• 제목/요약/키워드: pin-on-disk

검색결과 247건 처리시간 0.022초

유압피스톤 습동재료의 마멸특성 해석 (Analysis of Wear Characteristics for Sliding Members of Hydraulic Rotary Actuator)

  • 김성희;김동호;이광영;박흥식;전태옥
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1999년도 제29회 춘계학술대회
    • /
    • pp.101-108
    • /
    • 1999
  • This paper was undertaken to do morphological analysis of wear particles for sliding members hydrauric rotary acuator. The lubricating wear test was performed under different experimental conditions using the wear test device and wear specimens of the pin on disk type was rubbed in paraffinic base oil by three kinds of lubricating materials, varying applied load, sliding distance. The four shape parameters (50% volumetric diameter, aspect, roundness and reflectivity) are used for morphological analysis of wear particles. The results showed that the four shape parameters of wear particles depend on a kind of the lubricating materials. It was capable of presuming wear volume for three kinds of materials on driving time.

  • PDF

경두레일 용접부의 미끄럼 환경변화에 따른 마찰 및 마멸특성 연구 (Experimental Study on Friction and Wear Characteristics of Head Hardened Weld Rails Under Various Sliding Environments)

  • 김청균;황준태
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1999년도 제29회 춘계학술대회
    • /
    • pp.345-353
    • /
    • 1999
  • This paper presents friction and wear related results of thermite and gas pressure welded rails under various environmental contact conditions. A welded rail which is manufactured by thermite welding and gas pressure one has been tested rail full range of test conditions in a pin-on-disk wear testing machine. The results show that the friction coefficient and wear rates of a welded rail are heavily dependent on the contact pressures and sliding environments for two welding methods such as thermite and gas pressure weldings.

  • PDF

B$_{4}$C의 첨가에 따른 동계소결합금 마찰재의 마찰특성 변화에 관한 연구 (A Study on the Frictional Characteristics of B$_{4}$C Added Cu Base Sintered Friction Material)

  • 정동윤;김기열;조정환
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1996년도 제23회 춘계학술대회
    • /
    • pp.99-107
    • /
    • 1996
  • Examined in this paper is the effect of B$_{4}$C addition on the frictional characteristics of Cu-Sn based sintered friction material. For the specimens 1%, 2% and 4% of B$_{4}$C were added into the reference material. A pin-on-disk type friction tester was used to measure the friction and wear with respect to the surface temperature and sliding distance. Wear mechanism of each specimen is analyzed in the view point of the oxide film formation. The specimen containing 4% of B$_{4}$C showed stable friction and low wear since the oxide film was sustained up to higher surface temperature ranges.

  • PDF

마멸입자 해석을 통한 유압로터용 Slipper - Pad의 손상상태 추정 (Presumption of Slipper-pad Fault Condition for Hydraulic Rotary Actuator)

  • 전성재;조연상;서영백;박흥식
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2000년도 제31회 춘계학술대회
    • /
    • pp.62-67
    • /
    • 2000
  • This paper was undertaken to do morphological analysis of wear debris for slipper-Pad of hydraulic rotary acuator. The lubricating wear test was performed under different experimental conditions using the wear test device and wear specimens of the pin on disk type was rubbed in paraffinic base oil by three kinds of lubricating materials, varying applied load, sliding distance. The four shape parameters(50% volumetric diameter, aspect, roundness and reflectivity) are used for morphological analysis of wear debris. The results showed that the four shape parameters of wear debris depend on a kind of the lubricating condition. It was capable of presuming wear volume for slipper-pad of hydraulic rotary acuator on driving time.

  • PDF

B.390 알루미늄 합금의 마모특성에 미치는 초정Si 입자크기와 잔류응력의 영향 (Effect of Primary Si size and Residual Stress on the Wear Properties of B.390 Al Alloys)

  • 김헌주;김성재
    • 열처리공학회지
    • /
    • 제19권1호
    • /
    • pp.20-29
    • /
    • 2006
  • Wear behaviour of B.390 aluminum alloy with different particle sizes of primary Si against a SM45C counterface was studied as a function of wear load and sliding velocity, using pin-on-disk apparatus under dry condition. The wear rate of specimen with fine primary Si particles showed increased wear resistance at high wear load, on the other side wear resistance of coarse primary Si particle size was improved at low wear load. As the compressive residual stress in the matrix increased remarkably by liquid nitrogen(LN) treatment, wear resistance of the LN treated specimen was more excellent than that of T6 treated specimen.

