• Title/Summary/Keyword: oxygen annealing

Search Result 506, Processing Time 0.027 seconds

Physical Property Change of the Gapless Semiconductor $PbPdO_2$ Thin Film by Ex-situ Annealing

  • Choo, S.M.;Park, S.M.;Lee, K.J.;Jo, Y.H.;Park, G.S.;Jung, M.H.
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.371-372
    • /
    • 2012
  • We have studied lead-based gapless semiconductors, $PbPdO_2$, which is very sensitive to external parameters such as temperature, pressure, electric field, etc[1]. We have fabricated pure $PbPdO_2$, Co- and Mn-doped $PbPdO_2$ thin films using the pulsed laser deposition. Because of the volatile element of Pb, it is very difficult to grow the films. Note that in case of $MgB_2$, Mg is also volatile element. So in order to enhance the quality of $MgB_2$, some experiments are carried out in annealing with Mg-rich atmosphere [2]. This annealing process with volatile element plays an important role in making smooth surface. Thus, we applied such process to our studies of $PbPdO_2$ thin films. As a result, we found the optimal condition of ex-situ annealing temperature ${\sim}650^{\circ}C$ and time ~12 hrs. The ex-situ annealing brought the extreme change of surface morphology of thin films. After ex-situ annealing with PbO-rich atmosphere, the grain size of thin film was almost 100 times enlarged for all the thin films and also the PbO impurity phase was smeared out. And from X-ray diffraction measurements, we determined highly crystallized phases after annealing. So, we measured electrical and magnetic properties. Because of reduced grain boundary, the resistivity of ex-situ annealed samples changed smaller than no ex-situ sample. And the carrier densities of thin films were decreased with ex-situ annealing time. In this case, oxygen vacancies were removed by ex-situ annealing. Furthermore, we will discuss the transport and magnetic properties in pure $PbPdO_2$, Co- and Mn-doped $PbPdO_2$ thin films in detail.

  • PDF

Thermal Stability of $\textrm{RuO}_2$ Thin Film Annealed at High Temperature in Oxygen Atmosphere ($\textrm{RuO}_2$ 박막의 산소 분위기 열처리시 열적 안정성에 관한 연구)

  • O, Sang-Ho;Park, Chan-Gyeong;Baek, Hong-Gu
    • Korean Journal of Materials Research
    • /
    • v.8 no.12
    • /
    • pp.1090-1098
    • /
    • 1998
  • $RuO_2$ thin films were deposited on Si and Ru/Si substrates by rf magnetron reactive sputtering and annealed in oxygen atmosphere(1atm) to investigate their thermal stability and diffusion barrier property. $RuO_2$ thin films were thermally stable up to 700\ulcorner for 10min. in oxygen atmosphere and showed excellent barrier property against the interdiffusion of silicon and oxygen. After annealing at $750^{\circ}C$ , however, volatilization to higher oxide occurred at the surface and inside of $RuO_2$ thin film and diffusion barrier property was also deteriorated. When annealed at $800^{\circ}C$, $RuO_2$thin film showed a different microstructure from that of $RuO_2$ thin film annealed at 75$0^{\circ}C$. It is likely that surface defect structure of $RuO_2$, $RuO_3$, and excess oxygen had an influence on the mode of volatilization with increasing annealing temperature.

  • PDF

Study of the effect of vacuum annealing on sputtered SnxOy thin films by SnO/Sn composite target (SnO/Sn 혼합 타겟으로 스퍼터 증착된 SnO 박막의 열처리 효과)

  • Kim, Cheol;Cho, Seungbum;Kim, Sungdong;Kim, Sarah Eunkyung
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.24 no.2
    • /
    • pp.43-48
    • /
    • 2017
  • Conductive $Sn_xO_y$ thin films were fabricated via RF reactive sputtering using SnO:Sn (80:20 mol%) composite target. The composite target was used to produce a chemically stable composition of $Sn_xO_y$ thin film while controlling structural defects by chemical reaction between tin and oxygen. During sputtering pressure, RF power, and substrate temperature were fixed, and oxygen partial pressure was varied from 0% to 12%. Annealing process was carried out at $300^{\circ}C$ for 1 hour in vacuum. Except $P_{O2}=0%$ sample, all samples showed the transmittance of 80~90% and amorphous phase before and after annealing. Electrically stable p-type $Sn_xO_y$ thin film with high transmittance was only obtained from the oxygen partial pressure at 12%. The carrier concentration and mobility for the $P_{O2}=12%$ were $6.36{\times}10^{18}cm^{-3}$ and $1.02cm^2V^{-1}s^{-1}$ respectively after annealing.

