• Title/Summary/Keyword: mechanical texture

Search Result 474, Processing Time 0.024 seconds

Preferred Orientation, Microstructure, Surface Morphology and Mechanical Properties of Electrodeposited Copper Foils (電解銅薄의 優先方位, 斷面組織, 表面形態 및 機械的 性質)

  • Kim, Yoon-Keun;Lee, Dong-Nyung
    • Journal of the Korean institute of surface engineering
    • /
    • v.18 no.3
    • /
    • pp.95-104
    • /
    • 1985
  • A study has been made of preferred orientation, crose sectional microstructure, surface morphology and mechanical properties of copper foils fabricated by electrodeposition on 304 stainless steel plate from copper sulfate baths for high speed plating. The preferred orientation of the copper foils changed from the [110] to the [111] to ture with decreasing bath temperature and increasing cathode current density. The foils with the [110] texture had the field oriented texture type structure and the surface of many asperities grooved approximately perpendicular to the subtrate. A specimen with the [111]+[311] texture had the lower strength than one with the [10] texture, if they were obtained under similar electrolysis conditions.

  • PDF

Quality Characteristics of Salku-Pyun with Various Starches (전분 종류를 달리한 살구편의 품질 특성)

  • 박금순;권진희;허성미
    • Journal of the East Asian Society of Dietary Life
    • /
    • v.9 no.4
    • /
    • pp.452-460
    • /
    • 1999
  • This study was conducted in order to investigate the quality characteristics of Salku Pyun which was made by using mungbean, potato, sweet potato and corn starches. The pH of salku juice was 3.45 to 3.50 and the brix of that was 7.0%. The water content and water activity of salku pyun with potato starch was highest. The result of sensory evaluation showed that appearance, flavor, overall quality were highest in the Salku Pyun made with potato starch while texture, taste were highest in the Salku Pyun made with mungbean starch. Mechanical properties of salku pyun with mungbean starch was significantly higher in adhesiveness, hardness, chewiness. Texture of sensory evaluation were positively correlated with springiness, hardness, and chewiness of mechanical measurement. The factors which affect the overall quality on sensory evaluation were texture quality, taste quality, hardness, color and springiness.

  • PDF

Study on the Frictional Behavior, Wear and Corrosion Resistance of Textured TiN Coated Layers (집합조직이 존재하는 TiN 코팅 층의 마찰, 마멸, 내부식 특성에 관한 연구)

  • 김희동;김인수;성동영;이민구
    • Transactions of Materials Processing
    • /
    • v.12 no.4
    • /
    • pp.394-400
    • /
    • 2003
  • TiN coated films exhibit excellent mechanical properties such as high wear, erosion and corrosion resistances and a high thermal stability. Therefore, they are widely applied to a coating material in tools, ornaments, parts and semiconductors. However, the fracture of TiN coated films frequently occurs. The distribution of preferred orientations, i.e., texture, of TiN coated films strongly influences the fracture behavior of these films. In the present study. various TiN coating layers having different textures were prepared by the reactive ion physical vapor deposition and the texture dependence of friction coefficient, erosion and corrosion in these coating layers was investigated. The sample depicting the (115) texture parallel to the coating layer normal displayed a flatter surface than that observed from the sample having the (111) texture. The friction coefficient of TiN thin films was hardly dependent on the texture of coated samples. The samples having (115) texture displayed higher wear, erosion and corrosion resistances than the samples having (111) texture.

Experimental Investigation of Concave and Convex Micro-Textures for Improving Anti-Adhesion Property of Cutting Tool in Dry Finish Cutting

  • Kang, Zhengyang;Fu, Yonghong;Chen, Yun;Ji, Jinghu;Fu, Hao;Wang, Shulin;Li, Rui
    • International Journal of Precision Engineering and Manufacturing-Green Technology
    • /
    • v.5 no.5
    • /
    • pp.583-591
    • /
    • 2018
  • Tool-chip adhesion impacts on cutting performance significantly, especially in finish cutting process. To promote cutting tools' anti-adhesion property, the concave micro-grooves texture (MGT) and convex volcano-like texture (VLT) were fabricated separately on lathe tools' rake faces by laser surface texturing (LST). Various orientations of MGT and different area densities (9% and 48%) and regions (partial and full) of VLT were considered in textured patterns designing. The following orthogonal cutting experiments, machining of aluminum alloy 5038, analyzed tools' performances including cutting force, cutting stability, chip shape, rake face adhesion and abrasion. It indicated that under dry finish cutting conditions, MGT contributed to cutting stability and low cutting forces, meanwhile friction and normal force reduced by around 15% and 10%, respectively with a weak correlation to the grooves' orientation. High density VLT tools, on the other hand, presented an obvious anti-adhesion property. A $5{\mu}m$ reduction of crater wear's depth can be observed on textured rake faces after long length cutting and textured rake faces presented half size of BUE regions comparing to the flat tool, however, once the texture morphologies were filled or worn, the anti-adhesion effect could be invalid. The bearing ratio curve was employed to analysis tool-chip contact and durability of textured surfaces contributing to a better understanding of anti-adhesion and enhanced durability of the textured tools.

