• 제목/요약/키워드: major oxides

검색결과 150건 처리시간 0.029초

Fly Ash를 이용한$\beta$-Sialon 분말합성 (Synthesis of $\beta$-Sialon Powder from Fly Ash)

  • 최희숙;노재승;서동수
    • 한국세라믹학회지
    • /
    • 제33권8호
    • /
    • pp.871-876
    • /
    • 1996
  • It is believed that fly ash could be suitable for preparing the sialon by carbothermal reduction method because the total amount of SiO2 and Al2O3 is above 80% and the unburned residual carbon is above 5% within the fly ash. The effects of reaction temperature (1350, 1400, 145$0^{\circ}C$) reaction time (1, 5, 10 hours) and the amount of carbon additions (C/SiO2=2, 3, 4 mole) on the $\beta$-sialon synthesis were obserbed, It was conformed that $\beta$-sialon (Z=2.15~2.18) was formed as major phase under all of the synthesis conditions and small amount of Si2ON2 SiC, AlN and Si3N4 was formed depending on the synthesis conditions. FeSix intermetal-lic compound was formed above 140$0^{\circ}C$ reaction temperature due to the large amount of iron oxides within the raw fly ash.

  • PDF

얇은 산화막의 wear out에 관한 광 조사 효과 (The effect of irradiation on the wear out of thin oxide film)

  • 김재호;최복길;성영권
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1989년도 추계학술대회 논문집 학회본부
    • /
    • pp.114-118
    • /
    • 1989
  • Due to the increased integration density of VLSI circuits a highly reliable thin oxide film is required to fabricate a small geometry MOS device. The behavior of thermal $SiO_2$ under high electric field and current condition has a major effect on MOS device degration and also the practical use of MOS device under irradiation has cause the degration of thin oxide films. In this paper, in order to evaluate the reliability of thin oxides with no stress applied and stressed by the irradiation under low electric field, the tests of TDDB (Time-dependent-dielectric breakdown) are used. Failure times against electric field are examined and acceleration factor is obtained for each case. Based on the experimental data, breakdown wear out limitation for thin oxide films is characterised.

  • PDF

Numerical Investigation for Combustion Characteristics of Vacuum Residue in a Test Furnace

  • Sreedhara, S.;Huh, Kang-Y.;Park, Ho-Young
    • 한국연소학회:학술대회논문집
    • /
    • 한국연소학회 2006년도 제32회 KOSCO SYMPOSIUM 논문집
    • /
    • pp.121-127
    • /
    • 2006
  • It has become inevitable to search for alternative fuels due to severe energy crisis these days. Use of alternative fuels, which are typically of lower quality, tends to increase environmental pollution, including formation of nitrogen oxides (NOx). In this paper performance of vacuum residue has been investigated experimentally as well as numerically in typical operating conditions of a furnace. Heat release reaction is modeled as sequential steps of devolatilization, simplified gas phase reaction and char oxidation as that for pulverized coal. Thermal and fuel NOx are predicted by conditional estimation of elementary reaction rates and are compared against measured experimental data. On the overall reasonable agreement is achieved for spatial distributions of major species, temperature and NOx for all test cases.

  • PDF

태백산분지내 백악기화강암류의 화학조성과 관련광상 (Chemical Composition of the Cretaceous Granitoids and Related Ore Deposits in the Taebaegsan Basin, Korea)

  • 이재영;이인호;황덕환
    • 자원환경지질
    • /
    • 제29권3호
    • /
    • pp.247-256
    • /
    • 1996
  • Mineral commodities of metallic ore deposits related to Cretaceous granitoids in the Taebaegsan basin are distinguishable by rock types, diffferenciation index (D.I.) and chemical compositions. Deposits of Fe-Cu are related to granodiorite-quartz monzonite, those of Pb-Zn and W-Mo to granite-granodiorite and granite respectively. The ranges of D.I. of the granitoids are 39~71 for Fe-Cu deposits, 68~81 for Pb-Zn deposits, 78~89 for W-Mo deposits and 91~94 for Mn deposits. Major oxides of $K_2O$, CaO, MgO, FeO and $TiO_2$ and some trace elements and Rb/K, Sr/Ca and Cu/Fe also show distinguishable differences among the Cretaceous granitoids related to various mineral commodities of the ore depsits.

