• Title/Summary/Keyword: leached

Search Result 489, Processing Time 0.024 seconds

The Analysis of Environmental Loads and Material Recycling of the Nutrients by the Livestock Wastewater Originating from Imported Feeds (수입사료에 의한 가축분뇨 물질순환 및 환경부하 분석)

  • Yoon, Young-Man;Lee, Sang-Eun;Chung, Doug-Young;Cho, Gyu-Yong;Kim, Jong-Duk;Kim, Chang-Hyun
    • Journal of The Korean Society of Grassland and Forage Science
    • /
    • v.28 no.2
    • /
    • pp.139-154
    • /
    • 2008
  • The nearly 75% of animal feed materials used for livestock production are imported every year in Korea. Most of imported feed ingredients are concentrated feeds such as com, wheat, soybean, soybean meal, etc. and they are used as the source materials for the production of assorted feed. The imported concentrated feeds are high in nitrogen and phosphorus. Therefore, the consistent import of feed ingredients may cause an increase of nutrient deposit in our agricultural ecosystem. In the current review, it was discussed with the situation of the feed importation and its nutritional composition to evaluate the nutrient load by the imported feeds onto agricultural ecosystem. The nutrient load caused by imported feeds in agricultural environment was compared with the nutrient demand for crop production. The amounts of N, $P_2O_5\;and\;K_2O$ introduced by the imported fteds in Korea were 371, 140 and 143 Ktons. And, the N, $P_2O_5\;and\;K_2O$ loads excreted from imported feeds in livestock were 148, 84 and 86 Ktons of N, $P_2O_5\;and\;K_2O$ and These nutrient loads by the imported feeds are at the percentage of N 52%, $P_2O_5$ 52% and $K_2O$ 42% in the comparison of total nutrient amounts excreted from livestock animals in Korea. The 82.3% of nutrients excreted from livestock was recycled to crop land as compost and liquid fertilizer, and the others were discharged to river after water treatment processing or disposed to ocean. Also, passing through the recycling process far the production of compost and liquid fertilizer, the amount of nutrients was reduced by the ammonia vaporization of livestock feces and urine. Accordingly, N 81, $P_2O_5$ 74 and $K_2O$ 76 Ktons in the nutrients excreted from livestock were estimated to be utilized in the crop land. Consequently, it was estimated that 44, 48 and 69 Ktons of N, $P_2O_5\;and\;K_2O$ were taken up with crops in the consideration of the ratio of mineralization, and the amounts of leached or deposited N, $P_2O_5\;and\;K_2O$ in crop land were estimated to be 37, 27 and 7 Ktons, respectively. It is estimated that 12%, 34% and 48% of N, $P_2O_5\;and\;K_2O$ introduced by the imported feeds were used by crops, and 10%, 34% and 5% of N, $P_2O_5\;and\;K_2O$ were leached or deposited in agricultural ecosystem. Therefore, considering the leached and deposited amounts of N, $P_2O_5\;and\;K_2O$ originated from the imported feed ingredients, the consistent import of feeds may gradually increase the nutrient load onto agricultural ecosystem.

Mineral Phase Transitions of Jarosite Substituted by Oxyanions during the Reductive Dissolution Using Oxalate Solution (옥살레이트 용액을 이용한 환원성 용해 시 산화음이온으로 치환된 자로사이트의 광물 상변화)

  • Lee, Myoungsin;Lee, Dongho;Chun, Herin;Kim, Yeongkyoo;Baek, YoungDoo
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.34 no.2
    • /
    • pp.95-106
    • /
    • 2021
  • The SO4 in the jarosite structure can be substituted by other oxyanions, and therefore, the transition of jarosite to goethite plays a very important role in controlling the behavior of oxyanions. In this study, the phase change according to the species of the oxyanion in jarosite and the related behavior of the oxyanion was studied by mineralogical and geochemical methods when jarosite, which is coprecipitated with various oxynions, undergoes a phase change by a reductive dissolution. Jarosite substituted by five oxyanions by 5 mol% was used in this study. The mineral phase change induced by reductive dissolution using ammonium oxalate was investigated, and the order of phase transition rate of jarosite to goethite was MoO4-jarosite ≥ SeO4-jarosite ≥ CrO4-jarosite > pure jarosite > SeO3-jarosite > AsO4-jarosite, showing that the transition rates vary depending on the substituted oxyanion. The resultant concentration of the leached Fe was slightly different depending on the type of oxyanion and time but did not show a noticeable difference. The concentration of each oxyanion leached according to the change of the mineral phase showed that the order of concentration of oxyanions was Mo > Se(SeO3) > As > Se(SeO4) > Cr in general, and showed a slight increase with time. This trend was related to the species of oxyanions rather than mineral phase change. The results of this study showed that the phase transition of jarosite to goethite was affected by the species of oxyanions, but this tendency did not affect the concentrations leached oxyanions.

