• 제목/요약/키워드: pre-wetting time

검색결과 12건 처리시간 0.018초

Control of Wettability Using Regularly Ordered Two-Dimensional Polymeric Wavy Substrates

  • Yi, Dong Kee
    • Nano
    • /
    • 제13권10호
    • /
    • pp.1850120.1-1850120.9
    • /
    • 2018
  • Two-dimensional poly(dimethylsiloxane) (PDMS) films with wavy patterns were studied in order to investigate reversible and irreversible wetting effects. Pre-strained, surface oxidized layers of PDMS were used to form relieved wavy geometries, on which hydrophobic functionalization was carried out in order to produce irreversible wetting effects. Wavy-patterned PDMS films showed time-dependent reversible wetting effects. The degree of surface wettability could be tuned by the choice of wavy groove geometries. And the groove geometries were controlled via $O_2$ plasma treatment and mechanical pre-straining. The pre-strained, buckled PDMS films were applied to the fabrication of hydrophobic polystyrene nano-patterns using colloidal self-assembly, where the colloids were arrayed in two-dimensional way. The wavy polystyrene films were found to be more hydrophobic relative to flat polystyrene films. The grooving methodology used in this study could be applied to enhancing the hydrophobicity of other types of polymeric thin films, eliminating the need for chemical treatment.

기판의 건조시간에 따른 Solderability에 관한 연구 (A Study on Solderability by Lasting time of PCB in Pre-Baking)

  • 신규현;최명기;정재필;서창제
    • 마이크로전자및패키징학회지
    • /
    • 제6권1호
    • /
    • pp.59-64
    • /
    • 1999
  • 본 연구에서는 솔더링(soldering)공정 전, 기판의 최적의 건조 시간과 PCB기판에 묻은 수분이 솔더링에 미치는 영향에 대하여 조사하고자 하였다. 실험결과, 솔더링 중 건조시간이 증가할수록 솔더링성(solderabillity)이 향상됨을 알 수 있었다. 즉, 건조된 시편이 함습한 시편에 비해 젖음 시간(wetting time)이 약 0.2초 짧고 젖음력(wetting force)이 2~4mN증가되었다. 338k에서 30분 이상 건조시켰을 때 최소 미납 결함과 리드와 기판의 최고 인장강도가 얻어 졌다. 또, 건조시간을 45분가지 증가시킬 때, 건조시간 증가에 따라 솔더볼 발생 양이 감소하였다.

  • PDF

대기 습도변화에 따른 콘크리트 보수체의 비정상적인 습도응력 조사 (Non-Stationary Stress Analysis of Repaired Concrete Structures due to Hygral Transient Condition)

  • 윤우현
    • 콘크리트학회지
    • /
    • 제9권3호
    • /
    • pp.157-166
    • /
    • 1997
  • 본 연구에서는 대기 습도변화에 의한 콘크리트 보수체(기층 콘크리트/보수 모르터)의 파괴현상을 조사하기 위해서 보수체내의 비정상적인 습도분포 및 습도응력을 계산하였다. 이러한 계산은 시멘트 모르터로 보수된 접촉면이 없는 보수체에서 보수층 두께(Do=05-2.5cm)와 보수 작업전 기층 콘크리트 표면의 습윤처리 시간(tc=1-5days) 및 대기습도(Ho=50~80%)를 주요변수로 하여 수행되었다. 계산 및 조사 결과에 의하면 접합면의 응력이 압축상태를 유지하기 위해서는 각 대기 습도마다 일정값 이상의 보수층 두께와 습윤처리 시간이 필요함을 알 수 있다.

Interaction of Mechanics and Electrochemistry for Magnesium Alloys

  • Han, En-Hou;Wang, JianQiu;Ke, Wei
    • Corrosion Science and Technology
    • /
    • 제7권5호
    • /
    • pp.243-251
    • /
    • 2008
  • Magnesium alloys become popular research topic in last decade due to its light weight and relatively high strength-to-weight ratio in the energy aspiration age. Almost all structure materials are supposed to suspend stress. Magnesium is quite sensitive to corrosive environment, and also sensitive to environmental assisted cracking. However, so far we have the limited knowledge about the environmental sensitive cracking of magnesium alloys. The corrosion fatigue (CF) test was conducted. Many factors' effects, like grain size, texture, heat treatment, loading frequency, stress ratio, strain rate, chemical composition of environment, pH value, relative humidity were investigated. The results showed that all these factors had obvious influence on the crack initiation and propagation. Especially the dependence of CF life on pH value and frequency is quite different to the other traditional structural metallic materials. In order to interpret the results, the electrochemistry tests by polarization dynamic curve and electrochemical impedance spectroscopy were conducted with and without stress. The corrosion of magnesium alloys was also studied by in-situ observation in environmental scanning electron microscopy (ESEM). The corrosion rate changed with the wetting time during the initial corrosion process. The pre-charging of hydrogen caused crack initiated at $\beta$ phase, and with the increase of wetting time the crack propagated, implying that hydrogen produced by corrosion reaction participated in the process.

