• Title/Summary/Keyword: microstructure and pore size control

Search Result 19, Processing Time 0.022 seconds

Fabrication of nanoporous ceramic membrane for water treatment (수처리용 나노스케일 다공성 세라믹 멤브레인 제조)

  • Han, Hyuk Su;Lee, Ho Jun;Ryu, Jeong Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.29 no.2
    • /
    • pp.77-81
    • /
    • 2019
  • Recently, as the problem of environmental pollution emerges, various methods of eco-friendly water treatment method are being developed. Polymer membranes, which are currently leading the market, are inexpensive, but have many problems in terms of chemical resistance and durability. Thus, ceramic membrane has been attracted great attention as high-efficiency water treatment due to excellent durability and chemical resistant. In this study, ceramic membranes were developed via pore structure, size control, and surface treatment. The pore size of the membrane was controlled through the formation of $ZrO_2$ and $TiO_2$ coating films. Tape casting and sol-gel process were used to form a ceramic coating film with nanopores on the surface of the membrane. Microstructure analysis of ceramic membrane and pore size analysis of the coating film were conducted and the change of water treatment characteristics was observed.

Effect of Strontium Carbonate Content on Flexural Strength of Clay-Based Membrane Supports

  • Eom, Jung-Hye;Kim, Young-Wook;Song, In-Hyuck
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.6
    • /
    • pp.467-472
    • /
    • 2015
  • The effect of $SrCO_3$ content on the microstructure, porosity, flexural strength, and pore size distribution of clay-based membrane supports was investigated. Green compacts prepared from low cost materials such as kaolin, bentonite, talc, sodium borate, and strontium carbonate were sintered at $1000^{\circ}C$ for 8 h in air. It was possible to control the porosity of the clay-based membrane supports within the range of 33% to 37% by adjusting the $SrCO_3$ content. The flexural strength of the clay-based membrane supports was found to strongly depend on their porosity. In turn, the porosity was affected by the $SrCO_3$ content. The average pore size and flexural strength of the clay-based membrane supports containing 4 wt% $SrCO_3$ were $0.62{\mu}m$ and 33 MPa at 34% porosity.

Highly-closed/-Open Porous Ceramics with Micro-Beads by Direct Foaming

  • Jang, Woo Young;Seo, Dong Nam;Park, Jung Gyu;Kim, Hyung Tae;Lee, Sung Min;Kim, Suk Young;Kim, Ik Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.6
    • /
    • pp.604-609
    • /
    • 2016
  • This study reports on wet-foam stability with respect to porous ceramics from a particle-stabilized colloidal suspension that is achieved through the addition of polymethyl methacrylate (PMMA) using a wet process. To stabilize the wet foam, an initial colloidal suspension of $Al_2O_3$ was partially hydrophobized by the surfactant propyl gallate (2 wt.%) and $SiO_2$ was added as a stabilizer. The influence of the PMMA content on the bubble size, pore size, and pore distribution in terms of the contact angle, surface tension, adsorption free energy, and Laplace pressure are described in this paper. The results show a wet-foam stability of more than 83%, which corresponds to a particle free energy of $2.7{\times}10^{-12}J$ and a pressure difference of 61.1 mPa for colloidal particles with 20 wt.% of PMMA beads. It was possible to control the uniform distribution of the open/closed pores by increasing the PMMA content and by adding thick struts, leading to the achievement of a higher-stability wet foam for use in porous ceramics.

Phase Transformation and Microstructural Change of Alumina Membrane (알루미나 여과막의 상전이와 미세구조 변화)

  • Cheong, Hun;Choi, Duck-Kyun;Cheong, Deck-Soo
    • Korean Journal of Materials Research
    • /
    • v.10 no.9
    • /
    • pp.619-623
    • /
    • 2000
  • Alumina membrane was prepared by sol-gel coating method using boehmite powder(${\Upsilon}-AlOOH$). The supported and the unsupported alumina membrane were fabricated to investigate the phase transformation and change of microstructure. It is important to control the homogeneous pore size and distribution in application of filtering process. The ${\theta}-to\;{\alpha}-AL_2O_3$ phase transformation (XRD) and the change of microstructure was investigated using scanning electron microscopy(SEM). XRD patterns showed that the supported membrane had $100^{\circ}C$ higher ${\theta}-to\;{\alpha}-AL_2O_3$ transformation temperature compared to the unsupported membrane. The similar effect was also observed for microstructural change of the membrane.

