고로슬래그 미분말 기반 모르타르의 품질향상에 미치는 시멘트치환의 영향 (Effect of quality enhance of blast furnace slag-based mortar by utilizing cement)

  • 송원루;여량량;한동엽;백병훈;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 추계 학술논문 발표대회
    • /
    • pp.154-155
    • /
    • 2014
  • The object of this research is showing the effect of additional hydration of BS with OPC and less amount of gypsum in WA for the binder of BS with RFA mortar on strength development. The test performed was using factors of 0, 10, 30, and 50 % of OPC replacement for effect on strength development with additional stimulation.

  • PDF

마모기로 분쇄한 Reject Ash를 활용한 고강도 모르타르의 품질특성 (Quality properties of high compressive strength mortar that uses Reject ash ground by an abraser)

  • 문병룡;백철;이재진;박병문;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 추계 학술논문 발표대회
    • /
    • pp.45-46
    • /
    • 2016
  • As coal fly ash emissions have increased due to additional constructions of domestic heat power plants, the amount of embedded reject ash (Rj henceforth) is increasing as well. Most Rj is embedded, so if it is used as an alternative admixture instead of cement, embedded quantities will decrease, leading to economic and environmentally positive effects. Therefore this study conducted an experiment to contemplate the usability of Rj ground in the Los Angeles abraser, and what effects ground Rj has on the engineering properties of high compressive strength mortar. The result was that as the number of grinding turns increased, liquidity, air quantity and intensity were improved, proving Rj a possible alternative admixture to cement.

  • PDF

마모기로 분쇄한 Reject Ash가 빈배합 모르타르의 공학적 특성에 미치는 영향 (Quality Properties of Poor-mix mortar that uses reject ash ground by an abraser)

  • 문병룡;박용준;조만기;박병문;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 추계 학술논문 발표대회
    • /
    • pp.96-97
    • /
    • 2016
  • As coal fly ash emissions have increased due to additional constructions of domestic heat power plants, the amount of embedded reject ash (Rj henceforth) is increasing as well. Most Rj is embedded, so if it is used as an alternative admixture instead of cement, embedded quantities will decrease, leading to economic and environmentally positive effects. Therefore this study conducted an experiment to contemplate the usability of Rj ground in the Los Angeles abraser, and what effects ground Rj has on the engineering properties of poor-mix mortar. The result was that as the number of grinding turns increased, liquidity, air quantity and intensity were improved, proving Rj a possible alternative admixture to cement.

  • PDF

플라이애쉬 혼입 모르터의 역학적 특성에 관한 실험적 연구 (An Experimental Study on Mechanical Properties of Fly Ash in Mortar)

  • 박일용;백민수;손종규;최수;정상진
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표회 논문집(I)
    • /
    • pp.127-132
    • /
    • 1998
  • The purpose of this study is to find mechanical properties of fly ash ratio in mortar as flowing, setting time, compressive strength, suction ratio of water, length change ratio. As a result, it was shown that proper fly ash ratio replaced by cement weight in mortar was generally positive effect to flowing, compressive strength suction ratio of water, length change ratio. So if fly ash is well done quality control is considered as good replacement of cement.

  • PDF

저품질의 순환골재를 혼입한 초속경 시멘트 모르타르의 기초물성 및 부피안정성 (Basic Properties and Dimension Stability of Ultra Rapid Setting Cement Mortar Containing Low-Quality Recycled Aggregate)

  • 전상민;김형기
    • 한국건설순환자원학회논문집
    • /
    • 제9권3호
    • /
    • pp.246-252
    • /
    • 2021
  • 초속경 시멘트 모르타르에 KS 기준보다 흡수율이 높고 비중이 낮은 저품질의 순환골재가 혼입되었을 때 모르타르의 기초물성과 부피안정성을 실험적으로 확인하였다. 순환골재를 사용하지 않는 배합은 관련 업체에서 사용하고 있는 일반 보수 모르타르의 것을 따랐다. 라텍스 혼입 및 미혼입 배합에 대해 잔골재에 대해 부피비로 15%, 30% 치환하였으며, 모르타르의 슬럼프, 응결시간, 압축/휨강도, 그리고 밀봉/노출 양생에 따른 길이변화량을 확인해 보았다. 실험 결과 저품질의 순환골재가 사용될 때, 사용하지 않은 경우에 비해 24시간 이내 극초기 강도가 최대 50%까지 감소하거나, 건조수축이 최대 2배 까지 증가할 위험이 있는 것을 확인하였다.

바닥용 건조시멘트 모르타르 배합 내 In-situ 탄산화 적용을 위한 CO2 주입 특성 및 물리적 특성 검토 (Evaluating the Effectiveness of In-Situ Carbonation in Floor Dry Cement Mortar Applications)

  • 김진성;조성현;김춘식
    • 한국건축시공학회지
    • /
    • 제24권1호
    • /
    • pp.1-10
    • /
    • 2024
  • In-situ 탄산화 기술은 시멘트 기반 건설재료의 제조과정에서 CO2를 주입하여 시멘트 수화과정에서 용출되는 Ca2+ 이온과 CO2의 탄산화 반응을 통해 CaCO3의 형태로 CO2를 격리하는 광물탄산화 기술이며, 본 연구에서는 현재 국내 건설현장에서 시공되고 있는 바닥용 건조시멘트 모르타르 배합의 범위에서 In-situ 탄산화 기술을 적용 시, CO2의 주입 유량 및 총 주입량을 검토하고, 바인더인 단위시멘트량 감축에 따른 제품의 품질 검토를 실시하였다.

