• Title/Summary/Keyword: polypropylene and steel fiber

Search Result 80, Processing Time 0.023 seconds

Effect of Amorphous Steel Fiber on the Spalling Characteristics of High-strength Concrete (고강도콘크리트의 폭렬특성에 미치는 비정질 강섬유의 영향)

  • Kim, Jong-Ho;Kim, Gyu-Yong;Lee, Sang-Kyu;Hwang, Eui-Chul;Son, Min-Jae;Nam, Jeong-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2019.05a
    • /
    • pp.32-33
    • /
    • 2019
  • This study evaluated the effect of amorphous steel fibers on the spalling characteristics of high-strength concrete. with mix proportions of polypropylene (PP) fibers of 0.15% by concrete volume, and proportions of amorphous steel fibers of 0.3% and 0.5% by concrete volume. In the range of 0.3 vol% of amorphous steel fiber, the effect of suppression of the spalling and the prevention of degradation of strength was shown, but it was evaluated to be ineffective in the suppression of the spalling due to interferences in formation of pore network in the range of 0.5 vol.%.

  • PDF

Fire Resistance Performance for Hybrid Fiber Reinforced High Strength Concrete Column Member (하이브리드 섬유보강 고강도콘크리트 기둥부재의 내화성능)

  • Won, Jong-Pil;Jang, Chang-Il;Lee, Sang-Woo;Kim, Heung-Youl;Kim, Wan-Young
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.6
    • /
    • pp.827-832
    • /
    • 2008
  • This study evaluated fire resistance performance for hybrid (polypropylene+steel) fiber reinforced high strength concrete column. Full-size columns were constructed and tested with or without fibers using ISO-834 fire curve. As the result of test, Control specimen occurred serious spalling and indicated rapidly internal temperature increasing. Specimen with polypropylene fiber occurred not spalling but steady internal temperature increasing. Specimen with hybrid fiber occurred not spalling as well as does not propagated temperature distribution. Therefore, hybrid fiber reinforced column specimen indicated a good fire resistance performance than other cases.

Properties of Advanced Synthetic Fiber Reinforced Concrete for Improvement of Tunnel Shotcrete Performance (터널 숏크리트 성능 향상을 위한 고기능성 합성섬유 보강 콘크리트의 물성 평가)

  • Jeon, Chanki;Jeon, Joongkyu
    • Journal of the Society of Disaster Information
    • /
    • v.7 no.1
    • /
    • pp.43-50
    • /
    • 2011
  • The Application of Steel Fiber Shotcrete in tunneling construction has become part of tunneling practice at least since the 1970s because of its high bending and tensile properties. Over the past 3 decades, researcher from all over the world have been significantly developing the associated technologies for improved performance of SFRS. But still it has some major drawbacks in terms of durability, damage of pumping hose, wastage due to rebound concrete, corrosion and it costs high. To overcome this situation researcher has to look for some alternative material. Therefore, this part study deals with the three types of fiber in order to find good alternative for steel fiber. Polyamide and Polypropylene fiber were used in this study with 0.6, 0.5% mixing ratio. To evaluate its fresh and harden properties air content, slump, compressive, split tensile and bending strength were measured. After comparing the results of all three types of fiber reinforced concrete with its different mixing proportion this study propose that polyamide fiber with addition ratio of 0.6 % for field use.

Evaluation on Water Vapor Pressure of Amorphous Steel Fiber reinforced High Strength Concrete (비정질 강섬유 혼입 고강도콘크리트의 수증기압력 평가)

  • Kim, Duck-Woo;Kim, Gyu-Yong;Hwang, Eui-Chul;Son, Min-Jae;Baek, Jae-Wook;Nam, Jeong-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2018.11a
    • /
    • pp.44-45
    • /
    • 2018
  • In this study, water vapor pressure of high strength concrete reinforced with amorphous steel fiber(AF) was evaluated. Experimental results show that spalling occurs when the incorporation rate of amorphous steel fiber is 0.5 vol.% or more. This is because the ratio of AF increased per unit area influenced the formation of the water vapor pressure discharge passage by the polypropylene fiber(PPF) melting. Therefore, it is necessary to find the proper mixing ratio of AF and PPF to prevent spalling.

