Application of silk composite to decorative laminate

  • Kimura, Teruo;Aoki, Shinpei
    • Advanced Composite Materials
    • /
    • 제16권4호
    • /
    • pp.349-360
    • /
    • 2007
  • Recently, natural fiber reinforced composite is attracting attention and considered as an environmentally friendly material. Usually cellulosic fibers are used to reinforce the composites, but some protein fibers such as silk and wool serve the same purpose. In this paper, we proposed a method of producing artistic composite from artistic fabric by using silk fiber reinforced biodegradable plastic, which is designated as 'silk composite', for reinforcement. In order to expand applications of the silk composite, we performed the compression molding of decorative laminates with woody material, which was selected as a core material, and examined the properties of molded decorative laminates with various content of the silk composite. Since plywood and medium-density fiberboard (MDF) are widely used for decorative laminates, we selected them as core materials. As a result, flexible decorative laminates with high flexural strength were obtained by compounding the silk composite with wood materials.

모시/실크 교직물의 제작과 표백 (Weaving and Bleaching of Ramie/Silk Mixture Fabrics)

  • 김영대;권해용;이용우;우순옥
    • 한국잠사곤충학회지
    • /
    • 제41권3호
    • /
    • pp.222-227
    • /
    • 1999
  • The weavability and bleaching of ramie/silk mixture fabrics were examined. When silk fiber was used as warp or weft in the mixture fabrics, the weaving properties became higher than that of ramile fabrics. Especially, the highest weavabiliy of mixture fabrics was obtained when used as warp silk fiber. The whiteness of ramie and tussah fiber treated with hydrogen peroxide, bleaching agent. was increased up to about 80% without significant changes of tenacity and elongation. As the increase of bleaching agent and treatment time, the whiteness of mixture fabrics was increased and the yellowness was decreased. Also, as the whiteness of mixture fabrics increased, the drape stiffness in warp direction was decreased but crease recovery was increased.

  • PDF

수용성 고분자를 이용한 견의 염색 (Effects of the Addition of Water-soluble Polymers on Silk Dyeing)

  • 황은경;김문식;이동수
    • 한국잠사곤충학회지
    • /
    • 제40권2호
    • /
    • pp.136-142
    • /
    • 1998
  • The low-pollution dyeing condition and dyeing method suitable for the silk fiber were investigated. Instead of surfactants, water-soluble polymers and electrolytes were added as auxiliary agents in the new process of dyeing. By the new method, the level dyeing and sufficient exhaustion were achieved. The K/S values of silk fabrics were little different among electrolytes added in the dye-bath.

  • PDF

견/Polyester 혼방직물의 염색에 관한 연구 (A Study on the Dyeing Method of Silk/Polyester Blend Fabrics)

  • Park, Hyun-Tea;Song, Mi-Kyoung;Kim, Gong-Ju
    • 한국염색가공학회지
    • /
    • 제3권2호
    • /
    • pp.16-24
    • /
    • 1991
  • The textile fabric have the functions of sanitation, decoration, wearing style and washing in the practical use. Among various texitle fiber, silk has less utilities than synthetic fiber in practical use although silk has good benefits of the high quality. Thus no textile fiber, neither natural nor synthetic, has all the functions. In this sence, many blend yarns have been improved various functions of fabric. However, this has been disturbed with the problem of dyeing, especially in the case of blend fabric of silk. In this study, we dyed silk/PET blend fabric in one step useing one bath dyeing method by acid dyes/disperse dyes. The results of the experiments can be summarized as follows; 1) Yellow index of silk fabric treated at $130^{\circ}C$ increased about 7.8 (color difference 4.5 NBS) and whiteness decrease about 5%. 2) Both elongation and tensile strength of silk fabric treated at $130^{\circ}C$ of pH 5-6 decreased about 10% and tensile strength of silk spun yarn treated at $60^{\circ}C$ of pH 10 have little changed. 3) While silk/PET blend frbric dyeing, silk soiling of disperse dyes causes from difference of dyeing rate and degree of silk soiling with dyes. 4) Fastness and soiling of silk/PET blend fabric dyed by one bath dyeing method of acid dyes/disperse dyes was same as two bath dyeing method.

  • PDF

폐견사류의 미세분말화 및 표면 가공제 적용 (Preparation of Fine Silk Powder and It′s Application for Surface Modification)

  • 이용우;이광길;여주홍;김종호
    • 한국잠사곤충학회지
    • /
    • 제43권1호
    • /
    • pp.41-48
    • /
    • 2001
  • The purification, dissolution and powdering of stained waste silk obtained from weaving and dyeing process were studied for the surface modification of textile fabric and plastic materials. The whiteness of stained waste silk could be improved through degumming and bleaching with sodium hydrosulfite. The water-soluble fibroin solution can be obtained by dissoving the degummed waste silk in a boiling solution of 50% calcium chloride for 60 minutes. The salts and heavy metals contained in fibroin solution were removed by electric dialysis, wool fiber filtration and gel filtration chromatography. The fibroin powder was prepared by using a fine grinder after the alkali treatment for weakening the silk fiber. The fine fibroin powder of particle size around 30 ㎛ was obtained with a ultra fine-mill, while it was finer below 10 ㎛ with a ball-mill. The dissolved or powdered silk was applied to the surface of fabric with addition of the binder (a urethane resin). The moisture content of polyester and nylon fabrics treated with the silk solution was improved due to hygroscopic property of silk. The fine fibroin powder mixed with the binder ws coated on the surface of synthetic film by use of the air pressed sprayer. It was revealed that the hygroscopicity as well as the softness of fibroin powder coated film was much improved. Therefore, it is thought that the fine silk fibroin powder is applicable as an coating agent for the surface modification of plastic and synthetic leather.