Effects of Annealing Conditions on the Properties of Bi1-xLaxTi3O12 Thin Films (열처리 조건이 Bi1-xLaxTi3O12 (x=0.75) 박막의 특성에 미치는 효과)

  • Park Moon Heum;Kim Sang Su;Gang Min Ju;Ha Tae Gon
    • Korean Journal of Materials Research
    • /
    • v.14 no.10
    • /
    • pp.701-706
    • /
    • 2004
  • Bismuth layered structure ferroelectric thin films, La-substituted $Bi_{4}Ti_{3}O_{12}$ ($Bi_{1-x}La_{x}Ti_{3}O_{12}$, x=0.75, BLT) were prepared on the $Pt(111)/Ti/SiO_2/Si(100)$ substrates by a sol-gel spin coating process. The thin films were annealed in various conditions, i.e., oxygen, nitrogen and vacuum atmospheres for various annealing time. We investigated the annealing condition effects on the grain orientation and ferroelectric properties. The measured XRD patterns revealed that the BLT thin films showed only $Bi_{4}Ti_{3}O_{12}$-type phase with random orientation. $La^{3+}$ ion substitution for $Bi^{3+}$ ion in perovskite layers of $Bi_{4}Ti_{3}O_{12}$ decreased the degree of c-axis orientation and increased the remanent polarization ($2P_{r}$). The remanent polarization ($2P_{r}$) and the coercive field ($2E_{c}$) of the BLT thin film annealed at $650^{\circ}C$ for 5 min in oxygen atmosphere were $87{\mu}C/cm^2$ and 182 kV/cm, respectively, at an applied electric field of 240 kV/cm. For all of the BLT thin films annealed in various conditions, the fatigue resistance was shown. The improvement of ferroelectric properties with La substitution in $Bi_{4}Ti_{3}O_{12}$ could be attributed to the changes in space charge densities and grain orientation in the thin film.

Effects of W-N/Pt Bottom Electrode on the Ferroelectric Degradation of $Sr_{0.8}Bi_{2.4}Ta_2O_9/Pt/Si$ Structure due to the Hydrogen Annealing ($Sr_{0.8}Bi_{2.4}Ta_2O_9/Pt/Si$ 구조의 수소열처리에 의한 강유전특성 열화에 미치는 W-N/Pt 전극효과)

  • Lee, Chang-Woo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.11 no.4 s.33
    • /
    • pp.87-91
    • /
    • 2004
  • We have investigated the effects of W-N/Pt bottom electrode on the ferroelectric degradation of $Sr_{0.8}Bi_{2.4}Ta_2O_9(SBT)/Pt$ due to hydrogen annealing at $350^{\circ}C$ in $N_2$ gas atmosphere containing $5{\%}\;H_2$ gas for 1hr. As a result, inserting the W-N thin films between SBT and Pt, this W-N thin film prevents hydrogen molecules to be chemisorbed at the Pt electrode surface of at the electrode/ferroelectric interface during hydrogen annealing. These hydrogen atoms can diffuse into the SBT and react with the oxide causing the oxygen deficiency in the SBT film, which will result in the ferroelectric degradation. Experimental results show that W-N thin film is a good diffusion barrier during the hydrogen annealing.

  • PDF

Effects of Film Thickness and Post-Annealing Temperature on Properties of the High-Quality ITO Thin Films with RF Sputtering Without Oxygen (산소 유입 없이 RF 스퍼터로 증착한 고품질 ITO 박막의 두께와 열처리 온도에 따른 박막의 특성 변화)

  • Jiha Seong;Hyungmin Kim;Seongmin Shin;Kyunghwan Kim;Jeongsoo Hong
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.37 no.3
    • /
    • pp.253-260
    • /
    • 2024
  • In this study, ITO thin films were fabricated on a glass substrate at different thicknesses without introducing oxygen using RF sputtering system. The structural, electrical, and optical properties were evaluated at various thicknesses ranging from 50 to 300 mm. As the thickness of deposited ITO thin film become thicker from 50 to 100 mm, carrier concentration, mobility, and band gap energy also increased while the resistivity and transmittance decreased in the visible light region. When the film thickness increased from 100 to 300 mm, the carrier concentration, mobility, and band gap energy decreased while the resistivity and transmittance increased. The optimum electrical properties were obtained for the ITO film 100 nm. After optimizing the thickness, the ITO thin films were post-annealed at different temperatures ranging from 100 to 300℃. As the annealing temperature increased, the ITO crystal phase became clearer and the grain size also increased. In particular, the ITO thin film annealed at 300℃ indicated high carrier concentration (4.32 × 1021 cm-3), mobility (9.01 cm2/V·s) and low resistivity (6.22 × 10-4 Ω·cm). This means that the optimal post-annealing temperature is 300℃ and this ITO thin film is suitable for use in solar cells and display application.

