Synthesis of Mn-Zn Ferrite Powder by Alcoholic Dehydration and Properties of Sintered Body (알콜탈수법에 의한 Mn-Zn Ferrite 분체제조 및 소결특성)

  • 이대희;김창현;이병교
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.8
    • /
    • pp.843-849
    • /
    • 1998
  • Fine powders of Mn-Zn ferrite were prepared by the alcoholic dehydration method and densification beha-vior of synthesized powder was investigated. The concentration and pH of solution for optimal precipitation was 0.4M and 2.5 respectively. The spinel single phase metastable state was formed by thermal decom-position of precipitate and then spinel phase was disintegrated into hematite and spinel {{{{ { { ZnFe}_{2 }O }_{4 } }} at 600$^{\circ}C$ With increase of temperature reaction of solid solution between hematite and spinel was proceeded and resulted in the spinel single phase (Mn, Zn Fe){{{{ { {Fe }_{2 }O }_{4 } }} On account of high reactivity of uncalcined powders densification started at 200$^{\circ}C$ lower and completed at 50$^{\circ}C$ lower in comparison with calcined powders.

  • PDF

Mossbauer Study for the Cation Distribution of Co-ferrite (CoxFe1-xO4) Thin Films (Co-ferrite 박막에서 양이온 거동에 관한 Mössbauer 분광 연구)

  • Park, Jae-Yun;Park, Young-Ran;Kim, Hee-Kyung;Kim, Kwang-Joo
    • Journal of the Korean Magnetics Society
    • /
    • v.16 no.1
    • /
    • pp.1-5
    • /
    • 2006
  • The crystallographic properties and cation distribution of oxyspinels ferrite $Co_xFe_{1-x}O_4$ thin films have been explored by X-ray diffraction, vibrating sample magnetometer (VSM), and conversion electron $M\"{o}ssbauer$ spectroscopy (CEMS). Thin films are prepared by sol-gel method. Normal spinel structure is transformed to inverse spinel structure with increasing Co concentration CEMS results indicate that most of $Fe^{3+}$ ions are substituted to $Co^{3+}$ions. Accordingly $Co^{2+}$ ions on octahedral site migrate to tetrahedral site. Magnetic moment is decreased with increasing Co concentration, which means high spin $Fe^{3+}$ ions are replaced by low spin $Co^{3+}$.

Formation Reaction of Mn-Zn Ferrite by Wet Process (습식합성에 의한 Mn-Zn Ferrite의 생성반응에 관한 연구)

  • 이경희;이병하;허원도;황우연
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.1
    • /
    • pp.25-33
    • /
    • 1993
  • Formation reaction of Mn-Zn ferrite depending on various synthetic conditions of wet process was investigated using FeCl2.nH2O(n≒4), MnCl2.4H2O, ZnCl2 as starting materials. A stable intermediate precipitate was formed by the addition of H2O2. And the precipitate was hard to transform to spinel phase of Mn-Zn Fe2O4. Single phase of Mn-Zn Fe2O4 spinel was obtained above 8$0^{\circ}C$ reaction temperature. The powder had spherical particle shape and 0.02~0.05${\mu}{\textrm}{m}$ particle size. Fe(OH)2 solid solution, -FeO(OH) solid solution, -FeOOH, Mn-Zn Fe2O4 spinel were formed with air flow rate 180$\ell$/hr. However, single phase of Mn-Zn Fe2O4 spinel with cubic particle shape and 0.1~0.2${\mu}{\textrm}{m}$ particle size was formed with synthetic conditions of 8$0^{\circ}C$ and 90 munutes. The particle shape of the -FeOOH was needle-like.