  • PDF

Experimental and statistical analysis of hybrid-fiber-reinforced recycled aggregate concrete

  • Tahmouresi, Behzad;Koushkbaghi, Mahdi;Monazami, Maryam;Abbasi, Mahdi Taleb;Nemati, Parisa
    • Computers and Concrete
    • /
    • v.24 no.3
    • /
    • pp.193-206
    • /
    • 2019
  • Although concrete is the most widely used construction material, its deficiency in shrinkage and low tensile resistance is undeniable. However, the aforementioned defects can be partially modified by addition of fibers. On the other hand, possibility of adding waste materials in concrete has provided a new ground for use of recycled concrete aggregates in the construction industry. In this study, a constant combination of recyclable coarse and fine concrete aggregates was used to replace the corresponding aggregates at 50% substitution percentage. Moreover, in order to investigate the effects of fibers on mechanical and durability properties of recycled aggregate concrete, the amounts of 0.5%, 1%, and 1.5% steel fibers (ST) and 0.05%, 0.1% and 0.15% polypropylene (PP) fibers by volumes were used individually and in hybrid forms. Compressive strength, tensile strength, flexural strength, ultrasonic pulse velocity (UPV), water absorption, toughness, elastic modulus and shrinkage of samples were investigated. The results of mechanical properties showed that PP fibers reduced the compressive strength while positive impact of steel fibers was evident both in single and hybrid forms. Tensile and flexural strength of samples were improved and the energy absorption of samples containing fibers increased substantially before and after crack presence. Growth in toughness especially in hybrid fiber-reinforced specimens retarded the propagation of cracks. Modulus of elasticity was decreased by the addition of PP fibers while the contrary trend was observed with the addition of steel fibers. PP fibers decreased the ultrasonic pulse velocity slightly and had undesirable effect on water absorption. However, steel fiber caused negligible decline in UPV and a small impact on water absorption. Steel fibers reduce the drying shrinkage by up to 35% when was applied solely. Using fibers also resulted in increasing the ductility of samples in failure. In addition, mechanical properties changes were also evaluated by statistical analysis of MATLAB software and smoothing spline interpolation on compressive, flexural, and indirect tensile strength. Using shell interpolation, the optimization process in areas without laboratory results led to determining optimal theoretical points in a two-parameter system including steel fibers and polypropylene.

An Experimental Study on the Crack and Fracture Behavior of FRC Column (섬유보강콘크리트기둥의 균열 및 파괴거동에 관한 실험적 연구)

  • 박승범;김의성;홍석주;윤준석
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1997.10a
    • /
    • pp.333-338
    • /
    • 1997
  • This paper describes an experimental study on the crack and fracture behavior of the FRC column. The test were carried out as Fiber contents in the Steel Fiber Reinforced Concrete and addition of Polypropylene Fiber in PFRC for evaluate the ability of ductility. In this study, the width and size of crack reduced remarkably and the progress of cracks were restrained by the steel fiber contents increasing, and in the case of PFRC the occurrence of initial crack reduced conspicuously. Accordingly, the addition of steel fiber in Reinforced Concrete Columns considerably prevent an unexpected buckle and rupture, secure durability and stability of columns.

  • PDF

Performance of fire damaged steel reinforced high strength concrete (SRHSC) columns

  • Choi, Eun Gyu;Kim, Hee Sun;Shin, Yeong Soo
    • Steel and Composite Structures
    • /
    • v.13 no.6
    • /
    • pp.521-537
    • /
    • 2012
  • In this study, an experimental study is performed to understand the effect of spalling on the structural behavior of fire damaged steel reinforced high strength concrete (SRHSC) columns, and the test results of temperature distributions and the displacements at elevated temperature are analyzed. Toward this goal, three long columns are tested to investigate the effect of various test parameters on structural behavior during the fire, and twelve short columns are tested to investigate residual strength and stiffness after the fire. The test parameters are mixture ratios of polypropylene fiber (0 and 0.1 vol.%), magnitudes of applied loads (concentric loads and eccentric loads), and the time period of exposure to fire (0, 30, 60 and 90 minutes). The experimental results show that there is significant effect of loading on the structural behaviors of columns under fire. The loaded concrete columns result more explosive spalling than the unloaded columns under fire. In particular, eccentrically loaded columns are severely spalled. The temperature distributions of the concrete are not affected by the loading state if there is no spalling. However, the loading state affects the temperature distributions when there is spalling occurred. In addition, it is found that polypropylene fiber prevents spalling of both loaded and unloaded columns under fire. From these experimental findings, an equation of predicting residual load capacity of the fire damaged column is proposed.

