• Title/Summary/Keyword: sinter-hardening

Search Result 13, Processing Time 0.023 seconds

Establishing CCT Diagrams for Sinter Hardening Grade Cr-Mo Prealloyed Steels

  • Stetina, G.;Kalss, G.;Gierl, C.;Danninger, H.;Orth, P.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.836-837
    • /
    • 2006
  • A CCT diagram for Cr-Mo prealloyed sintered steels suitable for sinter hardening was established by combining dilatometry data, microstructural studies and microhardness measurements of the material. CCT diagrams deepen the understanding of material properties after sinter hardening and support the design of materials on an industrial scale by providing information about required cooling rates for successful sinter hardening of these materials.

  • PDF

Joining of the Sinter Hardening Pully by Sinter Brazing

  • Cheng, Chao-Hsu;Lin, Yi-Ching;Lin, Yan-Cherng;Hwang, Lih-Ren
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1002-1003
    • /
    • 2006
  • This research mainly focuses on the development of sinter brazing technology for improving the process related to belt pulley made by sinter hardening. As the machine process of belt pulley takes up more than half of the total manufacturing hours, we propose changing the process to pulley groove brazed and bonded with pulley disc by applying sinter brazing to belt pulley. With the new process, the belt pulley is expected to reduce manufacturing cost to 70% of the original process by applying the sinter brazing technology; and the belt pulley bound by sinter brazing only loses 10% bonding strength compared with the original process.

  • PDF

Prediction of Martensite Fraction in the Sintering Hardening Process of Ni/Mo Alloy Powder (FLC-4608) Using the Finite Element Method (Ni/Mo 합금분말(FLC-4608)의 소결경화 공정에서 유한요소법을 이용한 마르텐사이트 분율의 예측)

  • Park, Hyo Wook;Joo, Soo-Hyun;Lee, Eon Sik;Kwon, Ki Hyuk;Kim, Hyong Seop
    • Journal of Powder Materials
    • /
    • v.22 no.1
    • /
    • pp.10-14
    • /
    • 2015
  • In recent years, industrial demands for superior mechanical properties of powder metallurgy steel components with low cost are rapidly growing. Sinter hardening that combines sintering and heat treatment in continuous one step is cost-effective. The cooling rate during the sinter hardening process dominates material microstructures, which finally determine the mechanical properties of the parts. This research establishes a numerical model of the relation between various cooling rates and microstructures in a sinter hardenable material. The evolution of a martensitic phase in the treated microstructure during end quench tests using various cooling media of water, oil, and air is predicted from the cooling rate, which is influenced by cooling conditions, using the finite element method simulations. The effects of the cooling condition on the microstructure of the sinter hardening material are found. The obtained limiting size of the sinter hardening part is helpful to design complicate shaped components.

Sinter-hardening Process of P/M Steels and its Recent Developments

  • Yi, Jianhong;Ye, Tuming;Peng, Yuandong;Xia, Qinglin;Wang, Hongzhong
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.303-304
    • /
    • 2006
  • The mechanical properties of ferrous powder metallurgy (P/M) materials are directly related to their microstructure. Ferrous P/M materials with sufficient hardenability will develop microstructures containing significant percentages of martensite in the as-sintered condition. Recently, sinter-hardening has developed into a highly cost effective production method through hardened P/M parts without the need for additional heat-treatments. This paper reviews the advances of sinter-hardening as well as some key processing parameters such as sintering temperature, cooling rate, tempering required to produce high quality sinter-hardened components. Specific topics including effect of alloying elements, alloying methods, and the Characterization and observation of microstructure are discussed.

  • PDF

Dimensional Precision in Sinter-hardening PM Steels

  • Lindsley, Bruce;Murphy, Thomas
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.407-408
    • /
    • 2006
  • Dimensional precision is a critical parameter in net shape processing of ferrous PM components. Sinter-hardening alloys undergo a transformation from austenite to martensite. Martensite formation expands the sintered compact, while tempering hardened steels results in shrinkage. In addition, martensitic regions with high Cu and C contents may contain large amounts of retained austenite. The presence of martensite and retained austenite, in addition to the tempering step, all play a role in the final dimensions of a component. This paper investigates the dimensional and microstructural changes to two sinter-hardening grades through different post-sintering thermal treatments.