Visual Texture Image and Preference of Men's suit Fabrics (남성 수트소재의 시각적 질감 이미지와 선호도)

  • Ryu Hyo-seon;Roh Eui-Kyung
    • Science of Emotion and Sensibility
    • /
    • v.8 no.2
    • /
    • pp.117-128
    • /
    • 2005
  • The purpose of this study was to clarify the effects of constituent characteristics and the mechanical properties by KES-FB system on the visual texture images and preference of men's suit fabrics. Twenty different kinds of black fabrics, which were used mainly for the spring and summer men's suits, were selected and the subjective evaluation of the visual texture images was tested. Sixty experts in department of clothing and apparel industries participated in the subjective evaluation. Factor analysis showed visual texture images were classified into 4 categories : 'bulkiness', $'extensibility{\cdot}rapability'$, 'flexibility' and 'smoothness'. All of relationships were established between the mechanical properties and the visual texture images except the relation between 'flexibility' and bending properties. The significant factors affecting preference were 'smoothness', compression energy(WC), fabric count and 'flexibility', As the fabrics had higher value for 'smoothness' and 'flexibility' , and lower ones for compression energy and fabric count, they tended to be more preferred.

  • PDF

Microstructure Control and Tensile Property Measurements of Hot-deformed γ-TiAl alloy (열간가공된 γ-TiAl 합금의 미세조직 제어 및 기계적 특성 평가)

  • Park, Sung-Hyun;Kim, Jae-Kwon;Kim, Seong-Woong;Kim, Seung-Eon;Park, No-Jin;Oh, Myung-Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.32 no.6
    • /
    • pp.256-262
    • /
    • 2019
  • The microstructural features and texture development by both hot rolling and hot forging in ${\gamma}-TiAl$ alloy were investigated. In addition, additional heat treatment after hot forging was conducted to recognize change of the microstructure and texture evolution. The obtained microstructural features through dynamic recrystallization after hot deformed ${\gamma}-TiAl$ were quite different because two kinds of formation process were occurred depending on deformation condition. However, analyzed texture tends to be random orientation due to intermediate annealing up to ${\alpha}+{\beta}$ region during the hot deformation process. After additional heat treatment, microstructure transformed into fully lamellar microstructure and randomly oriented texture was also observed due to the same reason as before. Tensile test at room temperature demonstrated that anisotropy of mechanical properties were not appeared and transgranular fracture was occurred between interface of ${\alpha}_2/{\gamma}$. As a result, it could be suggested that microstructural features influenced much more than texture development on mechanical properties at room temperature.

Prediction of Rolling Texture for Mg Alloy AZ31B Sheet using Finite Element Polycrystal Model (유한요소 다결정 모델을 이용한 마그네슘 합금 AZ31B 판재의 압연 집합 조직 예측)

  • Won S. Y.;Kim Y. S.;Na K. H.;Takahashi Hiroshi
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.08a
    • /
    • pp.72-82
    • /
    • 2004
  • The deformation mechanism of hexagonal close-packed materials is quite complicate including slips and twins. A deformation mechanism, which accounts for both slip and twinning, was investigated for polycrystalline hop materials. The model was developed in a finite element polycrystal model formulated with initial strain method where the stiffness matrix in FEM is based on the elastic modulus. We predicted numerically the texture of Mg alloy(AZ31B) sheet by using FEM based on crystal plasticity theory. Also, we introduced the recrystallized texture employed the maximum energy release theory after rolling. From the numerical study, it was clarified that the shrink twin could not be the main mechanism for shortening of c-axis, because the lattice rotation due to twin rejects fur c-axis to become parallel to ND(normal direction of plate). It was showed that the deformation texture with the pyramidal slip gives the ring type pole figure having hole in the center.

