Analytical study on nickel content in ceramic, metal and plastic materials (세라믹, 금속 및 플라스틱 소재의 니켈 함유량 분석에 관한 연구)

  • Choi, Zel-Ho
    • Analytical Science and Technology
    • /
    • v.24 no.6
    • /
    • pp.443-450
    • /
    • 2011
  • Quantitative analytical condition for nickel in ceramic, metal and plastic materials using complexation and solvent extraction followed by inductively coupled plasma-atomic emission spectrometry (ICP-AES) and atomic absorption spectrophotometry (AAS) was studied. Ceramic, metal and plastic samples were dissolved by acid digestion. Nickel was determined by ICP-AES and AAS after extraction of Ni $(DMG)_2$ in $CHCl_3$. Recovery efficiency of nickel was satisfactory, and most of matrix elements causing interference could be effectively eliminated by the separation. Nickel in the certified reference materials (BAM-376 and PACS-2) were quantitatively determined without influence of sample matrix.

Low-grade waste heat recovery and repurposing to reduce the load on cooling towers

  • McLean, Shannon H.;Chenier, Jeff;Muinonen, Sari;Laamanen, Corey A.;Scott, John A.
    • Advances in Energy Research
    • /
    • v.7 no.2
    • /
    • pp.147-166
    • /
    • 2020
  • Industrial cooling towers are often ageing infrastructure that is expensive to maintain and operate. A novel approach is introduced in which a heat pump circuit is incorporated to reduce the load upon the towers by extracting low-grade energy from the stream sent to the towers and repurposing in on-site processing operations. To demonstrate the concept, a model was constructed, which uses industrial data on cooling towers linked to a smelter's sulphuric acid plant, to allow direct economic and environmental impact comparison between different heat recovery and repurposing scenarios. The model's results showed that implementing a heat pump system would significantly decrease annual operating costs and achieve a payback period of 3 years. In addition, overall CO2 emissions could be reduced by 42% (430,000 kg/year) and a 5% heat load reduction on the cooling towers achieved. The concept is significant as the outcomes introduce a new way for energy intensive industrial sectors, such as mineral processing, to reduce energy consumption and improve long-term sustainable performance.

Highly Selective Derivative Spectrophotometry for Determination of Nickel Using 1-(2-Pyridylazo)-2-naphthol in Tween 80 Micellar Solutions

  • Eskandari, Habibollah
    • Bulletin of the Korean Chemical Society
    • /
    • v.25 no.8
    • /
    • pp.1137-1142
    • /
    • 2004
  • A spectrophotometric and first derivative spectrophotometric method was developed in aquatic Tween 80 micellar solutions for selective determination of nickel without using any pre-separation step. 1-(2-Pyridylazo)-2-naphthol (PAN), as a sensitive chromogenic complexing agent formed a red-colored Ni(II)-PAN complex in Tween 80 media with satisfactory solubility and stability. Conditions such as pH, PAN concentration, type and concentration of micellizing agent were optimized. Molar absorptivity of Ni-PAN complex was found $4.62\;{\times}\;10^4L\;cm^{?1}\;mol^{?1}$ at 569 nm, under the optimum condition. Calibration graphs were derived by zero, first and second derivative spectrophotometry at maximum wavelengths of 569, 578 and 571 nm with linear ranges of 30-1800, 20-2500 and 30-2000 ng $mL^{?1}$ , respectively. Precision as standard deviation as well as accuracy as recovery percent were in the range of 1-20 ng $mL^{?1}$, and 93.3-103.3%, respectively, for the entire of the linear ranges. Spectrophotometric detection limit was 3 ng $mL^{?1}$ and effects of diverse ions on the first derivative determination of nickel were studied to investigate selectivity of the method. Interferences of cobalt and copper on the nickel determination were prevented using o-phenanthroline as masking agent. The recommended procedures were applied to the various synthetic and stainless steel alloys, tea leaves and human hair, with satisfactory results.

