A comparison of marginal fit of glass infiltrated alumina copings fabricated using two different techniques and the effect of firing cycles over them

  • Bhowmik, Hirasankar;Parkhedkar, Rambhao
    • The Journal of Advanced Prosthodontics
    • /
    • 제3권4호
    • /
    • pp.196-203
    • /
    • 2011
  • PURPOSE. This study evaluated marginal fit of glass infiltrated alumina cores fabricated using two techniques and their marginal stability after firing cycles of veneering porcelain. MATERIALS AND METHODS. Fifteen standardized all-ceramic crowns were fabricated on a metal die using each technique: slip cast technique of VITA In-Ceram sprint Alumina (Group A as control) and plastic foil matrix technique of Turkom-Cera fused alumina core system (Group B). Copings were compared between groups and within groups at coping stage and after firing each layer of veneering porcelain. A device was used to standardize seating of copings on the metal die and positioning of the specimens under the microscope after each stage of fabrication. The specimens were not cemented and marginal gap was measured using an image analyzing software (Imagepro Express) on the photographs captured under an optical microscope. Two tailed unpaired 't test' was used to compare marginal gaps in two groups and one way ANOVA was used to analyze marginal distortion within each group at 95% confidence interval. RESULTS. The marginal gap was smaller at the coping stage in group B ($60+30{\mu}M$) than group A ($81+21{\mu}M$) with statistical significance. After firing of veneering porcelain the difference was insignificant. At the final stage, both groups exhibited lower mean marginal gaps than at the initial coping stage with the difference of $11.75{\mu}M$ for group A and $11.94{\mu}M$ for group B, but it was statistically insignificant due to high value of standard deviation. CONCLUSION. Within the limitations of this study, it was concluded that both techniques produced copings with comparable and acceptable marginal fit and marginal stability on firing veneering porcelain.

임플란트 지지 나사-시멘트 유지형 보철물에서 보철물-지대주 제거 후 변연부 연마의 효과: 증례보고 (Burnishing effect on marginal misfit of implant-supported screw-and-cement retained prostheses: A case report)

  • 김미주;이두형
    • 대한치과보철학회지
    • /
    • 제58권3호
    • /
    • pp.239-243
    • /
    • 2020
  • 고정성 보철물의 변연 적합도가 낮은 경우 치태침착, 치주질환, 치아과민, 보철물 구성요소 파절, 시멘트 상실 등의 생물학적, 기계적 합병증이 발생할 가능성이 증가할 수 있다. 이러한 합병증은 보철물의 장기간의 성공과 생존에 영향을 미친다. 본 증례는 임플란트 지지 나사-시멘트 유지형 보철물에서 보철물 장착 시 보철물-지대주를 제거하고 변연부를 연마하여 변연간극을 최소화할 수 있는 임상과정을 보여준다. 그리고 변연 간극을 연마 전과 후에 측정하여 비교 관찰하였다. 본 기술은 변연 적합도를 높여 보철물의 수명 연장에 기여할 수 있다.

시멘트 공간이 캐드캠 시스템으로 제작한 지르코니아 수복물의 변연과 내부 적합도에 미치는 효과 (Effect of cement space on the marginal and internal fit of zirconia restorations fabricated by CAD/CAM system)

  • 이정환;안재석
    • 대한치과기공학회지
    • /
    • 제39권4호
    • /
    • pp.235-242
    • /
    • 2017
  • Purpose: The aim of this study was to evaluate the marginal and internal gap of zirconia copings fabricated by CAD/CAM system and to research the effect of cement space on the fit of zirconia prosthesis. Methods: Zirconia copings were designed using 3shape software and then milled from presintered zirconia blocks by Kavo dental milling machine. The cement space was set at $0{\mu}m$ around the margins for all groups, and additional cement space appling 1 mm above the finish lines of tooth. The samples were classified into 4 groups according to the cement space setting(Cs-0, Cs-40, Cs-80, Cs-120). Replica technique used to investigate marginal and internal gap. The silicone film thickness was recorded using a optical microscope with image software analysis system at 75${\times}$magnification. The assessment performed on the six points in bucco-lingual and mesio-distal sections(4 groups, 10 copings per group, 12 measuring points per coping). The data were statistically analyzed with one-way ANOVA followed by pair-wise Tukey's post hoc tests(${\alpha}$<0.05). Results: Better marginal and internal fit values were exhibited by $80{\mu}m$ cement space. The results showed that different cement space values had statistically significant effect on the marginal and internal gap of zirconia copings(p<0.001). The gap of margin and axial wall area was smaller than that the gap of occlusal area in all groups(p<0.001). Conclusion : Effect of different cement spaces on the marginal and internal gap of zirconia copings.

