  • Most of cervical abrasion and erosion lesions show gingival margin where the cavosurface angle is on cementum or dentin. Composite resin restoration of cervical lesion shrink toward enamel margin due to polymerization contraction. This shrinkage has clinical problem such as microleakage and secondary caries. Several methods to diminish contraction stress of composite resin restoration, such as modifying cavity form and building up restorations in several increments have been attempted. The purpose of this study was to compare polymerization contraction stress of composite resin in Class V cavity subjected to cavity forms and placement methods. In this study, finite element model of 5 types of Class V cavity was developed on computer tomogram of maxillary central incisor. The types are : 1) Box cavity 2) Box cavity with incisal bevel 3) V shape cavity 4) V shape cavity with incisal bevel 5) Saucer shape cavity. The placement methods are 1) Incisal first oblique incremental curing 2) Bulk curing. An FEM based program for light activated polymerization is not available. For simulation of curing dynamics, time dependent transient thermal conduction analysis was conducted on each cavity and each placement method. For simulation of polymerization shrinkage, thermal stress analysis was performed with each cavity and each placement method. The time-temperature dependent volume shrinkage rate, elastic modulus, and Poisson's ratio were determined in thermal conduction data. The results were as follows : 1. With all five Class V cavifies, the highest Von Mises stress at the composite-tooth interface occurred at gingival margin. 2. With box cavity, V shape cavity and saucer cavity, Von Mises stress at gingival margin of V shape cavity was lower than the others. And that of box cavity was lower than that of saucer cavity. 3. Preparing bevel at incisal cavosurface margin decreased the rate of stress development in early polymerization stage. 4. Preparing bevel at incisal cavosurface margin of V shape cavity increased the Von Mises stress at gingival margin, but decreased at incisal margin. 5. At incisal margin, stress development by bulk curing method was rapid at early stage. Stress development by first increment of incremental curing method was also rapid but lower than that by bulk curing method, however after second increment curing final stress was the same for two placement methods. 6. At gingival margin, stress development by incremental curing method was suddenly rapid at early stage of second increment curing, but final stress was the same for two placement methods.

  • PDF

DENTAL TREATMENT OF A PATIENT WITH SWYER JAMES UNDER GENERAL ANESTHESIA: A CASE REPORT (Swyer James syndrome환아의 전신마취 하 치아우식 치료: 증례보고)

  • Sung, Young Jae;Song, Ji Soo;Hyun, Hong-Keun;Kim, Young-Jae;Kim, Jung-Wook;Jang, Ki-Taeg;Lee, Sang-Hoon;Shin, Teo Jeon
    • The Journal of Korea Assosiation for Disability and Oral Health
    • /
    • v.15 no.1
    • /
    • pp.60-64
    • /
    • 2019
  • Swyer-James syndrome (SJS), also known as Swyer-James-MacLeod syndrome and unilateral hyperlucent lung syndrome, is rare acquired pulmonary disorder develops secondary to infectious etiologies in early childhood. Viral respiratory infection such as adenoviruses or Mycoplasma pneumoniae in infancy or early childhood rarely cause Swyer-James syndrome. It is generally characterized on radiographs by a unilateral small lung with hyperlucency and air trapping on expiration. In many cases unaffected lung tissue functions normally, compensating for affected lung portion. Preoperative assessment is needed to determinate individual's pulmonary function. A 4-year-old boy with Swyer-James syndrome visited Seoul National University Dental Hospital Department of pediatric dentistry for caries treatment. Clinical and radiographic examinations revealed multiple carious lesions on deciduous teeth. Considering patient's underling disease, age, and level of cooperation, dental treatment under general anesthesia was scheduled. Dental treatment was done with composite resin and stainless-steel crown. Since ventilation of Swyer-James syndrome patients was diminished because of airway obstruction, close monitoring of ventilation is necessary during dental treatment. Considering pulmonary pathology, general anesthesia rather than sedation is recommended when special behavior management is required for dental treatment. Swyer-James syndrome patients can tolerate general anesthesia and surgery well, according to several reports.