Recovery of nickel from the spent nickel-cadmium battery (폐 Ni-Cd 전지로부터 니켈의 회수)

  • 박제신;박경호;전호석;손정수;김병규
    • Resources Recycling
    • /
    • v.8 no.5
    • /
    • pp.28-33
    • /
    • 1999
  • Trus paper presenls a hydrometallurgical process Tor recovcnng ~uckcals mckcl sulfate fiom the spent nickel-cadrnlum bauery in whch c:,dmi~lm war re~novcdb y vapowing m e h d in vacuum. F ~ s ts,e lcct~vcc rushing and classification mell~odw ere performed to separate iron physically and the nickel-rich sample (over 80% nickel) was obtained. Ths sarnple was dissolved in sulf~ uiuica cid to obtain a luckcl sulfatc soluho~d~o se to its seluradon painl. TIE Cree acid in the unpurificd nickcl solut~onw as neutl-dized and iron war ve~novedk om the solulmn Thc mckel sulhte solution was c~yst~llizeadt around 45'C to obtain ruckel sulfate henahyril-ate.

  • PDF

Enhanced extraction of copper and nickel based on the Egyptian Abu Swayeil copper ore

  • Somia T. Mohamed;Abeer A. Emam;Wael M. Fathy;Amany R. Salem;Amr B. ElDeeb
    • Analytical Science and Technology
    • /
    • v.37 no.1
    • /
    • pp.63-78
    • /
    • 2024
  • The continuous increasing of the global demand of copper and nickel metals raises the interest in developing alternative technologies to produce them from copper sulfide ore. Also, in line with Egypt's vision 2030 for achieving the sustainable socioeconomic development which aims at developing alternative and eco-friendly technologies for processing the Egyptian ores to produce these strategic products instead of its importing. These metals enhance the advanced electrical and electronic industries. The current work aims at investigating the recovery of copper and nickel from Abu Swayeil copper ore using pug leaching technique by sulfuric acid. The factors affecting the pug leaching process including the sulfuric acid concentration, leaching time and temperature have been investigated. The copper ore sample was characterized chemically using X-ray fluorescence (XRF) and scanning electron microscope (SEM-EDX). A response surface methodology develops a quadratic model that expects the nickel and copper leaching effectiveness as a function of three controlling factors involved in the procedure of leaching was also investigated. The obtained results showed that the maximum dissolution efficiency of Ni and Cu are 99.06 % and 95.30%, respectively which was obtained at the following conditions: 15 % H2SO4 acid concentration for 6 hr. at 250 ℃. The dissolution kinetics of nickel and copper that were examined according to heterogeneous model, indicated that the dissolution rates were controlled by surface chemical process during the pug leaching. The activation energy of copper and nickel dissolution were 26.79 kJ.mol-1 and 38.078 kJ.mol-1 respectively; and the surface chemical was proposed as the leaching rate-controlling step.

Recovery of Nickel from sulfuric acid solution using Lewatit TP 220 ion exchange resin (황산용액(黃酸溶液)으로부터 이온교환수지(交換樹脂) Lewatit TP 220에 의한 니켈의 회수(回收))

  • Kang, Nam-Hee;Park, Kyung-Ho;Parhi, P.K.
    • Resources Recycling
    • /
    • v.20 no.6
    • /
    • pp.28-36
    • /
    • 2011
  • The adsorption of nickel(Ni) from sulfuric acid solution was carried out by ion exchange method. A series of batch tests in synthetic solutions were carried out using Lewatit Monoplus TP 220 resin. The following experimental parameters, such as temperature, shaking rate, reaction time, pH, resin dosage and concentration of nickel ions etc. were investigated to establish the effective optimum conditions of nickel adsorption. The solution pH(2.0~5.0) and shaking rate had little effects on the adsorption of nickel and adsorption time of 72hours was required to reach equilibrium. The experimental results show a good agreement with Feundlich isotherm and pseudo-second order reaction. The adsorption behavior of Ni obtained from synthetic solution was compared with that of waste electroplating solution. Elution of nickel from loaded resin increased with increase in $H_2SO_4$ concentration.

