• Title/Summary/Keyword: mixed aggregate

검색결과 359건 처리시간 0.023초

증기양생한 플라이애쉬 혼입 재생골재 콘크리트의 강도특성에 관한 실험적 연구 (An Experimental Study on The Strength Property of the Concrete Using Recycled Aggregate Mixed Fly Ash in Steam Curing)

  • 심종성;박성재;이희철;김동희
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.326-329
    • /
    • 2003
  • In practice, recycled aggregate is not used for a structural member due to its high absorbability and abrasion. It is, however, highly expected that the usage of recycled aggregate increases as the processing technique of the recycled aggregate progresses. In this study herein, the compressive strength of the recycled aggregate concrete was investigated. Coarse aggregate was replaced with 100% of the recycled aggregate, and cement and fine aggregate was replaced with various amount. The specimen was steam-cured at $80^{\circ}C$. It was shown that the concrete can obtain desirable strength when fine aggregate was replaced with up to 60% of recycled fine aggregate, and when cement was replaced with up to 15% of fly ash.

  • PDF

설계기준강도별 순환 잔골재 혼합비율에 따른 순환골재 콘크리트 특성에 관한 연구 (A Study on the Characteristics of Recycled Aggregate Concrete According to the Mixing Ratio of Recycled Fine Aggregate at Specific Concrete Strengths)

  • 윤상혁;이세현
    • 한국건설순환자원학회논문집
    • /
    • 제10권4호
    • /
    • pp.367-375
    • /
    • 2022
  • 순환 잔골재 혼합비율에 따른 압축강도는 설계기준강도별 보통콘크리트 대비 순환 잔골재 혼합비율에 따라 유사하거나 다소 낮은 강도 발현을 보였으며, 순환 잔골재 혼합비율이 증가할수록 압축강도는 감소하는 경향을 보였다. 재령일이 증가할수록 강도저하는 발생하지 않았으며, 설계기준강도 대비 강도 발현이 가능할 것으로 판단된다. 순환 잔골재 15 %, 20 %, 25 %로 혼합비율에 따른 순환골재 콘크리트의 길이변화 및 동결융해에 대한 내구특성은 보통콘크리트와 유사한 경향으로 나타났다. 콘크리트용 순환 잔골재의 비율은 총 골재량의 25 %(총잔골재의 50 %)까지 적용하면 슬럼프 및 공기량에 문제가 없을 것으로 판단되며, 설계기준강도에 따른 분체량과 단위수량 및 공기연행제량에 대한 관리가 필요할 것으로 판단된다.

플라이애쉬와 실리카흄을 사용한 재생골재 콘크리트의 공학적 특성 (The Engineering Properties of Recycled Aggregate Concrete using Silica-Fume and Fly-Ash)

  • 구봉근;이상근;신재인;이현석
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.229-232
    • /
    • 1999
  • This study provided the engineering properties of the recycled aggregate concrete with fly-ash and silica-fume. There are considered recycled aggregate substitution ratio, and fly-ash silica-fume mix ratio as the experimental variable. From the experimental result, we could know that the recycled aggregate concrete mixed silica-fume is superior on the compressive strength but, is poor on the construction property than fly-ash. The optimal mix ratio of the fly-ash and silica-fume is 10% in all.

  • PDF

혼합골재에 리젝트애시를 프리믹스하여 활용하는 시멘트 모르타르의 공학적 특성 분석 (Analyzing the Engineering Properties of Cement Mortar Using Mixed Aggregate with Reject Ash)

  • 한천구;박병문
    • 한국건설순환자원학회논문집
    • /
    • 제5권3호
    • /
    • pp.247-252
    • /
    • 2017
  • 본 연구는 Reject Ash(Rj)를 혼합골재에 프리믹스하여 활용함에 따르는 가능성을 분석한 것이다. 즉, 서로 다른 입자특성의 저품질 잔골재인 석산 B+해사(CSb+SS), 발파석+해사(BS+SS)의 혼합골재에 대한 Rj의 치환율 변화에 따른 시멘트 모르타르의 기초적 특성을 파악하고자 하였다. 실험결과, 먼저 플로는 CSb+SS의 경우 Rj의 치환율이 증가함에 따라 거의 변화가 없었으며, 공기량은 CSb+SS와 BS+SS의 경우 모두 Rj의 치환율이 증가함에 따라 감소하는 것으로 나타났다. 압축강도는 CSb+SS와 BS+SS의 경우 모두 Rj의 치환율이 증가함에 따라 증가하는 것으로 나타났다. 따라서 혼합골재에 Rj를 5% 정도 치환할 경우에 품질이 양호한 골재를 사용한 경우와 유사한 것으로 판단되며, 5% 이상 치환할 경우에도 콘크리트의 유동성 확보 및 강도증진에 긍정적으로 기여하게 됨을 확인할 수 있었다.