Fabrication of branched Ga2O3 nanowires by post annealing with Au seeds

  • Lee, Mi-Seon;Seo, Chang-Su;Gang, Hyeon-Cheol
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2015.08a
    • /
    • pp.203-203
    • /
    • 2015
  • Gallium Oxide (Ga2O3) has been widely investigated for the optoelectronic applications due to its wide bandgap and the optical transparency. Recently, with the development of fabrication techniques in nanometer scale semiconductor materials, there have been an increasing number of extensive reports on the synthesis and characterization of Ga2O3 nano-structures such as nano-wires, nano-belts, and nano-dots. In contrast to typical vapor-liquid-solid growth mode with metal catalysts to synthesis 1-dimensional nano-wires, there are several difficulties in fabricating the nano-structures by using sputtering techniques. This is attributed to the fact that relatively low growth temperatures and higher growth rate compared with chemical vapor deposition method. In this study, Ga2O3 nanowires (NWs) were synthesized by using radio-frequency magnetron sputtering method. The NWs were then coated by Au thin films and annealed under Ar or N2 gas enviroment with no supply of Gallium and Oxygen source. Several samples were prepared with varying the post annealing parameters such as gas environment annealing time, annealing temperature. Samples were characterized by using XRD, SEM, and PL measurements. In this presentation, the details of fabrication process and physical properties of branched Ga2O3 NWs will be reported.

  • PDF

The post annealing effect on the properties of AZO films (AZO 박막의 후 열처리에 따른 특성변화)

  • Ko, Ki-Han;Seo, Jae-Keun;Kim, Jae-Kwang;Cho, Hyung-Jun;Hong, Byung-You;Choi, Won-Seok
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.06a
    • /
    • pp.457-458
    • /
    • 2009
  • In this work, transparent conducting Al-doped zinc oxide (AZO) films were prepared on Coming glass substrate by RF magnetron sputtering using an Al-doped ZnO target (Al: 2 wt.%) at room temperature and all films were deposited with athickness of 150 nm. We investigated the effects of the post-annealing temperature and the annealing ambient on structural, electrical and optical properties of AZO films. The films were annealed at temperatures ranging from 300 to $500^{\circ}C$ in steps of $100^{\circ}C$ using rapid thermal annealing equipment in oxygen. The thickness of the film was observed by field emission scanning electron microscopy (FE-SEM) and grain size was calculated from the XRD spectra using the Scherrer equation and their electrical properties were investigated using a hole measurement and the reflectance of AZO films was investigated by UV-VIS spectrometry.

  • PDF

Preparation of Sr2FeMoO6 Thin Films by RF Magnetron Sputtering and Their Electrical Conduction Properties (RF 스퍼터법을 이용한 Sr2FeMoO6 박막 제조 및 전기전도 특성)

  • Ryu, Hee-Uk;Sun, Ho-Jung
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.12
    • /
    • pp.966-972
    • /
    • 2010
  • Single-phase $Sr_2FeMoO_6$ thin films were produced by RF magnetron sputtering for use as electrodes in integrated sensors and found to be good conductors at room temperature. The films were deposited from a powder-type sputtering target under various conditions, and were crystallized by annealing. Elimination of $O_2$ gas during deposition, by the use of a solely Ar sputtering gas under a working pressure as low as possible, and vacuum annealing were important to promote the $Sr_2FeMoO_6$ phase. However, oxygen exclusion from sputtering and annealing was not enough to yield single-phase $Sr_2FeMoO_6$: hydrogen annealing was also required. Film production was optimized by varying the deposition parameters and hydrogen annealing conditions. The film had good electrical conduction, with a low resistivity of $1.6{\times}10^{-2}\Omega{\cdot}cm$ at room temperature.

Influence of Thermal Treatment on Surface Morphology of Tin Dioxide Thin Films (열처리에 따른 SnO2 박막의 표면형상)

  • Park, Kyung-Hee;Ryu, Hyun-Wook;Seo, Yong-Jin;Lee, Woo-Sun;Hong, Kwang-Jun;Park, Jin-Seong
    • Korean Journal of Materials Research
    • /
    • v.13 no.7
    • /
    • pp.442-446
    • /
    • 2003
  • Tin dioxide ($SnO _2$) thin films were deposited at $375^{\circ}C$ on alumina substrate by metal-organic chemical vapor deposition. A few hillocks like a cauliflower were observed and the number of hillock on thin film surface increased with annealing temperature in air atmosphere. The oxygen content and the binding energy during air annealing at$ 500^{\circ}C$ came to close the stoichiometric $SnO_2$. The cauliflower hillocks seem to be the result of the continuous migration of the tiny grains to release the stress of an expanded grain. Sensitivity of CO gas depended on annealing temperature and increased with increasing annealing temperature.