Bond Strength of Mortar mixed Activated Hwangtoh

  • Go, Seong-Seok;Yeo, Sang-Ku;Lee, Hyun-Chul
    • Journal of the Korea Institute of Building Construction
    • /
    • v.12 no.5
    • /
    • pp.468-477
    • /
    • 2012
  • This study aimed to mix and test mortar incorporating activated Hwangtoh to improve the Hwangtoh brick bond strength of brick structures. To do this, the bond strength correlation of mortar was analyzed by means of materials and experiment factors and levels, and the optimum conditions were suggested after analyzing the physical properties of brick and the mix ratio of mortar and additive. Furthermore, the compressive strength and bond strength were found to be in inverse proportion, and in terms of the materials and mixing level, W/C ratio, substitution ratio of activated Hwangtoh, and fine aggregate grading were shown to have a considerable influence on the strength. In conclusion, the optimum mixing conditions to improve the bond strength are found to set W/C ratio at 65% and replacmenet ratio of activated Hwangtoh at 10%.

Fundamental Study of Mix Proportions of High-Flow Cement-Based Mortar for Gravel-Fill Used in Restoration of Collapsed Roads (도로유실 복구를 위한 골재 충전 고흐름도 모르타르의 기초 배합 연구)

  • Cho, Hyun Myung;Jeon, Sang Pyo;Kim, Seung Won;Yun, Kyong Ku;Park, Cheol Woo
    • International Journal of Highway Engineering
    • /
    • v.17 no.2
    • /
    • pp.63-70
    • /
    • 2015
  • PURPOSES: As a part of our research into repair techniques for roads that have collapsed as a result of a natural disaster, this study set out to find the optimum mix proportion for gravels to be used to restore a damaged area. METHODS: This study considered flow and strength-development characteristics. The experimental variables were the W/C ratio, the usage of the admixture, the types of cement, and the quantity of fine aggregate over three different experimental stages. The compressive strength was measured at 12 hours, one day, three days, and seven days. RESULTS : The flow varied with the amount of fine aggregate and the use of a high-range water-reducing (HRWR) admixture. The compressive strength also varied with respect to the type of cement and the W/C ratios. The strength satisfied the expected requirement of 21 MPa after one day, provided the mix proportion was appropriate. CONCLUSIONS: A gravel-filling high-flow cement-based mortar exhibited strength and consistency with a W/C ratio in the range of 0.40 to 0.45, assuming the use of HRWR at 0.5 to 0.7% and a fine aggregate/cement ratio of 1.0 to 1.5.

Properties of the high strength and self-compacting concrete according to the replacement ratio of fly ash (플라이애쉬의 치환율에 따른 고강도 자기충전 콘크리트의 특성)

  • Kwon, Yeong-Ho;Lee, Hyun-Ho;Lee, Hwa-Jin;Ha, Jae-Dam
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.05b
    • /
    • pp.85-88
    • /
    • 2006
  • This study describes the optimum mix proportion of the high strength and self-compacting concrete placed in main structures of LNG above tank. This concrete requires high strength level about $60{\sim}80MPa$, low hydration heat, balance between workability and consistency without vibrating in the actual work. For this purpose, low heat portland cement and fly ash are selected and design factors including water-binder ratio, replacement ratio of fly ash are tested. As experimental results, low heat portland cement shows lower the confined water ratio than another cement type and the optimum replacement ratio of fly ash in order to improve properties of the binder-paste shows 10% by cement weight considering test results of the confined water ratio$({\beta}p)$. Also, flowability of the high strength and self-compacting concrete by using fly ash about $10{\sim}20%$ is improved. The replacement ratio of fly ash 10% and water-binder ratio $25{\sim}27%$ are suitable to the design strength 80MPa and cost, In case of the design strength 60MPa, the replacement ratio of fly ash and water-binder ratio show 20% and $25{\sim}30%$ separately. Based on the results of this study, the optimum mix proportions of the high strength and self-compacting concrete will be applied to the construction of LNG above tank as a new type.

  • PDF

Suggesting Optimum Mix Proportion of Hardener for Soil-pavement Concrete Incorporating Natural Organic Lime and Magnesia-lime (천연유기석회 및 고토석회를 조합한 흙 포장 콘크리트용 경화재의 최적배합안 도출)

  • Han, Min-Cheol;Han, Jun-Hui
    • Journal of the Korea Institute of Building Construction
    • /
    • v.20 no.2
    • /
    • pp.113-121
    • /
    • 2020
  • Lots of soil-pavement concrete placed showed a number of problems such as decreasing strength, and durability. In this research, to provide a solution of the problem reported the wasting materials of natural organic lime and magnesia lime were used as a hardener to achieve sufficient performance of soil-pavement concrete. Namely, as a stimulus of blast furnace slag, the natural organic lime and magnesia lime were tested within the mix proportion of 0 to 10 % for each lime to make a new hardener. As a result, in the case of mortar with 1 to 3 % of cement to fine aggregate, 30 % replaced blast furnace slag showed the more favorable results with 5 to 5 % of mix proportion for natural organic lime and magnesia lime.

A Study of light Weight Porous Concrete Using Meta-kaolin (경량기포콘크리트에 고령토의 첨가효과에 관한 연구)

  • Ganbileg, Gayabazar;Kong, Kyoung-Rok;Kang, Heon-Chan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.905-908
    • /
    • 2006
  • In this study examines physical and mechanical properties the use of domestic low grade meta-kaolin in light weight porous concrete. For this purpose light weight porous concrete incorporating low grade meta-kaolin admixture, was tested for tensile strength and acoustic characteristics. Checking tensile strength of cement and low grade meta-kaolin mixture was used to determine the optimum mix proportion of the low grade meta-kaolin admixture. In this paper sound absorbing material has been investigated by using the light weight porous concrete.

