Kim, Jin-Ho;Im, Sung-Woo;Chang, In-Hwa;Shiga, Atsumi
Journal of Korean Society of Steel Construction
/
v.10
no.2
s.35
/
pp.303-315
/
1998
Four types of repair procedures are applied to the fatigue cracked crane runway gilders, which are stop-holes as crack arrester stop-holes reinforced with high strength bolts, welding repair and reinforcement with high strength bolted splices. The fatgiue cracks are reinitiated at the region where stop-holes and weld repairments are applied, while none of the cracks are observed in the cases of stop-holes reinforcement and reinforcement with high strength bolted splices. When using stop-holes and hole-reinforcement all repaired regions show a same fatigue strength to the one before the repairments. The experiments also reveal that the proper weldment is an essential factor when applying the welding repairement as a properly welding produces the same level of fatigue strength after the repairement. When the situation permits to use reinforcement with high strength boilted splices, the experiments shows the repairment is the best possible method among the procedures available.
KSCE Journal of Civil and Environmental Engineering Research
/
v.7
no.4
/
pp.115-124
/
1987
Stop-hole method is one of the conventional methods for the temporary repair or reinforcement of the member in the case that the structural steel member has a fatigue crack. In this study, the stop-hole method. have been estimated quantitatively in terms of survival life time of the side edge cracked specimen. For this purpose, fatigue tests have been performed on the test specimens and the fatigue crack growth rates of the structural steel (SS41) members have been measured under load of constant amplitude. The results of this experiment show that it is desirable to use the stop-hole method before the crack reaches the region of elasto-plastic behaviour.
In steel bridges fatigue cracks are sometimes repaired by placing drilled holes at the crack tips. From the meaning that the drilled holes stop the propagation of cracks, they are called stop-holes. Since stop-holes are regarded as an emergency measure to delay crack propagation, usually some substantial repair follows. However, if the stress at the stop-holes is below their fatigue limit, fatigue cracks would not be expected to occur. The purpose of this study is to present the conditions under which stop-holes prevent the reinitiation of fatigue cracks. The fatigue limit of stop-holes and the equations necessary to estimate the maximum stress on the circumference of the stop-holes are provided.
Fatigue cracks are inevitable in circumstances in which the cyclic loading exists. Therefore, many of mechanical components are in a risk of being in exposure to fatigue cracks. On the other hand, renewing the facilities or infrastructures is not always possible. Therefore, retrofitting the structures by means of the available methods, such as crack arrest methods is logical and in some cases inevitable. In this regard, this paper considers three popular crack arrest methods (e.g., drilling stop-hole, steel welded patch, and carbon fiber reinforced (CFRP) patch), which have been compared by using extended finite element method (XFEM). In addition, effects in terms of the width and thickness of patches and the configuration of drilling stop holes have been evaluated. Test results indicated that among the considered methods, CFRP patches were the most effective means for arresting cracks. Besides, in the case of arresting by means of drilling stop holes, drilling two holes next to the crack-tip was more effective than blunting the crack-tip by drilling one hole. In other words, the results indicated that the use of symmetric welded metal patches could lead to a 21% increase in fatigue life, as compared to symmetric stop holes. Symmetric CFRP patches enhanced the fatigue life of cracked specimen up to 77%, as compared to drilling symmetric stop holes. In addition, in all cases, symmetric configurations were far better than asymmetric ones.
Transactions of the Korean Society of Automotive Engineers
/
v.9
no.4
/
pp.204-213
/
2001
This paper develops the compliance approach to the problem of load sharing between a cracked plate and a cover plate used to bridge the crack. The theory is validated by using calculated stress intensity factors for the covered and uncovered cases and by using stop hole method to reduce experimentally observed growth rates to a common base. Calculations are then made on the effect of cover plate width on fatigue crack retardation in order to demonstrate the predictive capability of the technique.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2002.05b
/
pp.12-15
/
2002
In this paper, we fabricated a electro-chemical discharge machine for drilling microscopic glass hole. In this research, we used a glass plate and NaOH solution. From the experimental result, we knew that the change of voltage wave was caused by drilling microscopic hole of glass using electro-chemical discharge method. So, we can give a function of the power auto stop to electro-chemical discharge machine with the change of voltage wave.
