액상가압공정으로 제조된 탄탈륨 연속섬유 강화 비정질 복합재료의 미세조직과 기계적 성질 (Microstructure and Mechanical Properties of Tantalum-Continuous-Fiber-Reinforced Amorphous Matrix Composites Fabricated by Liquid Pressing Process)

  • 이규홍;이상복;이상관;이성확
    • 대한금속재료학회지
    • /
    • 제46권7호
    • /
    • pp.403-411
    • /
    • 2008
  • Zr-based amorphous alloy matrix composites reinforced with tantalum continuous fibers were fabricated by liquid pressing process, and their microstructures and mechanical properties were investigated. About 60 vol.% of tantalum fibers were homogeneously distributed inside the amorphous matrix, which contained a small amount of polygonal crystalline particles. The ductility of the tantalum-continuous-fiber-reinforced composite under tensile or compressive loading was dramatically improved over that of the monolithic amorphous alloy, while maintaining high strength. The consequential observation of the tensile deformation and fracture behavior of the composite showed the formation of multiple shear bands and multiple necking, crack deflection in the amorphous matrix, and obstruction of crack propagation by ductile fibers, thereby resulting in very high tensile elongation of 7.2%. These findings suggested that the liquid pressing process was useful for the development of amorphous matrix composites with improved ductility.

액상 성형 가압법을 이용한 탄소나노섬유 강화 Cu 기지 나노 복합재료 개발 (Development of Carbon Nanofiber Reinforced Cu Matrix Composites Using Liquid Pressing Process)

  • 이상관;김두현;엄문광;하동호;김상식
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2003년도 추계학술발표대회 논문집
    • /
    • pp.50-53
    • /
    • 2003
  • Carbon nannofiber reinforced Cu matrix composite has potential applications for electrically conducting materials having high strength and electrical conductivity. In this study, we have developed fabrication technology of the nanocomposites using a liquid pressing process. The process is to use the low pressure for infiltration of Cu melt into carbon nanofiber mat as the Cu melt is pressurized directly. The minimum pressure required for infiltration was calculated from force balance equation, permeability measurement and compaction behavior of carbon nanofiber. Also, the melting temperature and the holding time have been optimized.

  • PDF

롤러 가압 임프린트 공정에서 잔류막 두께 예측에 관한 연구 (A Study on the expectation of residual layer thickness in roller pressing imprint process)

  • 조영태;정윤교
    • 한국기계가공학회지
    • /
    • 제12권1호
    • /
    • pp.104-109
    • /
    • 2013
  • In order to apply nano imprint technology in large area process, roller pressing is promising because of its low cost and high productivity. When pressing mold by roller, liquid resin is locally squeezed between mold and substrate. In this study, the main focus is to understand which process parameter affects residual layer. To do this, a simple analytical model was introduced. Especially, we consider the aspect ratio of patterns as essential cause of variation of the thickness in the equation. As a result, when the aspect ratio of pattern in the mold increases, the thickness of residual layer also increases. In conclusion, we show that the uniformity of residual layer could be accomplished by the control of velocity and pressing force in roller pressing imprint process.

반용융 성형공정에 있어서 액상편석제어를 위한 압축 D/B 및 응용 (Compression D/B for Liquid Segregation Control in Semi-Solid Forming Process and Its Application)

  • 정경득
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 고액공존금속의 성형기술 심포지엄(III) SYMPOSIUM ON SEMISOLID FORMING TECHNOLOGY(III)
    • /
    • pp.15-32
    • /
    • 1999
  • A relationship between stress and stain is very important to design a die to avoid defects of products during semi-solid forming process. Since the liquid will be of eutectic composition in alloys liquid segregation will result in significant or undesirable situation. The materials used in this experiment are A 357. A390, Al2024 alloys that is fabricated by the electro-magnetic stirring process from Pechiney in France. The compression test was performed by induction heating equipment and MTS. In order to prevent the liquid segregation these measured temperature would be useful to control of strain rate during compression test. The liquid segregation is controlled as change of the strain rate and solid fraction during the compression process, The characteristics of flow between solid and liquid phase considering liquid segregation is examined through the above experiments. In the case of medium and high volume fractions of solid the distribution of strain rate is calculated by using compression test data of semi-solid materials (SSM). The thixoforming experiments with the designed die are carried out successfully. The die filling patterns of SSM for variation of die temperature and pressing force have been investigated. The hardness of the thixoformed scroll products is evaluated in terms of the microstructure for each position.

