LTCC 공정 중 적층 및 소결이 유전율과 회로 형상에 미치는 영향 (Influence of Laminating and Sintering Condition on Permittivity and Shrinkage During LTCC Process)

  • 정명식;황상현;정형욱;임성한;오수익
    • 소성∙가공
    • /
    • 제16권5호통권95호
    • /
    • pp.396-400
    • /
    • 2007
  • LTCC(Low Temperature Co-fired Ceramic) which offers a good performance to produce multilayer structures with electronic circuits and components has emerged as an attractive technology in the electronic packaging industry. In LTCC module fabrication process, the lamination and the sintering are very important processes and affect the electrical characteristics of the final products because the processes change the permittivity of ceramics and the dimension of the circuit patterns which have influences on electronic properties. This paper discusses the influence of lamination pressure and sintering temperature on the permittivity and the dimensional change of LTCC products. In the present investigation, it is shown that the permittivity increases along with increasing of the lamination pressure and the sintering temperature.

고에너지 밀링에 따른 PMN-PNN-PZT 세라믹의 유전 및 압전 특성 (Piezoelectric and Dielectric Properties of PMN-PNN-PZT Ceramic according to the High Energy Ball Milling)

  • 이유형;류주현;백동수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.203-204
    • /
    • 2008
  • In this study, in order to develop the multilayer piezoelectric actuator and ultrasonic resonator, PMN-PNN-PZT ceramics were fabricated by the variations of ball size at sintering temperature of $900^{\circ}C$ and their piezoelectric and dielectric characteristics were investigated as a function of the variations of ball size. When the ball size was 3mm$\phi$, density, dielectric constant$({\varepsilon}r)$, electromechanical coupling factor(kp) and piezoelectric d constant$(d_{33})$ were increased. At the ball size of 3mm$\phi$, the specimen showed the optimum values of density=7.909g/$cm^3$, kp=0.592, Qm=1292, $d_{33}$=368pC/N, $\varepsioln_r$=1502, respectively.

  • PDF

적층 칩 캐패시터 제작에 있어 $BaTiO_3$ 분말 크기에 따른 유전 특성 (Dielectric properties of $BaTiO_3$ Ceramic for Mutilayer Ceramic Capacitor)

  • 윤중락;이헌용
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.33-34
    • /
    • 2008
  • Barium titanate (BaTiO3) is one of the most important dielectric materials for the electronic devices, such as MLCC (Multilayer Ceramic Capacitor). The thickness of the dielectric thin film in MLCC has become thinner and reached about 0.8 ${\mu}m$. Further down sizing is required for the higher performance. For this reason, we should take into account for the size effect of Barium titanate powders. In this study, we demonstrated that size effect for BaTiO3 (0.2 ~ 0.5 ${\mu}m$, hydrothermal BT) could be estimates by using dielectric properties analysis together with the powder properties.

  • PDF

Switching Converter의 응용을 위한 압전 트랜스포머의 제작 및 특성 (The Properties and Manufacture of Piezoelectric Transformer for Application of Switching Converter)

  • 김성진;이수호;류주현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.630-633
    • /
    • 1999
  • This paper presents a new sort of multilayer piezoelectric ceramice transformer for switching regulatied power supplies. And this paper presents the study and development of a DC-DC converter with a transformer made from piezoelectric materials. This piezoelectric transformer operate, in the second thickness extensional vibration mode. Its resonant frequency is higher than 1MHz, This piezoelectric transformer was used the PbTiO$_3$ family ceramics because it was a material large anisotropy between electromechanical coupling factors k$_{t}$ and k$_{p}$. The input and output layer consists of two piezoelectric ceramic layer for eleivater of outpur power.wer.

  • PDF

LTCC 기판의 Particle Size 에 따른 Ag-Pd 전극의 Soldering 특성 변화 (Soldering characteristics of Ag-Pd electrodes in relationship to differing particle size of LTCC substrate)

  • 조현민;유명재;박종철
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2002년도 춘계 기술심포지움 논문집
    • /
    • pp.130-133
    • /
    • 2002
  • Solder leaching resistance of the metal electrode is an important factor with regard to adhesion properties of ceramic substrate. In the Low Temperature Co-fired Ceramics (LTCC), Ag-Pd or Ag-Pt pastes are used instead of pure Ag paste to prevent leaching. Solder leaching behavior of the Ag-Pd paste in relation to LTCC raw material powder size was investigated. First fabrication of LTCC green tape with different particle size was done. LTCC substrates with Ag-Pd electrode were prepared using conventional multilayer ceramic process. Dipping test was performed to test solder leaching behavior of the electrode. Ag-Pd electrode on LTCC substrate with smaller particle size achieved higher solder leaching resistance.

  • PDF

Thickness-Vibration-Mode Piezoelectric Transformer for Power Converter

  • Su-Ho lee;Yoo, Ju-Hyun;Yoon, H.S.
    • Transactions on Electrical and Electronic Materials
    • /
    • 제1권3호
    • /
    • pp.1-5
    • /
    • 2000
  • This paper presents a new sort of multilayer piezoelectric ceramic transformer for switching regulation power supplies. This piezoelectric transformer operate in the second thickness resonant vibration mode. Accordingly its resonant frequency is higher than 1 NHz, Because output power is low if input and output part of transformer are consisted of single layer, this research suggests a new method, which is consisted of both input and output part of transformer have 2-layered piezoelectric ceramics, The size of transformer is 20 mm in width and length, and 1.4 mm in thickness, respectively, To design a high efficient switching circuit of the transformer, internal circuit parameters were measured and then weve calculated a parameter of inductor nd capacitor to design a driving circuit, Weve used a MISFET and its driver circuit modified a calp oscillator circuit as the primary switching circuit.