  • PDF

The Effect of Dissolution Condition on the Yield, Molecular Weight, and Wet- and Electro-spinnability of Regenerated Silk Fibroins Prepared by LiBr Aqueous Solution

  • Cho, Hee-Jung;Um, In-Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • 제20권2호
    • /
    • pp.99-105
    • /
    • 2010
  • In this paper, the regenerated silk fibroins were dissolved in LiBr aqueous solution with different dissolution temperature and time, and the effects of the dissolution condition on the regeneration yield, molecular weight, wet spinnability, and electrospinnability of regenerated silk fibroin were investigated. The regeneration yield, molecular weight distribution, and wet spinnability of regenerated silk fibroin were nearly affected by the dissolution temperature and time. However, the electrospinning performance of silk fibroin was influenced by the dissolution condition implying the electrospinning of silk fibroin is more sensitive process than the wet spinning in the range tested in this study. While $25^{\circ}C$ of dissolution temperature resulted in a good electrospinnability of regenerated silk fibroin, the electrospinnability was slightly deteriorated when silk fibroin was dissolved at $60^{\circ}C$ for 6 hours. Also, though the fiber diameters of electrospun silk fibroin produced by the dissolution at $25^{\circ}C$ for 6 hours and 24 hours were 443 and 451 nm, respectively, that at $60^{\circ}C$ for 5 min was reduced to 411 nm. The fiber diameter was more decreased to 393 nm when the dissolution time increased up to 6 hours at $60^{\circ}C$.

새로운 천연염재로서 메타쉐콰이어 열매의 활용(2) : 견섬유의 염색성과 항균성을 중심으로 (Utilization of Metasequoia(Metasequoia glyptostroboides) Cone as a New Natural Dye Resource(2): Dyeing Properties and Antimicrobial Functionality of Silk Fiber)

  • 염준;류동일;신윤숙
    • 한국염색가공학회지
    • /
    • 제27권4호
    • /
    • pp.281-287
    • /
    • 2015
  • The aim of this study was to investigate the possibility utilizing Metasequoia(Metasequoia glyptostroboides) cone as a new natural dye resource. In previous study, dyeing onto cotton fiber was carried out and Metasequoia cone colorant showed low affinity to cotton fiber and maximum dye uptake was obtained at pH 3.5 showing YR Munsell color. For further evaluation of its efficacy as a new natural dye resource, effects of dyeing conditions and mordanting on dye uptake, color change, and colorfastness were investigated for silk fiber. Metasequoia cone colorant showed good affinity toward silk fiber showing YR Munsell color and maximum dye uptake was shown at pH 3.5. Post-mordanting with Cu and Fe improved dye uptake, especially Fe($C_5H_{10}FeO_6$) mordant was effective as much as 2 times higher dye uptake comparing with un-mordanted sample. The color of dyed fabrics with mordanting showed YR Munsell color. Fe mordanted fabrics appeared dark gray~black color. Colorfastness to washing was relatively good, whereas lightfastness of the dyed fabrics showed grade 2. It was confirmed that Metasequoia cone colorant can be used as a new dye resource for silk fiber getting brownish yellow to dark gray/black color depending on mordant type. In addition, it showed antimicrobial functionality.

Doxyclycline and Ciprofloxacin Treatment of Silk to Produce Novel Infection Resistance Biomaterials

  • Park, Hyung-Min;Martin Bide;Matthew Phaneuf;William Quist;Frank Logerfo
    • 한국섬유공학회:학술대회논문집
    • /
    • 한국섬유공학회 2003년도 The Korea-Japan Joint Symposium
    • /
    • pp.81-82
    • /
    • 2003
  • Two antibiotics, doxycycline (doxy) and ciprofloxacin (cipro) were applied under a variety of conditions to silk, and to silk that had previously been hydrolyzed. FTIR-ATR analyses indicated that the drastic increase in sorption of antibiotics by hydrolyzed silk was attributable to both chemical and conformational changes that occurred on hydrolysis. A high sorption of doxy by hydrolyzed silk did not necessarily give a more infection-resistant material as determined by a zone of inhibition test. Conversely, the same hydrolysis considerably increased both sorption of cipro and zone of inhibition of cipro-treated silk dyed at 65$^{\circ}C$ and 85$^{\circ}C$.

  • PDF

Relationships between Antithrombogenicity and Surface Free Energy of Regenerated Silk Fibroin Films

  • Park, Won Ho;Ha, Wan Shik;Ito, Hiraku;Miyamoto, Takeaki;Inagaki, Hiroshi;Noishiki, Yasuharu
    • Fibers and Polymers
    • /
    • 제2권2호
    • /
    • pp.58-63
    • /
    • 2001
  • Silk fibroin (SF) was dissolved in calcium chloride/ethanol/water mixture(1/2/8 in mole ratio) at $70^{\circ}C$ for 4h. The dissolved silk fibroin was regenerated by casting the dialyzed solution into films. The films were treated with 50% aqueous solution of methanol for different times, and their antithrombogenicity was evaluated by in vivo tests. In vivo blood tests were made by a method of peripheral vein indwelling suture. It was found that the silk fibroin had a good antithrombogenicity and an absorbability even though the polymer showed foreign body reaction. Finally, the blood compatibilty of silk fibroin films which were subjected to structural change by the methoanl treatment, was examined in connection with their interfacial surface energy, and a correlation between these properties was found to be present.