In this study, the $Ni_{0.9}Co_{0.05}Ti_{0.05}(OH)_2$ precursor was prepared by the concentration gradient co-precipitation method. In order to overcome the structural change due to oxygen desorption in the cathode active material with high nickel content, the physical and electrochemical analysis of the cathode active material according to the calcination temperature were investigated. Physical properties of $Li_{1.05}Ni_{0.9}Co_{0.05}Ti_{0.05}O_2$ were analyzed by FE-SEM, XRD and TGA. The electrochemical performance of the coin cell using a cathode active material and $LiPF_6$(EC:EMC=1:2 vol%) electrolyte was evaluated by the initial charge/discharge efficiency, cycle retention, and rate capabilities. As a result, the initial capacity and initial efficiency of cathode materials were excellent with 244.5~247.9 mAh/g and 84.2~85.8% at the calcination temperature range of $750{\sim}760^{\circ}C$. Also, the capacity retention exhibited high stability of 97.8~99.1% after 50cycles.
Objectives : Several factors, such as biological markers, clinical correlates, and course of the depressive disorders with psychotic symptoms differ from those without psychotic symptoms. Therefore, specification of a treatment algorithm for depressive disorder with psychotic symptoms is legitimated. This article provides a systematic review of somatic treatments for depressive disorder with psychotic symptoms. Methods : According to the search strategy of the Clinical Research Center for Depression of Korean Health 21 R & D Project, first, PubMed and EMBASE were searched using terms with regard to the treatment of depressive disorders with psychotic symptoms(until July 2006). Reference lists of related reviews and studies were searched. In addition, relevant practice guidelines were searched using PubMed. All identified clinical literatures were reviewed and summarized in a narrative manner. Results : Treatment options, such as a combination of an antidepressant and an antipsychotic versus an antidepressant or an antipsychotic alone are summarized. In addition, issues regarding the electroconvulsive therapy( ECT), combination therapy, and maintenance treatment are discussed. Conclusion : In former times, the combination of an antidepressant and an antipsychotic or ECT were recommended as the first line treatment for depressive disorder with psychotic symptoms. Recently, however, there was a suggestion that there was no conclusive evidence that the combination of an antidepressant and an antipsychotic drug is more effective than an antidepressant alone. More evidence regarding the pharmacological treatment for depressive disorder with psychotic symptoms is needed.
L $i_{0.5}$F $e_{2.5-{\chi}}$R $h_{\chi}$$O_4$ ($\chi$ = 0.25, 0.50, 0.75, 1.00) has been prepared by solid state reaction. Crystallographic and magnetic properties were investigated by Mossbauer spectroscopy, SQUID magnetometry, and x-ray diffraction. The crystal structure is found to be a cubic spinel structure with space group Fd3m for all the samples. The lattice constant $a_{0}$ increases from 8.3365 $\AA$ to 8.3932 $\AA$ with increasing Rh concentration $\chi$. The migration of Li ion has been confirmed by x-ray patterns and the results of applied field Mossbauer analysis. The temperature dependence of the absorption area of each site was analyzed with the Debye model for the recoil-free fraction. The Debye temperature for the octahedral sites is almost as large as for the tetrahedral sites, thereby suggesting similar inter-atomic binding forces for the octahedral and the tetrahedral sites. The saturated magnetic moment and the Mossbauer spectra taken at 4.2 K under the applied field (6 T) show that the spin structure of L $i_{0.5}$F $e_{2.5-{\chi}}$R $h_{\chi}$$O_4$ is compatible with the collinear Neel Model.