Recovery of Nickel Metal from the Spent FeCl$_3$ Etching Solution by Solvent Extraction and Chemical Reduction (FeCl$_3$ 에칭廢液으로부터 溶媒抽出과 化學沈澱에 의한 니켈金屬 回收)

  • Lee, Man-Seung;Kim, Myoung-Sik
    • Resources Recycling
    • /
    • v.14 no.3
    • /
    • pp.48-54
    • /
    • 2005
  • Solvent extraction and chemical reduction experiments have been performed to separate iron and nickel from a spent FeCl$_3$ etching solution and to recover nickel metal. It was possible to separate iron and nickel by extracting the spent solution with Alamine336. At the O/A ratio of 7:1, iron extraction percentage of 99% was obtained. In the stripping of the loaded organic with 0.01 M HCl solution, iron stripping percentage of 99% was obtained when the A/O ratio was 7:1. When the pH of the raffinate was controlled to be 10.5, nickel metal powder with 99% purity was obtained by using hydrazine as a reducing agent at 100$^{\circ}C$. A process was suggested to recover nickel metal from the spent FeCl$_3$ solution and to regenerate etching solution.

Preparation and Characterization of Microfiltration Membrane by Metal Particles (금속입자를 이용한 정밀여과막 제조와 특성평가)

  • Kim, In-Chul;Lee, Kew-Ho;Park, Joo-Young;Jeong, Bo-Reum;Kwon, Ja-Young
    • Membrane Journal
    • /
    • v.17 no.4
    • /
    • pp.381-386
    • /
    • 2007
  • Hollow fibers were made using the nickel slurry containing nickel particles and polymers by phase inversion method. And then, metallic filters were fabricated by sintering method at $1,150^{\circ}C$ under reduction condition. Metallic microfiltration membranes were prepared by coating nickel particles on the metallic filter. The properties of the metallic hollow fiber filters and microfiltration membranes such as pore size and strength were investigated. The metallic membrane showed good resistance against acid, base and chlorine. It was observed that the membrane exhibited good recovery rate by back washing.

A Study on the Recovery of Sn and Ni from the Steel Ball Scraps for Barrel Plating (바렐도금용(鍍金用) Steel Ball 스크랩에서 주석(Sn) 및 니켈(Ni) 회수(回收)에 관한 연구(硏究))

  • Kim, Dae-Weon;Jang, Seong-Tae;Choi, Soon-Ryung
    • Resources Recycling
    • /
    • v.20 no.4
    • /
    • pp.46-51
    • /
    • 2011
  • A study on the recovery of tin from the steel ball scraps for barrel plating has been carried out the physical treatment and leaching experiment. The recovery of iron component was over 95% by the physical treatment, and the recovery of tin component was also over 95% by the hydro process.

Adsorption Properties of Nickel ion from Plating Rinse Water Using Hybrid Sulfonated Bead and Fibrous Ion Exchanger (설폰산형 비드와 섬유 혼성체를 이용한 도금수세수 중의 니켈 흡착 특성)

  • 황택성;조상연
    • Polymer(Korea)
    • /
    • v.27 no.1
    • /
    • pp.61-68
    • /
    • 2003
  • In this study, we have investigated the preparation of mixed bead and fiber type hybrid ion-exchanger for recovering nickel ion from plating rinse water. There was little dependence of adsorption capacity for nickel ion on the mixing ratio of resin type and fiber type of ion exchangers. However, it increased with increasing the resin content in the mixed bed. It was shown that the data Langmuir and Freundlich's adsorption isotherm model were well fitted to the linear. Affinity between the functional groups in the ion exchanger and nickel ion in the process was confirmed. The pressure drop decreased with increasing the number of stage in the multistage bed, but it increased with increasing the resin content in the mixing bed. The initial breakthrough time in the multistage bed was short due to the increase of number of stage in the continuous process. It was found that the final breakthrough time of the multistage bed was little changed. The breakthrough time decreased with increasing the amount of fibrous ion exchanger in the mixed bed. The maximum adsorption capacities of the mixed and multistage beds were 2.51 meq/g and 2.69 meq/g, respectively. The desorption time for the nickel ion with $1N H_2SO_4$ solution was lower than 10 minutes and the yield of desorption was greater than 98 percent.