This paper describes the effect of fly ash replacement on the setting time of antiwashout underwater concrete, where cement was replaced by 0% to 50%. Experimental work was performed on the condition of sea water and in air to find out the characteristics of setting time between the concretes that were cast in air and cast in 15$^{\circ}C$ of sea water. The experimental results show that the setting time of underwater concrete with 50% replacement was delayed about 10 hours than normal concrete. And it can be concluded that, at the case of underseawater concrete addicted with fly ash, the delayed final setting times are shown as the function Tf=0.069F+7.69, where Tf is the delayed final setting time and F is quantity of fly ash, respectively. These results confirm that the setting time underseawater concrete could be prolonged.
Jeon Chung Keun;Kim Jong;Han Min Cheol;Shin Dong An;Oh Sean Kyo;Han Chean Goo
Proceedings of the Korea Concrete Institute Conference
/
2005.11a
/
pp.643-646
/
2005
This paper reports the influence of super retarding agent(SRA) on the setting time of concrete incorporating mineral admixture including fly ash(FA), expansive additive(EA), silica fume(SF), blast furnace slag(BS) and blast furnace slag along with fly ash(BS+FA). An increase in SRA resulted in retarding the setting time of control concrete, while the use of mineral admixture led to a delay of setting time markedly, compared with that of control concrete under no SRA content. Meanwhile, An increase in SRA in concrete with mineral admixture exhibited comparable setting delay with control concrete. Furthermore, in case of the use of BS and SF, acceleration of setting time was observed with increase of SRA content. It is considered that proper dosage of SRA of concrete with SF and BS to secure similar setting delay with control concrete require rather larger than that of control concrete. Accordingly, For concrete with mineral admixture, in order to decide the proper dosage of SRA, application of correction factors is needed.
Proceedings of the Korea Concrete Institute Conference
/
2001.11a
/
pp.935-938
/
2001
This paper reports the relation of concrete setting characteristic and lateral pressure in mass concrete wall such as side wall of LNG underground storage tank. In order to estimate the lateral pressure, initial setting time of low heat cement concrete with type of mineral admixture was measured for three concrete mixtures(W/P=41.6%) containing limestone powder, fly ash, and slag powder. As a result, the lateral pressure of the concrete containing limestone powder was the smallest than those of other concretes as well as the initial setting time.
Journal of the Korea Institute of Building Construction
/
v.8
no.3
/
pp.111-117
/
2008
This study provides the setting time prediction method of super retarding concrete incorporating mineral admixtures at the same time including fly ash(FA), blast furnace slag(BS) based on maturity method. The setting time was retarded, as super retarding agent contents increase and curing temperature decreases. In addition, apparent activation energy by Arrhenius function was ranged from $24{\sim}35KJ/mol$ with slightly difference along with mixture proportion. This value is smaller than existing value $30{\sim}50KJ/mol$. It is Indicated that equivalent age using setting time can be a proper method to predict setting time and it also exhibited comparable relativity between prediction value and measurement value. Therefore, this study provided setting time prediction value with super retarding agent contents and mineral admixture combination. Setting time prediction equation provided herein is possibly valid for estimating precise setting time of the super retarding concrete at the job site.
Proceedings of the Korean Institute of Building Construction Conference
/
2003.05a
/
pp.95-98
/
2003
This paper presents the results of field experiment to apply the difference of setting tine method using super retarding agent for reducing hydration heat of mass concrete of foundation. According to the results, as the properties of fresh concrete, base concrete satisfies aimed slump and air content, and there is no difference of slump and air content with mixture of super retarding agent. The mixing ratio of super retarding agent is determined for setting time to be retarded by 12 hours in comparison with base concrete, but because the temperature of the air and concrete is low, the difference of setting time is retarded to 24 hours. In man concrete of foundation to which the difference of setting time method is applied, crack by hydration heat is not seen because the lower concrete of super retarding agent generates heat after generation of hydration heat of the upper concrete.
Proceedings of the Korea Concrete Institute Conference
/
1998.04b
/
pp.707-711
/
1998
Ultrasonic test usually was used for defect detection, crack depth measurements and strength estimation of hardened concrete. The essence of the pulse velocity method is that the transition time of an ultrasonic longitudinal pulse is measured in concrete. Ultrasonic velocity was propagated to the age of concrete, made a radical change at that time when concrete was setted. This study which monitored the change in a concrete by ultrasonic test was performed to estimate initial setting and final setting.
