강용접부의 표면균열 성장거동에 관한 연구 1

  • 정세희;박재규;이종기
    • Journal of Welding and Joining
    • /
    • v.6 no.2
    • /
    • pp.30-39
    • /
    • 1988
  • Generally, as the welded region of weld structures has the incomplete bead and welded deposit which are able to behave like the surface cracks occasinally, there is a high possibility that the fatigue fracture of the weld structures is due to the surface cracks on the wlded region. This study was done to investigate the effects of post weld heat treatment (PWHT) on the fatigue behaviors of the surface crack of the heat affected zone (HAZ) for the multi-pass welds under the repetitive pure bending moment. The obtained results are summarized as follows : 1. The crack grows to the depth direction initially as the number of cylces increase, the amount of crack length is increased for the surface dir3ction and cive versa for the depth direction. 2. The fatigue life is increased in a order of as weld, PWHT specimens and parent. 3. As the number of cycles increase, the crack length is increased to th surface direction. The increase of the depth length is blunted at the center of specimen thickness. 4. The fatigue crack growth of PWHT specimens to the surface direction is dependent upon the holding time and applied stress during PWHT. In order words, the crack growth rate decreases with the holding time and increases with the applied stress during PWHT. 5. As the crack grows, the aspect formed in the course of crack propagation approaches to semicircle for parent and ellipse with the largest semidiameter for PWHT ($1/4hr, 15kgf/mm^2$) 6. At depth direction, it is difficult to apply to the paris' equation because of the scattered data between the crack growth rate and the stress intensity factor range.

  • PDF

Study on Characteristics of SCC and AE Signals for Weld HAZ of HT-60 Steel (HT-60강 용접부의 SCC및 AE신호특성에 관한 연구)

  • Na, Eui-Gyun;Yu, Hyo-Sun;Kim, Hoon
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.21 no.1
    • /
    • pp.62-68
    • /
    • 2001
  • In order to characterize the microscopic fracture behaviour of the weldment din stress corrosion cracking(SCC) phenomena, SCC and acoustic emission(AE) tests were carried out simultaneously and the correlation between mechanical paramenters obtained from SCC and AE tests was investigated. In the case of base metal, much more AE events were produced at -0.5V than at -0.8V because of the dissolution mechanism before the maximum load. Regardless of the applied voltages to the specimens, however, AE events decreased after the maximum load. In the case of weldment, lots of AE events with larger amplitude $range(40{\sim}100dB)$ were produced because of the singularities of weld HAZ in comparision to the base metal and post-weld heat-treated(PWHT) specimens. Numerous and larger cracks for the weldment were observed on the fractured surfaces by SEM examination. From these results, it was concluded that SCC for the weldment appeared most severely in synthetic seawater. Weld HAZ was softened by PWHT which also contributed to the reduced susceptibility to corrosive environment in comparison to the weldment.

  • PDF

Study on Softening Characteristics of 9Cr-1Mo Steel Weldments for High Temperature and Pressure Vessels Application (고온고압장치 적용을 위한 9Cr-1Mo강 용접부의 연화특성에 관한 연구)

  • 이영호;이규천;윤의박;김기철
    • Journal of Welding and Joining
    • /
    • v.10 no.3
    • /
    • pp.40-53
    • /
    • 1992
  • 고온고압장치(High Temperature and Pressure Vessels)의 적용을 위한 기초연구로서 9Cr-1Mo강 용접부의 연화특성에 대하여 검토하였다. 9Cr-1Mo 강재에 Bead-on-Plate용접을 실시한 후, 용접부의 기계적 성질과 그 현미경조직관찰 및 미세경도를 측정한 결과, As-Welded 및 용접 후열처리(PWHT)등의 조건에 관계없이 용접열향부의 변태역과 템퍼링역의 경계에서 모재의 경 도보다 낮은 경도값(연화역)을 나타내었으며 이러한 원인은 결정립계(Grain boundary)에 석출 되는 탄화물의 형성에 의한 뜨임 현상임이 판명되었다.