개량입도 혼합모래를 사용한 콘크리트의 품질특성에 관한 연구 (A Study on the Properties of Quality of Concrete Using Mixed Sand Improved Grading)

  • 김기훈;한민철;박구병;윤기원;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2004년도 학술대회지
    • /
    • pp.55-58
    • /
    • 2004
  • This paper investigated the results of quality of concrete using mixed sand with grading adjustment in order to find out the applicability of fine aggregate with bad grading, According to test results, fluidity of concrete with fine level grading river sand was decreased while with coarse level grading crushed sand increased compared with that with medium level grading crushed sand. Use of mixed sand with grading adjustment(MSG) resulted in an improvement in fluidity. Increase in fineness modulus led to an increase in bleeding, For compressive strength, use of MSG increased compressive strength. For drying shrinkage, use of fine level grading river sand resulted in an increasing drying shrinkage due to the larger presence of fine particles, while use of MSG led to a reduction in drying shrinkage

  • PDF

Experimental investigation on hardened properties of recycled coarse aggregate concrete

  • Shohana, Shanjida A.;Hoque, Md. I.;Sobuz, Md. H.R.
    • Advances in concrete construction
    • /
    • 제10권5호
    • /
    • pp.369-379
    • /
    • 2020
  • Reduction of disposal of waste materials due to construction demolition has become a great concern in recent decades. The research work presents the hardened properties of concrete where the partial substitution of recycled coarse aggregate with natural aggregate in amount of 0%, 10%, 30% and 50%. By using different mixed proportions, fresh and hardened properties of concrete were conducted for this investigation. These properties were compared with control concrete. It can be seen that all of the hardened properties of concrete were decreased with the increasing percentage of recycled aggregate in concrete mixes. It was noticed that up to 30% recycled aggregate replacement can be yielded the optimum strength when it used in normal concrete. Finally, it can be said that disposed recycled concrete utilizing as a partial replacement in natural aggregate is a great way to reuse and reduce environmental hazards which achieve sustainability approach in the construction industry.

전기로제강 분진의 복합안정화 처리를 통한 에코이공경량골재의 개발 및 콘크리트 적용 연구 (A Study on the Development of the Artigicial Eco Light-Weight Aggregate using EAF-Dust and Application of the Concrete)

  • 이진우;김경민;정철희;배연기;이재삼
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.149-152
    • /
    • 2005
  • To make artificial light-weight aggregate with EAF-dust and estimate ability to apply to concrete, characteristics of the aggregate were considered in density, weight of unit volume, fineness modulus and so on. And then it was executed to experiments of the concrete mixed with the light-weight aggregate. As it was results that artificial light-weight aggregate with EAF-dust was heavier and more watertight than with only clay, concrete weight of unit volume was heavier than with expended clay aggregate. But it was regarded that concrete with EAF-dust artificial aggregate was able to field application as light-weight concrete because concrete of the weight of unit volume was lighter and compress strength and workability were similar to normal concrete.

  • PDF

건설폐기물인 순환골재를 이용한 수용액상에서의 혼합 중금속 제거 특성 (Removal Characteristics of Mixed Heavy Metals from Aqueous Solution by Recycled Aggregate as Construction Waste)

  • 신우석;김영기
    • 한국해양환경ㆍ에너지학회지
    • /
    • 제16권2호
    • /
    • pp.115-120
    • /
    • 2013
  • 본 연구에서는 순환골재를 이용하여 수용액상에서 혼합중금속의 제거능을 평가하였다. 순환골재는 주요 성분인 CaO, $SiO_2$, $Al_2O_3$, $Fe_2O_3$가 약 95% 함유되어 흡착제로서 유리한 조성을 가지고 있다. 동적흡착결과를 유사 1차 모델과 유사 2차 모델로 분석한 결과 두 모델 모두 실험결과에 잘 부합하는 것으로 나타났다. 평형흡착 실험은 Langmuir 모델에 잘 부합했고, $Cu^{2+}$ > $Pb^{2+}$ > $$Zn^{2+}{\simeq_-}Ni^{2+}$$ > $Cd^{2+}$순으로 흡착량이 높았다. 용액의 pH가 6에서 10로 증가함에 따라서 흡착률은 증가하는 것으로 나타났다. 또한, 순환골재의 양이 증가함에 따라서 중금속의 흡착률은 증가하였지만, 단위 질량당 흡착량은 감소하였다. 본 연구 결과를 통해 순환골재는 중금속을 효율적으로 제거할 수 있는 흡착제로 판단된다.