Glass Ionomer Cement의 변록누출(邊綠漏出)에 관(關)한 실험적(實驗的) 연구(硏究) (AN EXPERIMENTAL STUDY ON THE MARGINAL LEAKAGE OF GLASS IONOMER CEMENT)

  • 주광섭;유근원
    • Restorative Dentistry and Endodontics
    • /
    • 제7권1호
    • /
    • pp.101-106
    • /
    • 1981
  • The purpose of this study was to estimate the ability of the marginal fit of Glass ionomer cement. Using the human extracted teeth and 2% acqueous solution of methylene blue, the author investigated the marginal penetration of dye in restorative materials such as Amalgam, Hi-Pol, Glass ionomer cement, Estic microfill and Restodent. The results were as follows. 1. All filling materials showed some degree of marginal penetration. 2. Glass ionomer cement revealed nearly the same microleakage as Estic microfill and Hi-Pol, but showed inferior effect of the marginal seal as compared with Restodent. 3. It is appeared that Amalgam has more effective ability of the marginal fit than the others within a week.

  • PDF

Celay/In-Ceram, Conventional In-Ceram, Empress 2 전부도재관의 변연적합도에 관한 비교 연구 (MARGINAL FIT OF CELAY/IN-CERAM, CONVENTIONAL IN-CERAM AND EMPRESS 2 ALL-CERAMIC SINGLE CROWNS)

  • 양재호;여인성;이선형;한중석;이재봉
    • 대한치과보철학회지
    • /
    • 제40권2호
    • /
    • pp.131-139
    • /
    • 2002
  • There have been many studies about marginal discrepancy of single restorations made by various systems and materials. But many of statistical inferences are not definite because of sample size, measurement number, measuring instruments. etc. The purpose of this study was to compare the marginal adaptations of the anterior single restorations made by different systems and to consider more desirable statistical methods in analysing the marginal fit. The in vitro marginal discrepancies of three different all-ceramic crown systems (Celay In-Ceram. Conventional In-Ceram. IPS Empress 2 layering technique) and one control group (PFM) were evaluated and compared. The crowns were made from one extracted maxillary central incisor prepared with a 1mm shoulder margin and $6^{\circ}$ taper walls by milling machine. 10 crowns per each system were fabricated. Measurements or a crown were recorded at 50 points that were randomly selected for marginal gap evaluation. Non-parametric statistical analysis was performed for the results. Within the limits of this study, the following conclusions were drawn: 1 Mean gap dimensions and standard deviations at the marginal opening for the maxillary incisor crowns were $98.2{\pm}40.6{\mu}m$ for PFM, $83.5{\pm}18.7{\mu}m$ for Celay In-Ceram, $104.9{\pm}44.1{\mu}m$ for conventional In-Ceram, and $45.5{\pm}11.5{\mu}m$ for IPS Empress 2 layering technique. The IPS Empress 2 system showed the smallest marginal gap (P<0.05). The marginal openings of the other three groups were not significantly different (P<0.05). 2 The marginal discrepancies found in this study were all within clinically acceptable standards ($100\sim150{\mu}m$). 3. When the variable is so controlled that the system may be the only one, mean value is interpreted to be the marginal discrepancy of a restoration which is made by each system and standard deviation is to be technique-sensitivity of each one. 4. From the standard deviations. the copy-milling technique (Celay/In-Ceram) was not considered to be technique-sensitive in comparison with other methods. 5. Parametric analysis is more reliable than non-parametric one in interpretation of the mean and standard deviation. The sample size of each group has to be more than 30 to use parametric statistics. The level of clinically acceptable marginal fit has not been established. Further studies are needed.

