• Title/Summary/Keyword: soft magnetic materials

Search Result 267, Processing Time 0.027 seconds

Magnetic Properties of Hard/Soft Nanocomposite Ferrite Synthesized by Self-Combustion Precursors (자전 연소 전구체로 합성한 나노 크기 경/연 복합페라이트의 자기 특성)

  • Oh, Young Woo;Ahn, Jong Gyeon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.22 no.3
    • /
    • pp.45-50
    • /
    • 2015
  • The goal of this research is the create novel magnets with no rare-earth contents, with larger energy product by comparison with currently used ferrites. For this purpose we developed nano-sized hard-type/soft-type composite ferrite in which high remanent magnetization (Mr) and high coercivity (Hc). Nano-sized Ba-ferrite, Ni-Zn ferrite and $BaFe_{12}O_{19}/Ni_{0.5}Zn_{0.5}Fe_2O_4$ composite ferrites were prepared by sol-gel combustion method by use of glicine-nitrate and citric acid. Nanocomposite ferrites were calcined at temperature range $700-900^{\circ}C$ for 1h. According to the X-ray diffraction patterns and FT-IR spectra, single phase of NiZn-ferrite and Ba-ferrite were detected and hard/soft nanocomposite ferrite was indicated to the coexistence of the magnetoplumbite-structural $BaFe_{12}O_{19}$ and spinel-structural $Ni_{0.5}Zn_{0.5}Fe_2O_4$ that agreed with the standard JCPDS 10-0325 data. The particle size of nanocomposite turn out to be less than 120 nm. The nanocomposite ferrite shows a single-phase magnetization behavior, implying that the hard magnetic phase and soft magnetic phase were well exchange-coupled. The specific saturation magnetization ($M_s$) of the nanocomposite ferrite is located between hard ($BaFe_{12}O_{19}$) and soft ferrite($Ni_{0.5}Zn_{0.5}Fe_2O_4$). The remanence (Mr) of nanocomposite ferrite is much higher than that of the individual $BaFe_{12}O_{19}$ and $Ni_{0.5}Zn_{0.5}Fe_2O_4$ ferrite, and $(BH)_{max}$ is increased slightly.

Nanocrystalline Materials-an Overview

  • Suryanarayana, C.
    • Journal of Powder Materials
    • /
    • v.3 no.4
    • /
    • pp.233-245
    • /
    • 1996
  • Nanocrystalline materials, with a grain size of typically <100 nm, are a new class of materials with properties vastly different from and often superior to those of the conventional coarse-grained materials. These materials can be synthesized by a number of different techniques and the grain size, morphology, and composition can be controlled by controlling the process parameters. In comparison to the coarse-grained materials, nanocrystalline materials show higher strength and hardness, enhanced diffusivity, improved ductility/toughness, reduced, density, reduced elastic modulus, higher electrical resistivity, increased specific heat, higher coefficient of thermal expansion, lower thermal conductivity, and superior soft and hard magnetic properties. Limited quantities of these materials are presently produced and marketed in the US, Canada, and elsewhere. Applications for these materials are being actively explored. The present article discusses the synthesis, structure, thermal stability, properties, and potential application of nanocrystalline materials.

  • PDF

Magnetic Microstructures and Corrosion Behaviors of Nd-Fe-B-Ti-C Alloy by Ga Doping

  • Wu, Qiong;Zhang, Pengyue;Ge, Hongliang;Yan, Aru;Li, Dongyun
    • Journal of Magnetics
    • /
    • v.18 no.3
    • /
    • pp.240-244
    • /
    • 2013
  • The influences of Gallium doping on the magnetic microstructures and corrosion behaviors of Nd-Fe-B-Ti-C alloys are investigated. The cooling rate for obtaining fully amorphous structure is raised, and the glassforming ability is improved by the Ga addition. The High Resolution Transmission Electron Microscopy image shows that the ${\alpha}$-Fe and $Fe_3B$ soft magnetic phases become granular surrounded by the $Nd_2Fe_{14}B$ hard magnetic phase. The rms and $({\Delta}{\varphi})_{rms}$ value of Nd-Fe-B-Ti-C nanocomposite alloy thick ribbons in the typical topographic and magnetic force images detected by Magnetic Force Microscopy(MFM) decreases with 0.5 at% Ga addition. The corrosion resistances of $Nd_9Fe_{73}B_{12.6}C_{1.4}Ti_{4-x}Ga_x$ (x = 0, 0.5, 1) alloys are enhanced by the Ga addition. It can be attributed to the formation of more amorphous phases in the Ga doped samples.

Synthesis and characterization of soft magnetic composite in Fe2O3-Mg system by mechanical alloying (기계적합금화에 의한 Fe2O3-Mg계 연자성 콤포지트의 합성 및 평가)

  • Lee, Chung-Hyo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.25 no.6
    • /
    • pp.245-251
    • /
    • 2015
  • We have applied mechanical alloying (MA) to produce soft magnetic composite material using a mixture of elemental $Fe_2O_3$-Mg powders. An optimal milling and heat treatment conditions to obtain soft magnetic ${\alpha}$-Fe/MgO composite with fine microstructure were investigated by X-ray diffraction, differential scanning calorimetry (DSC) and vibrating sample magnetometer (VSM) measurement. It is found that ${\alpha}$-Fe/MgO composite powders in which MgO is dispersed in ${\alpha}$-Fe matrix are obtained by MA of $Fe_2O_3$ with Mg for 30 min. The saturation magnetization of ball-milled powders increases with increasing milling time and reaches to a maximum value of 69.5 emu/g after 5 h MA. The magnetic hardening due to the reduction of the ${\alpha}$-Fe grain size by MA was also observed. Densification of the MA powders was performed in a spark plasma sintering (SPS) machine at $800{\sim}1000^{\circ}C$ under 60 MPa. X-ray diffraction result shows that the average grain size of ${\alpha}$-Fe in ${\alpha}$-Fe/MgO nanocomposite sintered at $800^{\circ}C$ is in the range of 110 nm.

