• 제목/요약/키워드: microstructure, SEM-EDS

검색결과 196건 처리시간 0.031초

윤활조건에 따른 Mo-Cu-N 코팅의 마모특성에 관한 연구 (Study of anti wear resistance of Mo-Cu-N coatings deposited by reactive magnetron sputtering process with single alloying target)

  • 문경일;박현준;이한찬
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.95.1-95.1
    • /
    • 2017
  • In this study, it has been tried to make the single Mo-Cu alloying targets with the Cu showing the best surface hardness that was determined by investigation on the coatings with the double target process. The single alloying targets were prepared by powder metallurgy methods such as mechanical alloying and spark plasma sintering. The nanocomposite coatings were prepared by reactive magnetron sputtering process with the single alloying targets in $Ar+N_2$ atmosphere. The microstructure changes of the Mo-Cu-N coatings with diverse Cu contents were investigated by using XRD, SEM and EDS. The mechanical properties of the coatings were evaluated by using nano-indentor, scratch test, and ball on disc methods. Especially, the coated samples were tested by using various lubricating oil to compare the property of anti wear-resistance. In this study, the nano-composite MoN-Cu coatings prepared using an alloying target was eventually compared with the coatings from the multiple targets.

  • PDF

가스분무 Mg-Zn-Y 합금분말 및 압출재의 특성 (Materials Properties of Gas Atomized and Extruded Mg-Zn-Y Alloys)

  • 채홍준;이진규;배정찬;김택수
    • 한국분말재료학회지
    • /
    • 제13권6호
    • /
    • pp.427-431
    • /
    • 2006
  • Mg-4.3Zn-0.7Y (at%) alloy powders were prepared using an industrial scale gas atomizer, followed by warm extrusion. The powders were almost spherical in shape. The microstructure of atomized powders and those extruded bars was examined using Scanning Electron Microscopy (SEM), Energy Dispersive X-ray Spectroscope (EDS) and X-ray Diffractometer (XRD). The grain size of the powders was coarsen as the initial powder size increased. After the extrusion, the grain size became fine due to the severe plastic deformation during the extrusion with the ratio of 10:1. Both the ultimate strength and elongation were enhanced with the decrease of initial particle size.

A357을 이용한 알루미늄 반응고 브레이징 접합 계면 특성 (Microstructures of Bonding Interfaces after Semi-Solid Brazing of Aluminum Using A357 as a Filler Metal)

  • 이상용
    • 소성∙가공
    • /
    • 제21권8호
    • /
    • pp.506-511
    • /
    • 2012
  • Aluminum brazing normally requires a careful control of temperature due to the small interval between brazing and melting temperatures for base materials. Unsuitable processing conditions, including brazing temperature outside admissible range, gap between brazed materials or inadequate flux feeding, can lead to joining defects. In this study, A357 was used as a filler metal for the brazing of pure aluminum base materials and brazed at temperatures in the semi-solid state. Interface microstructures with base materials were observed using optical metallography(OM) and scanning electron microcopy(SEM) with energy dispersive spectroscopy(EDS), and compared to conventional aluminum brazing.

Hollandite-rich Synroc for Immobilization of Sr/Cs Separated from HLW Liquid

  • Zhao Yulong;Ii Baojun;xu Jianhua;Zhang Chuanzhi
    • 한국방사성폐기물학회:학술대회논문집
    • /
    • 한국방사성폐기물학회 2005년도 Proceedings of The 6th korea-china joint workshop on nuclear waste management
    • /
    • pp.329-337
    • /
    • 2005
  • Synroc which comprises hollandite-rich ($Ba_{1-x}Cs_{2x}\;(Al_yTi_{2-y})\;Ti_{6}O_{16},\;75wt\%$), perovskite ($Ca_{1-x}Sr_xTiO_3,\;15wt\%$) and rutile ($TiO_2,\;10wt\%$) is devised for the immobilization of Sr/Cs (1:3, wt$\%$) separated from HLW liquid. Especially, hollandite-rich Synroc with different contents of Al element is fabricated, and its mineral phase assemblage and microstructure are determined by using XRD and SEM/EDS. The durability test is carried out by using MCC-1 method, leachate is analyzed by using ICP/MS and ICP/ AES. The results indicate that hollandite-rich Synroc variants is a suitable host for Immobilization of Sr/Cs separated from HLW liquid.

  • PDF

Ion release and Biocompatibility of Ti-6Al-4V Alloys for Dental application

  • Kang, Jung-In;Son, Mee-Kyoung;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2015년도 추계학술대회 논문집
    • /
    • pp.303-303
    • /
    • 2015
  • In order to investigate ion release and biocompatibility of Ti-6Al-4V dental alloy by electrochemical corrosion test and MTT assay, commercial Ti-6Al-4V alloy rod (99.99% Ti, USA, Co) were used in the study. The microstructure of the alloys was examined by optical microscopy (OM), Field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDS), X-ray diffraction (XRD), MTT assay, and corrosion test. From the polarization curves, very low current densities were obtained for Ti-6Al-4V alloys, indicating a formation of stable passive layer.