주조도재관과 도재전장주조관의 치경부 변연적합도에 관한 비교 연구 (A Comparative Study on the Marginal Fit between Castable Ceramic(Dicor) Crowns and Metal-Ceramic Crowns)

  • 김정호;양재호;이선형
    • 대한치과보철학회지
    • /
    • 제26권1호
    • /
    • pp.51-61
    • /
    • 1988
  • The recently introduced castable glass ceramics incorporate properties characteristic of natural teeth and they are regarded as an ideal material to restore lost tooth structure. The purpose of this study was to compare the marginal fit of castable ceramic crown with that of the metal-ceramic crown in the process of heat treatment. Two master dies for castable ceramic crowns and metal-ceramic crowns were fabricated from being cast with the base metal. Each master die was duplicated with addition silicone and hard stone. Ten castable ceramic crowns were made on each hard stone die and their marginal openings were measured three times first, after casting; second, after ceramming; third, after shading. The other ten metal-ceramic crowns were made on each hard stone die and their marginal openings were measured three times : first, after casting; second, after degassing; third, after porcelain veneering. Each crown was seated on its master die with the constant force delivered by loading jig. And then, marginal openings were measured on four locations by optical projector at X50 magnification. The results were as follows: 1. The mean marginal openings of castable ceramic crowns were $31.1{\pm}12.7{\mu}m$ after casting; $44.6{\pm}12.8{\mu}m$ after ceramming; $51.2{\pm}16.8{\mu}m$ after shading. 2. The mean marginal openings of the metal-ceramic crowns were $26.2{\pm}13.8{\mu}m$ after casting; $29.8{\pm}10.3{\mu}m$ after degassing; $38.0{\pm}14.5{\mu}m$ after porcelain veneering. 3. There was significant increase in the marginal opening of castable ceramic crowns after ceramming, while metal-ceramic crowns sho(wed significant increase after porcelain veneering (p<0.05). 4. Marginal fit of metal-ceramic crown was better than that of castable ceramic crown (p<0.01).

  • PDF

Marginal fit of anterior 3-unit fixed partial zirconia restorations using different CAD/CAM systems

  • Song, Tae-Jin;Kwon, Taek-Ka;Yang, Jae-Ho;Han, Jung-Suk;Lee, Jai-Bong;Kim, Sung-Hun;Yeo, In-Sung
    • The Journal of Advanced Prosthodontics
    • /
    • 제5권3호
    • /
    • pp.219-225
    • /
    • 2013
  • PURPOSE. Few studies have investigated the marginal accuracy of 3-unit zirconia fixed partial dentures (FPDs) fabricated by computer-aided design/computer-aided manufacturing (CAD/CAM) system. The purpose of this study was to compare the marginal fit of zirconia FPDs made using two CAD/CAM systems with that of metal-ceramic FPDs. MATERIALS AND METHODS. Artificial resin maxillary central and lateral incisors were prepared for 3-unit FPDs and fixed in yellow stone. This model was duplicated to epoxy resin die. On the resin die, 15 three-unit FPDs were fabricated per group (45 in total): Group A, zirconia 3-unit FPDs made with the Everest system; Group B, zirconia 3-unit FPDs made with the Lava system; and Group C, metal-ceramic 3-unit FPDs. They were cemented to resin dies with resin cement. After removal of pontic, each retainer was separated and observed under a microscope (Presize 440C). Marginal gaps of experimental groups were analyzed using one-way ANOVA and Duncan test. RESULTS. Mean marginal gaps of 3-unit FPDs were $60.46{\mu}m$ for the Everest group, $78.71{\mu}m$ for the Lava group, and $81.32{\mu}m$ for the metal-ceramic group. The Everest group demonstrated significantly smaller marginal gap than the Lava and the metal-ceramic groups (P<.05). The marginal gap did not significantly differ between the Lava and the metal-ceramic groups (P>.05). CONCLUSION. The marginal gaps of anterior 3-unit zirconia FPD differed according to CAD/CAM systems, but still fell within clinically acceptable ranges compared with conventional metal-ceramic restoration.