  • PDF

Study of texture, mechanical and electrical properties of cold drawn AGS alloy wire

  • Zidani, M.;Bessais, L.;Farh, H.;Hadid, M.D.;Messaoudi, S.;Miroud, D.;Loudjani, M.K.;Helbert, A.L.;Baudin, T.
    • Steel and Composite Structures
    • /
    • v.22 no.4
    • /
    • pp.745-752
    • /
    • 2016
  • An investigation has been done to study the evolution of the microstructure, mechanical and electrical properties of AlMgSi alloy destined for the transport of electric energy, in function of the deformation caused by the cold drawing process. We identified that drawing of aluminum wire causes development of a fibrous texture of type <111> and <100>. We notice also that the electrical resistivity and mechanical resistance increases with the increasing of the deformation level. Characterization methods used in this work is: The Electron Back Scattered Diffraction EBSD, X-Ray diffraction, Vickers microhardness, Tensile test, Measuring electrical resistivity, the Scanning Electron Microscope (SEM) and Energy Diffraction Spectrum (EDS).

Effects of Soil Texture and Bulk Density on the Least-Limiting Water Range (토성(土性)과 용적밀도(容積密度)가 최소생육제한수분범위(最小生育制限水分範圍)에 미치는 영향(影響))

  • Jo, In-Sang;Hyun, Byung-Keun;Cho, Hyun-Jun;Jang, Yong-Seon;Shin, Jae-Sung
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.30 no.1
    • /
    • pp.51-55
    • /
    • 1997
  • Three soils, sandy loam, loam and silty clay loam, were selected and three inches soil cores with 4 bulk density(BD) levels were made by compressing the soils wetted with 3 levels water. Mechanical and water characteristics were measured and analyzed the mechanical resistance limiting water, available water and least-limiting water range. Mechanical resistance limiting water(MRLW) were appeared at higher bulk density than $1.6Mg/m^3$ in sandy loam, and $1.4Mg/m^3$ in loam and silty clay loam. The least-limiting water ranges were sharply decreased at the bulk density $1.6Mg/m^3$ in sandy loam and loam, $1.4Mg/m^3$ in silty clay loam. There were big deferences between available water contents and least limiting water ranges in finer texture and higher bulk density soils.

  • PDF

Improvement of Mechanical Properties of Mg alloys through Control of Grain Size and Texture (결정립크기와 집합조직제어를 통한 마그네슘 합금의 기계적 성질 개선)

  • Kim, W.J.;Lee, J.B.;Kim, W.Y.;Jeong, H.G.;Park, J.D.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2006.05a
    • /
    • pp.57-58
    • /
    • 2006
  • The effects of lowering ECAP temperature during ECAP process and Post-ECAP annealing on microstructure, texture and mechanical properties of the AZ31 alloys have been investigated in the present study. The as-extruded materials were ECAP processed to 2 passes at 553K prior to subsequent pressing up to 6 passes at 523K or 493K. When this method of lowering ECAP temperature during ECAP was used, the rods could be successfully deformed up to 6 passes without any surface cracking. Grain refinement during ECAP process at 553K might have helped the material to endure further straining at lower deformation temperatures probably by increasing the strain accommodation effect by grain boundary sliding, causing stress relaxation. Texture modification during ECAP has a great influence on the strength of Mg alloys because HCP metals have limited number of slip systems. As slip is most prone to take place on basal planes in Mg at room temperature, the rotation of high fraction of basal planes to the directions favorable for slip as in ECAP decreases the yield stress appreciably. The strength of AZ31 Mg alloys increases with decrease of grain size if the texture is constant though ECAP deformation history is different. A standard positive strength dependence on the grain size for Mg alloys with the similar texture (Fig. 1) supports that the softening of ECAPed Mg alloys (a negative slope) typically observed despite the significant grain refinement is due to the texture modification where the rotation of basal planes occurs towards the orientation for easier slip. It could be predicted that if the original fiber texture is restored after ECAP treatment yielding marked grain refinement, yield stress as high as 500 MPa will be obtained at the grain size of ${\sim}1{\mu}m$. Differential speed rolling (DSR) with a high speed ratio between the upper and lower rolls was applied to alter the microstructure and texture of the AZ31 sheets. Significant grain refinement took place during the rolling owing to introduction of large shear deformation. Grain size as small as $1.4{\mu}m$ could be obtained at 423K after DSR. There was a good correlation between the (0002) pole intensity and tensile elongation. This result indicates that tensile ductility improvement in the asymmetrically rolled AZ31 Mg alloys is closely related to the weakening of basal texture during DSR. Further basal texture weakening occurred during annealing after DSR. According to Hall-Petch relation shown in Fig. 1, the strength of the asymmetrically rolled AZ31 is lower than that of the symmetrically rolled one when compared at the same grain size. This result was attributed to weakening of fiber texture during DSR. The DSRed AZ31, however, shows higher strength than the ECAPed AZ31 where texture has been completely replaced by a new texture associated with high Schmid factors.

  • PDF