  • PDF

니켈기 인코넬 713합금의 800-1100℃에서의 대기중 고온산화 (High-temperature Oxidation of Ni-based Inconel 713 Alloys at 800-1100℃ in Air)

  • 이동복
    • 한국표면공학회지
    • /
    • 제44권5호
    • /
    • pp.196-200
    • /
    • 2011
  • The Ni-based superalloy, Inconel 713, was oxidized at $800{\sim}1100^{\circ}C$ for 50 and 100 hours in air. It displayed excellent oxidation resistance, forming a few micrometer-thick scales. The major scale was ${\alpha}-Al_2O_3$. Other scales formed were $TiO_2$, $NiAl_2O_4$ and $Cr_2O_3$. Generally, uniform oxidation occurred over the alloy surface, resulting in the formation of ${\alpha}-Al_2O_3$ with and without $Cr_2O_3$. Other oxides such as $TiO_2$ and $NiAl_2O_4$ sometimes also formed. Locally, nodular oxidation occurred at the nodules that consisted of diverse alloying elements. The scales were adherent at $800^{\circ}C$. However, they spalled a little at $900{\sim}1100^{\circ}C$.

분석 조건에 따른 p-MOSFET의 게이트에 유기된 드레인 누설전류의 열화 (Degradation of Gate Induced Drain Leakage(GIDL) Current of p-MOSFET along to Analysis Condition)

  • 배지철;이용재
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권1호
    • /
    • pp.26-32
    • /
    • 1997
  • The gate induced drain leakage(GIDL) current under the stress of worse case in -MOSFET's with ultrathin gate oxides has been measured and characterized. The GIDL current was shown that P-MOSFET's of the thicker gate oxide is smaller than that of the thinner gate oxide. It was the results that the this cur-rent is decreased with the increamental stress time at the same devices.It is analyzed that the formation components of GIDL current are both energy band to band tunneling at high gate-drain voltage and energy band to defect tunneling at low drain-gate voltage. The degradations of GIDL current was analyzed the mechanism of major role in the hot carriers trapping in gate oxide by on-state stress.

  • PDF

Aluminizing and Corrosion of Carbon Steels in N2/0.5%H2S Gas at 650-850℃

  • Abro, Muhammad Ali;Lee, Dong Bok
    • 한국표면공학회지
    • /
    • 제48권3호
    • /
    • pp.110-114
    • /
    • 2015
  • The effect of hot-dip aluminizing on the corrosion of the low carbon steel was studied at $650-850^{\circ}C$ for 20-50 h in $N_2/0.5%\;H_2S$ gas. The aluminized steel consisted primarily of the Al topcoat and the underlying Al-Fe alloy layer. Aluminizing drastically improved the corrosion resistance by forming the ${\alpha}-Al_2O_3$ surface scale. Without aluminizing, the steel formed nonadherent, fragile, thick scales, which consisted of FeS as the major phase and iron oxides such as FeO, $Fe_3O_4$ and $Fe_2O_3$ as minor ones.

Mechanisms of Cu(II) Sorption at Several Mineral/Water Interfaces: An EPR Study

  • Cho, Young-Hwan;Hyun, Sung-Pil;Pilsoo Hahn
    • 한국자기공명학회:학술대회논문집
    • /
    • 한국자기공명학회 2002년도 International Symposium on Magnetic Resonance
    • /
    • pp.72-72
    • /
    • 2002
  • In most traditional sorption study in environmental conditions, experimental sorption data have been measured and interpreted by empirical ways such as partition coefficient and sorption isotherms. A mechanistic understanding of heavy metal interactions with various minerals (metal oxides, clay minerals) in aqueous medium is required to describe the behavior of radioactive metal ions in the environment. Various spectroscopic methods provide direct or indirect information on sorption mechanisms involved. We applied EPR (Electron Paramagnetic Resonance) spectroscopy to investigate the nature of metal ion sorption at water/mineral interfaces using Cu(II) as a spin probe. The major sorbed species and their motional state was identified by their EPR spectra. They showed distinct signals due to their strength of binding, local structure and motional state. The EPR results together with macroscopic sorption data show that sorption involved at least three different mechanisms depending on chemical environments (1).