  • PDF

SPECTRO-ELLIPSOMETRIC STUDIES OF STRUCTURE AND OPTICAL PROPERTIES OF PLSMA-GROWN DLC FILMS

  • Rhee, Sung-Gyu;Lee, Soon-Il;Oh, Soo-Ghee;Lee, Kwang-Ryeol
    • 한국표면공학회지
    • /
    • 제29권5호
    • /
    • pp.532-539
    • /
    • 1996
  • Diamond-like carbon (DLC) films were deposited on silicon substrates by the plasma decomposition of hydrocarbons under various conditions, and studied by the spectroscopic ellipsometry (SE). We used the effective medium approximation with the dispersion model developed by Forouhi and Bloomer to determine simultaneously both the structure and the optical constants of the DLC films from their ellipsometric spectra. Especially, we investigated the variation of the multilayer structure including the interface layer, of the refractive indices, and of the extinction coefficients as the deposition conditions were varied; substrate pretreatment procedure, hydrocarbon precursors, and the substrate bias voltage were varied.

  • PDF

소결조제 변화에 따른 PZW-PMN-PZT 압전 세라믹의 압전 및 유전 특성 (Piezoelectric and dielectric properties of PZW-PMN-PZT piezoelectric ceramic according to variation of sintering aids.)

  • 이갑수;이일하;류주현;류성림
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.290-291
    • /
    • 2007
  • In this study, in order to develop the low temperature sintering multilayer piezoelectric actuator, PZW-PMN-PZT system ceramics were manufactured according to variation of sintering aids. At the sintering temperature of $900^{\circ}C$, $0.3wt%Li_2CO_3$, $0.2wt%Bi_2O_3$ and 0.2wt%CuO added specimen showed a maximum value of kp = 0.552, $d_{33}\;=\;344pC/N$ and Qm = 1320, respectively.

  • PDF

Ba5Nb4O15 세라믹스의 저온소결 및 마이크로파 유전특성 (Low Temperature Sintering and Microwave Dielectric Properties of Ba5Nb4O15 Ceramics)

  • 김종대;김응수
    • 한국세라믹학회지
    • /
    • 제41권10호
    • /
    • pp.783-787
    • /
    • 2004
  • [ $Ba_5Nb_4O_{15}$ ] 세라믹스의 소결 온도를 낮추기 위하여 $PbO-B_2O_3-SiO_2$계 glass frit를 $0.5\~10w\%$ 첨가하고 소결 조건 변화에 따른 마이크로파 유전특성과 미세구조를 조사하였다. $Ba_5Nb_4O_{15}$ 유전체의 소결 밀도와 마이크로파 유전특성은 액상 소결조제로서 첨가한 glass frit의 첨가량에 따라 크게 변화하였다. $PbO-B_2O_3-SiO_2$계 glass frit을 $3wt\%$ 첨가하고 $900^{\circ}C$에서 2시간 소결한 시편은 유전상수(K) 41.4, 품질계수(Q$\times$f) 13,485 GHz, 공진주파수 온도계수(TCF) 9 ppm/$^{\circ}C$의 마이크로파 유전특성을 나타내었다. 또한, 상기 조성의 유전체 재료는 Ag 전극과의 동시소결에도 물리, 화학적 반응이 없어 적층형 유전체 필터 재료로서 적합한 재료라고 판단된다.

ZrO2 첨가된 0.96(K0.5Na0.5)NbO3-0.04SrZrO3 압전세라믹스의 환원분위기 소결 (Sintering of ZrO2-modified 0.96(K0.5Na0.5)NbO3-0.04SrZrO3 Piezoelectric Ceramics in a Reduced Atmosphere)

  • 강경민;조정호;남중희;고태경;전명표
    • 한국전기전자재료학회논문지
    • /
    • 제24권7호
    • /
    • pp.563-567
    • /
    • 2011
  • The most widely used piezoelectric ceramics are lead oxide based ferroelectrics (PZT). However, the toxicity of lead oxide and its high vapor pressure during processing have led to a demand for alternative lead-free piezoelectric materials. We synthesized Lead-free piezoelectric ceramics of $0.96(K_{0.5}Na_{0.5})NbO_3-0.04SrZrO_3+x$ mol% $ZrO_2$ [KNN-SZ+$xZrO_2$; x= 0~0.10] doped with 0.1 wt% $MnO_2$ by a conventional solid state method. We investigated the piezoelectric properties and microstructures of these disk samples sintered in reduced atmosphere in order to evaluate the possibility of the multilayered piezoelectric ceramics having the base metal such as Ni as a internal electrode. All of these KNN-SZ samples sintered in 3%$H_2-97%N_2$ atmosphere at $1,140^{\circ}C$ exhibit pure perovskite structure irrespective of the content of $ZrO_2$. Meanwhile, the sintering denisty and piezoelectric properties such as $K_p$, $Q_m$ and $d_{33}$ of KNN-SZ samples as a function of $ZrO_2$ content show the maxima ($k_p$=28.07%, $Q_m$= 101.34, $d_{33}$= 156 pC/N) at x= 0.04 and it is likely that there is some morphotropic phase boundary(MPB) in this KNN-SZ+$xZrO_2$ composition system. These results indicate that the ceramic composition is a promising candidate material for applications in lead free multilayer piezoelectric ceramics.