Interaction of magnetic water and polypropylene fiber on fresh and hardened properties of concrete

  • Ansari, Mokhtar;Safiey, Amir
    • Steel and Composite Structures
    • /
    • v.39 no.3
    • /
    • pp.307-318
    • /
    • 2021
  • Utilizing fibers is an effective way to avoid the brittle behavior of the conventional concrete and can enhance its ductility. In particular, propylene fibers can improve concrete properties, including energy absorption, physical and mechanical properties, controlling shrinkage cracks. The increase of fiber density leads to an increase of the overlapping surface of the fiber of concrete and, in turn, a decrease of cracks developed in the concrete. However, the workability of fiber reinforced concrete tends to be lower than the conventional concrete owing mainly to the hairline thickness and excessive concentration of fibers. The low slump of concrete impedes the construction of reinforced concrete members. In this research, we study if the utilization of magnetic water can alleviate the workability issue of young fiber reinforced concrete. To this end, the compressive and flexural strength of four types of concrete (conventional concrete, fiber reinforced concrete, magnetic concrete, magnetic fiber-reinforced concrete) is studied and compared at three different ages of 7, 14, and 28 days. In order to study the influence of the fiber density and length, a study on specimens with three different fiber density (1, 2, 5 kg of fiber in each cubic meter of concrete) and fiber length (6, 12, 18 mm) is undertaken. The result shows the magnetic fiber concrete can result in an increase of the flexural and compressive strength of concrete at higher ages.

Fire Resistance Performance of Fiber-Cocktail Reinforced 50 MPa High Strength Concrete (섬유혼입된 50 MPa 고강도 콘크리트의 내화성능)

  • Youm, Kwang-Soo;Jeon, Hun-Kyu;Park, Jong-Heon
    • Journal of Korean Society of societal Security
    • /
    • v.2 no.3
    • /
    • pp.55-60
    • /
    • 2009
  • After applying the fiber cocktail(polypropylene and steel fibers) into the mixture of high strength concrete with a compressive strength of 50 MP, the fire test was carried out on specimens in order to evaluate the fire resistance performance, such as possible explosive spalling, temperature distributions of concrete and rebar. According to an enforcement ordinance, four column specimens were exposed to the fire for 180 minutes based on the standard curve of ISO-834. No explosive spalling has been observed. The required minimum quantity of polypropylene to prevent explosive spalling is more than 0.57 kg per unit concrete volume. The comparing test results from temperature distributions of concrete and rebar has found that the difference of fiber quantity is insignificant.

  • PDF

Experimental and numerical study of large high strength bolt shear connector embedded in HFRC

  • Yuliang He;Zhengxin Wang;Weiming Wu;Ying Yang;Yiqiang Xiang
    • Steel and Composite Structures
    • /
    • v.49 no.2
    • /
    • pp.197-213
    • /
    • 2023
  • To investigate the static properties of large high strength bolt shear connector in hybrid fiber-reinforced concrete (HFRC) and normal concrete (NC), eight push-out test specimens with single/double nut and HFRC/NC slabs were designed and push-out tests were conducted. A fine 3D nonlinear finite element (FE) model including HFRC constitutive model was established by using ANSYS 18.0, and the test results were used to verify FE models of the push-out test specimens. Then a total of 13 FE models were analyzed with various parameters including fiber volume fractions of HFRC, bolt diameter and thickness of steel flange. Finally, the empirical equations considering the contribution of polypropylene fiber (PF) and steel fiber (SF) obtained from the regression of the test results and FE analysis were recommended to evaluate the load-slip curve and ultimate capacity of the large high strength bolt shear connector embedded in HFRC/NC.