  • PURPOSE. The purpose of this study was to evaluate the efficacy of two different metal conditioners for non-precious metal alloys for the bonding of porcelain to a cobalt-chromium (Co-Cr) alloy. MATERIALS AND METHODS. Disk-shaped specimens ($2.5{\times}10.0mm$) were cast with Co-Cr alloy and used as adherend materials. The bonding surfaces were polished with a 600-grid silicon carbide paper and airborne-particle abraded using $110{\mu}m$ alumina particles. Bonding specimens were fabricated by applying and firing either of the metal conditioners on the airborne-particle abraded surface, followed by firing porcelain into 5 mm in diameter and 3 mm in height. Specimens without metal conditioner were also fabricated. Shear bond strength for each group (n=8) were measured and compared (${\alpha}=.05$). Sectional view of bonding interface was observed by SEM. EDS analysis was performed to determine the chemical elements of metal conditioners and to determine the failure modes after shear test. RESULTS. There were significant differences among three groups, and two metal conditioner-applied groups showed significantly higher values compared to the non-metal conditioner group. The SEM observation of the sectional view at bonding interface revealed loose contact at porcelain-alloy surface for non-metal conditioner group, however, close contact at both alloy-metal conditioner and metal conditioner-porcelain interfaces for both metal conditioner-applied groups. All the specimens showed mixed failures. EDS analysis showed that one metal conditioner was Si-based material, and another was Ti-based material. Si-based metal conditioner showed higher bond strengths compared to the Ti-based metal conditioner, but exhibited more porous failure surface failure. CONCLUSION. Based on the results of this study, it can be stated that the application of metal conditioner is recommended for the bonding of porcelain to cobalt-chromium alloys.

카복실레이트계 시멘트의 접착력에 관한 비교 연구 (COMPARATIVE STUDIES OF THE ADHESIVE QUALITIES OF POLYCARBOXYLATE CEMENTS)

  • 이한무
    • 대한치과보철학회지
    • /
    • 제17권1호
    • /
    • pp.23-34
    • /
    • 1979
  • In this study, the adhesive strength of three commercial polycarboxylate cements to ten types of dental casting alloys, such as gold, palladium, silver, indium, copper, nickel, chromium, and human enamel and dentine were measured and compared with that of a conventional zinc phosphate cement. The $8.0mm{\times}3.0mm$ cylindrical alloy specimens were made by casting. The enamel specimens were prepared from the labial surface of human upper incisor, and the dentine specimens were prepared from the occulusal surface of the human molar respectively. Sound extracted human teeth, which had been kept in a fresh condition since, extraction, were mounted in a wax box with a cold-curing acrylic resin to expose the flattened area. The mounted teeth were then placed in a Specimen Cutter (Technicut) and were cut down under a water spray, and then the flat area on the all specimens were ground by hand with 400 and 600 grit wet silicone carbide paper. Two such specimens were then cemented together face-to-face with freshly mixed cement, and moderate finger pressure was applied to squeeze the cement to a thin and uniform film. All cemented specimens were then kept in a thermostatic humidor cabinet regulated at $23{\pm}2^{\circ}C.$ and more than 95 per cent relative humidity and tested after 24 hours and 1 week. Link chain was attached to each alloy specimen to reduce the rigidity of the jig assembly, and then all the specimens were mounted in the grips of the Instron Universal Testing Machine, and a tensile load was delivered to the adhering surface at a cross head speed of 0.20 mm/min. The loads to which the specimens were subjected were recorded on a chart moving at 0.50 mm/min. The adhesive strength was determined by measuring the load when the specimen separated from the cement block and by dividing the load by the area. The test was performed in a room at $23{\pm}2^{\circ}C.$ and $50{\pm}10$ per cent relative humidity. A minimum of five specimens were tested each material and those which deviated more than 15 per cent from the mean were discarded and new specimens prepared. From the experiments, the following results were obtained. 1) It was found that the adhesive strength of the polycarboxylate cement to all alloys tested was considerably greater than that of the zinc phosphate cement. 2) The adhesive strength of the polycarboxylate cements was superior to the non precious alloys, such as the copper, indium, nickel and chromium alloys, but it was inferior to the precious gold, silver and palladium alloys. 3) Surface treatment of the alloy was found to be an important factor in achieving adhesion. It appears that a polycarboxylate cement will adhere better to a smooth surface than to a rough one. This contrasts with zinc phosphate cements, where a rough helps mechanical interlocking. 4) The adhesion of the polycarboxylate cement with enamel was found superior to its adhesion with dentine.

