kerr Corp., Romulus, Michigan, U.S.A.), $Impregum^{TM}$ $Penta^{TM}$(3M ESPE, Seefeld, Germany), and Aquasil Ultra Monophase Regular Set Smart Wetting.(Dentsply Caulk, Milford, Delaware, U.S.A.), were used in this study, and tray adhesives from the same manufacturers of the impression materials were used, which were Rubber Base Adhesive, Polyether Adhesive, and Silfix, respectively. The tray specimens were prepared by autopolymerizing the tray material(Instant Tray Mix, Lang, Wheeling, Illinois, U.S.A.), and a PVC pipe was used to house the impression material. In group A, tray adhesives were applied in multiple thin layers of 1 to 5 and in group B, adhesives were applied only once, in the thickness equivalent to several applications. Lightness($L^*$) of the adhesion surface was measured with a spectrophotometer(CM-3500d, Konica Minolta, Sakai, Osaka, Japan). The tensile bond strength of the elastomeric impression material and the tray resin was measured with universal materials testing machines(Instron, Model 3366, Instron Corp, Nowood, Massachusetts, U.S.A.). A formula between the number of adhesive application layers and the lightness of the adhesion surface was deduced in group A, and the number of adhesive layers in group B was estimated by applying the lightness($L^*$) to the deduced formula. Results. 1. In group A, a statistically significant increase in tensile bond strength appeared when the number of application layers increased from 1 to 2 and from 4 to 5, and no significant difference was present between 2, 3, and 4 layers in Permlastic. In Impregum, the tensile bond strength was significantly increased when the number of adhesive layers increased from 1 to 3, but no significant difference after 3 layers. In Aquasil, the tensile bond strength significantly increased as the number of application layers increased up to 4 but showed no significant difference between 4 and 5. 2. In group B, the tensile bond strength was decreased when the thickness of the adhesive increased in Permlastic. Impregum showed an increased tensile bond strength when the thickness of the adhesive was increased. In Aquasil, the tensile bond strength increased as the number of adhesive application layers increased up to approximately 2.5 layers but it sharply decreased after approximately 4.5. Conclusion. From the study, the common idea that it is better to apply a thin and single coat of tray adhesive needs correction in more detailed ways, and instructions on some of the tray adhesives should be reconsidered since there were several cases in which the tensile bond strength increased according to the increase in the thickness of the adhesives.

Effect of liners and primers on tensile bond strength between zirconia and resin-based luting agent

  • Jo, Eun-Hye;Huh, Yoon-Hyuk;Ko, Kyung-Ho;Park, Chan-Jin;Cho, Lee-Ra
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권5호
    • /
    • pp.374-380
    • /
    • 2018
  • PURPOSE. The effect of silica-based glass-ceramic liners on the tensile bond strength between zirconia and resin-based luting agent was evaluated and compared with the effect of 10-methacryloyloxydecyl dihydrogen phosphate (MDP)-containing primers. MATERIALS AND METHODS. Titanium abutments and zirconia crowns (n = 60) were fabricated, and the adhesive surfaces of the specimens were treated by airborne-particle abrasion. The specimens were divided into 5 groups based on surface treatment: a control group, 2 primer groups (MP: Monobond Plus; ZP: Z Prime Plus), and 2 liner groups (PL: P-containing Liner; PFL: P-free Liner). All specimens were cemented with self-adhesive resin-based luting agent. After 24-hour water storage and thermocycling (5,000 cycles, $5^{\circ}C/55^{\circ}C$), the tensile bond strength was measured using a universal testing machine. Failure mode analysis and elemental analysis on the bonding interface were performed. The data were analyzed using Kruskal-Wallis test, Dunn's post hoc test, and Fisher's exact test. RESULTS. The liner groups and primer groups showed significantly higher tensile bond strengths than that of the control group (P<.05). PFL showed a significantly higher tensile bond strength than the primer groups (P<.05). The percentage of mixed failure was higher in the primer groups than in the control group (P<.001), and all the specimens showed mixed failure in the liner groups (P<.001). A chemical reaction area was observed at the bonding interface between zirconia and liner. CONCLUSION. The application of liner significantly increased the tensile bond strength between zirconia and resin-based luting agent. PFL was more effective than MDP-containing primers in improving the tensile bond strength with the resin-based luting agent.

브라켓 접착시 타액 오염이 레진 강화형 글래스 아이오노머 시멘트의 인장 접착 강도에 미치는 영향 (The effects of salivary contamination on tensile bond strength of resin modified glass ionomer cements in bonding brackets)

  • 이경아;권오원
    • 대한치과교정학회지
    • /
    • 제30권1호
    • /
    • pp.83-89
    • /
    • 2000
  • 레진 강화형 글래스 아이오노머 시멘트의 접착 강도를 알아보고, 타액 오염이 접착제의 종류에 따라 접착 강도에 어떠한 영향을 미치는지 관찰하여 봄으로써 임상적 효용성을 알아보기 위하여 본 연구를 시행하였다. 교정 치료를 목적으로 발거된 소구치에 교정용 복합 레진 접착제로 Ortho-One, 레진 강화형 글래스 아이오노머 시멘트로는 Fuji Ortho LC, Vitremer, Advance를 사용하여 통상적인 과정의 브라켓 접착을 하였으며, 타액 오염군은 타액 오염후에 건조 한 뒤 브라켓을 접착한 후 증류수에 침적하고 $37^{\circ}C$ 항온조에 24시간 보관하였다. 만능시험기로 인장 접착 강도를 측정하여 다음과 같은 결과를 얻었다. 1. 통상의 방법으로 브라켓을 부착한 경우 인장 접착 강도는 Ortho-One군에서는 $7.68\pm1.76$ 이었으며, Advance군에 서는 $7.87\pm2.80$, Fuji Ortho LC군에서는 $4.99\pm2.53$, Vitremer군에서 는 $2.80\pm0.88$ MPa 나타났다. 타액 오염시킨 경우 인장 접착 강도는 Ortho-One군에서 는 $4.12\pm1.67$, Advance군에서는 $5.37\pm0.68$, Fuji Ortho LC군에서는 $4.41\pm1.61$, Vitremer군에서는 $2.60\pm1.10$ MPa 로 나타났다. 2. 타액 오염시킨 경우 Fuji Ortho LC와 Vitremer는 거의 영향이 없었고 (p>0.05), Ortho-One과 Advance는 큰 폭의 접착 강도 저하 현상을 나타냈다 (p<0.05). 3. Advance와 Ortho-One, Fuji Ortho LC는 만족할 만한 인장 접착 강도를 나타내어 브라켓 접착시 임상적 유용성이 있으리라 생각된다.

  • PDF