프리웨팅된 인공경량골재의 흡수 특성 (Water absorption characteristics of artificial lightweight aggregates preparedby pre-wetting)

  • 김유택;장창섭;류유광
    • 한국결정성장학회지
    • /
    • 제21권2호
    • /
    • pp.82-86
    • /
    • 2011
  • 인공경량 골재는 다결정질 소성체를 주 구성으로 하므로 골재 내부에 다량의 공극이 일정비율로 형성되는 것이 특징이다. 이러한 인공경량 골재는 조직 구조의 특성상 외부환경의 변화에 의해 수분이 비정상적인 이동을 보이는 경향이 있다. 다공질 재료의 수분 방출 특성은 일반적으로 기공률 및 기공크기 분포에 크게 좌우되지만, 인공적으로 소결 제조된 경우에는 표면에 생성된 치밀한 구조의 표피층에도 많은 영향을 받을 것으로 생각된다. 인공경량 골재 내부의 수분 이동에 미치는 요인은 골재내의 세공 및 공극의 분포와 형상, 크기, 그리고 프리웨팅 방법 등이 있으며 각 조건에 따라 상당한 차이를 보인다. 본 연구에서는 인공경량 골재를 제조하여 골재의 가압시 흡수 특성이나 침수시간에 대한 흡수율의 거동에 대한 명확한 규명을 함으로써 경량골재 펌프압송을 위한 기초적 자료를 제공하고자 하였다. 본 실험에 사용된 인공경량골재는 독일 'L'사의 상업용 인공경량골재와 본 연구팀이 제조한 2가지 조성의 인공경량골재를 사용하였으며, 골재 수분함침시간, 진공압력, 급냉조건을 변화시켜 골재의 흡수율을 측정하였다. 인공경량골재를 $300^{\circ}C$ 에서 급냉 하였을 경우 24시간 침수보다 높은 흡수율을 보였고, 진공압력에 따라 흡수율이 증가하는 경향이 있으며, -300 mmHg의 진공 압력시 24시간 침수보다 "L"사 골재는 54 %의 높은 증가를 보였으나 K622와 K73 골재는 비교적 적은 2 % 내외의 흡수율 증가양상을 보였다.

인공경량골재 사용 경량투수블록의 제조시간 변화에 따른 배합 및 압축강도 특성 (A Compressive Strength and Mixing Properties of Lightweight Porous Block Using Lightweight Aggregate by Variation of Manufacture Time)

  • 김영욱;이경수;오태규;정수빈;반준모;최세진
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2018년도 추계 학술논문 발표대회
    • /
    • pp.118-119
    • /
    • 2018
  • The purpose of this study is to investigate the compressive strength and mixing properties of the lightweight block, which has been manufactured without the pre-wetting process, in the lightweight block using domestic artificial lightweight aggregate. The test results of the specimens produced within 30 minutes after the preparation showed high compressive strength but poor permeability. Therefore, the elapsed time after the manufacture, which is expected to have required compressive strength and permeability, was about 60 minutes in this study.

  • PDF

종자 전처리 및 환경조절이 삽주 종자 발아에 미치는 영향 (Effects of Seed Pretreatment and Environment Controls on Germination of Atractylodes japonica Seeds)

  • 전권석;송기선;윤준혁;김창환;김종진
    • 한국약용작물학회지
    • /
    • 제21권5호
    • /
    • pp.394-400
    • /
    • 2013
  • This study was carried out in order to examine the germination characteristics of Atractylodes japonica seeds, and it was to develop the more efficient pre-treatment and production system of the seeds. Experiment was performed by two ways-temperature control (10, 15, 20, $25^{\circ}C$) and shading treatment (full sunlight, 35, 50, 75, 95% of full sunlight). Seed pre-treatment before the each experiment was carried out by temperature (with low temperature and wetting treatment (LTW) for 0, 15, 30, 45 and 60 days) and shading treatment (with drying at room temperature (DRT), drying at low temperature (DLT) and water soaking (WS) for 48 hours). Seeds of A. japonica were germinated well under temperature control (overall 85.3~100%), especially high temperature. And, the seeds pre-treated with LTW for 45 days germinated with a 100% success rate. Under the surveying shading treatment, the highest germination rate was 95.8% with DRT and overall 63.2~95.8%. Germination rate under seeds with WS was 63.2~7.8%. As a result of surveying the whole experiment, A. japonica seeds don't need to pre-treat cause of high germination, but if it is performed with LTW for a certain period of time, it would be more productive.