  • PDF

Crystallographic and Magnetic Properties of Li0.7Co0.2Ti0.2V0.2Fe1.7O4 Ferrite

  • Chae, Kwang-Pyo;Kwon, Woo-Hyun;Lee, Jae-Gwang
    • Journal of Magnetics
    • /
    • v.15 no.1
    • /
    • pp.25-28
    • /
    • 2010
  • This study examined the crystallographic and magnetic properties of vanadium-substituted lithium cobalt titanium ferrite, $Li_{0.7}Co_{0.2}Ti_{0.2}V_{0.2}Fe_{1.7}O_4$. Ferrite was synthesized using a conventional ceramic method. The samples annealed below $1040^{\circ}C$ showed X-ray diffraction peaks for spinel and other phases. However, the sample annealed above $1040^{\circ}C$ showed a single spinel phase. The lattice constant of the sample was $8.351\;{\AA}$, which was relatively unaffected by vanadium-substitution. The average grain size after vanadium-substitution was $13.90\;{\mu}m$, as determined by scanning electron microscopy. The M$\ddot{o}$ssbauer spectrum could be fitted to two Zeeman sextets, which is the typical spinel ferrite spectra of $Fe^{3+}$ with A and B sites, and one doublet. From the absorption area ratio of the M$\ddot{o}$ssbauer spectrum, the cation distribution was found to be ($Co_{0.2}V_{0.2}Fe_{0.6})[Li_{0.7}Ti_{0.2}Fe_{1.1}]O_4$. Vibrating sample magnetometry revealed a saturation magnetization and coercivity of 36.9 emu/g and 88.6 Oe, respectively, which were decreased by vanadium-substitution.

Phase Equilibria of the Ferrous Ferrite System of $(Mg_{0.29}-yMnyFe_{0.71})_{3-}\delta$O_4$ ($(Mg_{0.29}-yMnyFe_{0.71})_{3-}\delta$O_4$ 훼라이트계의 상평형)

  • 채정훈;유한일;강선호;강대석;유병두
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.3
    • /
    • pp.394-402
    • /
    • 1995
  • Electrical conductivity and thermoelectric power of the ferrous ferrite system of (Mg0.29-yMnyFe0.71)3-$\delta$O4 have been measured as function of the thermodynamic variables, cationic composition(y), temperature(T) and oxygen partial pressure(Po2) under thermodynamic equilibrium conditions at elevated temperatures. On the basis of the electrical properties-phase stability correlation, the stability regions of the ferrite spinel and its neighboring phases have been subsequently located in the log Po2 vs. y and log Po2 vs. 1/T planes in the ranges of 0 y 0.29, 1100 T/$^{\circ}C$ 1400 and 10-14 Po2/atm 1. The stability region, Δlog Po2(y, 1/T), of the ferrite spinel single phase widens with increasing Mn-content(y) and the boundaries of each region are linear against 1/T with negative slopes.

  • PDF

Microstructure and Magnetic Property of Nanostructured NiZn Ferrite Powder

  • Nam, Joong-Hee
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.12
    • /
    • pp.1119-1123
    • /
    • 2002
  • Nanostructured spinel NiZn ferrites were prepared by the sol-gel method from metal nitrate raw materials. Analyses by X-ray diffraction and scanning electron microscopy showed the average particle size of NiZn ferrite was under 50 nm. The single phase of NiZn ferrites was obtained by firing at 250${\circ}C$, resulting in nanoparticles exhibiting normal ferrimagnetic behavior. The nanostructured $Ni_{1-X}Zn_XFe_2O_4$ (x=0.0∼1.0) were found to have the cubic spinel structure of which the lattice constants ${\alpha}_2$ increases linearly from 8.339 to 8.427 ${\AA}$ with increasing Zn content x, following Vegard's law, approximately. The saturation magnetization $M_s$ was 48 emu/g for x=0.4 and decreased to 8.0 emu/g for higher Zn contents suggesting the typical ferrimagnetism in mixed spinel ferrites. Pure NiZn ferrite phase substituted by Cu was observed before using the additive but hematite phase was partially appeared at $Ni_{0.2}Zn_{0.2}Cu_{0.6}Fe_2O_4$. On the other hand, the hematite phase in this NiZn Cu ferrite was disappeared after using the additive of acethyl aceton with small amount. The saturation magnetization Ms of $Ni_{0.2}Zn_{0.8-y}Cu_yFe_2O_4$(y=0.2∼0.6) as measured was about 51 emu/g at 77K and 19 emu/g at room temperature, respectively.