  • PDF

핵연료피복관용 Zr 합금의 부식특성 및 산화막 미세구조 (Corrosion Characteristics and Oxide Microstructure of Zirconium Alloys for Nuclear Fuel Cladding)

  • 정용환;백종혁;김선재;김경호;최병권;정연호
    • 한국재료학회지
    • /
    • 제8권4호
    • /
    • pp.368-374
    • /
    • 1998
  • Zr합금의 부식거동을 평가하기 위하여 여러 가지 1족 알칼리 수산화물 용액 (LiOH, NaOH, KOH, RbOH, CsOH)에서 autoclave를 이용하여 300일까지 부식시험을 실시하였다. 산화막 특성은 TEM을 이용하여 천이전과 천이후에 동일 산화막두께를 갖도록 준비된 부식시편에 대해 수행되었다. 실험결과를 고려할 때 금속이온은 부식과정에서 매우 중요한 역할을 하는 것으로 사료된다. 즉 $Li^+$$Zr^{4+}$ 치환하여 산소농도는 증가하고 부식은 가속되는데 산화막 내부의 barrier layer에서 $Li^-$치환이 부식을 제어하는 것으로 판단된다.동일 두께의 산화막 일지라도 산화막의 구조는 모두 다르다. 32.5mmol LiOH에서 생성된 산화막온 천이전,후에 관계 없이 많은 기공이 함유된 등축정 구조를 갖는다. 반면에 NaOH에서 생성된 산화막은 천이전에는 주상정 구조를 갖지만 천이후에는 다공성의 등축정 구조로 바뀐다. KOH용액에서는 천이전에는 주상정과 비정질 산화막의 이중 구조를 갖지만 천이후에는 비정질 산화막은 사라직 전반적으로 주상정 구조가 형성된다. 부식거동과 산화막 관찰로부터 금속이온의 산화막내 치환이 부식속도와 산화막 미세구조를 지어한다는 것을 알 수 있었다.

  • PDF

FeO/Fe(II) 시스템에서 TCE의 제거 특성 (Characteristics of the TCE removal in FeO/Fe(II) System)

  • 성동준;이윤모;최원호;박주양
    • 대한토목학회논문집
    • /
    • 제28권1B호
    • /
    • pp.149-152
    • /
    • 2008
  • 철의 환원 특성에 관한 연구는 이미 널리 수행되었으며 특히 미네랄과 2가철의 반응 메커니즘은 2가철의 흡착이나 바운드를 통해 Fe(II)-Fe(III) (hydr)oxides를 생성하여 2가철이 3가철로 산화됨으로써 물질을 환원시키는 것으로 받아들여지고 있다. 그러나 2가철로 개질된 재강슬래그를 이용한 DS/S 실험과정에서 이러한 메커니즘으로 설명하기 힘든 현상을 발견하였다. 재강슬래그의 주요 성분중의 하나인 FeO와 Fe(II)만을 이용하여 TCE의 분해과정을 실험해 본 결과 초기 TCE의 분해가 이루어지지 않다가 급속히 분해되는 현상을 보였으며 이러한 시스템에서 TCE의 분해는 예상치 못한 결과였다. FeO/Fe(II) 시스템은 3가철이 존재하지 않기 때문에 기존의 Fe(II)-Fe(III) (hydr)oxides를 형성하는 환원 메커니즘으로는 설명할 수 없었다. 따라서 본 연구에서는 TCE의 분해실험과 분해 부산물의 측정, 2가철과 3가철을 확인함으로써 FeO/Fe(II) 시스템의 환원특성을 확인해 보고자 하였다. 실험 결과 2가철이 FeO에 흡착 또는 바운드 되는 것을 확인 할 수 는 있었으나 기존의 메커니즘으로 설명하기에는 부족한 부분이 있었다. 분해부산물들을 통해 환원으로 인한 TCE의 분해는 의심의 여지가 없었으나 FeO/Fe(II) 시스템이 새로운 species를 형성하는지, 혹은 FeO에 Fe(II)가 흡착 또는 바운드 되어 이제껏 알려지지 않은 형태의 새로운 미네랄 상을 형성하는지는 좀 더 상세한 연구가 필요하다.