Glass ionomer cement와 혼합한 mineral trioxide aggregate의 물리적 및 화학적 성질 (Physical and chemical properties of experimental mixture of mineral trioxide aggregate and glass ionomer cement)

  • 정유나;양소영;박범전;박영준;황윤찬;황인남;오원만
    • Restorative Dentistry and Endodontics
    • /
    • 제35권5호
    • /
    • pp.344-352
    • /
    • 2010
  • 연구목적: 본 연구의 목적은 glass ionomer cement (GIC)와 혼합한 mineral trioxide aggregate (MTA)의 경화 시간, 압축 강도, 용해도, pH를 평가하고 이것을 MTA, GIC, IRM, SuperEBA와 비교하는 것이다. 연구 재료 및 방법: 경화 시간과 압축 강도는 ISO 9917, 그리고 용해도는 ISO 6876 기준에 따라 측정하였다. pH는 고체시편 전용 전극이 연결된 pH meter를 이용하여 측정하였다. 결과: GIC와 혼합한 MTA의 경화시간은 MTA보다 유의하게 짧았으며 압축 강도는 7일간 모든 시점에서 다른 재료보다 유의하게 낮았다. GIC와 혼합한 MTA 중에서 1 : 1과 2 : 1 시편의 용해도는 다른 실험군보다 유의하게 높았다. 또한 GIC와 혼합한 MTA의 pH는 혼합직후 2-4의 범위에서 1일 후 5-7 사이로 증가하였다. 결론: GIC와 혼합한 MTA의 경화시간은 MTA에 비해 개선되었으나 압축강도 및 pH와 같은 다른 성질들은 MTA에 비해 오히려 열등한 것으로 밝혀졌다. 임상적 사용이 가능하려면, MTA의 기존 장점을 저해하지 않으면서 단점을 개선하기 위한 적절한 혼합비를 찾아내고 생체친화성을 평가하는 추가적인 연구가 필수적이다.

Glass ionomer cement와 혼합한 mineral trioxide aggregate의 생체친화성 (Biocompatibility of experimental mixture of mineral trioxide aggregate and glass ionomer cement)

  • 오민제;정유나;배인호;양소영;박범전;고정태;황윤찬;황인남;오원만
    • Restorative Dentistry and Endodontics
    • /
    • 제35권5호
    • /
    • pp.359-367
    • /
    • 2010
  • 연구목적: 본 연구의 목적은 glass ionomer cement (GIC)와 혼합된 mineral trioxide aggregate (MTA)의 생체친화성을 평가하고 이것을 MTA, GIC, IRM, SuperEBA와 비교해보는 것이다. 연구 재료 및 방법: 재료의 세포독성을 평가하기 위해 MG-63세포를 이용해 주사전자 현미경 관찰과 XTT assay를 실시하였다. 결과: 주사전자 현미경 관찰에서는 GIC와 혼합한 MTA, MTA, GIC의 표면에서 세포질 돌기를 가진 많은 세포들이 밀집되고 융합된 형태로 관찰되었다. 반면 IRM과 SuperEBA에서는 세포들의 수가 적고 둥근 양상을 보여주었다. XTT assay에서는 GIC와 혼합한 MTA에서의 세포 활성도는 모든 시점에서 MTA 또는 GIC와 유사하였다. 반면 IRM과 SuperEBA에서는 모든 시점에서 세포활성도가 다른 그룹에 비해 유의하게 더 낮았다. 결론: 본 연구에서 GIC와 혼합된 MTA는 MTA, GIC와 유사한 세포 반응을 나타냈다. 이것은 GIC와 혼합된 MTA가 MTA, GIC와 마찬가지로 좋은 생체친화성을 가진 재료라는 것을 시사한다.