활성제를 사용한 슬래그 미분말 혼합 모르타르의 강도 (Strength of Alkali-Activated GGBF Slag Mortar)

  • 문한영;신화철;권태석
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.481-486
    • /
    • 2001
  • Ground granulated blast-furnace slag shows very high strength when proper alkali-activator exists. This paper deals with setting time, heat evolution rate and the strength development of alkali-activated slag cement activated by KOH, Ca(OH$)_{2}$, $Na_{2}$ $So_{4}$ , and alum(potassium aluminum sulfate). Alkali-activated slag mortar is studied by comparison with GGBF slag cement mortar. The experimental results indicate that for moisture curing at $25^{\circ}C$, the addiction of either 4% $Na_{2}$ $So_{4}$ or 4% alum increases the strength of GGBF slag cement mortar consisting of 50% GGBF slag and 50% portland cement at early age. Strength of activated GGBF slag cement mortars at 1, 3 and 7 days exceeded that of GGBF slag cement mortar. A conduction calorimeter was used to monitor early age hydration.

  • PDF

Setting and Strength Properties of Mortar Containing Steel Furnace Slag Dust

  • Choi, Yun-Wang;Chung, Jee-Seung;Moon, Dae-Joong;Shin, Hwa-Cheol;Jang, Lee-Duck
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.193-196
    • /
    • 2003
  • In this paper, the experimental investigation for the setting properties of cement paste, the consistency and strength properties of mortar with steel furnace slag dust was performed and compared with those of cement paste and mortar with ground granulated blast furnace slag. When steel furnace slag dust was replaced with normal portland cement, setting time and flow value indicated to good results like as mortar with ground granulated blast furnace slag. However, mortar with steel furnace slag dust expressed to appreciably strength devaluation according to containing ratio, and did not indicate the pozzolanic reaction like as ground granulated blast furnace slag.

  • PDF

페로니켈슬래그를 잔골재로 사용한 비소성 시멘트 모르타르의 강도 특성 (Strength Characteristics of Non-Sintered Cement Mortar Utilizing Ferro-Nickel Slag as Fine Aggregate)

  • 류지수;장경수;나형원;형원길
    • 한국건축시공학회지
    • /
    • 제23권4호
    • /
    • pp.359-367
    • /
    • 2023
  • 본 실험에서는 포틀랜드 시멘트와 모래를 비소성 시멘트와 페로니켈슬래그로 대체 사용하여 친환경 시멘트 모르타르를 제작하였다. 페로니켈슬래그가 적용된 비소성 시멘트 모르타르의 강도 특성을 파악하기 위해 골재 종류와 양생방법을 구분하였다. 휨 및 압축강도 시험 결과, 페로니켈슬래그가 적용된 비소성 시멘트 모르타르의 강도는 Plain과 증기양생을 실시한 비소성 시멘트 모르타르의 강도보다 높았다. 이는 페로니켈슬래그의 입도, 밀도 및 흡수율 특성에 따른 강도 향상 효과로 판단된다. 모르타르의 XRD 분석 결과, 페로니켈슬래그에 포함된 MgO 성분이 복합 산화물 형태로 존재하며, 이를 통해 페로니켈슬래그가 적용된 비소성 시멘트 모르타르의 안정적인 강도 발현을 확인하였다.

고로슬래그미분말의 입도와 양생방법에 따른 모르터 물성에 관한 연구 (A Study on the Properties of Mortar With Particle Size of Blast Furnace Slag Powder and Curing Methods)

  • 김승진;박유진;조재우;김영근;김대영
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.191-194
    • /
    • 1999
  • Recently in Korea, may workers have reported the effects of the granulated blast furnace slag[BFS] of high fineness on the strength development of slag cement. We have studied the effect of slag fineness on the strength development of mortar with curing conditions, in order to get the basic data of high strength concrete using BFS. In this paper, we discussed the effects of slag fineness and porosity of mortar and the reaction of slag in hardened slag cement.

  • PDF

황산으로 중화시킨 액상레드머드 첨가 슬래그시멘트 모르타르의 특성 (Properties of Slag Cement Mortar with Liquid Red Mud Neutralized with Sulfuric Acid)

  • 김상진;강석표
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.123-124
    • /
    • 2022
  • In this paper, the characteristics of slag cement mortar added with neutralized liquid red mud with sulfuric acid and reduced pH were reviewed to improve the strength degradation of cement concrete added with liquid red mud. As a result, in the case of compressive strength up to 7 days, the strength of the cement mortar added with liquid red mud tends to increase compared to Plain. This shows that adding liquid red mud to cement mortar tends to increase the initial age strength, and the compressive strength on the 28th shows 74% of Plain when adding non-neutralized liquid red mud and 89% when adding sulfate neutralized red mud. Therefore, it is judged that the compression strength is improved by neutralizing the liquid red mud with sulfuric acid.