In this study, a series of finite element analysis using LUSAS were performed in order to assess the quantitative effects of repair and retrofit of stringer in steel plate girder railway bridge with fatigue cracks. And cutoff types of end part of upper flange were considered as right-angled type and round-angled type. Also, as a method of repair and retrofit of fatigue cracks in stringer, perforation of stop-hole and installation of bracket were considered. From the analysis result, it was possible to assess the fatigue safety and fatigue life of stringer with fatigue cracks, and to estimate the stress intensity factor range in cut-off part of stringer using J-integral method. Also, according
to the method of perforation of stop-hole and installation of bracket, it was possible to calculate the crack propagation life at the cut-off part of stringer.
This study encompasses the performance of static and fatigue test for the 8 large scale test specimens to clarify the fatigue behavior of coped stringer and the effect of the repair and strengthening on the damaged stringer of the floor system in steel railway bridges. For the purpose of the research, the actual stress wave for the existing bridge was measured, the basic stress range frequency histogram was made and the equivalent stress range was calculated. Using the result from the equivalent stress range made by adjusting the stress range, the static and fatigue test was carried out by identifying the previous rehabilitation and after. As the result of the static tests, it was revealed that the level of local stress under the S1 specimen test of the real equivalent stress range was similar to tensile strength of the test material, and it was consistent with the requirement of the initiation condition of the fatigue crack. Through the various rehabilitation methods to the damaged specimens, the effects of the repair and reinforcement were analyzed. According to the results of the repair of effect, bolting the high tension bolt over the stop hole was confirmed to be more adequate method than drilling only stop hole to delay the fatigue crack growth. Futhermore, in case of the stringer subjected by bending moment, the reinforcement over the upper flange side was determined to be a useful strengthening method, and the reinforcement to the web of the stringer was not appropriate to accomodate as a adequate strengthening method. Also it was confirmed that the category of the fatigue design for the coped stringer met with the category E specified on the fatigue design criteria of the Highway Standard Specification in Korea.
Transactions of the Korean Society of Machine Tool Engineers
/
v.11
no.2
/
pp.103-111
/
2002
Out of all metal-cutting process, the hole-making process is the most widely used. It is estimated to be more than 30% of the total metal-cutting process. It is therefore desirable to monitor and detect drill wear during the hole-drilling process. One important aspect in controlling the drilling process is monitoring drill wear status. There are two systems, Basic system and Online system, to detect the drill wear. Basic system comprised of spindle rotational speed, feed rates, thrust torque and flank wear measured by tool microscope. Outline system comprised of spindle rotational speed feed rates, AE signal, flank wear area measured by computer vision, On-line monitoring system does not need to stop the process to inspect drill wear. Backpropagation neural networks (BPNs) were used for on-line detection of drill wear. The output was the drill wear state which was either usable or failure. This paper deals with an on-line drill wear monitoring system to fit the detection of the abnormal tool state.
Out of all metal-cutting processes, the hole-making process is the most widely used. It is estimated to be more than 30% of the total metal-cutting process. It is therefore desirable to monitor and detect drill wear during the hole-drilling process. One important aspect in controlling the drilling process is monitoring drill wear status. Accordingly, this paper deals with Basic system and Online system. Basic system comprised of spindle rotational speed, feed rates, thrust, torque and flank wear measured tool microscope. Online system comprised of spindle rotational speed, feed rates, AE signal, flank wear area measured computer vision. On-line monitoring system does not need to stop the process to inspect drill wear. Backpropagation neural networks (BPNs) were used for on-line detection of drill wear. This paper deals with an on-line drill wear monitoring system to fit the detection of the abnormal tool state.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.