  • PDF

The Selection of Optimal Mixing Proportion and Cost Analysis in the SFC (초유동 콘크리트의 최적배합 선정방법 및 경제성 분석)

  • Park, Chil-Lim;Kim, Moo-Han;Kwon, Yeong-Ho;Lee, Sang-Soo;Won, Cheol
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.10a
    • /
    • pp.262-268
    • /
    • 1998
  • This research is to examine the selected method of optimal mixing proportion and cost analysis in the super flowing concrete. As confined water $ratio($\beta_p$)$ and K is introduced, itis to establish optimal mixing design of super flowing concrete according to the steps of paste, mortar and concrete. From paste and mortar test, it was led to $$\beta_p$$ and $K_p$satisfying the optimum condions depending on the kinds of binders. Then $$\beta_p$$ and $K_p$ is reflected to the mix condition of super flowing concrete. The result of test, the mix condition of super flowing concrete satisfied the quality performance of concrete with adjustment of additional rate of the superplasticizer. Besides, in case of design strength $350kg/\textrm{cm}^2$ of concrete, material cost in super flowing concrete is able to be reduced 5~16% in replacement of fly ash 30% in ordinary portland cement and slag cement.

  • PDF

Application of PBMD for High Strength Concrete Mix Proportion Design (고강도 콘크리트의 성능기반형 배합설계방법)

  • Lee, Sang-Won;Oh, Il-Sun;Lee, Hoo-Seok;Park, Sung-Hwan;Kim, Jang-Ho
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2010.05a
    • /
    • pp.405-406
    • /
    • 2010
  • This paper is a study about application of recently proposed Performance Based Mixture Design (PBMD) for design of high strength concrete (HSC) to obtain HSC mix proportion that satisfies required performances. Based on extensive experimental results obtained for various material and performance parameters of HSC, the application feasibility of the developed PBMD procedure for HSC has been verified. Also, the proposed PBMD procedure has been used to perform application examples to obtain desired target performances of HSC with optimum concrete mixture proportions using locally available materials, local environmental conditions, and available concrete production technologies.

  • PDF

Optimum Mix Design of Alkali-Activated Cement Mortar Using Bottom Ash as Binder (바텀애쉬를 결합재로 사용한 알칼리 활성화 시멘트 모르타르의 최적배합에 관한 연구)

  • Kang, Su-Tae;Ryu, Gum-Sung;Koh, Kyoung-Taek;Lee, Jang-Hwa
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.4
    • /
    • pp.487-494
    • /
    • 2011
  • In this research, the possibility of using bottom ash as a binder for the alkali-activated cement mortar is studied. Several experiments were performed to investigate the variation of the material properties according to the mix proportion. In the experimental program, the flowability and compressive strength were evaluated for various values of water/ash ratio, activator/ash ratio, sodium silicate to sodium hydroxide ratio, curing temperature, and the fineness of bottom ash as the main variables. The experimental results showed that high strength of 40 MPa or greater could be achieved in $60^{\circ}C$ high temperature curing condition with proper flowability. For $20^{\circ}C$ ambient temperature curing, the 28 days compressive strength of approximately 30MPa could be obtained although the early-age strength development was very slow. Based on the results, the range of optimized mix design of bottom-ash based alkali-activated cement mortar was suggested. In addition, using the artificial neural network analysis, the flowability and compressive strength were predicted with the difference in the mix proportion of the bottom-ash based alkali-activated cement mortar.

A Study on the Properties of the Confined water ratio for Binder type and Replacement ratio (결합재의 종류 및 치환율에 따른 구속수비의 특성에 관한 연구)

  • Kwon Yeong-Ho;Lee Hyun-Ho;Lee Hwa-Jin;Ha Jae-Dam
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.05a
    • /
    • pp.584-587
    • /
    • 2004
  • This research investigates the rheological behavior and the confined water ratio of the cement paste and binder condition in order to predict mix design proportion of the high flowing concrete. The purpose of this study is to determine the optimum replacement ratio of binders including fly ash, and lime stone powder by the cement weight. For this purpose, belite cement, blast furnace slag cement and ordinary portland cement are selected. As test results, the confined water ratio shows the following range ; OPC>blast furnace slag cement>belite cement. Therefore, belite cement is proved very excellent cementitious materials in a view point of the flowability. The optimum replacement ratio of lime stone powder is shown over $30\%$ in case of belite cement and about $10\%$ in case of slag cement type. Also, the optimum replacement ratio of fly ash is shown $30\%$ by the cement weight considering the confined water ratio and deformable coefficient of the paste condition.

  • PDF

Strength Characteristics of No-Fine Concrete Containing Recycled Aggregates (재생골재를 함유한 무잔골재 콘크리트의 강도특성)

  • 김태근;이광명;김낙경;고용일
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.10c
    • /
    • pp.1-6
    • /
    • 1998
  • Recently, as to destruction and renovation of aged building, waste concretes have been reclaimed near foreshore and filled up underground. Recycling demolished concrete as aggregate helps to settle economic and environmental problems of obtaining superior aggregates from natural sources and to dispose waste concretes. An experimental study was carried out to investigate the strength characteristics of no-fine concrete containing recycled aggregates. The cement-aggregate weight ratios of 1: 5, 1: 6, 1: 7 and water-cement ratios of 30, 35, 40, 45% were chosen for the mix design of no-fine concretes. The compressive and splitting tensile strength at 7 and 28 days were measured for 12 different mixes. On the basis of test results, the optimum mix proportion of no-fine concrete containing recycled aggregates was determined and applied to the production of retaining wall block.