  • PDF

Goldish Yellow Color인 수종(數種)의 치과용(齒科用) 비귀금속합금(非貴金屬合金) 경도(硬度), 강도(强度) 및 미세조직(微細組織)의 비교(比較)에 관(關)한 연구(硏究) (A Study on the Comparison of hardness, Strength and Microstructure of dental Non-precious Metal Alloys Colored Goldish Yeller)

  • 김재도
    • 대한치과기공학회지
    • /
    • 제14권1호
    • /
    • pp.55-65
    • /
    • 1992
  • The purpose of this study was to investigate the comparison of physical properties of nonprecious metal alloys colored goldish yellow. The experimental groups were copper based dental alloy and control group was Ni-Cr based dental alloy used crown and bridges frameworks. Hardness was tested by vickers hardness tester, tensile strength was tested by universal tension tester. After testing the tensile strength of castings, the microstrucure and the pattern of fracture were investigated by scanning electron microscope and metallurgical microscope. The results were as follows : Hardness of Ni based alloy was higher than Cu based alloys. Hardness number of A group was 200.41$\pm$16.10 Hv, B group was 194.33$\pm$1.69 Hv, C group was 139.29$\pm$2.19 Hv and D group was 293.81$\pm$27.17 Hv, respectively. Tensile strength of D group was 56.42$\pm$6.17 $kg/m^2$, A group was 50.39$\pm$5.68 $kg/m^2$, C group was 45.13$\pm$4.53 $kg/m^2$, B group was 45.25$\pm$9.25 $kg/m^2$, in order, and D group was maximum tensile strength. The fractured surfaces of tensile specimens in the all groups showed the tendency to form large voids in the center of specimens. Thus the ductile fracture was changed into the brittle fracture with the fine grain size.

  • PDF

치과용 주조 합금의 방전가공에 따른 표면 성분 변화 (Elemental alteration of the surface of dental casting alloys induced by electro discharge machining)

  • 장용철;이명곤
    • 대한치과기공학회지
    • /
    • 제31권1호
    • /
    • pp.55-61
    • /
    • 2009
  • Passive fitting of meso-structure and super-structures is a predominant requirement for the longevity and clinical success of osseointegrated dental implants. However, precision and passive fitting has been unpredictable with conventional methods of casting as well as for corrective techniques. Alternative to conventional techniques, electro discharge machining(EDM) is an advanced method introduced to dental technology to improve the passive fitting of implant prosthesis. In this technique material is removed by melting and vaporization in electric sparks. Regarding the efficacy of EDM, the application of this technique induces severe surface morphological and elemental alterations due to the high temperatures developed during machining, which vary between $10,000{\sim}20,000^{\circ}C$. The aim of this study was to investigate the morphological and elemental alterations induced by EDM process of casting dental gold alloy and non-precious alloy used for the production of implant-supported prosthesis. A conventional clinical dental casting alloys were used for experimental specimens patterns, which were divided in three groups, high fineness gold alloy(Au 75%, HG group), low fineness gold alloy(Au 55%, LG group) and nonprecious metal alloy(Ni-Cr, NP group). The UCLA type plastic abutment patterns were invested with conventional investment material and were cast in a centrifugal casting machine. Castings were sandblasted with $50{\mu}m\;Al_2O_3$. One casting specimen of each group was polished by conventional finishing(HGCON, LGCON, NPCON) and one specimen of each group was subjected to EDM in a system using Cu electrodes, kerosene as dielectric fluid in 10 min for gold alloy and 20 min for Ni-Cr alloy(HGEDM. LGEDM, NOEDM). The surface morphology of all specimens was studied under an energy dispersive X-ray spectrometer (EDS). The quantitative results from EDS analysis are presented on the HGEDM and LGEDM specimens a significant increase in C and Cu concentrations was found after EDM finishing. The different result was documented for C on the NPEDM with a significant uptake of O after EDM finishing, whereas Al, Si showed a significant decrease in their concentrations. EDS analysis showed a serious uptake of C and Cu after the EDM procedure in the alloys studied. The C uptake after the EDM process is a common finding and it is attributed to the decomposition of the dielectric fluid in the plasma column, probably due to the development of extremely high temperatures. The Cu uptake is readily explained from the decomposition of Cu electrodes, something which is also a common finding after the EDM procedure. However, all the aforementioned mechanisms require further research. The clinical implication of these findings is related with the biological and corrosion resistance of surfaces prepared by the EDM process.