  • PDF

Fe-Si계 재료의 열전성에 미치는 산화의 효과 (Effect of Oxidation ont he Thermoelectricity of Fe-Si based Materials)

  • 송태호;최준영;이홍림;배철훈
    • 한국세라믹학회지
    • /
    • 제33권1호
    • /
    • pp.74-82
    • /
    • 1996
  • Fe-Si based powders prepare by melting the metals in the composition of FeSi2,.Fe0.95Mn0.05Si2 and Fe0.95Co0.05Si0.2 were used as the starting materials together with a commercial FeSi2 powder to study the effect of oxidation on their thermoelectric properties. The powders were heated at 650~80$0^{\circ}C$ in dired air before forming and sintering at 1190 and 120$0^{\circ}C$ in Ar+7%H2. The microstructure and phases of the annealed specimens were observed using the optical microscopty SEM, EDS and XRD. The thermoelectric properties of the specimens were also measured. The temperature at which Seebe다 coefficient showed the maximum value increased with the degree of oxidation. Electrical conductivity showed a tendency to decrease in the oxidized samples regardless of their compositions. Seebeck coefficient of the specimen showed almost the same value even after oxidation which may be explained by the formation of the discontinuous second phases from impurities in the oxidized specimens.

  • PDF

Synthesis of Fe-TiB2 Nanocomposite by a combination of mechanical activation and heat treatment

  • ;;김지순;강태훈;김진천;권영순
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2012년도 춘계학술발표대회
    • /
    • pp.91.2-91.2
    • /
    • 2012
  • The TiB2-reinforced iron matrix nanocomposite (Fe-TiB2) was in-situ fabricated from titanium hydride (TiH2) and iron boride (FeB) powders by a simple and cost-effective process that combines the mechanical activation (MA) and a subsequent heat treatment (HT). Effect of milling factors and synthesized temperatures on the formation of the nanocomposite were presented and discussed. A differential thermal analyser (DSC-TG) was employed for examination of thermal behavior of MAed powders. Phases of the nanocomposite were confirmed by X-ray diffraction analysis (XRD). The morphologies and microstructure of nanocomposite were investigated by field emission-scanning electron microscopy (FE-SEM) and energy-dispersive X-ray spectroscopy (EDS). Phase composition and distribution were analyzed by electron probe X-ray microanalysis (EPMA). Results showed that TiB2 particles formed in nanoscale were uniformly distributed in alloyed Fe matrix.

  • PDF

용탕단조 공정을 응용한 액상이 제거된 Al7075 레오로지 소재의 T6 열처리 후 기계적 특성 (The Mechanical Property of Al7075 Rheology Material with Heat Treatment T6 to Eliminate Liquid Phase)

  • 강성식;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.150-153
    • /
    • 2007
  • Apply electromagnetic stirring system to making rheology slurry of Al7075. This experiment has important element which is the relation between solid fraction percent and melt temperature of Al7075. The rheology slurry of Al7075 eliminated liquid phase to include alloying element of copper and zinc by squeeze casting process. In result the most structure was composed entirely of globular primary $\alpha$. Used this material for this study. This study made a comparison of mechanical property according to heat treatment T6 at each melt temperature ($619^{\circ}C$ and $615^{\circ}C$). The microstructure and component are observed how heat treatment T6 weight with the mechanical property by SEM-EDS.

  • PDF

Effect of Filler Metal Powder on Microstructure and Polishing Characteristics of the Brazing Diamond

  • Kim, Hoon-Dong;An, Jung-Soo
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1138-1139
    • /
    • 2006
  • The present study has shown that the effect of boron and phosphorus in Ni-Cr-Si-X alloy to interfacial reactions and bonding strength of diamond-steel substrate, and the influence of various construction parameters on the formation of the topography of the tool. And these factors are required to making a good brazed tool. The microstructures and phase change of the brazed region were analyzed into SEM, EDS. According to the electron probe microanalysis, while brazing, the chromium present in the brazing alloy segregated preferentially to the surface of the diamond to form a chromium rich reaction product, which was readily wetted by the alloy.

  • PDF

Effect of Powder Size of Mg-Zn-Y Alloy on the Consolidation

  • Kim, Taek-Soo;Chae, H.J.;Lee, J.K.;Jung, H.G.;Kim, Y.D.;Bae, J.C.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1266-1267
    • /
    • 2006
  • [ $MgZn_{4.3}Y_{0.7}$ ] alloy powders were prepared using an industrial scale gas atomizer, followed by warm extrusion. The powders were almost spherical in shape. The microstructure of powders as atomized and bars as extruded was examined as a function of initial powder size distribution using Scanning Electron Microscope (SEM), Energy Dispersive X-ray Spectroscope (EDS) and X-ray Diffractometer (XRD). The grain sizes were decreased with extruding as well as decreasing the initial powder sizes. Both the ultimate strength and elongation were enhanced as the initial powder sizes were decreased.

  • PDF