The effect of the addition of $Al^{3+}$ dopant on the electrochemical characteristics of $Li_{4}Ti_{5}O_{12}$ was investigated. $Li_{4}Ti_{5}O_{12}$ is known as a 2ero-strain material, and $Li_{3.95}Al_{0.15}Ti_{4.9}O_{12}$ has been manufactured by solid-state reaction with high energy ball milling (HEBM). The samples were heated at 800, 900 and $1000^{\circ}C$ in electric furnace. The structural and surface structures were measured by XRD (X-ray diffraction) and SEM (scanning electron microscopy). Cut-off voltage of charge/discharge cycles was $1.0{\sim}3.0 V$ to investigate reversible capacity, cycle stability and plateau voltage. The reversible capacity of $Li_{3.95}Al_{0.15}Ti_{4.9}O_{12}$ was 138 mAh/g.
$SiO_x/ZnO$ composites were prepared from sol-gel method for excellent cycle life characteristics. The composites were coated by PVC as a carbon precursor. ZnO removal to create a void space therein was able to buffer the volume change during charge and discharge. To determine the crystal structure and the shape of the synthesized composite, XRD, SEM, TEM analysis was performed. The carbon contents in the composites were confirmed by TGA. The pore structure and pore size distribution of the composite was measured with the BET specific surface area analysis and BJH pore size distribution. Enhanced electric conductivity by carbon addition was determined from powder resistance measurement. Electrochemical properties were measured with the AC impedance and the charge and discharge cycle life characteristics. When carbon was coated on the $SiO_x/ZnO$ sample, the electrical conductivity and the discharge capacity were increased. After removal of ZnO with HCl the surface area of the sample was increased, but the discharge capacity was decreased. $SiO_x/ZnO$ sample without acarbon coating showed very low discharge capacity, and after carbon coating the sample showed high discharge capacity. For cycle life characteristics, $C-SiO_x/ZnO$ composite (Zn : Si : C = 1 : 1 : 8) with a capacity of $815mAh\;g^{-1}$ at 50 cycle and 0.2 C has higher capacity than existing graphite-based anode materials.
Synthesis and Biological activity test are described for the (E)-11-tetradecen-1-yl acetate and (Z)-11-tetradecen-1-yl acetate, the sex pheromone of the Asiatic leafroller moth (Archippus breviplicanus Walsingham). 10-Bromodecan-1-ol THP ether was prepared from 10-bromodecan-1-ol. In liquid ammonia with THF and HMPA as cosolvents, sodium acetylide could be alkylated with 10-bromodecan-1-al THP ether to give 11-dodecyn-1-ol THP ether. 11-Dodecyn-1-ol THP ether was then treated with n-Buli in THF to give the lithium acetylide, which was alkylated with bromoethane to afford 11-tetradecyn-1-ol THP ether. 11-Tetradecyn-1-ol THP ether was then reduced over $Pd/BaSO_4$ and with Na in liquid $NH_3$ to give (Z)-11-tetradecen-1-ol THP ether and (E)-11-tetradecen-1-ol THP ether, respectively. (Z)-and (E)-11-Tetradecen-1-ol THP ether thus obtained were deprotected by refluxing in the presence of PPTS and ethanol. (Z)-and (E)-11-tetradecen-1-ol were acetylated with acetic anhydride to afford the final products, (Z)-11-tetradecen-1-yl acetate (1) and (E)-11-tetradecen-1-yl acetate (2), respectively. The synthetic pheromone thus obtained was attractive to the males of the Asiatic leafroller moth in the field.
Kim, K.H.;Choi, K.H.;Kum, J.S.;Kim, B.C.;Kim, J.R.
Solar Energy
/
v.19
no.4
/
pp.45-53
/
1999
This report Introduces a total heat exchanger in a solar air-conditioning system using Lithium Chloride(LiCl) solution. The hot and humid outside air is cooled and dehumidified by LiCl solution that is sprayed on the packed layer of the total heat exchanger. LiCl solution once diluted is concentrated again in a regenerator using solar energy. Three types as the packed materials were used in this experiment and the dehumidification performance was evaluated by the value of $k_xa(kg/h{\cdot}m^3{\cdot}{\Delta}x)$, overall mass transfer coefficient based on a humidity ratio potential difference, the influence of inlet LiCl solution flow rate, air flow rate, packed layer height on $k_xa$ was investigated. It was found that air flow rate, LiCl solution flow rate, packed layer height for all types had a great influnce on the value of $k_xa$.
