• 제목/요약/키워드: pore morphology

검색결과 296건 처리시간 0.025초

Polymerization of Polyethylene Using Bimodal TiCl4/MgCl2/SBA-15/MCM-41

  • Moonyakmoon, Mattanawadee;Klinsrisuk, Sujitra;Poonsawat, Choosak
    • 한국입자에어로졸학회지
    • /
    • 제11권3호
    • /
    • pp.87-92
    • /
    • 2015
  • MCM-41 (Mobil Composition of Matter) and SBA-15 (Santa Barbara Amorphous) were used as a supported catalyst for ethylene polymerization due to their combination of large surface area and wide range of pore size distribution. The morphology of supports was used to control the morphology of the resulting polymer. Different molar ratios of Al/Ti were used for ethylene polymerization at $60^{\circ}C$ under atmospheric pressure. The effect of different mass ratios of MCM-41/SBA-15 and 1-hexene concentration on polymerization activity and polymer properties was investigated. The catalytic activity and the crystallinity reached the highest value at Al/Ti of 480. Upon incorporation of MCM-41 and SBA-15 into $MgCl_2/TiCl_4$ catalyst, the molecular weight and crystallinity of polyethylene were enhanced. The obtained polyethylene showed melting temperature between 130 and $135^{\circ}C$. The polyethylene with replication structure of support and bimodal MWD was expected.

Morphology Change of Nanotube and Micropore on the Ti-25Nb-xHf Alloys with Hf Contents after Anodization

  • Kim, Sung-Hwan;Ko, Yeong-Mo;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2012년도 춘계학술발표회 논문집
    • /
    • pp.333-333
    • /
    • 2012
  • In this study, we investigated morphology of nanotube and micropore on the Ti-25Nb-xHf alloys with Hf contents after anodization. Ti-25Nb-xHf ternary alloys contained from (0~15) wt.% Hf contents were manufactured by vacuum arc-melting furnace. The obtained ingots were homogenized in an argon atmosphere at $1000^{\circ}C$ for 12h and then water quenching. The specimens were cut from ingots to 3mm thickness and first ground and polished using SiC paper (grades from 100 to 2000). 2steps anodization treatments on Ti-25Nb-xHf alloys were carried out at room temperature for experiments. Micro-pore formation was performed in Ca+P mixed solution at 265V for 3min. After that, nanotube formation was in 1M $H_3PO_4$ electrolytes containing 0.8wt.% NaF solutionat 10V for 120min. Morphologies of micropore and nanotube depended on the Hf content in Ti-25Nb-xZr ternary system.

  • PDF

양이온성 계면활성제를 이용한 수산화인회석 합성 (Synthesis of Hydroxyapatite Using a Cationic Surfactant)

  • 이근영;권기영
    • 공업화학
    • /
    • 제30권5호
    • /
    • pp.639-642
    • /
    • 2019
  • 본 연구에서는 침전법을 이용하여 양이온성 계면활성제인 hexadecyltrimethylammonium chloride (CTAC)를 도입한 수산화인회석을 합성하였다. X-선 회절 분석법과 투과전자현미경, 비표면적 분석기를 이용하여 수산화인회석과 CTAC을 도입한 수산화인회석의 결정성, 형태, 비표면적을 분석하였다. 열처리 후, HAP와 CTAC-HAP는 열처리 전과 비교하여 비표면적이 감소하였다. 또한 열처리는 뾰족한 막대 모양에서 종횡비가 감소한 둥근 모양으로의 CTAC-HAP의 형태변화를 유도하였다. 이러한 형태의 변화는 순수한 HAP에서도 관찰되었다. 그러므로 형태 변화와 열처리 후의 비표면적 감소는 열처리 중 CTAC의 제거로 생성된 기공들이 형태 변화로 인해 유지되지 않는 것으로 판단된다.