A STUDY ON MICROLEAKAGE OF SEALED AMALGAM RESTORATION (Sealed amalgam restoration의 미세누출에 관한 연구)

  • Lee, Sang-Heon;Lee, Jae-Cheoun;Lee, Sang-Hoon
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.27 no.1
    • /
    • pp.54-61
    • /
    • 2000
  • Amalgam, though a widely used dental material, does not bond to the tooth substrate Therefore, retentive preparation of the cavity is necessary. Such amalgam restorations, until corrosion products form and plug the margin, will show significant marginal leakage. Unless this is prevented early on, saliva and bacteria may enter the cavity causing postoperative hypersensitivity, dissolution and collapse of the restoration, discoloration of the margin and secondary caries, leading to shortened life-span of the restoration and pulpal pathosis. Recently, a method of restoration has been introduced whereby tooth material can be preserved, cavity margin can be sealed and preventive treatment of pit and fissure can be administered while retaining all the advantages of conventional amalgam restorations. Such sealed amalgams involve removing the carious lesion without extending the cavity for prevention and using pit and fissure sealants to seal cavity margins and pit and fissures to reduce microleakage. In this study, finishing of the amalgam and sealant application were performed after different intervals following of amalgam restoration to compare the microleakage of sealed and conventional amalgam restorations. Thirty bicuspids were prepared with Class V cavity preparations on the buccal and lingual surfaces. After amalgam placement, they were divided into the following groups and treated accordingly. Group 1 : Polishing after 24 hours Group 2 : Immediate sealant application without polishing Group 3 : No polishing, but sealant applied after thermocycling 500 times After treatment, the samples were thermocycled 500 times between $5^{\circ}C$ and $55^{\circ}C$ with a dwell time of 30 seconds. After thermocycling, the samples were dipped into 1% methylene blue kept in a $37^{\circ}C$ incubator at 100% humidity for 24 hours. The teeth were then embedded in resin and cut bucco-lingually along the tooth axis and observed with a stereomicroscope to determine the degree of microleakage, The following results were obtained : 1. Group 2 showed the least microleakeage, while group 1 showed the greatest. 2. Group 1 showed significantly greater microleakage compared to group 2 (p<0.05). However, no significant differences were found between group 1 and 3(p>0.05). No significant differences in microleakage were also found between cup 2 and 3(p<0.05).

  • PDF

A Study on Oral Symptoms and Oral Health Behavior among Secondary Students (S중, 고등학생의 구강검진에 따른 구강 증상 및 구강건강행태 조사)

  • Hong, Min-Hee;Jeong, Mi-As
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.11 no.4
    • /
    • pp.1534-1539
    • /
    • 2010
  • This study carried out dental checkup targeting 251 students in the 1st grade of S middle school and 220 students in the 1st grade of S high school in Seoul Metropolis. The results are as follows. As for the experience of dental hypersensitivity to oral symptoms in middle-and-high school students, 23.2% of high school students had experience of painful tooth when drinking or eating cold and hot beverage or food, compared to 14.3% of middle school students, and showed significant difference($\chi^2=6.08$, p<.05). As for the experience of painful teeth, 9.1% of high school students had experience of being sore, aching, and painful in the teeth, compared to 4.4% of middle school students, and showed significant difference($\chi^2=4.23$, p<.05). As a result of the oral health behavior in middle-and-high school students, 48.6% of middle school students were indicated to be higher than 26.4% of high school students in the experience of having ever gone to dentist for the past 1 year, and showed statistically significant difference($\chi^2=24.56$, p<.001). As for the period of toothbrushing during one day, 68.5% of middle school students brushed teeth after having breakfast($\chi^2=6.39$, p<.05) more than 57.3% of high school students. After having lunch, 16.8% of high school students brushed teeth more than 7.2% of middle school students, and showed statistically significant difference($\chi^2=10.58$, p<.01). As a result of judging dental checkup in middle-and-high school students, 44.1% of high school students had dental caries($\chi^2=25.36$, p<.001) more than 22.3% of middle school students. 9.6% of middle school students had tooth loss more than 4.1% of high school students, and showed statistically significant difference($\chi^2=5.39$, p<.05).

PROPERTIES OF LIGHT-CURED COMPOSITE RESINS CONTAINING $SrF_2$, GLASS FILLER ($SrF_2$계 충진재를 함유한 광중합형 복합레진의 특성)