Si-C composites were prepared by the carbonization of silicon powder covered by polyaniline(PAn). Physical and electrochemical properties of the Si-C composites were characterized by the particle size analysis, X-ray diffraction technique, scanning electron microscope, and electrochemical test of battery. The average particle size of the Si was increased by the coating of PAn and somewhat reduced by the carbonization to give silicone-carbon composites. XRD analysis' results were confirmed co-existence of crystalline silicon and amorphous-like carbon. SEM photos showed that the silicon particle were well covered with carbonacious materials depend on the PAn content. Si-C|Li cells were fabricated using the Si-C composites and were tested using the galvanostatic charge-discharge test. Si-C|Li cells gave better electrochemical properties than that of Si|Li cell. Si-C|Li cell using the Si-C from HCl undoped PAn Precursor showed better electrochemical properties than that from HCl doped PAn Precursor. Using the electrolyte containing FEC as an additive, the initial discharge capacity was increased. After that the galvanostatic charge-discharge test with the GISOC(gradual increasing of the state of charge) condition was carried out. Si-C(Si:PAn:50:50 wt. ratio)|Li cell showed 414 mAh/g of the reversible specific capacity, 75.7% of IIE(initial intercalation efficiency), 35.4 mAh/g of IICs(surface irreversible specific capacity).
The cathode material, $LiNi_{0.5}Mn_{1.5}O_4$, for high voltage applications of Li-ion batteries exhibits impurity phases due to oxygen deficiency during the high temperature heat treatment. The impurity phase reduces the electrochemical properties of the electrode since the deficiency spinel structure disturbs the lithium ion intercalation and deintercalation. In this study, Cr-substituted $LiNi_{0.5-x}Mn_{1.5}Cr_xO_4(0{\leq}x{\leq}0.05)$ powders are synthesized by a sol-gel method in order to reduce the amount of the impurity phases in the $LiNi_{0.5-x}Mn_{1.5}Cr_xO_4$. Thermal analysis of the cathode material shows that the $LiNi_{0.5}Mn_{1.5}O_4$ without Cr substitution looses $2\%$ of its weight due to oxygen deficiency but the amount of weight loss is diminished when Cr is substituted. XRD analysis also supports the reduction of the impurity phases in the cathode after chromium substitution, suggesting that the improvement of the electrochemical properties such as the capacity retention and electrochemical stability are attributed to the low content of impurity phases in the Cr-substituted $LiNi_{0.5-x}Mn_{1.5}Cr_xO_4.$
Kim, Sun-Ah;Cho, Woo-Ram;Jeong, Koo-Hyun;Cho, Byung-Won;Na, Byung-Ki
Journal of the Korean Electrochemical Society
/
v.14
no.1
/
pp.27-32
/
2011
The electorchemical properties of $Li_4Ti_5O_{12}$ added with Cr was tested. The addition or substitution of atoms to $Li_4Ti_5O_{12}$ are expected to modify the crystal structure, and therefore to change the electrochemical performances of $Li_4Ti_5O_{12}$. After the spinel structure $Li_4Ti_{5-x}Cr_xO_{12}$ (x = 0~0.2) were obtained via sol-gel method, the gel was heated in a muffle furnace at $800{\sim}850^{\circ}C$ for 12 h in air. The physical properties of the samples were characterized by TG-DTA, XRD, SEM, FT-IR, and the electrochemical properties were tested with battery cycler at 0.01~2.0 V range. The $Li_4Ti_5O_{12}$ exhibited 169.9 mAh/g at 1C and capacity recovery was 97.5% of the initial capacity at 0.1C. $Li_4Ti_{4.9}Cr_{0.1}O_{12}$ (Cr 1% added) showed best performance of 193.8 mAh/g at 1C and the capacity recovery was increased to 98.8% of the initial capacity at 0.1C.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.