  • PDF

원자로압력용기강 용접열영향부(HAZ)의 샤피시험편 노치 위치설정에 대하여

  • 김주학;변택상;지세환;국일현;홍준화
    • Proceedings of the Korean Nuclear Society Conference
    • /
    • 1996.11b
    • /
    • pp.557-562
    • /
    • 1996
  • 조사전 및 감시시험시 용접열영향부(heat affected zone, HAZ)의 인성평가를 위해 제작되는 샤피(Charpy) 충격시험편의 노치(notch) 위치에 대하여 현재의 규정에 대한 타당성을 검토하였다. 적용규정은 HAZ 시험편의 노치위치를 용접용융선(fusion line, FL) + 모재측 0.8 mm 로 제한하고 있다. 그러나, 본 연구결과, 이 부위는 다층(multipass) 용접시 후속열이력에 의해 결정립이 미세화되어, 인장강도와 경도 및 충격인성이 모재나 용접부에 비하여 양호하게 나타났다. 한편, FL + 4 mm 이상의 다른 위치에서는 강도와 경도 및 충격인성이 모두 모재와 용접부에 비하여 낮은 값을 보였다. 이는 다층용접에 의한 후속열이력 및 용접후열처리(post weld heat treatment, PWHT)에 의해 금속조직학적 영향을 받은 것으로 판단되었다. 일련의 시험결과로부터, 조 사전 및 감시시험용 샤피충격시험편의 HAZ 에 있어서의 노치위치에 대한 현재의 규정을 재검토할 필요가 있음을 제안하였다.

  • PDF

The Effect of PWHT on Fracture Toughness in HAZ of Cr-Mo Steel(II) (Cr-Mo鋼 熔接熱影響部 의 破壞靭性 에 미치는 熔接後 熱處理 의 影響 II)

  • 임재규;정세희
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.9 no.1
    • /
    • pp.40-46
    • /
    • 1985
  • Some problems such as toughness decrement and stess relief cracking (SRC), many occur when post weld heat treatment (PWHT) is applied to remove residual stress adn hydrogen. In this paper PWHT was carried out under the stress of 0, 98, 196 and 294 MPa (0, 10, 20 and 30kgf/mm$^{2}$ each) to simulate residual stress in HAZ of Cr-Mo steel. The effect of applied stress during PWHT on fracture toughness was evaluated by COD fracture toughness test, micro-hardnes test and observation of SEM. The experimental results are as follows; (1) Fracture toughness of weld HAZ was improved by PWHT, but it decreased as heat treated under the stress. (2)Hardness ratio under the stress of 294MPa (30kg/mm$^{2}$) was lower and fracture toughness was decreased than that of the no stress. (3) Applied stress in weld HAZ during PWHT assisted precipitation of over saturated alloying elements in the structure, so fracture surface at the stress of 294MPa (30kg/mm$_{2}$) appeared the grain boundary failure possibly one of the reasons for PWHT embrittlenment.

Residual Stress Analysis of Repair Welded Rail Using the ABAQUS User Subroutine (ABAQUS 서브루틴을 이용한 레일 보수용접 잔류응력 해석)

  • Kim, Dong Wook;Jun, Hyun Kyu;Lee, Sang Hwan;Chang, Yoon Suk
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.33 no.7
    • /
    • pp.551-558
    • /
    • 2016
  • Reduction of welding residual stress is very important in the railway industry, but calculating its distribution in structures is difficult because welding residual stress formation is influenced by various parameters. In this study, we developed a finite element model for simulating the repair welding process to recover a surface damaged rail, and conducted a series of parametric studies while varying the cooling rate and the duration of post weld heat treatment (PWHT) to find the best conditions for reducing welding residual stress level. This paper presents a three-dimensional model of the repair welding process considering the phase transformation effect implemented by the ABAQUS user subroutine, and the results of parametric studies with various cooling rates and PWHT durations. We found that heat treatment significantly reduced the residual stress on the upper rail by about 170 MPa.

Effect of welding residual stress on operating stress of nuclear turbine low pressure rotor

  • Tan, Long;Zhao, Liangyin;Zhao, Pengcheng;Wang, Lulu;Pan, Jiajing;Zhao, Xiuxiu
    • Nuclear Engineering and Technology
    • /
    • v.52 no.8
    • /
    • pp.1862-1870
    • /
    • 2020
  • The purpose of this study is to investigate the effect of welding residual stress on operating stress in designing a nuclear turbine welded rotor. A two-dimensional axisymmetric finite element model is employed to calculate the residual stress before and after post weld heat treatment (PWHT), and then the superposition of residual stress after PWHT and operating stress at normal speed and overspeed were discussed. The investigated results show that operating stress can be affected significantly by welding residual stress, and the distribution trend of superposition stress at the weld area is mainly determined by welding residual stress. The superposition of residual stress and operating stress is linear superposition, and the hoop stress distribution of superposition stress is similar with the distribution of residual stress. With the increasing overspeed, the distribution pattern of the hoop superimposed stress remains almost unchanged, while the stress level increases.

