Evaluation of Material Properties for Yonggwang Nuclear Piping Systems(II) - Safety Injection System- (영광원자력 배관소재의 재료물성치 평가 (II) -안전주입계통-)

  • 김영진;석창성;장윤석
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.19 no.6
    • /
    • pp.1451-1459
    • /
    • 1995
  • The objective of this paper is to evaluate the material properties of SA312 TP316 and SA312 TP304 stainless steels and their associated welds manufactured for safety injection system of Yonggwang 3,4 nuclear generating stations. A total of 62 tensile tests and 46 fracture toughness tests were conducted and the effects of various parameters such as pipe size, crack plane orientation, tests were conducted and the effects of various parameters such as pipe size, crack plane orientation, test temperature, welding on material properties were discussed. Test results show that the effect of test temperature on fracture toughness was significant while the effects of pipe size and crack plane orientation on fracture toughness were negligible. Fracture toughness of the weld metal was in general higher than that of the base metal.

Effect of Side Groove on the Elastic Plastic Fracture Toughness of Gas Piping Material (가스배관재의 탄소성파괴인성에 미치는 측면홈 영향)

  • 임만배;차귀준;윤한기;공유식;김정호
    • Journal of Ocean Engineering and Technology
    • /
    • v.15 no.3
    • /
    • pp.63-68
    • /
    • 2001
  • SG-365 steel is an important material and used for manufacturing a pressure vessel which the gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the an unloading compliance method according to the ATM E813-97 method on the smooth and side groove 1CT specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the $J_IC. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides, it improves the accuracy of toughness values, decreases the scattering of them and tunneling and shear lip by the side groove.

  • PDF

Effect of Side Grooved on the Elastic Plastic Fracture Toughness of Gas Piping Meterial (가스배관재의 탄소성파괴인성에 미치는 측면홈영향)

  • 임만배;차귀준;윤한기;김정호
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2001.05a
    • /
    • pp.350-356
    • /
    • 2001
  • SG-50 steel is an important material and used for manufacturing a pressure vessel which the gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the an unloading compliance method according to the ASTM E813-97 and E1152-97 method on the smooth and side groove 1CT specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the J$_{IC}$. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides, it improves the accuracy of toughness values, decreases the scattering of them and tunneling and shear lip by the side groove.e.

  • PDF

A Study on the Fracture Resistance Curve and Effect of Side Grooves of SG365 Material (SG365강의 파괴저항곡선과 측면홈효과에 관한 연구)

  • 임만배
    • Journal of the Korean Society of Safety
    • /
    • v.16 no.4
    • /
    • pp.14-21
    • /
    • 2001
  • SG-365 steel is an important material End used for manufacturing a pressure vessel and gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the unloading compliance method according to the ASTM E8l3-97 and E1152-97 method on the smooth and side groove In specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the $J_{IC}$. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides. it improves the accuracy of toughness values, decreases the scattering of them and crack tunneling effect and shear lip by the side groove.

  • PDF

The Fracture Toughness and Crack Propagation behavoir of Short-fiber Reinforced Ruber (단섬유 강화고무의 파괴인성 및 크랙진전 거동)

  • Ryu, Sang-Ryeoul;Lee, Dong-Joo
    • Proceedings of the KSME Conference
    • /
    • 2000.04a
    • /
    • pp.85-90
    • /
    • 2000
  • The fracture toughness and crack propagation behaviors of short nylon66 fiber reinforced Chloroprene rubber nave been Investigated as functions of fiber aspect ratio, fiber content and interphase conditions. The J for crack initiation and rupture were determined for short-fiber reinforced rubber. The values of $J_c$ for most reinforced rubbers were low compared that of matrix. But, $J_r$ at rupture showed a higher value than that of matrix. The crack propagation behaviors were analyzed into 3 patterns with increasing fiber aspect ratio and fiber content. The tearing mechanisms of matrix and fiber reinforced rubber were observed by CCD camera focused on the tip of crack and load-displacement graph. Both cases showed a completely different behaviors

  • PDF

A Study on Fatigue Crack Growth Behavior and R-Curve Characteristics of Gas Piping Material (가스배관재의 피로균열진전거동과 파괴저항특성곡선에 관한 연구)

  • Son, J.D.;Lim, M.B.
    • Journal of Power System Engineering
    • /
    • v.11 no.1
    • /
    • pp.127-133
    • /
    • 2007
  • SG-365 steel is an important material and used for manufacturing a pressure vessel which the gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the unloading compliance method according to the ASTM E813-97 and E1152-97 method on the smooth and side groove 1CT specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the $J_{IC}$. It is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides, it improves the accuracy of toughness values, decreases a phenomenon of the tunneling and shear lip by the side groove.