효소촉매 담지체용 다공성 베마이트 제조 (Formation of Porous Boehmite for Supporting Enzyme Catalyst)

  • 염혜숙;김기도;전창림;김희택
    • 공업화학
    • /
    • 제17권2호
    • /
    • pp.188-193
    • /
    • 2006
  • 용액의 pH, 주입방법, 온도, 유량의 변화를 주면서 질산알루미늄($Al_{3}(NO_{3})_3{\cdot}9H_{2}O$)을 암모니아수($NH_{4}OH$)로 침전시켜 베마이트(Boehmite)를 합성하였다. 베마이트 상이 형성되는 pH 범위와 입자의 형상과 기공특성에 미치는 합성 조건의 영향을 조사하였다. 베마이트는 반응 용액의 pH가 7.5~9일 때 형성되었고, P2jet 주입방법은 침전이 일어나는 동안 pH를 일정하게 유지할 수 있어 용액내의 반응에 참여하는 이온의 농도가 일정하게 유지되어 균일한 크기의 입자와 기공을 형성할 수 있게 하였다. 따라서 비표면적과 기공부피 두 가지 동시에 향상되었다. 온도가 올라갈수록, 유량이 감소할수록 비표면적과 기공부피가 증가함을 보이고, $60^{\circ}C$ 이상에서는 미세섬유모양의 입자를 얻을 수 있었다. 최적의 조건은 pH 9에서 P2jet 방법으로 주입하고 반응온도 $90^{\circ}C$와 유량 2.5 mL/min을 유지하였을 경우로 비표면적은 $385.46m^2/g$이고 기공 부피는 1.0252 mL/g을 가지는 평균 10 nm의 기공이 형성된 다공성 베마이트를 얻을 수 있었다.

화학기상증착법을 이용한 알루미나 복합 분리막의 제조 (Preparation of Alumina Composite Membranes by Chemical Vapor Deposition)

  • 안상욱;최두진;현상훈
    • 한국세라믹학회지
    • /
    • 제31권8호
    • /
    • pp.927-933
    • /
    • 1994
  • Alumina composite membranes were prepared by chemical vapor deposition (CVD) using aluminum-tri-isopropoxide as a precursor. Porous alumina supports were used in deposition, which were in disk shape with mean pore diameter of 0.1 ${\mu}{\textrm}{m}$ and prepared by slip-coasting process. film deposition morphology on porous support was simulated through depositing alumina film on polycrystalline silicon pattern, and its step coverage observed by SEM showed one deviated from uniform step coverage. N2 permeability through composite membranes and the pressure dependence decreased as the deposition time increased. Initially, the N2 permeability of the top layer was tend to decrease rapidly, and then the degree of decrease in N2 permeability was tend to diminish with deposition time. The N2 permeability increased with heat treatment temperature and the crack was generated in top layer at 100$0^{\circ}C$.

  • PDF

First Record and Morphological Features of the Dinoflagellate Peridinium aciculiferum Lemm. (Dinophyceae) in Korean Freshwater

  • Ki Jang-Seu;Han Myung-Soo
    • 환경생물
    • /
    • 제23권4호
    • /
    • pp.323-327
    • /
    • 2005
  • Two morphologically different species of Peridinium were frequently observed in natural samples collected monthly from Togyo Reservoir. One was previously identified as P. bipes Stein f. occultatum (Lindem.) Lef. (Ki and Han 2005), the other was remained uncertainly so far. We resolved their identity, based on the morphological observations with scanning electron microscopy. The formula of epithecal plate was recorded with 7 precingular, 3 intercalary and 4 apical plates (4', 3a, 7'). An apical pore was apparently present. The conspicuous morphology of the Peridinium was three spines on the hypothecal plates. The average body length and width were $33.6\;{\mu}m$ with a range of $26\~45{\mu}m$, and 25.7 with a range of $19\~31{\mu}m$, respectively; the cell was, therefore, shown slightly elongated. Based on their morphological characteristics, the causative organism was identified as P. aciculiferum (Lemm.), which was reported for the first time in Korean freshwater.