  • PDF

도재용 비금속합금의 표면처리에 따른 결합강도에 관한 실험적 연구 (An Experimental Study on the Bond Strength after Surface Treatment of Non-precious Metal Alloy for porcelain Crown)

  • 소명섭
    • 대한치과기공학회지
    • /
    • 제9권1호
    • /
    • pp.39-49
    • /
    • 1987
  • This study done to evaluate some surface treatment methods in metal coping which can increase the bond strength between porcelain and metal. Therefore this experiment was performed according to the Mc Lean's Theory of bond strength between porcelain and strength between porcelain and metal. In the experiment the author measured respective thermal expansion coefficents in three types of metal(Tallasium, Vera Bond and Rexillium) and Vita Porcelain to get the differences in the coefficents between porcelain and metals. And using insteron testing machine, the author also performed Planar interface shear bond tests on the 45 specimens(15 specimens in oxide surface, rough surface and fine surface treatment methods respectively) to measure bond strength between metal and porcelain. The results Were as follows, 1. The differences in thermal expansion coefficients between three types of metal and Vita procelain: Talladium - $1.2\;10^{-6/0}\;C$, Vera Bond - $1.6\;10^{-6/0}\;C$, Rexillium - $1.9\;10^{-6/0}\;C$. 2. The bond strength in oxide surface on the Shear bond test was the lowest among the treatment methods. 3. There was no significant differences in treatment methods of rough surface of fine surface. 4. In the oxide surface treatment method, there were significant differences(P<0.05)between Vera bond and Rexillium, and between Talladium and Rexillium. 5. In the fine surface treatment, there was a significant difference(P<0.05)between Talladium and Rexillium.

  • PDF

베릴륨이 포함되지 않은 도재용착용 비귀금속 합금과 세라믹간의 전단결합강도와 계면특성 (Shear Bond Strength and Interfacial Characterization of Ceramic to Beryllium Free Nonprecious Alloys for Porcelain Fused to Metal Crown)

  • 정인성;김치영
    • 한국콘텐츠학회논문지
    • /
    • 제10권11호
    • /
    • pp.228-234
    • /
    • 2010
  • 치과도재용 합금으로 사용되는 합금 중 베릴륨이 함유된 비귀금속 Ni-Cr합금과 베릴륨이 함유되지 않은 비귀금속 Ni-Cr합금 그리고 베릴륨이 함유되지 않은 비귀금속 Co-Cr 합금과 세라믹간의 결합강도와 파절양상 그리고 계면특성을 분석하고자 하였다. 결합강도는 만능시험기를 이용하여 전단력시험을 통하여 전단결합력을 측정하였으며, 전단시험에 의한 파단면을 이용하여 파절양상을 관찰하였다. 그리고 합금-도재간의 계면을 관찰하였다. 전단결합강도 측정 결과, 베릴륨이 포함된 T-3가 41.13(${\pm}5.11$)MPa로 가장 높게 나타났으며, 베릴륨이 포함된 VeraBond(40.72(${\pm}5.98$)MPa), Co-Cr 합금인 Wirobond(38.40(${\pm}9.66$)MPa), 베릴륨이 포함되지 않은 Verabond 2V(32.77(${\pm}4.31$)MPa), Bellabond N(28.63(${\pm}6.39$)MPa), Bellabond plus(24.97(${\pm}6.13$)MPa), Argeloy N.P. Star(22.69(${\pm}3.41$)MPa) 순으로 나타났다. 비귀금속 합금들과 세라믹간의 파절양상은 모든 시편에서 금속표면에 세라믹이 일부 부착된 복합파절(mixed failure) 양상을 보였다.

