  • We conducted a micromagnetic modeling study to investigate the spin torque oscillator (STO) using a perpendicular polarizer. We used an additional layer of negative anisotropy constant materials (NAM) on a conventional STO. For the NAM layer, the magnetic easy plane is parallel to the in-plane easy axis of the free layer, and inhibits the development of the out-of-plane component of the magnetization in the free layer. As a result, this new type of STO provides a high frequency limit up to 50 GHz.

$(Sm_{0.5}RE_{0.5})Fe_{11}Ti$ 화합물의 구조 및 자기특성 (Structure and Magnetic Properties of $(Sm_{0.5}RE_{0.5})Fe_{11}Ti$ Compounds)

  • 김희태;김윤배;김창석;김택기;권혁무
    • 한국자기학회지
    • /
    • 제3권3호
    • /
    • pp.196-200
    • /
    • 1993
  • $(Sm_{0.5}RE_{0.5})Fe_{11}Ti$ 화합물(RE=Ce, Pr, Nd, Sm, Gd, Tb, Dy)은 정방정(tetragonal) $ThMn_{12}$ 형 구조로 형성되며 c축을 자화용이축으로하는 일축결정자기이방성을 갖 는다. 주조한 $(Sm_{0.5}RE_{0.5})Fe_{11}Ti$ 화합물은 RE=Sm일 때 가장 높은 이방성자장 11200 kA/m(140 kOe)을 가지며, RE=Nd일 때 포화자화가 $122.3\;Am^{2}/kg$(122.3 emu/g)로 가장 크며, RE=Gd일 때 큐리온도가 $326^{\circ}C$로 가장 높다.

  • PDF

수직자기기록매체용 Fe-Co-B/M 하지연자성층의 미세결정구조 및 자기특성 (Microstructure and Magnetic Properties in Fe-Co-B/M Films for Soft Magnetic Underlayer of Perpendicular Magnetic Recording Media)

  • 공석현;손인환;금민종;최형욱;박용서;김경환
    • 한국전기전자재료학회논문지
    • /
    • 제17권8호
    • /
    • pp.888-892
    • /
    • 2004
  • It is necessary to develop soft magnetic layer with high saturation magnetization 4 $\pi{M}_s$ and in-plane magnetic anisotropy field Hk for soft magnetic underlayer of perpendicular magnetic recording media with high signal to noise ratio. Fe-Co-B layer with high 4 $\pi$Ms of about 23 kG deposited on Ni-Fe and Ni-Fe/Si seedlayer exhibited very high in-plane magnetic anisotropy filed Hk of about 280 and 380 Oe, respectively, In-plane XRD studies clarified that the lattice spacing of planes along the easy axis direction was longer than that along the hard axis direction in the Fe-Co-B layers with high Hk. These results indicate that high Hk of Fe-Co-B/Ni-Fe and Fe-Co-B/[Ni-Fe/si] layers were resulted from magnetoelastic anisotropy owing to a residual stress. Moreover, the high Hk in the Fe-Co-B/Ni-Fe layer was maintained until 30$0^{\circ}C$ annealing temperature.

A Metallurgical Study on Sputtered thin Film Magnet of high $_{i}\textrm{H}_{c}$ Nd-(Fe, Co)-B alloy and Magnetic

  • Kang, Ki-Won;Kim, Jin-Ku;Song, Jin-Tae
    • 한국재료학회지
    • /
    • 제4권5호
    • /
    • pp.535-540
    • /
    • 1994
  • Thin film magnet was fabricated by radio frequency magnetron sputtering using $Nd_13/(Fe.Co)_{70}B_{17}$ alloy target and magnetic properties were investigated according to sputtering conditions from the metallurgical point of view. we could obtain the best preferred orientation of $Nd_2Fe_{14}B$ phase at substrate temperatures between $450^{\circ}C$ and $460^{\circ}C$ with the input power 150W, and thin films had the anisotropic magnetic properties. But, as the thickness of thin film increased, the c-axis orientation gradually tended to be disordered and magnetic properties also become isotropic. Just like Nd-Fe-B meltspun ribbon, the microstructure of thin film magnet was consisted of very find cell shaped $Nd_2Fe_{14}B$ phase and the second phase along grain boundary. While, domain structure showed maze patterns whose magnetic easy axis was was perpendicular to film plane of thin film. It was concluded from these results that the perpendicualr anisotropy in magnetization was attributed to the perpendicular alignment of very find $Nd_2Fe_{14}B$ grains in thin film.

  • PDF

NiFe 박막의 두께에 따른 강자성 공명 특성 분석 (Thickness Dependence of Ferromagnetic Resonance Properties in NiFe Thin Films)

  • 김동영;윤석수
    • 한국자기학회지
    • /
    • 제23권2호
    • /
    • pp.37-42
    • /
    • 2013
  • 본 연구에서는 NiFe 박막 시편을 마그네트론 스퍼터링 방법으로 제조하여 박막면 기준으로 수직면(out-of-plane) 자기장 방향과 수평면(in-plane) 자기장 방향에 따른 강자성 공명 자기장을 측정하였다. 수직면 자기장 방향에 따른 강자성 공명 자기장으로부터 유효자화량($M_{eff}$)을 도출하였으며, NiFe 두께에 따른 $M_{eff}$의 감소는 $K_s=-0.23\;erg/cm^2$의 값을 갖는 표면 이방성 상수에 기인하였다. 또한 수평면 자기장 방향에 따른 강자성 공명 자기장으로부터 수평면에서의 일축 이방성 자기장을 도출하였다. 한편, 일축 이방성 에너지의 자화 용이축이 두께가 감소함에 따라 시편 제조 시 인가한 자기장의 반대 방향으로 회전하고 있었으며, 이러한 현상은 시편 표면에 형성된 NiFeO의 반강자성 특성에 의한 현상으로 설명하였다.

