• 제목/요약/키워드: microtexture

검색결과 25건 처리시간 0.031초

AZ31 마그네슘합금 레이저 용접부의 미세조직 및 미소경도의 분포에 관한 연구 (A study on the microstructure and micro-hardenss distribution in laser welded AZ31 magnesium alloy)

  • 최영환;이목영;최시훈
    • 한국레이저가공학회지
    • /
    • 제15권3호
    • /
    • pp.11-15
    • /
    • 2012
  • The laser weld of AZ31 magnesium alloy was characterized with OM, EBSD and micros vickers hardness tester in experiment. EBSD analysis and micro-hardness measurements were carried out at the three regions (Equiaxed Zone, Columnar Dendrite Zone, Base Metal) of the welded AZ31Mg alloy sheets. The magnesium alloy show the rectangular shape bead in laser weld. EBSD analysis revealed that the three regions show the heterogeneous distribution of grain size and microtexture. Micro-hardness measurement also revealed that the heterogeneous distribution of microstructure contributed to the heterogeneous micro-hardness distribution in the three regions.

  • PDF

화학적 풍화에 의한 결정질 암석내의 미세조직 발달특징과 암반공학적 의미 (Characterization of Microtextures formed by Chemical Weathering in Crystalline Rocks and Implications for Rock Mechanics)

  • 추창오;정교철
    • 지질공학
    • /
    • 제21권4호
    • /
    • pp.381-391
    • /
    • 2011
  • 암석의 풍화작용은 암석의 강도를 약화시키고 궁극적으로는 지질공학적 대상물의 안정성을 저하시키게 된다. 화학적 풍화지수와 같이 암석의 풍화등급을 이용하여 암반의 안정성을 평가하는 여러 가지 지표가 널리 사용되고 있다. 본 연구에서는 편광현미경 관찰, XRF 전암분석에 의한 화학적 풍화지수, X-선회절 (XRD)분석에 의한 광물의 종류와 함량분석, 전자현미경(SEM/EDS)에 의한 미세조직 분석, BET측정법에 의한 기공크기와 비표면적 분석, 미소촛점 X-선 CT 등을 이용하여 결정질 암석(편마암, 화강암)의 풍화정도와 미세조직, 공극의 특성을 분석하였다. 이차광물의 생성과 미세구조의 발달특정은 광물의 용해, 침전, 파쇄반응과 같이 복합적인 요소에 의하여 영향을 받게 된다. 그러므로 단순히 전암분석치를 이용하여 계산하는 풍화지수(CIA, CWI 등)와 같은 기존의 화학적 풍화지표들은 암석의 풍화정도를 제대로 반영하지 못함이 밝혀졌다. 따라서 이 외에도 광물조성비, 미세조직, 미세공극의 특성을 고려한 새로운 평가기법이 요구된다.

Synthesis and Properties of Self-hardening Calcium Phosphate Cemetns for Biological Application

  • Song, Tae-Woong;Kim, Han-Yeop
    • The Korean Journal of Ceramics
    • /
    • 제3권2호
    • /
    • pp.129-133
    • /
    • 1997
  • Fine powder of $\alpha$-tricalcium phosphate, tetracalcium phosphate and dicalcium phosphate were mixed together to prepare self-setting cements which form hydroxyapatite, one of the well-known biocompatible materials, as the end of products of hydration. Hardening behaviour of the cements was examined at the temperature range of 37~$70^{\circ}C$ and 150~$250^{\circ}C$ under the normal and hydrothermal condition respectively. The conversion of cements into hydroxyapatite was significantly improved ast elevated temperature and the paste was strengtheed by interlocking of hydroxyapatite crystals, indicating that the strength is determined by microtexture rather the amount of conversion of cements into hydroxyapatite.

  • PDF

낙산사 동종의 성분분석 및 금속학적 고찰 (Component Analysis and Metallurgical Study of Bronze Bell in the Naksan-sa)

  • 황진주;한민수
    • 보존과학연구
    • /
    • 통권26호
    • /
    • pp.27-40
    • /
    • 2005
  • This study is to be investigated through component analysis and metallurgical texture in order to save an information of the manufacturing technique for the bronze bell in Naksan-sa. The bronze bell was analyzed with nine samples not stirred by the fire and except the contents of tin is the maximum and minimum the average of Cu is 81.8wt%, Sn is15.8wt% and indicates that some impurities are in it. With the result of an analysis of component and microtexture for impurities material which exists in it with using the SEM-EDS, the material was revealed the sulfur. As the result of these factors, the bronze bell of Naksan-sa is used from ore which mainly consist of the Chalcopyrite($CuFeS_2$) or Bornite($Cu_5FeS_4$) containing much sulfur.