Marginal fit of three different nanocomposite inlays fabricated with computer-aided design/computer-aided manufacturing (CAD/CAM) technology: a comparative study

  • Hyunsuk Choi;Jae-Young Jo;Min-Ho Hong
    • Journal of Yeungnam Medical Science
    • /
    • 제41권2호
    • /
    • pp.80-85
    • /
    • 2024
  • Background: This study aimed to compare and evaluate the marginal fit of nanocomposite computer-aided design/computer-aided manufacturing (CAD/CAM) inlays. Three types of nanocomposite CAD/CAM blocks (HASEM, VITA Enamic, and Lava Ultimate) were used as materials. Methods: Class II disto-occlusal inlay restorations were prepared on a typodont mandibular right first molar using diamond rotary instruments. The inlays were fabricated using CAD/CAM technology and evaluated using the silicone replica technique to measure marginal gaps at five locations on each inlay. The data were analyzed by two-way analysis of variance and Tukey post hoc tests (α=0.05). Results: There were no significant differences in the marginal gaps based on the type of nanocomposite CAD/CAM inlay used (p=0.209). However, there was a significant difference in the marginal gaps between the measurement regions. The gingival region consistently exhibited a larger marginal gap than the axial and occlusal regions (p<0.001). Conclusion: Within the limitations of this in vitro study, the measurement location significantly influenced the marginal fit of class II disto-occlusal inlay restorations. However, there were no significant differences in the marginal gaps among the different types of CAD/CAM blocks. Furthermore, the overall mean marginal fits of the class II disto-occlusal inlay restorations made with the three types of nanocomposite CAD/CAM blocks were within the clinically acceptable range.

광간섭단층영상기를 이용한 치과용 지르코니아 코어의 적합도 분석 (Analysis of the Marginal and Internal Fit of Dental Zirconia Core Using Optical Coherence Tomography(OCT))

  • 김재홍;김기백
    • 한국콘텐츠학회논문지
    • /
    • 제12권8호
    • /
    • pp.240-247
    • /
    • 2012
  • 보철물이 구강 내 제 기능을 하기 위해 가장 중요한 요소 중 하나는 적합도이다. 본 연구의 목적은 그 동안 시도되지 않았던 광간섭단층영상기를 이용하여 비파괴적인 방법으로 적합도를 측정해보고, 측정된 값을 기존의 방법으로 측정된 값과 비교하여 보고자 한다. 실험을 위해 상악 우측 중절치가 지대치인 석고모형 10개를 제작하고 치과용 캐드캠으로 각각의 모형에 해당하는 지르코니아 코어를 10개 제작하였다. 시편 당 5부위 씩 광간섭단층영상기로 적합도를 측정하고, 같은 부위를 기존의 방법인 실리 복제본 기술로 측정하였다. 두 집단 간의 평균 값에 유의한 차이가 있는지 알아보기 위해 독립표본 t-검정을 실시하였다(${\alpha}$=0.05). 그 결과 측정된 두 집단 간의 평균 값에는 유의한 차이를 보이지 않았고(P>0.05), 이러한 결과로 미루어 볼 때 앞으로 광간섭단층영상기를 이용한 보철물의 적합도 측정이 가능할 것으로 사료된다.

Effect of span length on the fit of zirconia framework fabricated using CAD/CAM system

  • Lee, Jeong-Yol;Choi, Sang-Jin;Kim, Min-Soo;Kim, Ha-Young;Kim, Young-Soo;Shin, Sang-Wan
    • The Journal of Advanced Prosthodontics
    • /
    • 제5권2호
    • /
    • pp.118-125
    • /
    • 2013
  • PURPOSE. The purpose of this study was to evaluate the effect of the span length on the fit of zirconia framework fabricated using CAD/CAM system. MATERIALS AND METHODS. Abutments for single, 4-unit and 6-unit fixed partial prostheses were fabricated. Ten zirconia frameworks were fabricated for each group. The marginal and internal gap were presented by means of replica technique and measured by measuring microscope ($AXIO^{(R)}$, Carl Zeiss, Rochester, NY) and software (I-$solution^{(R)}$, IMT i-solution Inc., Vancouver, BC, Canada). The results were statistically analyzed by multivariate analysis test and Dunnett T3 test for post hoc test (${\alpha}$=.05). RESULTS. There were statistically significant differences at 2, 4, 7, 8 points (mesio-distal section) and b, d, e, f, g (labio-lingual section). In some marginal reference points of 6-unit group (P<.05), the marginal gap were larger than 120 ${\mu}m$. CONCLUSION. Span length of zirconia core may have an influence on marginal and internal fit. Within the limitation of this study, the increase of span length of zirconia framework of 6 or more-unit fixed partial denture may decrease the marginal and internal fit.