아말감과 이종(異種)금속의 거리에 따른 부식에 대한 고찰 (A Study on Corrosion according to Distance between Amalgam and Dissimilar Metals)

  • 김주원;정은경
    • 치위생과학회지
    • /
    • 제4권3호
    • /
    • pp.103-109
    • /
    • 2004
  • 본 실험은 제조회사 매뉴얼과 통법에 의해서 Amalgam 합금, Ni-Cr alloy의 Crown용 Verabond, Denture용 Talladium $^{TM}alloy$로 각각 24개의 총 72의 시편을 하악 제1대구치근 원심 치관 폭경과 임상에서의 MOD cavity를 고려하여 제작하였고 인공 타액 80ml를 담은 200ml 용 비이커에 시편을 넣어 0mm, 7mm, 40mm 거리에서 7일 후 갈바닉 부식을 측정하였다. 유리금속은 유도 플라즈마 방출 분광기(Inductively Coupled Plasma - Atomic Emission Spectrometer(ICP-AES, JY-50P, VG Elemental Co. France)로 전해액내의 Cu, Ag, Ni, Cr, Sn, Zn, Hg를 정량 분석했으며 그 결과 다음과 같은 결론을 얻었다. 첫째, Cu, Sn, Ag, Hg, Zn은 아말감이 금 합금과 접촉했을 때가 크라운용 Ni-Cr alloy와 덴쳐용 Talladium alloy 보다 아주 많이 유리 했으며 금 합금이 구강조직과 생체 적합성이 가장 좋다지만 아말감과 함께 있을 때 가장 불리 했슴을 알 수 있었다. 둘째, 아말감이 금 합금과 접촉했을 때, 금 합금의 조성에서 Ni, Cr 같은 중금속이 함유되지 않았기 때문인지 전혀 유리되지 않았으나 Sn은 조성에는 없었지만 $227.1{\pm}18.0035{\mu}g/cm^2$나 유리 되었고 Hg도 유리되었는데 이는 아말감 자체의 유리 물질임을 추측할 수 있었다. 셋째, 아말감 합금과 금 합금 사이에서의 0mm, 7mm, 40mm 거리에서는 Cu, Ag는 유의성이 있었으며 Hg는 유의성이 없었다. 이는 금합금은 절대 아말감과 같이 사용해서 안되며 이종 보철물 사이의 거리에 관계없이 사용을 금해야 하는 것으로 사료된다. 넷째, 아말감합금이 Crown용 Ni-Cr 합금과 접촉했을 때 아말감의 Ag이 유리 되지 않았으며 Zn, Ni, Sn, Hg, Cu의 순으로 유리되었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 다섯째, 아말감합금이 Denture용 Talladium alloy 합금과 접촉했을 때 0mm, 7mm, 40mm 거리에서도 유의성이 있었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 여섯째, 인공 타액에서 접촉 시 Amalgam alloy와 Gold, Verabond, Talladium alloy의 Cu, Sn, Ag, Hg, Zn, Ni, Cr의 ICPES 검사 결과 Cu, Hg가 유의성을 있었다. 일곱째, 인공타액에서 아말감합금과 두 비귀금속인 Ni-Cr alloy(crown용), Denture용 Talladium alloy가 접촉한 경우 거리에 따른 Hg, Ni, Cr의 유리 부산물에서 유의성을 확인했다.

  • PDF

치과용 비귀금속 합금과 전장용 강화형 복합레진의 인장결합강도 (TENSILE BOND STRENGTH BETWEEN NON-PRECIOUS DENTAL ALLOY AND VENEERING REINFORCED COMPOSITE RESINS)

  • 양병덕;박주미;고석민;강건구
    • 대한치과보철학회지
    • /
    • 제38권4호
    • /
    • pp.427-437
    • /
    • 2000
  • Recently the 2nd generation laboratory composite resins were introduced. Although the mechanical properties of these composite resins have been improved, there were some disadvantages such as discoloration, low abrasion resistance and debonding between metal and resin. The purpose of this study was to evaluate the tensile bond strength between non-pecious dental alloy(verabond) and four veneering reinforced composite resins ; Targis(Ivoclar Co., U.S.A.), Artglass(Kulzer CO., Germany), Sculpture(Jeneric Pentron Co., U.S.A.), and Estonia(Kurary Co., Japan). All test metal specimens were polished with #1,000 SiC paper, and sandblasted with $250{\mu}m$ aluminum oxide. After then. according to manufacturer's instructions metal adhesive primer and veneering resins were applied. All test specimens were divided into two groups. One group was dried in a desiccator at $25^{\circ}C$ for 3 days, the other group was subjected to thermal cycling($2,000{\times}$) in water($5/55^{\circ}C$). Tensile bond strength was measured using Instron Universal Testing machine and the fractured surface was examined under the naked eyes and scanning electron microscope. Within the limitations imposed in this study, the following conclusions can be drawn: 1. In no-thermal cycling groups, there were no significant differences between Estenia and VMK68 but there were significant differences between Targis, Artglass, Sculpture and VMK68(p<0.05). 2. In no-thermal cycling resin groups, the highest tensile bond strength was observed in Estenia and there were significant differences between Estenia and the other resins(p<0.05). 3. Before and after thermal cycling, there were significant differences in tensile bond strength of Targis and Artglass(p<0.05). The tensile bond strength of Artglass was decreased and that of Targis was increased. 4. In no-thermal cycling groups, Artglass showed mixed fracture modes(95%), but after thermal cycling, Artglass showed adhesive fracture modes(75%).