  • PDF

Severe Open Ankle Sprain (SOAS): A Case Report (중증 개방성 발목 염좌: 증례보고)

  • Yoon, Sung-Hyun;Hwang, Chang-Hwan
    • Journal of Trauma and Injury
    • /
    • v.27 no.2
    • /
    • pp.25-28
    • /
    • 2014
  • Ankle injury is a very common injury. Especially it is the most commonly injured site in cases sports injuries. However, severe open ankle sprain (SOAS), defined as the tearing of the skin over the torn ligament in the ankle, is extremely rare, and no cases have been reported in Korea. In our center, we encountered a patient with a severe ankle open sprain, so we report and discuss that case.

Estimation of fracture toughness of cast steel container from Charpy impact test data

  • Bellahcenea, Tassadit;Aberkane, Meziane
    • Steel and Composite Structures
    • /
    • v.25 no.6
    • /
    • pp.639-648
    • /
    • 2017
  • Fracture energy values KV have been measured on cast steel, used in the container manufacture, by instrumented Charpy impact testing. This material has a large ductility on the upper transition region at $+20^{\circ}C$ and a ductile tearing with an expended plasticity before a brittle fracture on the lower transition region at $-20^{\circ}C$. To assess the fracture toughness of this material we use, the $K_{IC}$-KV correlations to measure the critical stress intensity factor $K_{IC}$ on the lower transition region and the dynamic force - displacement curves to measure the critical fracture toughness $J{\rho}_C$, the essential work of fracture ${\Gamma}_e$ on the upper transition region. It is found, using the $K_{IC}$-KV correlations, that the critical stress intensity factor $K_{IC}$ remains significant, on the lower transition region, which indicating that our testing material preserves his ductility at low temperature and it is apt to be used as a container's material. It is, also, found that the $J_{\rho}-{\rho}$ energetic criterion, used on the upper transition region, gives a good evaluation of the fracture toughness closest to those found in the literature. Finally, we show, by using the ${\Gamma}_e-K_{IC}$ relation, on the lower transition region, that the essential work of fracture is not suitable for the toughness measurement because the strong scatter of the experimental data. To complete this study by a numerical approach we used the ANSYS code to determine the critical fracture toughness $J_{ANSYS}$ on the upper transition region.

TRAUMATIC TMJ INJURY (외상성 악관절 손상)

  • Kim, Young-Kyun
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • v.19 no.2
    • /
    • pp.191-199
    • /
    • 1997
  • Mandibular trauma is developed due to traffic accident, fall down, industrial injury, and others. TMJ disorder is usually also developed after facial traumatic injury. Many authors suggested that disc displacement or tearing, acute synovitis, TMJ ankylosis, traumatic arthritis, or effusion are developed after facial trauma. It is still very controversible what is the best treatment of TMJ injury such as condylar fracture and meniscal injury. In TMJ injury, synovial inflammation is developed and pain mediators such as prostaglandin E2 or leukotriene B4 are released from the synovial membrane. This can be a cause of TMJ disorder. I present a variety of experimental study about the condylar fracture and meniscal injury and enzyme-immunoassay of synovial fluid after mandibular trauma that have been studied since 1992 and establish the treatment criteria of traumatic TMJ injury. I think that the treatment option of condylar fracture depends upon the surgeon's criteria exclusively. There are no significant differences between conservative and surgical treatment. If the aggressive functional physical therapy and long-term followup be performed, the favorable functional recovery of TMJ can be obtained. And I think that the initial surgical management of meniscus of TMJ is unnecessary in condylar fracture. And also arthrocentesis can be available to release the patient's subjective symptoms and improve the healing of injured TMJ.

  • PDF

Fracture mechanics analysis of multipurpose canister for spent nuclear fuels under horizontal/oblique drop accidents

  • Jae-Yoon Jeong;Cheol-Ho Kim;Hune-Tae Kim;Ji-Hye Kim;Yun-Jae Kim
    • Nuclear Engineering and Technology
    • /
    • v.55 no.12
    • /
    • pp.4647-4658
    • /
    • 2023
  • In this paper, elastic-plastic fracture mechanics analysis is performed to determine the critical crack sizes of the multipurpose canister (MPC) manufactured using austenitic stainless steel under dynamic loading conditions that simulate drop accidents. Firstly, dynamic finite element (FE) analysis is performed using Abaqus v.2018 with the KORAD (Korea Radioactive Waste Agency)-21 model under two drop accident conditions. Through the FE analysis, critical locations and through-thickness stress distributions in the MPC are identified, where the maximum plastic strain occurs during impact loadings. Then, the evaluation using the failure assessment diagram (FAD) is performed by postulating an external surface crack at the critical location to determine the critical crack depth. It is found that, for the drop cases considered in this paper, the principal failure mechanism for the circumferential surface crack is found to be the plastic collapse due to dominant high bending axial stress in the thickness. For axial cracks, the plastic collapse is also the dominant failure mechanism due to high membrane hoop stress, followed by the ductile tearing analysis. When incorporating the strain rate effect on yield strength and fracture toughness, the critical crack depth increases from 10 to 20%.