이종에피에 의해 증착한 BiFeO3 박막의 전기 및 자기특성 (Electric and Magnetic Properties of Hetero-Epitaxially Deposited BiFeO3 Thin Films)

  • 이은구
    • 한국재료학회지
    • /
    • 제14권10호
    • /
    • pp.707-712
    • /
    • 2004
  • $BiFeO_3$ films grown on (111) $SrTiO_3$ substrate have a rhombohedral structure, identical to that of single crystals. On the other hand, films grown on (110) or (001) $SrTiO_3$ substrate are monoclinically distorted from the rhombohedral structure due to the epitaxial constraint. The easy axis of spontaneous polarization is close to [111] for the variously oriented films. Dramatically enhanced polarization and magnetization have been found for hetero-epitaxially grown $BiFeO_3$ thin films comparing to that of $BiFeO_3$ crystals. The results are explained in terms of an epitaxially-induced transition between cycloidal and homogeneous spin states, via magneto-electric interactions.

Soft-Lithographic Fabrication of Ni Nanodots Using Self-Assembled Surface Micelles

  • Seo, Young-Soo;Lee, Jung-Soo;Lee, Kyung-Il;Kim, Tae-Wan
    • Journal of Magnetics
    • /
    • 제13권2호
    • /
    • pp.53-56
    • /
    • 2008
  • This study proposes a simple nano-patterning process for the fabrication of magnetic nanodot arrays on a large area substrate. Ni nanodots were fabricated on a large area (4 inches in diameter) Si substrate using the soft lithographic technique using self-assembled surface micelles of Polystyrene-block-Poly(methyl methacrylate) (PS-b-PMMA) diblock copolymer formed at the air/water interface as a mask. The hexagonal array of micelles was successfully transferred to a Ni thin film on a Si substrate using the Langmuir-Blodgett technique. After ion-mill dry etching, a magnetic Ni nanodot array with a regular hexagon array structure was obtained. The Ni nanodot array showed in-plane easy axis magnetization and typical soft magnetic properties.

Magnetic Properties of SrRuO3 Thin Films Having Different Crystal Symmetries

  • Kim, Jin-I;Jung, C.U.
    • Journal of Magnetics
    • /
    • 제13권2호
    • /
    • pp.57-60
    • /
    • 2008
  • This study examined the effect of various types of epitaxial strain on the magnetic properties of $SrRuO_3$ thin films. Epitaxial $SrTiO_3$ (001), $SrTiO_3$ (110), and $SrTiO_3$ (111) substrates were used to apply different crystal symmetries to the grown films. The films were grown using pulsed laser deposition. The X-ray diffraction patterns of the films grown under optimum conditions showed very clear peaks for the $SrRuO_3$ film and $SrTiO_3$ substrates. The saturated magnetic moment at 5 K after 7 Tesla field cooling was $1.2-1.4\;{\mu}_B$/Ru. The magnetic easy axis for all three types of films was along the surface normal. The magnetic transition temperature for the $SrRuO_3$ film with lower symmetry was slightly larger than the $SrRuO_3$ film with higher symmetry.

졸겔법을 이용한 바륨페라이트 박막 제조 (Preparation of Barium Ferrite Thin Film by Sol-Gel Method)

  • 변태봉;조원덕;김태옥
    • 한국세라믹학회지
    • /
    • 제34권1호
    • /
    • pp.37-44
    • /
    • 1997
  • 졸겔법중 딥코팅법을 이용하여 조성비 2Fe/Ba=5.25 졸로부터 바륨페라이트 박막을 제조하였다. 졸의 겔화과정은 4단계로 구분할 수 있으며, 8$0^{\circ}C$에서 90분간 반응시켜 제조한 졸이 코팅용 졸로서 가장 적합한 특성을 나타내었다. 박막층에 형성된 침상 형태의 입자들은 기판에 수평 하게 위치하고 있었으며, 박막 두께가 증가함에 따라 그 경향은 증가하였다. 침상형 입자의 자화용이축 방향은 장축 방향이었다.

  • PDF

Rotation Effect of In-plane FM layer on IrMn Based GMR-SV Film

  • Khajidmaa, Purevdorj;Choi, Jong-Gu;Lee, Sang-Suk
    • Journal of Magnetics
    • /
    • 제22권1호
    • /
    • pp.7-13
    • /
    • 2017
  • The magnetoresistance (MR) properties of antiferromagnetic (AFM) IrMn based giant magnetoresistance-spin valve (GMR-SV) was investigated in view point of the artificial rotation effect of ferromagnetic (FM) layer in the plane induced by an applied field during the post annealing temperature. The MR curves measured with an azimuthal angle region of ${\phi}=0^{\circ}-360^{\circ}$ are depended on the annealing temperature and the magnetization easy axis of two free NiFe layers and two pinned NiFe layers in dual-type GMR-SV film. Especially, the annealing temperature and sample rotation angle(${\theta}$ ) maintained to the magnetic sensitivity (MS) of 1.4 %/Oe with an isotropic region angle of $110^{\circ}$ are $100^{\circ}C$ and $90^{\circ}$, respectively.