  • Kim, Hee-Jung;Kim, Kyung-Nam;Choi, Byung-Jai;Lee, Jong-Gap
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.28 no.1
    • /
    • pp.54-66
    • /
    • 2001
  • The aim of this study was to investigate the fluoride release and some mechanical properties including 3-point bending strength, amount of abrasion, surface hardness, water sorption/solubility and cytotoxicity of the newly developed composite resins containing 8, 16, 24 wt% $SrF_2$ glass filler (VF8, VF16, VF24) and four commercially available composite resins, Heliomolar(HE), Verdonfil(VE), Z100(ZH) and Aelitefil(AE). To investigate cytotoxic effect, agar overlay assay was done. Amount of fluoride released into distilled water was measured over a 62-days period from VF8, VF16, VF24 and HE. Results were as follows: 1. Experimental composite resins showed similar mechanical properties to commercial composite resins, but 3-point bending strength and surface hardness of experimental composite resins were inferior to ZH. 2. Over a 62-day Period, the amount of fluoride released was ordered: VF24>VF16>VF8>HE. In experimental composite resins, the amount of fluoride released was 9-23 times greater than HE and seemed to be proportional to the content of $SrF_2$ glass filler. 3. Experimental composite resins and all control composite resins showed mild cytotoxicity. This study showed significantly greater fluoride release from newly developed composite resins than control(HE) and addition of $SrF_2$ glass filler did not decrease mechanical properties or increase cytotoxicity of composite resin. The results from this study imply that newly developed composite resin have adequate mechanical properites, mild cytotoxicity and some potential for secondary caries prevention.

  • PDF

Comparison of marginal fit before and after porcelain build-up of two kinds of CAD/CAM zirconia all-ceramic restorations (두 종류의 CAD/CAM 지르코니아 전부도재관의 도재 축성 전후의 변연적합도 비교)

  • Shin, Ho-Sik;Kim, Seok-Gyu
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.46 no.5
    • /
    • pp.528-534
    • /
    • 2008
  • Purpose: Marginal fit is one of the important components for the successful prosthodontic restoration. Poor fitting margin of the restoration causes hypersensitivity, secondary caries, and plaque accumulation, which later result in prosthodontic failure. CAD/CAM zirconia all-ceramic restorations, such as $LAVA^{(R)}$ (3M ESPE, St.Paul, MN) and $EVEREST^{(R)}$ (KaVo Dental GmbH, Biberach, Germany) systems were recently introduced in Korea. It is clinically meaningful to evaluate the changes of the marginal fit of the CAD/CAM zirconia systems before and after build-up. The purposes of this study are to compare the marginal fit of the two CAD/CAM all-ceramic systems with that of the ceramometal restoration, before and after porcelain build-up Material and methods: A maxillary first premolar dentiform tooth was prepared with 2.0 mm occlusal reduction, 1.0 mm axial reduction, chamfer margin, and 6 degree taperness in the axial wall. The prepared dentiform die was duplicated into the metal abutment die. The metal die was placed in the dental study model, and the full arch impressions of the model were made. Twenty four copings of 3 groups which were $LAVA^{(R)}$, $EVEREST^{(R)}$, and ceramometal restorations were fabricated. Each coping was cemented on the metal die with color-mixed Fit-checker $II^{(R)}$ (GC Cor., Tokyo, Japan). The marginal opening of each coping was measured with $Microhiscope^{(R)}$ system (HIROX KH-1000 ING-Plus, Seoul, Korea. X300 magnification). After porcelain build-up, the marginal openings of $LAVA^{(R)}$, $EVEREST^{(R)}$,and ceramometal restorations were also evaluated in the same method. Statistical analysis was done with paired t-test and one-way ANOVA test. Results: In coping states, the mean marginal opening for $EVEREST^{(R)}$ restorations was $52.00{\pm}11.94\;{\mu}m$ for $LAVA^{(R)}$ restorations $56.97{\pm}10.00\;{\mu}m$, and for ceramometal restorations $97.38{\pm}18.54\;{\mu}m$. After porcelain build-up, the mean marginal opening for $EVEREST^{(R)}$ restorations was $61.69{\pm}19.33\;{\mu}m$, for $LAVA^{(R)}$ restorations $70.81{\pm}12.99\;{\mu}m$, and for ceramometal restorations $1115.25{\pm}23.86\;{\mu}m$. Conclusion: 1. $LAVA^{(R)}$ and $EVEREST^{(R)}$ restorations in comparison with ceramometal restorations showed better marginal fit, which had significant differences (P < 0.05) in coping state and also after porcelain build-up . 2. The mean marginal opening values between $LAVA^{(R)}$ and $EVEREST^{(R)}$ restorations did not showed significant differences after porcelain build-up as well as in coping state (P > .05). 3. $EVEREST^{(R)}$, $LAVA^{(R)}$ and ceramometal restorations showed a little increased marginal opening after porcelain build-up, but did not show any statistical significance (P > .05).