  • PDF

니켈-크롬 합금에 대한 다용도 접착 시스템의 전단결합강도 (Shear bond strength of Universal bonding systems to Ni-Cr alloy)

  • 송소연;손병화;김종엽;신상완;이정열
    • 대한치과보철학회지
    • /
    • 제53권4호
    • /
    • pp.295-300
    • /
    • 2015
  • 목적: 레진과 니켈-크롬 합금의 결합력에 미치는 금속 프라이머 및 다용도 접착제의 영향에 대하여 비교 평가하고자 한다. 재료 및 방법: 실험을 위해 120개의 니켈-크롬 합금(Vera Bond 2V) 디스크를 제작하여 아크릴 레진 실린더에 포매하였다. 시편의 표면은 220 grit, 600 grit의 실리콘 카바이드지로 연마한 뒤 $50{\mu}m$의 알루미늄옥사이드 입자를 분사하여 처리하였다. 실험군은 메탈 프라이머의 적용(Metal primer II, Alloy primer, Metal & Zirconia primer, MKZ primer)과 다용도 접착 시스템(Single Bond Universal, All Bond Universal)에 따라 6개 군으로 나뉘었다. 각 시편의 중앙에 높이 2 mm, 직경 3 mm로 복합레진을 충전하였으며, 제작된 모든 시편은 $37^{\circ}C$ 증류수에서 24시간 보관하였다. 만능시험기에 시편을 위치시킨 후 1 mm/min cross head speed로 전단결합강도를 측정하였다. 통계분석은0.05의 유의수준으로 일원분산분석을 시행하였고 Tukey's multiple coMParison test로 사후검정을 하였다. 결과: Single Bond Universal, All Bond Universal, Metal Primer II 3개 군과 Alloy Primer, MKZ Primer, Metal & Zirconia Primer 3개 군 사이에 통계학적으로 유의한 차이를 보였다(P<.001). 결론: 니켈-크롬 합금에 대한 다용도 접착 시스템의 전단결합강도는 Metal Primer II를 제외한 기존의 금속 프라이머를 적용했을 때 보다 높게 나타났다. 본 실험에서 더 나아가 다용도 접착 시스템 내 실란(Silane) 포함 여부에 따른 효과를 평가할 수 있는 연구가 필요할 것이다.

Sinfony 간접복합수지와 비귀금속합금간의 전단결합강도와 파절양상 (Shear Bond Strength and Failure Mode between Sinfony Indirect Composite Resin and Non Precious Metal)

  • 민병록;정인성
    • 대한치과기공학회지
    • /
    • 제30권2호
    • /
    • pp.79-86
    • /
    • 2008
  • The purpose of this study was to investigate the effect retention element formed by metal surface treatment method on the bond strength of indirect composite resin and metal. The metal specimens were cast from Ni-Cr alloy($Rexillium^{(R)}$ III). They were divided into 5 groups by applied retention element: $50{\mu}m$ aluminium oxide sandblasting group, $250{\mu}m$ aluminium oxide sandblasting group, 0.2mm retention crystal group, 10% $H_{2}SO_{4}$ solution etching group, $110{\mu}m$ $Rocatec^{TM}$ Plus system group. Total 50 metal specimens were veneered with Sinfony indirect composite resin system. Specimens were tested for shear bond strength on an Instron universal testing machine and fracture mode of fractured specimens were analyzed by SEM and EDS. 1. 0.2 mm retention crystals were most effective in improving the resin-metal shear bond strength (p<0.05). 2. Sandblasting by $250{\mu}m$ aluminium oxide were more effective than sandblasting by $50{\mu}m$ aluminium oxide in improving the resin-metal shear bond strength(p<0.05). 3. Fracture mode of resin-metal fractured surface were cohesive failure mode in 0.2mm retention crystal, mixed failure mode in sandblasted specimens, etched specimens and the specimens sandblasted with $110{\mu}m$ $Rocatec^{TM}$ Plus system.

  • PDF