$B_4C$의 첨가에 따른 동계소결합금 마찰재의 마찰특성 변화에 관한 연구 (A Study on the Frictional Characteristics of $B_4C$ Added Cu Base Sintered Friction Materials)

  • 정동윤;김기열;조정환
    • Tribology and Lubricants
    • /
    • 제12권3호
    • /
    • pp.48-54
    • /
    • 1996
  • Examined in this paper, is the effect of B$_{4}$C addition on the frictional characteristics of Cu-Sn based sintered friction materials. For the specimens 1wt%, 2wt% and 4wt% of B$_{4}$C were added into the reference material. A pin-on-disk type friction tester was used to,measure the friction torque with respect to the surface temperature and sliding distance. Wear mechanism of each specimen is analyzed in the view point of the oxide film formation. The specimen containing 4wt% of B$_{4}$C showed stable friction and low wear since the oxide film was sustained up to higher surface temperature ranges.

탄소강의 가공조건과 마찰.마멸과의 관계 (Effect of Machining Condition on Friction and Wear of Steel)

  • 정종현;김대은
    • 대한기계학회논문집A
    • /
    • 제20권5호
    • /
    • pp.1468-1476
    • /
    • 1996
  • Surface integrity is dictated by the fabrication process of the metal part. In this work, steel specimens were prepared under various mechine conditions to achieve different degrees of deformation state. The tribological characteristics of the speciments were tested using a pin-on-disk type apparatus and other surface characterization tools. It is shown that though frictional characteristics are similar, the wear rate is significantrly affected by the properties of the surface. In the case of steel, surface cracks resulted in high wear despite the relatively high hardness of the specimen. Also, the sliding action were found to reduce the residual stress on the surface. These results indicate that there is a strong relationship between surface integrity and the tribological properties of steel, and therefore the machining condition should be optimized woth respect to tribological performance of a steel part.

대기중의 습도에 따른 탄소강의 마모와 마찰 (Wear and Friction of the Carbon Steel for Atmospheric Humidity)

  • 연규현
    • 한국생산제조학회지
    • /
    • 제9권3호
    • /
    • pp.41-47
    • /
    • 2000
  • The atmospheric humidity is varied between 30% and 90% with season in Korea. Thus the influence of humidity on the behavior of wear for tools and dies. This paper presents the influence of atmospheric humidity on the wear of carbon the un-lubricated pin-on-disk sliding contact. it was found that the severe wear is dominant at a low humidity and the mild wear is strongly related with the carbon concentration of the steel at a high humidity in this study. The experiments were carried out in a chamber where the humidity was accurately maintained by humidifier. To investigate the relationship three different carbon steels such as 1020, 1041, and 1034 steels were used.

  • PDF

레일 용접부의 미끄럼 환경변화에 따른 마찰 및 마멸특성 연구 (A Study on Friction and Wear Characteristics of Welded Rails Under Various Sliding Environments)

  • 김청균;황준태;나성훈;민경주
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1998년도 제28회 추계학술대회
    • /
    • pp.59-66
    • /
    • 1998
  • This paper presents friction and wear related results of thermite and gas pressure welded rails under various environmental contact conditions. A welded rail which is fabricated by thermite welding and gas pressure one has been tested over full range of test conditions in a pin-on-disk wear testing machine. The results show that the friction coefficient and wear rates of a welded rail are heavily dependent on the contact pressures and sliding environments for two welding methods such as thermite and gas pressure weldings.

  • PDF

규칙화된 Fe-Al 계 금속간 화합물의 산화특성과 미끄럼 마모거동과의 관계에 대한 연구 (A Study on the Relationship between Oxidation and Sliding Wear Behavior of Ordered Fe-Al Intermetallic Alloys)

  • 김용석
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 춘계학술대회논문집
    • /
    • pp.144-148
    • /
    • 1999
  • The relationship between oxidation and sliding wear behavior of Fe-28 at%. Al alloys with B2 ordered structure has been investigated. Sliding wear tests of the alloys have been carried out under various environmental conditions using a pin-on-disk wear tester. The wear rate of the ordered alloys in an oxygen atmoshpere was found to be much lower than in an oxygen atmosphere showed that Fe2O oxides formed on the wearing surface. The oxide layer prevented direct contact of the two mating materials and therefore improved wear resistance of the Fe-Al intermetallic alloy. It was found that the surface Al2O3 oxide layer which provides good oxidation resistance and improved mechanical properties broke down easily and didnot function properly as an oxidation barrier.

  • PDF