  • PDF

청동 무기류의 성분조성 및 미세조직을 통한 제작기법 연구 (Study on Manufacturing Technique by Analysis of Compositions and Microtexture for Korean Bronze Weapons)

  • 황진주
    • 보존과학연구
    • /
    • 통권31호
    • /
    • pp.141-154
    • /
    • 2010
  • Many bronze artifacts have been excavated and preserved through conservation treatments in Korea but the analysis on artifacts was regarded as destruction of artifacts from the academic world of archaeology, Therefore, it is not so available to perform research on production techniques and provenances by with qualified analysis. Accordingly, there were only a few study cases about quality properties and production techniques But recently gradual change started to appear from the awareness of the need for the scientific approach to excavated artifacts. While Korean ancestors already had applied the different alloying ratios according to the use and shape of bronze artifacts, the analysis and study have been restrictedly performed. As a result, there was only a few analysis cases on a small minority of artifacts because they are the ancient relics, which made it hard to understand the bronze artifacts more deeply. This study researched into components rate, production techniques and hardness of bronze weapons such as a bronze sword and compared their alloying ratios with those of Chinese old records (周禮考工記, 金之六齊).

  • PDF

무기화합물 첨가에 의한 C/C복합재료의 매트릭스 조직제어 (The Role of Inorganic Compounds Additions on the Matrix Microtexture Control of C/C Composite)

  • 박세민
    • 한국세라믹학회지
    • /
    • 제34권11호
    • /
    • pp.1151-1158
    • /
    • 1997
  • Fracture of uni-directional carbon fiber reinforced carbon matrix composite is strongly dependent on the orientation of basal plane in graphite matrix when it is limited within matrix. The orientation of basal planes are vertically stacked to carbon fiber which results in the weakness for applied tensile or shear force in thermosetting resin derived-carbon matrix composite. Microtextural control of the matrix was tried through chemical interaction between metal carbides and furan resin derived-carbon matrix. SiC and TiO2 addition made the orientation disordered. However, porosity increased due to decomposition of SiC. Interfacial bonding could be controlled by TiO2 addition, but carbon fiber was considerably reacted with TiC during thermal treatment higher than 2$600^{\circ}C$. Therefore, it is desirable to control the thermal treatment temperature at which decomposition of SiC was not serious and TiC/C was not formed eutectoid.

  • PDF

산사태지역 토층의 미세조직과 지화학적 특성의 중요성 (Importance of Microtextural and Geochemical Characterizations of Soils on Landslide Sites)

  • 김경수;추창오;부성안;정교철
    • 지질공학
    • /
    • 제15권4호
    • /
    • pp.447-462
    • /
    • 2005
  • 본 연구의 목적은 산사태가 발생된 편마암, 화강암 및 퇴적암지역 자연사면의 토층을 대상으로 이들의 미세조직, 입도분포, 광물조성 및 지화학분석을 실시하여, 산사태 발생 에 영 향을 줄 수 있는 토층물질의 특성을 고찰하는데 있다. 이를 위하여 편마암류인 장흥지역, 화강암류인 상주지역, 제3기퇴적암류인 포항지역의 산사태현장 및 그와 대비되는 곳의 토층으로부터 채취 한 흙을 대상으로 레이저입도분석, X-선회절분석 (XRD), 주사전자현미경 (FE-SEM) 및 에너지분산스펙트럼(EDS)을 이용하여 분석하였다. 편마암류와 화강암류지 역은 산사태 발생지역의 토층이 미발생지역에 비해 점토광물의 함량이 더 높은 것으로 나타났는데, 이러한 양상은 화강암지역에서 특히 두드러지는 경향성을 보였다. 따라서 편마암류와 화강암류지역은 점토광물의 함유비율이 산사태에 유의한 영향인자로 간주될 수 있다. 점 토광물로는 일라이트(illite)가 가장 풍부하고 녹니석과 카올리나이트(kaolinite) 순으로 구성 비가 높고, 몬모릴로나이트(montmorillonite)도 부분적으로 함유된다. 제3기퇴적암지역은 편마암류와 화강암류지역에 비해서 점토광물의 함량이 전반적으로 높고 팽창성 점토광물인 몬모릴로나이트의 함유비율이 특히 높다 따라서 이들이 집중호우시 토층의 지지력에 크게 영향을 미침으로써 상대적으로 적은 강우조건에서도 다른 지역보다 산사태가 더 쉽게 발생된다. 그리고 산사태 발생지역과 미발생지역간 광물조성의 차별성이 특징적으로 관찰되지 않아 산사태가 광물조성의 차이에 큰 영향을 받기보다는 국지적인 지형조건이나 흙의 공학적 특성 등에 주로 지배를 받을 것으로 예측된다. 자연사면의 산사태를 연구할 때 기존의 토질 및 지질공학적 특성평가외에도 토층의 풍화특성과 구성 광물의 종류, 점토광물의 함량, 흙입 자의 미세조직과 같은 다양한 지화학적 정보가 추가된다면 산사태 발생 원인을 보다 정확하게 해석할 수 있을 것으로 기대된다.