  • PDF

질산으로 중화시킨 액상레드머드 첨가 슬래그시멘트 모르타르의 특성 (Properties of Slag Cement Mortar with Liquid Red Mud Neutralized with Nitric Acid)

  • 김상진;강석표
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.165-166
    • /
    • 2022
  • In this paper, the characteristics of slag cement mortar added with neutralized liquid red mud with nitric acid to reduce pH by neutralizing liquid red mud with nitric acid were reviewed to improve strength degradation of cement concrete added with liquid red mud. As a result, the compressive strength of cement mortar added with liquid red mud was higher than that of Plain on 1 and 3 days, and the strength of red mud neutralized with nitric acid was lower than that of cement mortar added with liquid red mud on 7 days, but the strength was recovered on 28th. It was found that the addition of red mud has the effect of improving the strength in the early age.

  • PDF

고로슬래그 미분말 모르터에 시멘트 및 순환잔골재 치환율 변화에 따른 품질특성 (Effect of Partial Replacement with Cement and Recycled Fine Aggregate on Properties of Blast Furance Slag-Based Mortar)

  • 김영희;펑해동;손호정;이향재;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 추계 학술논문 발표대회
    • /
    • pp.215-216
    • /
    • 2011
  • This study investigates the effect of partial replacement with cement on the properties of blast furnace slag-based mortar. Recycled fine aggregate with various contents was used to activate the hydration of blast furnace slag in the mortar and compared its effect on strength development. Results showed that increasing cement and recycled fine aggregate increased the strength of mortar specimens. However, this study found that the mortar made with partial replacement of river sand with recycled fine aggregate of 20% developed a similar strength to the strength that cement with 10% can achieved.

  • PDF

알파반수석고 치환 고로슬래그 시멘트 모르타르의 경화특성 및 미세구조 분석 (Hardening Characteristics and Microstructure Analysis of Blast Furnace Slag-Cement Mortar Replaced Alpha-calcium Sulfate Hemihydrate)

  • 김경태;김규용;이보경;윤민호;이상규;서원우
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2017년도 춘계 학술논문 발표대회
    • /
    • pp.18-19
    • /
    • 2017
  • In this study, hardening characteristics and microstructure of blast furnace slag-cement mortar replaced alpha-calcium sulfate hemihydrate were analyzed. As a result of replacing alpha-calcium sulfate hemihydrate with 0, 10, 20, 30%, it was confirmed that the initial and final setting times are faster than that of blast furnace slag-cement mortar. The compressive strength of the specimens containing alpha-calcium sulfate hemihydrate decreased in the range of 42 ~ 76% at age 28 days compared with blast furnace slag-cement mortar. In the case of replacing the alpha-calcium sulfate hemihydrate, the shrinkage did not occur more rapidly than the cement mortar, but the slope of the strain curve showed a linear behavior. The results of scanning electron microscopy images analysis showed that the formation of ettringite was increased at alpha-calcium sulfate hemihydrate replaced mortar.

  • PDF

고로슬래그와 폴리카르본산계 유기 혼화제를 첨가한 Belite-rich Cement 모르타르 유동특성 (Rheology Properties of Belite-rich Cement Mortar Added Blastfurnace Slag and Polycarbonate-based Superplasticizer)

  • 송종택;송종택;조현태;황인수;박춘근
    • 한국세라믹학회지
    • /
    • 제37권2호
    • /
    • pp.145-151
    • /
    • 2000
  • In order to investigate the rheological properties of belite-rich cement(BRC) added polycarbonate-based superplasticizer and blastfurnace slags which have different blaines at 4500, 6000 and 8000$\textrm{cm}^2$/g, the change of minislumps and mortar slumps are measured with time. The rheological properties improve as specific surface area of added slag decreases or amount of polycarbonate-based superplasticizer increases. The slump loss can be controlled effectively by the steric hinderance effect of polycarbonate-based superplasticizer. According to the results, when mix proportion of the mortar is 1.5% mass content of superplasticizer and 30% mass addition of blastfurnace slag which blaine is 4500$\textrm{cm}^2$/g, the best mortar slump can be achieved without any significant segregation of materials.

  • PDF

비소성 시멘트 모르타르의 작업성 및 강도 개선을 위한 페로니켈슬래그 골재의 적용방안 (Application of Ferronickel Slag Aggregate to Improve Workability and Strength of Non-Sintered Cement Mortar)

  • 장경수;나형원;형원길
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2023년도 봄 학술논문 발표대회
    • /
    • pp.309-310
    • /
    • 2023
  • Slag and ash generally have a higher powder degree than portland cement, so workability may deteriorate under the same unit quantity condition, and strength and durability decrease when the unit quantity is increased. At this time, if an aggregate having a low water absorption and an appropriate particle size is used to recover the loss of strength, it can contribute to reducing the unit quantity of the binder. Therefore, for the purpose of improving the workability and strength of non-sintered cement mortar using slag and ash, ferro nikel slag whose particle size was adjusted was used as an aggregate and its applicability was identified. In this experimental condition, it was confirmed that non-sintered cement mortar tends to improve workability and secure strength when ferro nikel slag having various particle size distributions is used as an aggregate. This can be analyzed as the effect of ferro nikel slag material properties including glassy properties and mixing conditions with a wide particle size distribution.