Influence of Percolation Rate on Nutrient Uptake and Yield of Paddy Rice (투수속도(透水速度)가 수도(水稻)의 양분흡수(養分吸收) 및 수량(收量)에 미치는 영향(影響))

  • Shin, Weon-Kyo
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.17 no.3
    • /
    • pp.218-223
    • /
    • 1984
  • In order to analyze the effects of percolation rate on the growth and yield of rice plants in paddy soils, pot (1a/2000) experiments were carried out. The soil used was highly concentrated with various salts in the horticulture area under vinyl house cultivation, and Samgang variety of Japanica rice was planted. With the increasing rates of percolation, $SiO_2$ and $Ca^{2+}$ were more leached out from soils than supplied by irrigation while $K^+$ and $NH_4{^+}$ were more supplied to soils than leached out. The root activity in the late growth stage was higher in the percolation pots than in the non-percolation pots. Amounts of nutrient uptake of T-N, $P_2O_5$, $K_2O$ and MgO were increased gradually with the increase of percolation rate, but that of $SiO_2$ was maximum at 10mm per day. The percolation rate of 5~10mm per day was considered to be the optimum condition for obtaining more than 95% of relative yield in rice cultivation.

  • PDF

Selective Phase Transformation of Arsenopyrite by Microwave Heating and their Enhancement Au Recovery by Thiocyanate Solution (마이크로웨이브 가열에 의한 황비철석의 선택적 상변환과 티오시안산염 용액에 의한 Au 회수율 향상)

  • Han, Oh-Hyung;Kim, Bong-Ju;Cho, Kang-Hee;Choi, Nag-Choul;Park, Cheon-Young
    • Journal of the Mineralogical Society of Korea
    • /
    • v.27 no.2
    • /
    • pp.73-83
    • /
    • 2014
  • In order to investigate selective phase transformations and to determine the maximum Au leaching factors from microwave treated Au-bearing complex sulfides, a microscope, SEM-EDS analysis, and thiocyanate leaching tests were performed. When the Au-bearing complex sulfides were exposed to microwave heating, increasing the microwave exposure time increased temperature and decreased weight. Arsenopyrite was first selectively transformed to hematite, which formed a concentric rim structure. In this hematite, oxygen and carbon was detected and always showed high iron content and low arsenic content due to arcing and oxidation from microwave heating. The results of the leaching test using microwave treated sample showed that the maximum Au leaching parameters was reached with 0.5 g concentration thiocyanate, 2.0 M hydrochloric acid, 0.3 M copper sulfate and leaching temperature at$60^{\circ}C$. Under the maximum Au leaching conditions, 59% to 96.69% of Au was leached from the microwave treated samples, whereas only 24.53% to 92% of the Au was leached from the untreated samples.

The Extraction of Ca in Electric arc Furnace Slag for CO2 Sequestration (CO2고정화(固定化)를 위한 전기로제강(電氣爐製鋼)슬래그의 칼슘성분(成分) 침출(浸出))

  • Youn, Ki-Byoung
    • Resources Recycling
    • /
    • v.22 no.1
    • /
    • pp.64-71
    • /
    • 2013
  • Mineral carbonation has been proposed as a possible way for $CO_2$ sequestration. The electric arc furnace slags consist of calcium, magnesium and aluminum silicates in various combinations. If they could be used instead of natural mineral silicates for carbonation, considerable energy savings and $CO_2$ emissions reductions could be achieved. Indirect aqueous carbonation of the slags consists of two steps, extraction of calcium and carbonation. Acetic acid leaching of electric arc furnace slags had been already studied to extract Ca in them, but it was reported that the carbonation of the extracted $Ca^{2+}$ in the leached solution would suffer from too slow kinetics, even at high pressure of $CO_2$. In this work, to develop more efficient extraction of the electric arc furnace slags, hydrochloric acid leaching to separate calcium from them was studied, and the results were compared with the acetic acid ones. The phase boundary between $Ca^{2+}$ and $CaCO_3$ in the solution with pH was determined by thermodynamic calculations. Hydrochloric acid was more effective than acetic acid for the extraction of Ca in electric arc furnace slag, and there is a possibility to recycle an unreacted hydrochloric acid in the leached solution by electrolysis or evaporation.

Liming Materials and Desalinization of Marine Originated Tidal Soil (석회(石灰)의 종류(種類)와 해성간척지(海成干拓地) 토양(土壤)의 제염(除鹽))

  • Oh, Wang-Keun
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.23 no.2
    • /
    • pp.107-113
    • /
    • 1990
  • In comparision with calcium sulphate, the effect of calcium-carbonate, -silicate and -hydroxide on desalinization of tidal saline soil was investigated in a continuous leaching column experiments after mixing with an equivalent amount of Ca to sodium plus magnessium in the saline soil. One half of liming materials was mixed to the top one-tenth of column soil and the remainder was spread on the surface. Results obtained are as follows ; 1. Gypsum made easy to percolate and desaline (Na) tidal marine soil but accumulated magnessium in subsoil. 2. $Ca(OH)_2$, $CaCO_3$, and $CaSO_3$ precipitated Mg in the soil which limes were mixed, but they washed down magnessium more severely from the immediate bellow the limed soil and less from the subsequent soil layers. This leaching was more severer at the treatment of $Ca(OH)_2$and lowest at the treatment of $CaSiO_3$. 3. The alkalinity of lime in addition to the dissociation of exchangeable Na raised pH of limed leached tidal soil and slowed down the percolation rate which retarded desalining Na from limed saline soils. This effect was most severe in the $Ca(OH)_2$ treated soil. 4. pH of leached soils was correlated possitively with exchangeable Na and negatively with exchangeable Mg giving follwing relationship pH= 7.77+0.489 Na/Mg r = 0.845.

