• Title/Summary/Keyword: microstructure effect

Search Result 2,436, Processing Time 0.029 seconds

The Characteristic and Formation of Ti(B,N) Films on Steel by EA Hot Filament CVD (EA hot filament CVD system을 이용하여 금형공구강에 증착한 Ti(B,N)박막의 합성과 특성에 관하여)

  • Yoon, Jung-H.;Choi, Yong;Choe, Jean-I.
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.61 no.4
    • /
    • pp.585-589
    • /
    • 2012
  • The characteristics of interface layer and the effect of mole fraction of inlet gas mixture($B_2H_6/H_2/N_2/TiCl_4$) on the microstructure of Ti(B,N) films were studied by microwave plasma hot filament CVD process. Ti(B,N) films were deposited on a substrate(STD-61) to develop a high performance of resistance wear coating tool. Ti(B,N) films were obtained at a gas pressure of 1 torr, bias voltage of 300 V and substrate temperature of $480^{\circ}C$ in $B_2H_6/H_2/N_2/TiCl_4$gas system. It was found that TiN, $TiB_2$, TiB and hexagonal boron nitride(h-BN) phases exist in thin layer on the STD-61.

The Effect of Thermomechanical Treatment on the Microstructural Changes and Fatigue Properties in 7050 Al Alloy (7050 AI 합금의 가공열처리가 미세조직변화와 피로성질에 미치는 영향)

  • Kim, M.H.;Kwun, S.I.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.4 no.4
    • /
    • pp.24-33
    • /
    • 1991
  • The effects of thermomechanical treatments on microstructure and fatigue properties of 7050 Al alloy were investigated. The precipitation kinetics changed to a faster rate due to cold deformation employed in this special TAHA thermomechanical treatments including pre-aging, plastic deformation and two step final-aging. The G.P. zones in the under-aged condition were cut by dislocations and dissolved during the plastic deformation. During the low cycle fatigue, the T6' condition showed cyclic hardening behavior whereas the TMT5, TMT27 and T76 conditions showed cyclic softening at above 0.7% total strain amplitudes. The ${\Delta}K_{th}$ value of TMT27 was improved more than two times, compared with that of T76 condition. The T6' with small shearable precipitates resulted in the markedly high ${\Delta}K_{th}$ value. This is thought to be resulted from dislocation reversibility and roughness-induced crack closure due to planarity of slip.

  • PDF

Effect of Microstructures on Cleavage Fracture Strength in Bainitic and Martensitic Steels (베이나이트 - 마르텐사이트 복합조직강에서 미세조직이 벽개파괴강도에 미치는 영향)

  • Lee, Chang-Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.27 no.3
    • /
    • pp.133-140
    • /
    • 2014
  • Cleavage fracture behaviors were investigated in Ni-Mo-Cr steels with mixed microstructure of lower bainite and martensite. As the size of carbide decreased, the cleavage fracture strength increased, which was independent of the sizes of grain and packet. The measured cleavage fracture strengths were in good agreement with cleavage fracture strengths calculated by Petch model rather than by modified Griffith model in micro-structures with fine carbides, the size of which were small below a few hundred nanometer.

Hardness and Electrical Conductivity Changes according to Heat Treatment of Cu-1.6Co-0.38Si Alloy (Cu-1.6Co-0.38Si 합금의 열처리에 따른 경도 및 전기전도도의 변화)

  • Kwak, Wonshin;Lee, Sidam
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.33 no.5
    • /
    • pp.226-231
    • /
    • 2020
  • The Cu-Co-Si alloy shows high strength by forming precipitates by aging precipitation heat treatment of supersaturated solid solution treated with solution treatment such as Cu-Ni-Si alloy, and the Co2Si precipitated phase is dispersed in the copper matrix. The effect of aging treatment on the microstructure, mechanical and electrical properties of Cu-Co-Si alloys for electronic devices was investigated. As a results of SEM/EDS analysis, it was found that Co2Si precipitates of 30~300 nm size were distributed in grains. By performing the double aging treatment, it was possible to improve the strength and electrical conductivity by dispersing the fine precipitate evenly.

The Effect of Ni Addition on the Sintering Kinetics of Ball-milled Mosi$_2$ Powder Compacts (Ni 첨가가 볼밀링한 MoSi$_2$분말성형체의 소결속도에 미치는 영향)

  • 최선호;홍경태;김영도;문인형
    • Journal of Powder Materials
    • /
    • v.5 no.4
    • /
    • pp.241-249
    • /
    • 1998
  • Sintering kinetics of ball-milled $MoSi_2$ was studied with the addition of Ni. $MoSi_2$ powder with the average particle size of 1 $\mu\textrm{m}$ was obtained from ball-milling of 10 $\mu\textrm{m}$ powder. Small amount of Ni was added to the ball-milled $MoSi_2$ powder by salt solution and reduction method. The powder was compacted into cylindrical shape at 200 MPa and isothermally sintered in a $H_2$ atmosphere at the temperature range of 1100~$1400^{\circ}C$ for 3~600 minutes. The changes of linear shrinkage and sintered density were monitored as a function of sintering time. The microstructure was observed by using optical microscopy and scanning electron microscopy. Phases were identified by X-ray diffratometer and electro-probe micro analysis. Sintering kinetics of Ni-added powder was compared to as-milled powder and the apparent activation energy was calculated from Arrhenius plot.