고흥 길두리 안동고분 출토 유리구슬의 화학조성 및 풍화특성 (Characteristics of Chemical Compositions and Weathering of Glass Beads excavated from Andong Tumulus in Gildu-ri, Goheung)

  • 한민수;이한형;문은정
    • 보존과학회지
    • /
    • 제27권3호
    • /
    • pp.323-332
    • /
    • 2011
  • 고흥 길두리 안동고분에서 파편상태로 출토되어 복원이 불가능한 유리구슬 7점에 대해 미세조직관찰과 성분분석을 실시하여 유리유물의 화학조성 및 풍화의 특성을 밝히고자 하였다. 먼저 유리의 풍화상태를 분석한 결과, 표면과 내부 균열부분에 주변 매장환경으로부터 기인한 것으로 추정되는 오염물질이 다량 관찰되고 검출되었다. 또한 Na과 K 등의 알칼리금속 성분이 균열부에서 주로 감소되는 것으로 보아 이 부분에 풍화현상이 집중적으로 일어났음을 알 수 있었다. 화학조성을 통한 특성분류에서는 potash glass group($K_2O-SiO_2$유리군) 2점, soda glass group($Na_2O-SiO_2$유리군) 4점, 알칼리혼합유리군(mixed alkali glass group) 1점으로 확인되었다. 유리의 발색원소를 추정해보면, 청색과 감색 유리는 코발트(Co), 벽색은 철(Fe)과 구리(Cu), 황갈색은 철(Fe)로 추정된다. 이러한 고분출토 유리구슬의 과학적 연구는 향후 4~5C 호남문화권의 교류관계를 밝히는데 중요한 자료로 이용될 것으로 기대된다.

고노슬라그의 이용에 관한 연구(I) (슬라그유리의 결정성장) (A Study on the Utilization of Blast Furnace Slag(I) (Grain-Growth of Slag-Glass))

  • 이준;지응업;한기성;최상욱
    • 한국세라믹학회지
    • /
    • 제15권3호
    • /
    • pp.157-167
    • /
    • 1978
  • The batch compositions and physical properties of slag-ceramics were studied with respect to their formability from the molten state and conditions of nucleation and crystal growth treatment. The selected batch compositions for nucleation and growth studies were slag, 56%; silica sand, 28%; $Na_2O+MgO$, 8% and $TiO_2+$chromite, 8%. The optimum nucleation condition was the temperature of 75$0^{\circ}C$ with 6 hrs. holding time and the optimum growth condition was the temperature 975$^{\circ}C$ with zero holding time. The slag-ceramics prepared under the above conditions showed the best developed microtexture. The grown crystals were identified as diopside with the average grain size of 5.7$\mu\textrm{m}$, and the amount of crystal grown were about 53% by weight. The prepared specimens of slag-ceramics showed the microhardness, 793kg/$\textrm{mm}^2$; MOR, 1,050 kg/$\textrm{cm}^2$ and thermal expansion coefficient, $85{\div}10^{-7}$cm/cm/$^{\circ}C$($25^{\circ}C$~$700^{\circ}C$).

  • PDF