  • PDF

Total pressure dependence of YBCO films in MOD method (MOD 공정에 의해 제조된 YBCO 박막의 압력 의존성)

  • Yoo, Jai-Moo;Chung, Kook-Chae;Ko, Jae-Woong;Kim, Young-Kuk;Wang, Xiao Lin;Dou, Shi Xue
    • Progress in Superconductivity and Cryogenics
    • /
    • v.8 no.1
    • /
    • pp.5-8
    • /
    • 2006
  • The growth properties of MOD-YBCO films were investigated. To enhance the growth rate of YBCO layer and inhibit the build-up of HF gas during the annealing process in TFA-MOD for YBCO coated conductors the method of low pressure annealing was employed. Total pressure was changed from 700Torr to 1Torr and its effect on growth of YBCO films was compared with atmospheric one. The lower Pressure was effective to control of the pore size in MOD method . Surface morphology of YBCO films processed at low total pres sure was rough and composed of random YBCO (103) grains. But large pores, usually observed at atmospheric process in MOD disappeared and also the number of pores was reduced at low pressure annealing. Also discussed ate the effects of Fluorine-free Y and Cu precursor solution on the development of microstructure. Dense surface me phology and with less and small pores can be provided through controlling Fluorine content.

Spalling Properties of High Strength Concrete Mixed with Various Mineral Admixtures Subjected to Fire

  • Han, Cheon-Goo;Han, Min-Cheol;Heo, Young-Sun
    • International Journal of Concrete Structures and Materials
    • /
    • v.2 no.1
    • /
    • pp.41-48
    • /
    • 2008
  • This study investigates the spalling properties of high strength concrete designed with various types of mineral admixture and diverse content ratios of polypropylene (PP) fiber. Experimental factors considered in series I are four pozzolan types of mineral admixture and series II consists of three shrinkage reducing types of mineral admixture. PP fiber was added 0.05, 0.10 and 0.15vol. % in each mixture of series I and series II, so that totally 27 specimens including control concretes in each series were prepared. Test results showed that the increase of fiber content decreased the slump flow of fresh concrete and increased or decreased the air content depending on the declining ratio of slump flow. For the properties of compressive strength, all specimens were indicated at around 50 MPa, which is high strength range; especially all specimens in series II were 60 MPa. Fire test was conducted in standard heating curve of ISO 834 with ${\phi}100{\times}200\;mm$ size of cylinder moulds for 1 hour. The specimens incorporating silica fume exhibited severe spalling and most specimens without the silica fume could be protected from the spalling occurrence in only 0.05vol % of PP fiber content. This fire test results demonstrated that the spalling occurrence in high strength concrete was not only affected by concrete strength related to the porosity of microstructure but also, even more influenced by micro pore structure induced by the mineral admixtures.

Quality and Texture Characteristics of Pumpkin Seed Tofu made with Soybean (Glycine max L. Merrill) and Pumpkin (Cucurbita moschata Duch.) Seed (대두(Glycine max L. Merrill)와 호박(Cucurbita moschata Duch.) 씨를 이용하여 제조한 호박씨 두부의 품질 및 조직감 특성)

  • Shin, So Yeon;O, Hyeonbin;Joung, Ki Youeng;Kim, Young-Soon
    • The Korean Journal of Food And Nutrition
    • /
    • v.31 no.1
    • /
    • pp.62-69
    • /
    • 2018
  • Pumpkin (Cucurbita moschata Duch.) seed is rich in protein and sulfur-containing amino acids. Tofu is a protein gel made from soybean, which is rich in lysine but lacking in sulfur-containing amino acids. This study was conducted to investigate the use of pumpkin seeds in tofu manufacture and to determine its quality and texture characteristics. Soybean was substituted with pumpkin seed to obtain pumpkin seed tofu at the following ratios: 10%, 30%, 50%, and 70% (P10, P30, P50 and P70). Tofu manufactured only with soybean was used as a control (Con). The higher rate of pumpkin seed substitution significantly decreased the moisture content and yield rate (p<0.05). In contrast, pH value and turbidity were significantly increased with the increase in the amount of pumpkin seed (p<0.05). The L-value (81.74~79.04), a-value (-0.19~-3.89) and b-value (12.40~9.84) of samples significantly decreased with the amount of pumpkin seed (p<0.05). No significant difference in syneresis was found among the samples (p<0.05). The hardness tended to decrease with the increase in the amount of pumpkin seed. The microstructure analysis revealed that the pore size of pumpkin seed tofu was smaller than that of Con. These results suggest that the pumpkin seed protein is a useful ingredient in the manufacture of tofu. Increasing the pumpkin seed substitution levels improves the texture of tofu.