대기 습도변화에 다른 콘크리트 보수체의 비정상적인 습도분포 (Non-Stationary Moisture Distribution of Repaired Concrete Structures due to Hygral Transient Condition)

  • 윤우현
    • 콘크리트학회지
    • /
    • 제8권1호
    • /
    • pp.121-129
    • /
    • 1996
  • 본 연구에서는 대기 습도변화에 의한 콘크리트 보수체(기층 콘크리트/보수 모르터)의 파괴현상을 조사하기 휘해서 보수체내의 비정상적인 습도분포를 계산하였다. 계산된 습도분포에 의해서 기층과 보수층 경계면 부위의 습도차이가 보수층 두께(0.5~2.5cm)와 보수작업전 기층 콘크리트 표면의 습윤처리시간(0~72hr)을 주요 변수로 하여 조사되었고, 이는 주로 시멘트 모르터로 보수된 접촉면이 없는 보수체에서 수행되었다. 계산 및 조사결과 보수층 두께가 감소하고 습윤 처리시간이 증가할수록 경계면 부위의 습도차이는 감소하는 경향을 보였고, 특히 보수후 습도차이가 음수값이 될 때의 시간을 하나의 수식으로 표시하였다.

중극(中極) 관원(關元) 혈입(穴位)를 이용한 전침 치료 야뇨 환아 3례 (Three cases report about enuritic children treated with electro-acupuncture on Zhongji(CV3), Guanyuan(CV4))

  • 장규태;김장현;오주영
    • 대한한방소아과학회지
    • /
    • 제19권1호
    • /
    • pp.103-115
    • /
    • 2005
  • Objectives : Nocturnal enuresis is common disorder in children and has important negative effects on the self-image and performance of children. Thus Successful treatment needed to increase self-esteem. Many studies of this symptoms were reported. But electro-acupuncture treatment not reported in Korea. Methods : We treated three cases enuretic children with different types. Their diagnosis were non-monosymptomatic primary, monosymptomatic primary, monosymptomatic secondary nocturnal enuresis. We used electro-acupuncture on Zhongji(CV3), Guanyuan(CV4) for 20 min. To investigate relapse. at least for 4 months after the end of the therapy we followed-up by telephone. Results : After treatment, diurnal urinary symptoms, such as increased frequency of urination, urgency, incontinence were dramatically improved. And the number of wet night decreased with nocturia and delayed wetting time. Compared to pre-treatment, findings, the number of wet nights decreased 80% or more. Conclusion : All of them tolerated electro-acupuncture well and kept reduction at least for 4 months follow-up. Further study is needed with more cases.

  • PDF

노반 및 공극 막힘 현상에 따른 투수성 보도블록의 불포화 상태에서의 배수 성능에 관한 실험적 연구 (Effect of Bedding Layer and Clogging on Drainage Capacity of Pervious Sidewalk Block in Unsaturated Condition)

  • 서다와;윤태섭
    • 한국지반공학회논문집
    • /
    • 제32권5호
    • /
    • pp.37-48
    • /
    • 2016
  • 본 연구는 실제 시공 환경에서 투수성 보도블록의 표면 유출 및 배수 특성을 알아보고자 하였으며, 표층 및 노반을 포함한 시편을 대상으로 불포화 상태에서 도심 내 우수 조건을 고려한 배수 실험을 진행하였다. 일정한 시간 간격을 두고 반복적인 배수 실험 및 공극 막힘 실험이 시행되었으며, 정량적 분석을 위하여 3D X-ray CT 이미지 분석 및 증발 실험을 시행하였다. 실험 결과, 시간 간격 동안 발생한 증발로 인해 공극 내 물이 공간적으로 재분포되어 표면 유출을 야기시키는 것으로 나타났다. 특히, 공기에 노출되어 있는 표층보다 시편 하부에 위치한 노반의 공극 변화가 투수성 보도블록의 배수, 증발 등 전체적인 수리학적 거동을 크게 저하시켰다. 또한 공극 내 침전물은 증발로 인한 변화를 증진 시키며, 이 때 저하된 배수 성능은 쉽게 회복되지 않는 것으로 나타났다. 그리고 선행우수조건에 의하여 배수 성능이 저감되면서 최대 표면 유출 높이가 증가하는 것으로 나타났다.