  • PDF

액상가압성형 공정을 이용한 SiC 연속섬유 강화 마그네슘 복합재료 개발 (Development of Continuous SiC Fiber Reinforced Magnesium Composites Using Liquid Pressing Process)

  • 조승찬;이동현;이영환;신상민;고성민;김정환;김양도;이상관;이상복
    • Composites Research
    • /
    • 제33권5호
    • /
    • pp.247-250
    • /
    • 2020
  • 본 연구에서는 액상가압성형 공정을 이용하여 SiC 연속섬유가 강화된 마그네슘 복합재료의 제조 가능성을 검토하였다. 액상가압성형 공정을 이용하여 SiC 섬유가 균일 분산된 AZ91 복합재료를 제조하였으며 열처리를 통하여 석출상을 제어하였다. SiC 섬유와 기지합금의 계면에 연속적인 Mg2Si상이 형성되면서 계면 결합력이 향상되었고, 제조된 복합재료의 상온 인장강도는 479 MPa로 우수한 기계적 특성을 나타내었다.

액상가압공정으로 제조된 탄탈륨 연속섬유 강화 Zr계 비정질 복합재료의 기계적 성질의 이방성 (Anisotropic Mechanical Properties of Tantalum-Continuous-Fiber-Reinforced Zr-based Amorphous Matrix Composites Fabricated by Liquid Pressing Process)

  • 이규홍;이상복;이상관;이성학
    • 대한금속재료학회지
    • /
    • 제47권9호
    • /
    • pp.542-549
    • /
    • 2009
  • Zr-based amorphous alloy matrix composites reinforced with tantalum continuous fibers were fabricated by the liquid pressing process, and their anisotropic mechanical properties were investigated by tensile and compressive tests of $0^{\circ}$(longitudinal)-, $45^{\circ}$-, and $90^{\circ}$(transverse)-orientation specimens. About 60 vol.% of tantalum fibers were homogeneously distributed inside the amorphous matrix, which contained a small amount of polygonal crystalline particles. The ductility of the tantalum-continuous-fiber-reinforced composite under tensile or compressive loading was dramatically improved over that of the monolithic amorphous alloy, while maintaining high strength. When the fiber direction was not matched with the loading direction, the reduction of the strength and ductility was not serious because of excellent fiber/matrix interfacial strength. Observation of the anisotropic deformation and fracture behavior showed the formation of multiple shear bands, the obstruction of crack propagation by fibers, and the deformation of fibers themselves, thereby resulting in tensile elongation of 3%~4% and compressive elongation of 15%~30%. These results suggest that the liquid pressing process was useful for the development of amorphous matrix composites with excellent ductility and anisotropic mechanical properties.

액상가압공정으로 제조된 금속 연속섬유강화 비정질 복합재료의 미세파괴거동 (Microfracture Behavior of Metallic-Continuous-Fiber-Reinforced Amorphous Matrix Composites Fabricated by Liquid Pressing Process)

  • 이규홍;이상복;이상관;이성학
    • 대한금속재료학회지
    • /
    • 제46권8호
    • /
    • pp.524-537
    • /
    • 2008
  • Zr-based amorphous alloy matrix composites reinforced with metallic continuous fibers were fabricated by liquid pressing process, and their fracture properties were investigated by directly observing microfracture process using an in situ loading stage installed inside a scanning electron microscope chamber. About 60 vol.% of metallic fibers were homogeneously distributed inside the amorphous matrix. Apparent fracture toughness of the stainless-steel- and tungsten-fiber-reinforced composites was lower than that of monolithic amorphous alloy, while that of the Ta-fiber-reinforced composite was higher. According to the microfracture observation, shear bands or cracks were initiated at the amorphous matrix, and the propagation of the initiated shear bands or cracks was effectively blocked by fibers, thereby resulting in stable crack growth which could be confirmed by the fracture resistance curve (R-curve) behavior. This increase in fracture resistance with increasing crack length improved fracture properties of the fiber-reinforced composites, and could be explained by mechanisms of formation of multiple shear bands or multiple cracks at the amorphous matrix and blocking of crack or shear band propagation and multiple necking at metallic fibers.