The Study of Magnetic Structure of Ni1-xMgxFe2O4 Ferrite System by Mössbauer Spectroscopy (Mössbauer 분광법에 의한 Ni1-xMgxFe2O4 Ferrite의 자기구조 연구)

  • Yoon, In-Seop;Baek, Seung-Do
    • Journal of the Korean Magnetics Society
    • /
    • v.19 no.3
    • /
    • pp.106-112
    • /
    • 2009
  • $Ni_{1-x}Mg_xFe_2O_4$ ferrite system was studied by using X-ray diffraction and $M{\ddot{o}}ssbauer$ spectroscopy. The samples were prepared by ceramic sintering method with Mg content x. The X-ray diffraction patterns of samples show phase of cubic spinel structure. There are no remarkable changes of lattice constants in $Ni_{1-x}Mg_xFe_2O_4$ ferrite system. The $M{\ddot{o}}ssbauer$ spectra were consisted of two sets of six lines, respectively, corresponding to $Fe^{3+}$ at tetrahedral and octahedral sites. The magnetic hyperfine field of samples was decreased as increasing Mg contents x in both sites and it was shown Yafet-Kittel magnetic structure. $NiFe_2O_4$ was shown complete inverse spinel, but $NiFe_2O_4$ was shown partial inverse spinel which absorption area ratio (oct/tet) was 1.449 in $M{\ddot{o}}ssbauer$ spectrum.

A Study on Electromagnetic Wave Absorbing Properties of Ni-Mn-Zn Spinel Ferrite-Rubber Composite (Ni-Mn-Zn Spinel Ferrite-Rubber Composite의 전파흡수특성에 관한 연구)

  • 박연준;김동일
    • Journal of the Korean Institute of Navigation
    • /
    • v.23 no.1
    • /
    • pp.15-22
    • /
    • 1999
  • In this paper, ferrite-rubber composite has been studied in order to apply to RF-A-PF in a super wideband electromagnetic absorber in RF-A-PF type, which can be used for a general purpose anechoic chamber. $Ni_x - Mn_0.1 - Zn_{(1-x-0.1)}ㆍFe_2O_4$ ferrite powder has been fabricated, then, using this, 〔$Ni_x - Mn_0.1 - Zn_{(1-x-0.1)}ㆍFe_2O_4$〕-Rubber composite for RF-layer in the RF-A-PF type absorber has been fabricated and it's characteristics have been analyzed. As a result, it has been clearly shown that the 〔$Ni_x - Mn_0.1 - Zn_{(1-x-0.1)}ㆍFe_2O_4$〕-Rubber composite has excellent electromagnetic wave absorbing properties.

  • PDF

Calcined Condition and Characteristic of Cu-Ni-Zn Ferrite Powder Made by Thermal Decomposition of Organic Acid Salt (유기산염 열분해법으로 합성한 Cu-Ni-Zn 페라이트분말의 특성과 하소조건)

  • 정재우
    • Journal of Powder Materials
    • /
    • v.2 no.1
    • /
    • pp.29-35
    • /
    • 1995
  • In this study the calcined condition and characteristic of Cu-Ni-Zn ferrite powder were investigated. The Cu-Ni-Zn ferrite powder has been synthesized by the thermal decomposition of the organic acid salt. This process did not require a strict pH control and provided the uniform composition and fine powder with about 0.3 $\mu\textrm{m}$. The XRD diffraction pattern of this powder showed about 50% spinel phase. The optimum calcination was found to be done at $700^{\circ}C$ for one hour. After the calcination, the amount of spinel increased to 90%. The distribution of the particle size showed bimodal peaks, one was about 0.5 $\mu\textrm{m}$ and the other was about 20 $\mu\textrm{m}$. The large particles of 20 $\mu\textrm{m}$ were the agglomeration of fine Particles. The mean Particle size of the powder was about 0.4 $\mu\textrm{m}$. The powder was compacted under 100 MPa pressure and sintered at 1100~ $1250^{\circ}C$ for one hour in air. The density of ferrites specimen was a function of the sintering temperature. The higher the temperature, the denser the ferrite. The maximum relative density of the sintered ferrite was about 93% at $1250^{\circ}C$. The grain size of sintered specimen at $1200^{\circ}C$ was 5 $\mu\textrm{m}$ and homogeneous.