Practical Calculation of Iron Loss for Cylindrical Linear Machine

  • Jeong, Sung-In
    • Journal of Electrical Engineering and Technology
    • /
    • v.13 no.5
    • /
    • pp.1901-1907
    • /
    • 2018
  • This paper is a study for accurate iron loss calculation of a cylindrical linear machine for free piston engine. This study presents that it is possible to accurately predict power loss in ferromagnetic laminations under magnetic flux by specially considering the dependence of hysteresis, classical, and excess loss components on the magnetic induction derivative. Significant iron loss in the armature core will not only compromise the machine efficiency, but may also result in excessive heating, which could lead to irreversible deterioration in the machine performance. Thus, correct prediction of power losses under a distorted flux waveform is therefore an important prerequisite to machine design, particularly when dealing with large apparatus where stringent efficiency standards are required. Finally, it will be discussed about the iron loss in various materials of cylindrical linear electric machine by geometric and electrical parameters. It will give elaborate information about the perfect design and design rules of cylindrical linear machine and in parallel tools for the calculation, simulation and design will be available.

Diagnosis of Residual Tumors after Unplanned Excision of Soft-Tissue Sarcomas: Conventional MRI Features and Added Value of Diffusion-Weighted Imaging

  • Jin, Kiok;Lee, Min Hee;Yoon, Min A;Kim, Hwa Jung;Kim, Wanlim;Chee, Choong Geun;Chung, Hye Won;Lee, Sang Hoon;Shin, Myung Jin
    • Investigative Magnetic Resonance Imaging
    • /
    • v.26 no.1
    • /
    • pp.20-31
    • /
    • 2022
  • Purpose: To assess conventional MRI features associated with residual soft-tissue sarcomas following unplanned excision (UPE), and to compare the diagnostic performance of conventional MRI only with that of MRI including diffusion-weighted imaging (DWI) for residual tumors after UPE. Materials and Methods: We included 103 consecutive patients who had received UPE of a soft-tissue sarcoma with wide excision of the tumor bed between December 2013 and December 2019 and who also underwent conventional MRI and DWI in this retrospective study. The presence of focal enhancement, soft-tissue edema, fascial enhancement, fluid collections, and hematoma on MRI including DWI was reviewed by two musculoskeletal radiologists. We used classification and regression tree (CART) analysis to identify the most significant MRI features. We compared the diagnostic performances of conventional MRI and added DWI using the McNemar test. Results: Residual tumors were present in 69 (66.9%) of 103 patients, whereas no tumors were found in 34 (33.1%) patients. CART showed focal enhancement to be the most significant predictor of residual tumors and correctly predicted residual tumors in 81.6% (84/103) and 78.6% (81/103) of patients for Reader 1 and Reader 2, respectively. Compared with conventional MRI only, the addition of DWI for Reader 1 improved specificity (32.8% vs. 56%, 33.3% vs. 63.0%, P < 0.05), decreased sensitivity (96.8% vs. 84.1%, 98.7% vs. 76.7%, P < 0.05), without a difference in diagnostic accuracy (76.7% vs. 74.8%, 72.9% vs. 71.4%) in total and in subgroups. For Reader 2, diagnostic performance was not significantly different between the sets of MRI (P > 0.05). Conclusion: After UPE of a soft-tissue sarcoma, the presence or absence of a focal enhancement was the most significant MRI finding predicting residual tumors. MRI provided good diagnostic accuracy for detecting residual tumors, and the addition of DWI to conventional MRI may increase specificity.

Magnetic Properties of FeZrN/$SiO_2$ Soft Magnetic Multilayer Thin Films (FeZrN/$SiO_2$ 연자성 다층 박막의 자기적 성질)

  • Kim, Taek-Su;Kim, Jong-O
    • Korean Journal of Materials Research
    • /
    • v.6 no.11
    • /
    • pp.1061-1066
    • /
    • 1996
  • RF magnetron reactive sputtering법으로 Fe75.5Zr8.3N16.2/SiO2(250$\AA$) 다층 박막을 FeZrN의 두께를 변화시키면서 제조하고, 제조된 박막을 진공 열처리하여 열처리 온도에 따른 포화자화, 보자력, 고주파에서의 투자율 그리고 열적 안정성을 조사하였다. Fe75.5Zr8.3N16.2/SiO2(250$\AA$) 다층박막은 FeZrN의 두께가 800$\AA$이상일 때 좋은 연자성을 나타내었다. Fe75.5Zr8.3N16.2/SiO2(250$\AA$)다층 박막을 45$0^{\circ}C$로 열처리 했을 때 포화자속밀도(1.08 T), 보자력 0.41 Oe, 1 MHz에서의 실효 투자율은 3000이상의 연자성을 나타내었다. 그 이유는 X-선 회절 분석 결과 열처리에 의해서 ZrN 미결정이 석출하여 $\alpha$-Fe 결정 성장이 억제되어 우수한 연자기적 성질이 나타난다고 판단된다. 이때 $\alpha$-Fe 입자 크기는 40-50$\AA$, ZrN의 입자 크기는 10-15$\AA$이다. 그리고 실효 투자율의 주파수 의존성에서 단층막에서는 5 MHz 이상에서 실효 투자율이 급격히 감소하는 경향을 보였으나, 다층막에서는 40MHz까지 실효 투자율이 1600이 되어 고주파에서의 연자성이 개선되었다.

  • PDF