Recent Research Trends of Mixed Matrix Membranes for CO2 Separation (이산화탄소 분리용 혼합 매질 분리막 최신 연구 동향)

  • Chi, Won Seok;Lee, Jae Hun;Park, Min Su;Kim, Jong Hak
    • Membrane Journal
    • /
    • v.25 no.5
    • /
    • pp.373-384
    • /
    • 2015
  • In the past few decades, polymeric membrane has played an important role in gas separation applications. For the separation of $CO_2$, one of greenhouse gases, high permselectivity, long-term stability and scale-up are needed. However, conventional polymeric membranes have shown a trade-off relation between permeability and selectivity while inorganic materials are highly permeable but expensive. Mixed matrix membranes (MMMs) combining the advantages of both polymeric and inorganic materials have become a possible breakthrough for the next-generation gas separation membranes. The MMMs could be either symmetric or asymmetric but the latter is more preferred to improve the permeance. Important factors influencing the MMM fabrication include homogeneous distribution of inorganic particles and good interfacial contact between inorganic filler and organic matrix. Recently, metal organic frameworks (MOFs) have received much attention as a new class of porous crystalline materials and a potential candidate for $CO_2$ separation. Zeolitic imidazolate frameworks (ZIFs), a sub-branch of MOFs, are the most widely used in MMMs due to small particle size and appropriate pore size for $CO_2$ separation. One of the major issues associated with the incorporation of porous particles in a polymeric membrane is to control the microstructure of the porous particle materials such as particle size, orientation, and boundary conditions etc. In this review, major challenges surrounding MMMs and the strategies to tackle these challenges are given in detail.

Microstructure and Strength of Class F Fly Ash based Geopolymer Containing Sodium Sulfate as an Additive (황산나트륨 첨가제에 따른 플라이애시 기반 지오폴리머의 미세구조 및 강도 특성)

  • Jun, Yubin;Oh, Jae-Eun
    • Journal of the Korea Concrete Institute
    • /
    • v.27 no.4
    • /
    • pp.443-450
    • /
    • 2015
  • This paper presents an investigation of the mechanical and microstructural properties of Class F fly ash based geopolymer containing sodium sulfate as an additive. Sodium sulfate was used as an chemical additive at the dosage levels of 0, 2, 4, and 6wt% of fly ash. Sodium hydroxide and sodium silicate solutions were used to activate fly ash. The compressive strengths of geopolymer pastes were measured at the age of 28 days. The microstructures of the geopolymer pastes were examined using XRD, MIP and SEM tests. The additions of 2wt% and 4wt% sodium sulfate produced geopolymers with high strength, while increasing the dosage of levels to 6% resulted in almost no changes in strength, comparing with the control geopolymer. The optimum increase in strength was obtained with the addition of 4wt% sodium sulfate. As the amount of sodium sulfate is increased, no additional crystalline phase was detected and no change of amorphous phase indicated despite the change in the strength development. The increase in the strength was due to the change of pore size distribution in samples. As addition of sodium sulfate altered the morphologies of reactive productions and Si/Al ratios of the reaction products, the strengths were thus affected. It was found that the strengths of geopolymer were larger for lower Si/Al ratios of reaction products formed in samples. The optimal amount of sodium sulfate in the fly ash based geopolymer helps to improve mechanical properties of the geopolymer, on the other hand, the high percentage of sodium sulfate could exist as an impurity in the geopolymer and hinder the geopolymer reaction.