Development of Small-Specimen Creep Tester for Life Assessment of High Temperature Components of Power Plant (발전소 고온부의 수명 평가를 위한 소형 시편용 크리프 시험기의 개발)

  • Kim, Hyo-Jin;Jeong, Yong-Geun;Park, Jong-Jin
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.10 s.181
    • /
    • pp.2597-2602
    • /
    • 2000
  • The most effective means of evaluating remaining life is through the creep testing of samples removed from the component. But sampling of large specimen from in-service component is actually impossible. So, sampling device and small-specimen creep tester have been applied. Sampling device has been devised to extract mechanically small samples by hemispherical, diamond -coated cutter from the surface of turbine rotor bores and thick-walled pipes without subsequent weld repairs requiring post weld heat treatment. A method of manufacturing small creep specimen, 2min gage diameter and 10min gage length, using electron beam welding to attach grip section, has been proven. Small-specimen creep tester has been designed to control atmosphere to prevent stress increment by oxidation during experiment. To determine whether the small specimens successfully reproduce the behavior of large specimens, creep rupture tests for small and large specimens have been performed at identical conditions. Creep rupture times based on small specimens have closely agreed within 5% error compared with that of large specimen. The errors in rupture time have decreased at longer test period. This comparison validates the procedure for fabricating and testing on small specimen. This technique offers potential as an efficient method for remaining life assessment by direct sampling from in -service high temperature components.

Effect of PWHT and stress ratio on fatigue behavior of welded joints in steel (강용접부의 피로거동에 미치는 용접후열처리 및 응력비의 영향)

  • 김경수;임재규;정세희
    • Journal of Welding and Joining
    • /
    • v.5 no.3
    • /
    • pp.53-61
    • /
    • 1987
  • Post weld heat treatment(PWHT) is usually carried out to remove the residual stress and to improve the microstructure and mechanical properties of welded joints. By the way, welding structure transformed owing to PWHT and reheating for repair loads the random cycles fatigue as offshore welding structure of constant low cycle fatigue as pressure vessel, and then, pre-existing flaws or cracks exist in a structural component and those cracks grow under cyclic loading. Therefore, the effects of PWHT and stress ratio on fatigue crack growth behaviors were studied on the three regions such as HAZ, sub-critical HAZ and deposit metal of welded joints in SM53 steel. Fatigue crack growth behavior of as-weld depended on microstructure and fatigue crack growth rate of HAZ was the lowest at eac region, but after PWHT it was somewhat higher than that of as-wel. In case of applying the stress($10kg/mm^2$) during PWHT, fatigue crack growth resistance tended to increase in the overall range of .DELTA.K.

  • PDF

Resistance, electron- and laser-beam welding of zirconium alloys for nuclear applications: A review

  • Slobodyan, Mikhail
    • Nuclear Engineering and Technology
    • /
    • v.53 no.4
    • /
    • pp.1049-1078
    • /
    • 2021
  • The review summarizes the published data on the widely applied electron-beam, laser-beam, as well as resistance upset, projection, and spot welding of zirconium alloys for nuclear applications. It provides the results of their analysis to identify common patterns in this area. Great attention has been paid to the quality requirements, the edge preparation, up-to-date equipment, process parameters, as well as post-weld treatment and processing. Also, quality control and weld repair methods have been mentioned. Finally, conclusions have been drawn about a significant gap between the capabilities of advanced welding equipment to control the microstructure and, accordingly, the properties of welded joints of the zirconium alloys and existing algorithms that enable to realize them in the nuclear industry. Considering the ever-increasing demands on the high-burnup accident tolerant nuclear fuel assemblies, great efforts should be focused on the improving the welding procedures by implementing predefined heat input cycles. However, a lot of research is required, since the number of possible combinations of the zirconium alloys, designs and dimensions of the joints dramatically exceeds the quantity of published results on the effect of the welding parameters on the properties of the welds.