Development of reference materials for mortar: Determination of the components and relation with mixing ratio

  • Lim, Dong Kyu;Choi, Myoung Sung
    • Advances in concrete construction
    • /
    • 제10권5호
    • /
    • pp.381-391
    • /
    • 2020
  • This study aimed to develop reference materials (RMs) for mortar that can simulate the initial flow characteristics with constant quality over a long period. Through the previous research on the development of RMs for cement paste, the combination of limestone, glycerol, and water was used as the basic matrix for developing RMs for mortar in this study. In addition, glass beads of three particle sizes (0.5, 1.0, and 2.0 mm) and ISO standard sand were selected as tentative candidates to derive fine aggregate substitutes. The mixture of glass beads could simulate the initial flow characteristics of mortar, but under the same mixing ratio, replicates showed an unstable tendency to indicate inconsistent values due to the generation of electrostatic properties between materials and equipment. On the other hand, the mixture using ISO standard Sand not only simulates the constant flow characteristics for a long period of time, but also shows stable results with little error in replicates. Therefore, limestone, glycerol, ISO standard sand, and water were finally determined as components that met the required properties of RMs for mortar. The effect of each component on the flow characteristics of RMs was analyzed. It was found that glycerol increased the cohesion between the particles of standard sand, resulting in a constant increase both in the plastic viscosity and yield stress. Both limestone and standard sand had a dominant effect on the yield stress. The relationships between various mortar mixing ratios and the corresponding mixing ratios of RMs were established. In addition, the results of the verification experiment showed that the rheological properties of the RMs obtained through the relationships correlated with various water/cement ratios and the fine aggregate volume fractions of mortar obtained with same manner. In other words, the RMs for mortar developed in this study can be used as standard samples because they can simulate the initial flow characteristics of mortar of various mixing ratios for a long period without any chemical changes.

재생(再生)잔골재(骨材)를 프리캐스트 콘크리트용(用) 골재(骨材)로 활용(活用)하기 위한 실험적(實驗的) 연구(硏究) (Experimental Study for Utilizing of Recycling Fine Aggregate as Precast Concrete Aggregate)

  • 문대중;문한영;김양배;임남웅
    • 자원리싸이클링
    • /
    • 제15권2호
    • /
    • pp.24-31
    • /
    • 2006
  • 폐콘크리트 파쇄시 발생하는 재생잔골재의 품질을 검토하였으며, 재생잔골재를 활용한 모르타르의 압축강도, 휨강도 및 흡수율을 검토하였다. 또한, 프리캐스트 콘크리트 제품용 골재로서의 적용성에 대하여 평가하였다. 재생잔골재의 밀도 및 흡수율은 각각 $2.31\;g/cm^3$ 및 8.07%로 KS F 2573의 2종에 해당되는 품질이었다. 혼합시멘트 MRS1, MRS2 및 MRS3 사용 모르타르의 재령 28일 압축강도는 물-시멘트비 35%, 양생온도 $40^{\circ}C$의 조건에서 각각 15.8, 27.4 및 48.7MPa로 최대값을 발현하였다. 모르타르의 최대휨강도는 혼합시멘트 MRS1 및 MRS2 사용시 물-시멘트비 35.0%, 양생온도 $40^{\circ}C$, 혼합시멘트 MRS3사용시 물-시멘트비 37.5%, 양생온도 $40^{\circ}C$의 조건에서 발현하였다. 혼합시멘트 MRS1, MRS2 및 MRS3를 사용한 모르타르의 흡수율의 범위는 각각 $8.3{\sim}7.3%,\;6.5{\sim}8.5%$$3.5{\sim}6%$의 범위로 나타났다. 그러므로 혼합시멘트와 재생잔골재의 비율을 적절히 조절함으로써 MRS1는 저강도용, MRS2는 보통강도용, MRS3는 고강도용으로 다양한 프리캐스트 콘크리트 제품에 적용될 수 있을 것으로 기대된다.

The Influence of FGD Gypsum Fabricated from Limestone Sludge on Cement Properties

  • Seo, Sung Kwan;Chu, Yong Sik;Shim, Kwang Bo;Lee, Jong Kyu;Song, Hun
    • 한국세라믹학회지
    • /
    • 제53권6호
    • /
    • pp.676-681
    • /
    • 2016
  • For the purpose of reducing the amount of limestone, which is used as a desulfurization agent to absorbing $SO_X$ gas in thermal power plants, and to recycle limestone sludge generated from a steel mill, limestone sludge was utilized as a desulfurization agent. In this study, cement, made of flue gas desulfurization (FGD) gypsum obtained in a desulfurization process using limestone sludge, was manufactured then, experiments were conducted to identify the physical properties of the paste and mortar using the cement. The results of the crystal phase and microstructure analyses showed that the hydration product of the manufactured cement was similar to that of ordinary Portland cement. No significant decline of workability or compressive strength was observed for any of the specimens. From the results of the experiment, it was determined that FGD gypsum manufactured from limestone sludge did not influence the physical properties of the cement also, quality change did not occur with the use of limestone sludge in the flue gas desulfurization process.

고강도 콘크리트용 고성능감수제 성능평가 (Tests on Superplasticizers for High Strength Concrete)

  • 노재호;김기철;조일호;한정호;박연동
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1994년도 가을 학술발표회 논문집
    • /
    • pp.151-156
    • /
    • 1994
  • This study is to investigate the quality of superplasticizers in domestic market. Therefore, the physico-chemical characteristics, the fluidity characteristics of fresh cement paste and mortar were tested. Also fresh and hardened properties of mortars and concretes using these superplasticizers were tested. From these results, differences of quality among superplasticizers are checked clearly in low water/cement ratio. And it is concluded that several superplasticizers have better dispersion ability than others in every tests. It has known that all samples are naphtalene sulfornate formaldehede types by the UV(ultra-violet) test.