  • PDF

Sintering Behavior of 2xxx Series Al alloys with Variation of Sintering Temperature (2xxx Al 합금계 혼합분말의 소결온도에 따른 소결거동)

  • 민경호;김대건;장시영;임태환;김영도
    • Journal of Powder Materials
    • /
    • v.10 no.1
    • /
    • pp.40-45
    • /
    • 2003
  • Sintering behavior of 2xxx series Al alloy was investigated to obtain full densification and sound microstructure. The commercial 2xxx series Al alloy powder. AMB2712, was used as a starting powder. The mixing powder was characterized by using particle size analyzer, SEM and XRD. The optimum compacting pressure was 200 MPa, which was the starting point of the "homogeneous deformation" stage. The powder compacts were sintered at $550~630^{\circ}C$ after burn-off process at $400^{\circ}C$. Swelling phenomenon caused by transient liquid phase sintering was observed below $590^{\circ}C$ of sintering temperature. At $610^{\circ}C$, sintering density was increased by effect of remained liquid phase. Further densification was not observed above $610^{\circ}C$. Therefore, it was determined that the optimum sintering temperature of AMB2712 powder was $610^{\circ}C$.}C$.

Multiscale modeling of the anisotropic shock response of β-HMX molecular polycrystals

  • Zamiri, Amir R.;De, Suvranu
    • Interaction and multiscale mechanics
    • /
    • v.4 no.2
    • /
    • pp.139-153
    • /
    • 2011
  • In this paper we develop a fully anisotropic pressure and temperature dependent model to investigate the effect of the microstructure on the shock response of ${\beta}$-HMX molecular single and polycrystals. This micromechanics-based model can account for crystal orientation as well as crystallographic twinning and slip during deformation and has been calibrated using existing gas gun data. We observe that due to the high degree of anisotropy of these polycrystals, certain orientations are more favorable for plastic deformation - and therefore defect and dislocation generation - than others. Loading along these directions results in highly localized deformation and temperature fields. This observation confirms that most of the temperature rise during high rates of loading is due to plastic deformation or dislocation pile up at microscale and not due to volumetric changes.

Experimental study of the effect of the glass fibers on reducing collapse of a collapsible soil

  • Bakir, Nassima;Abbeche, Khelifa;Panczer, Gerard
    • Geomechanics and Engineering
    • /
    • v.12 no.1
    • /
    • pp.71-83
    • /
    • 2017
  • Collapsible soil presents a porous unsaturated structure, its sudden settlement after humidification, without supplementary charge, can be of a big nuisance for the foundations and therefore for the constructions built on it. To improve its structure and limit its instability, samples of laboratory reconstituted soil, with different percentages of water contents and compacted at different compaction energies, were treated with glass-fiber. The study of the mechanical behavior was performed by oedometer tests. The microstructure was explored by the Scanning Electron Microscope (SEM). The results obtained show clearly the efficiency of the treatment with glass fiber on reducing the collapsibility of such soil.

Sustainable use of mine waste and tailings with suitable admixture as aggregates in concrete pavements-A review

  • Gayana, B.C.;Chandar, Karra Ram
    • Advances in concrete construction
    • /
    • v.6 no.3
    • /
    • pp.221-243
    • /
    • 2018
  • Utilization of mine waste rocks and tailings in concrete as aggregates will help in sustainable and greener development. The literature shows the potential use of iron ore tailings as a replacement of natural fine aggregates. As natural sand reserves are depleting day by day, there is a need for substitution for sand in concrete. A comprehensive overview of the published literature on the use of iron ore waste and tailings and other industrial waste in concrete is being presented. The effect of various properties such as workability, compressive strength, split tensile strength, flexural strength, durability and microstructure of concrete have been presented in this paper.

Advanced Powder Processing Techniques of Ti Alloy Powders for Medical and Aerospace Applications

  • Miura, Hideshi
    • Journal of Powder Materials
    • /
    • v.20 no.5
    • /
    • pp.323-331
    • /
    • 2013
  • In this paper, two kinds of advanced powder processing techniques Metal Injection Molding (MIM) and Direct Laser Forming (DLF) are introduced to fabricate complex shaped Ti alloy parts which are widely used for medical and aerospace applications. The MIM process is used to strengthen Ti-6Al-4V alloy compacts by addition of fine Mo, Fe or Cr powders. Enhanced tensile strength of 1030 MPa with 15.1% elongation was obtained by an addition of 4 mass%Cr because of the microstructural modification and also the solution strengthening in beta phase. However, their fatigue strength was lower compared to wrought materials, but was improved by HIP. Subsequently, the effect of feeding layer height (FLH) on the characteristics of the DLF compacts was investigated. In the case of 100 ${\mu}m$ FLH, surface roughness was improved and nearly full density (99.8%) was obtained. Also, tensile strength of 1080 MPa was obtained, which is higher than the ASTM value.