  • PDF

The Application of P/M Advanced Techniques to Sintered Gears

  • Chongxi, Bao;Zhouqiang, Shen;Zhengping, Shu
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.987-988
    • /
    • 2006
  • The processes of P/M affect the properties of sintered gears. The different techniques of P/M lead to the different properties of sintered gears. This paper summarizes new progress in powder metallurgy for sintered gears. These progresses include warm compaction, high velocity compaction, sinter hardening, high temperature sintering, infiltration, CNC powder press and surface densification etc.

  • PDF

Green Machining of the Warm Compacted Sinter Hardenable Material

  • Cheng, Chao-Hsu;Chiu, Ken;Guo, Ray
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.295-296
    • /
    • 2006
  • High hardness of P/M parts can be obtained in the cooling section of the sintering furnace by using sinter hardenable materials, thus the post-sintering heat treatment can be eliminated. However, the sinter hardened materials would have difficulties in secondary machining if it is required, which will limit the applications of sinter hardenable materials in the machined parts. Recent development in warm compaction technology can enable us not only to achieve the high green density up to $7.4\;g/cm^3$, but also the high green strength which is needed for green machining. Therefore by using warm compaction technology, the green machining can be applied to sinter hardenable materials for the high density, strength and hardness P/M parts. In the present study, a pre-alloyed steel powder, ATOMET4601, was used by mixing with 2.0% copper, 1.0% nickel, 0.9% graphite and a proprietary lubricant using a binder treatment process - FLOMET. The specimens were compacted and green machined with different machining parameters. The machined surface finish and part integrity were evaluated in selecting the optimal conditions for green machining. The possibility of applying the green machining to the high-density structural parts was explored.

  • PDF

Densification Behavior of Ti-6Al-4V Powder Compacts at Room and High Temperatures (Ti-6Al-4V 분말 성형체의 상온 및 고온에서의 치밀화 거동)

  • Hong, Seung-Taek;Kim, Gi-Tae;Yang, Hun-Cheol
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.5 s.176
    • /
    • pp.1124-1132
    • /
    • 2000
  • Viscoplastic response and densification behaviors of Ti-6AI-4V powder compacts under uniaxial compression are studied at room and high temperatures with various initial relative densities and strain rates. The yield function and strain-hardening law proposed by Kim and co-workers were implemented into a finite element program (ABAQUS) to compare experimental data with finite element calculations for porous Ti6A14V powder compacts. Displacement-relative density, displacement-load relations and deformed geometry of Ti-A14V powder compacts were compared with finite element results. Density distributions in Ti-6AI-4V powder compacts were also measured and compared with finite element results.

The Effect of Cr and Mo Additions on the Improvement in Microstructural Homogeneity and Mechanical Properties of Ni-containing P/M Steels

  • Wu, Ming-Wei;Hwang, Kuen-Shyang;Huang, Hung-Shang
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.931-932
    • /
    • 2006
  • The microstructures of Ni-containing P/M steels produced by admixed powders or diffusion alloyed powders are usually heterogeneous. To improve the microstructure homogeneity, the effects of Mo and Cr additions in the prealloyed powder form were examined. The results showed that the microstructural homogeneity was improved and superior mechanical properties were achieved with increases in the alloy content, particularly for the Cr. Such a beneficial effect was attained due to the reduction of the repelling effect between Ni and C, as was demonstrated through thermodynamic analysis using the Thermo-Calc software.

  • PDF

Effect of Carbon Addition and Sintering Temperature on Densification and Microstructural Evolution of Sinter-Hardening Alloys Steels

  • Verma, N.;Anand, S.;Upadhyaya, A.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.557-558
    • /
    • 2006
  • In all conventional sintered PM products, the pores present are of two types, primary and secondary. Primary pores forming during compaction and latter during sintering, due to penetration of formed liquid through the matrix grain boundary. Effect of carbon addition on diffusion of Cu in SH737-2Cu system was investigated. After compaction and transient liquid phase sintering at $1120^{\circ}C$ and $1180^{\circ}C$, samples were characterized for densification, showing rise in sintering density and reduction in swelling on carbon addition. Quantitative microstructural characterization (shape factor and pore size) revealed bimodal distribution for 0% carbon, more rounded pores for 0.9% carbon and higher sintering temperature, and pore coarsening at higher sintering temperature.

  • PDF