액상가압공정으로 제조된 STS304와 Ta 섬유 강화 Zr계 비정질 복합재료의 준정적 및 동적 변형거동 (Quasi-Static and Dynamic Deformation Behavior of STS304- and Ta-fiber-reinforced Zr-based Amorphous Matrix Composites Fabricated by Liquid Pressing Process)

  • 김용진;신상용;김진성;허훈;김기종;이성학
    • 대한금속재료학회지
    • /
    • 제48권6호
    • /
    • pp.477-488
    • /
    • 2010
  • Zr-based amorphous alloy matrix composites reinforced with stainless steel (STS) and tantalum continuous fibers were fabricated without pores or defects by a liquid pressing process, and their quasi-static and dynamic deformation behaviors were investigated by using a universal testing machine and a Split Hopkinson pressure bar, respectively. The quasi-static compressive test results indicated that the fiberreinforced composites showed amaximum strength of about 1050~1300 MPa, and its strength maintained over 700 MPa until reaching astrain of 40%. Under dynamic loading, the maximum stresses of the composites were considerably higher than those under quasi-static loading because of the strain-rate hardening effect, whereas the fracture strains were considerably lower than those under quasi-static loading because of the decreased resistance to fracture. The STS-fiber-reinforced composite showed a greater compressive strength and ductility under dynamic loading than the tantalum-fiber-reinforced composite because of the excellent resistance to fracture of STS fibers.

텅스텐 다공성폼 강화 Zr계 비정질 기지 복합재료의 미세조직과 기계적 성질 (Microstructure and Mechanical Properties of Amorphous Matrix Composite Reinforced with Tungsten Porous Foam)

  • 손창영;이상복;이상관;김충년;이성학
    • 대한금속재료학회지
    • /
    • 제48권2호
    • /
    • pp.109-115
    • /
    • 2010
  • In the present study, a Zr-based amorphous alloy matrix composite reinforced with tungsten porous foam was fabricated without pores or defects by liquid pressing process, and its microstructures and mechanical properties were investigated. About 69 vol.% of tungsten foam was homogeneously distributed inside the amorphous matrix, although the matrix of the composite contained a small amount of crystalline phases. The compressive test results indicate that the composite was not fractured at one time after reaching the maximum compressive strength, but showed considerable plastic strain as the compressive load was sustained by tungsten foam. The tungsten foam greatly improved the strength (2764 MPa) and ductility (39.4%) of the composite by homogeneously dispersing the stress applied to the matrix. This was because the tungsten foam and matrix were simultaneously deformed without showing anisotropic deformation due to the excellent bonding of tungsten/matrix interfaces. These findings suggest that the liquid pressing process is useful for the development of amorphous matrix composites with improved strength and ductility.

액상가압공정을 이용한 CNF/Mg 복합재료의 제조 및 특성평가 (Fabrication and Characterization of CNFs/Magnesium Composites Prepared by Liquid Pressing Process)

  • 김희봉;이상복;이진우;이상관;김양도
    • Composites Research
    • /
    • 제25권4호
    • /
    • pp.93-97
    • /
    • 2012
  • 본 연구에서는 액상가압공정을 이용하여 탄소나노섬유(carbon nano fiber, CNF)를 강화재로 하는 AZ91 마그네슘 복합재를 제조하였다. CNF의 분산성 및 마그네슘 합금 용탕과의 젖음성을 향상시키고자 CNF를 마이크로 크기의 실리콘 카바이드 입자(silicon carbide particle, $SiC_p$)와 혼합하였다. 또한, CNF와 $SiC_p$의 혼합분말에 무전해도금법으로 니켈을 코팅하였다. 액상가압공정에서 AZ91 용탕은 무처리된 CNF, CNF와 $SiC_p$의 혼합분말(CNF+$SiC_p$), 니켈 코팅된 CNF와 $SiC_p$의 복합분말((CNF+$SiC_p$)/Ni)과 같이 세 종류의 강화재로 정수압에 의해 함침하여 복합재를 제조하였다. 무처리된 CNF 강화 복합재료에서는 일부 CNF 응집체가 관찰되었으나 CNF+$SiC_p$ 및 (CNF+$SiC_p$)/Ni 강화 복합재에서는 CNF가 기지재 내에 균일하게 분산되었음을 확인하였다. 압축시험결과, CNF+$SiC_p$ 및 (CNF+$SiC_p$)/Ni 강화 복합재의 압축강도가 무처리된 CNF 강화 복합재보다 각각 38%와 28% 향상되었다.