탄소화합물/Polymer Binder 복합체를 이용한 기체확산층 제조 및 성능 평가 (Preparation and Performance Evaluation of Gas Diffusion Layer Made of Carbon Compounds/Polymer Binder Composites)

  • 이지정;최범철;박윤경;이재영;이홍기
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2011년도 춘계학술대회 초록집
    • /
    • pp.92.2-92.2
    • /
    • 2011
  • 고분자전해질 연료전지 (PEMFC)의 가격 결정 요인 중 막 전극 접합체 (MEA)가 차지하는 비중은 약 45%정도이며, 이것을 구성하는 주요 부품인 기체 확산층 (GDL)은 carbon paper나 carbon cloth 형태가 사용되고 있다. 그렇지만 GDL을 제조하는 공정은 매우 복잡하고, 그 가격이 너무 높은 단점이 있다. 본 연구에서는 카본블랙, 흑연 등의 탄소화합물과 polymer binder를 이용하여 단순화된 공정으로 GDL을 제조하였다. 또한, GDL의 물리적 특성이 전극 성능에 미치는 영향을 분석하기 위하여 표면 morphology, 접촉각 및 표면에너지, 전기전도도, 기체투과도, porosity, pore distrivution 등을 측정하였고, 각각의 GDL 표면에 동량의 Pt 촉매를 도포하여 MEA를 제작한 후 그 성능을 평가하였다.

  • PDF

전기화학증착법으로 양극산화 알루미늄(AAO) 템플레이트를 이용한 Ni 나노와이어의 제조 및 성장에 관한 연구 (Fabrication and Growth of Ni Nanowires by using Anodic Aluminum Oxide(AAO) Template via Electrochemical Deposition)

  • 심성주;조권구;김유영
    • 한국분말재료학회지
    • /
    • 제18권1호
    • /
    • pp.49-55
    • /
    • 2011
  • Ni nanowires were fabricated using anodic aluminum oxide (AAO) membrane as a template by electrochemical deposition. The nanowires were formed within the walls of AAO template with 200 nm in pore diameter. After researching proper voltage and temperature for electrochemical deposition, the length of Ni nanowires was controlled by deposition time and the supply of electrolyte. The morphology and microstructure of Ni nanowires were investigated by field emission scanning electron microscope (FE-SE), X-ray diffraction (XRD) and transmission electron microscope (TEM).

양극산화 알루미나 주형 기반의 전해 증착법을 이용한 니켈 나노선의 합성 및 특성 연구 (Synthesis and Characterization of Nickel Nanowires by an Anodic Aluminum Oxide Template-Based Electrodeposition)

  • 임효령;좌용호;이영인
    • 한국분말재료학회지
    • /
    • 제22권3호
    • /
    • pp.216-220
    • /
    • 2015
  • Vertically oriented nickel nanowire arrays with a different diameter and length are synthesized in porous anodic aluminium oxide templates by an electrodeposition method. The pore diameters of the templates are adjusted by controlling the anodization conditions and then they are utilized as templates to grow nickel nanowire arrays. The nickel nanowires have the average diameters of approximately 25 and 260 nm and the crystal structure, morphology and microstructure of the nanowires are systematically investigated using XRD, FE-SEM and TEM analysis. The nickel nanowire arrays show a magnetic anisotropy with the easy axis parallel to the nanowires and the coercivity and remanence enhance with decreasing a wire diameter and increasing a wire length.

Fabrication of Macroporous Carbon Foam with Uniform Pore Size Using Poly(methyl methacrylate) Particles As The Template

  • Kim, Jin-Sil;Rhym, Young-Mok;Shim, Sang-Eun
    • 한국분말재료학회지
    • /
    • 제18권2호
    • /
    • pp.129-134
    • /
    • 2011
  • Herein, macroporous carbon materials were readily prepared by carbonization of cured body of resorcinol and formaldehyde using poly(methyl methacrylate) colloid microspheres which were employed as the template in the gelation of resorcinol with formaldehyde. The gel in the water was solvent exchanged with methanol and the wet gel was dried. After carbonization of the template-gel composite at $800^{\circ}C$, it was found that pores were left corresponding to the size of the template, yielding carbon materials with a fine porous structure with enlarged surface area and significant porosity. Properties of the carbon foams including the structure, morphology, thermal stability, and porosity were investigated. Finally, it was concluded that the method using polymer colloids as the template provided a facile route to prepare carbon foams.