Setting time of cement-based materials can represent a developing strength in early-age mixture, and it can be used a significant parameter of high-performance concrete having various mix-proportions. Generally, initial and final setting time of concrete is measured by penetration resistance method that used a wet-sieving mortar mixture, therefore, it hardly represents the setting time of sound concrete including coarse aggregate. Recently, several nondestructive methods, such as ultrasonic velocity and impendence measurement, are proposed to evaluate the setting time of fresh concrete. This study attempts to measure an electrical resistivity using four-electrode method for evaluation of setting time in early-age cement-based materials. For this purpose, total 10 mixtures are prepared as different mix-proportions including chemical admixture. Based on the experimental results, two electrical parameters, such as initial electrical resistivity and rising time, are proposed to reflect a microstructure development by hydration of cement-based materials. As a result, proposed parameter is also discussed with the measured setting time by penetration resistance method.
Proceedings of the Korea Concrete Institute Conference
/
2005.11a
/
pp.707-710
/
2005
This experimental study investigate temperature dependency affecting setting and strength development of concrete using mineral admixtures such as CKD, FA and BS. For the properties of setting at $5^{\circ}C$, setting time of concrete with mineral admixture was delayed about $3\~14$ hour compared with that of plain concrete. Use of CKD had a desirable effect on reducing setting retard under $5^{\circ}C$ because of $CaCO_3$ of CKD while use of FA and BS retarded setting time greatly. For compressive strength under $5^{\circ}C$, concrete with CKD had the most compressive strength in early age compared with the other mineral admixtures but exhibited slight strength loss in $-5^{\circ}C$ at 28days. Especially, concrete with FA and BS was observed in early stage at low curing temperature because of strength loss remarkably in $-5^{\circ}C$.
Journal of the Korea Institute of Building Construction
/
v.9
no.3
/
pp.95-101
/
2009
Constructing large-scale mat foundation mass concrete is increasing for the stability of building structure, because a lot of high rise building are being built in order to make full use of limited space. However, It is of increasing concerns that because limited placing equipments, available job-site and systems for mass concete placement in construction field do not allow to place great quantity of concrete at the same time in large scale mat foundation, consistency between placement lift can not be secured. And also, it is likely to crack due to stress caused by the difference of hydration heat generation time. To find out the solution against above problems, this study is to reconfirm the performance of normal concrete designed by mix proportion and super retarding concrete. The Fundamental test shows what happens if low heat proportioning and control method of setting time are applied at the job-site of newly constructed high rise building. The test result show that slump flow of concrete has been somewhat increased as the target retarding time gets longer, while the air content has been slightly decreased but this is no great difference from normal concrete. The setting time shows to be retarded as target retarding time gets longer, the range of retarding time increases. It is necessary to increase the amount of mix of super retarding agent in the proportion ration by setting curing temperature high since outdoor curing is about 6 hours faster than standard curing, which means the temperature of the concrete will be higher than the temperature of the surrounding environment, due to its high hydration heat when applying in a construction site. The compressive strength of super retarding concrete appears to be lower than normal concrete due to the retarding action in the early stage. However, as the time goes by, the compressive strength gets higher, and by the 28th day the strength becomes the same or higher than normal concrete.
Kim Jong;Song Seung Heon;Jeon Chung Keun;Han Min Cheol;Oh Seon kyo;Han Cheon Goo
Proceedings of the Korea Concrete Institute Conference
/
2004.11a
/
pp.505-508
/
2004
This paper investigated the setting and compressive strength of concrete with the combination of mineral and chemical admixture. According to test results, plain concrete with high early strength development type AE water reducing agent(HEAEWRA) and $10\%$ of CKD respectively had earlier setting time than concrete with AE water reducing agent by $0.5\~1.5$ hours. Setting time of concrete with retarding type AE water reducing agent(RAEWRA) and FA $30\%$, BS $60\%$ respectively retarded by as much as $4\~7.5$ hours compared with plain concrete. Plain concrete with HEA WRA, $10\%$ of CKD and RAEWRA had higher strength than that of AE water reducing agent by as much as 5MPa at 28days. From the result of the paper, it is found that the combination of mineral admixture and setting accelerating or retarding agent can reduce the hydration heat cracks by setting time difference and hydration heat reduction effects.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.