  • PDF

Leaching of CMSX-4 Superalloy in Hydrochloric Acid Solutions (염산(鹽酸)에 의한 CMSX-4 초내열합금(超耐熱合金)의 침출(浸出))

  • Kim, Min-Seuk;Lee, Jae-Chun;Kim, Eun-Young;Yoo, Young-Soo
    • Resources Recycling
    • /
    • v.19 no.5
    • /
    • pp.25-30
    • /
    • 2010
  • Leaching of CMSX-4 superalloy was done in hydrochloric acid solutions. The leaching behaviors of main alloy components, such as Ni, Co, Cr, Al, was investigated by controlling acid concentration, temperature, leaching time and pulp density. Increasing acid concentration enhanced the leaching rate till the rate decreased over 3 M acid concentration. Raising temperature increased the leaching amount of the metal components. After the leaching for 60 minutes at $90^{\circ}C$ and 10 g/L pulp density in 4 M acid solution, 93.2% nickel, 89.9% aluminum, 80.4% cobalt, and 79.1% chromium were leached. Nickel and aluminum were preferentially leached out, while the leaching rate of cobalt and chromium were relatively high only after 60 minutes, Increasing pulp density lowered the leaching rate and especially serious on cobalt and chromium, The optimum leaching condition for CMSX-4 was obtained at $90^{\circ}C$, 120 minutes, and less than 125 g/L in 4 M hydrochloric acid solution.

Separation and Recovery of Tin and Indium from Spent ITO Sludge (폐 ITO 슬러지로부터 주석과 인듐의 분리·회수)

  • Lee, Ki-Woong;Kim, Hong-In;Son, Hyun-Tae;Ahn, Jae-Woo;Kim, Yong-Hwan
    • Resources Recycling
    • /
    • v.23 no.2
    • /
    • pp.53-60
    • /
    • 2014
  • In order to separate Indium and Tin from spent indium tin oxide (ITO) sludge, direct hydrochloric acid leaching and thermal reduction followed by HCl leaching were applied. In case of direct leaching of spent ITO, leaching rate of In and Sn was 18.5% and 19.95%, respectively. Whereas, in case of thermal hydrogen treatment of ITO sludge at different temperatures such as $700^{\circ}C$, $800^{\circ}C$, $900^{\circ}C$ and $1100^{\circ}C$, followed by HCl leaching, we obtained the result of more than 97% leaching rate of Sn. Specially, thermal treatment at $800^{\circ}C$ showed the highest leaching rate of 98.2% of Sn. Precipitation method was used for separation and recovery of Sn from leached mixed solution. If the solution pH were adjusted 2.0, 99.69% of Sn precipitated and 10.3% of In was precipitated. This confirmed the possibility of separation of Sn and In from leached solution by precipitation method.

Formation and Preservative Effectiveness of Inorganic Substances in Wood Treated with Potassium Carbonate and Calcium Chloride (탄산칼륨과 염화칼슘을 이용한 무기질 복합화 목재 중에 있어서 무기염의 생성과 방부효력)

  • Yoon, Sun-Mi;Lee, Jong-Shin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.29 no.2
    • /
    • pp.126-132
    • /
    • 2001
  • This research is carried out to investigate the formation and preservative effectiveness of inorganic substance, calcium carbonate($CaCO_3$), in wood. The specimens were prepared by the impregnation with saturated solutions of potassium carbonate($K_2CO_3$) into the wood followed by precipitation in saturated solutions of calcium chloride($CaCl_2$) for 24h, 72h and 120h, and then they were leached in instrument flowing with water for 24h. The weight percent gains of $K_2CO_3$ solution impregnated specimens reached approximately a maximum value (108.1%) by 72h precipitation in $CaCl_2$ solutions. Inorganic substances were observed to he produced in the lumina of tracheids of specimens. From these inorganic substances filling in the tracheids, characteristic X-rays of calcium(Ca-$K_{\alpha}$) were detected by energy dispersive X-ray analyzer. Moreover, it was shown from a leaching treatment that these substances could not he leached easily from the specimens. Therefore, they were could he considered to be insoluble calcium carbonates. The weight losses of the prepared specimens were hardly occurred by test fungi attacks. Thus inorganic substances in specimens can be said to have preservative effectiveness.

  • PDF

A Study on the Removal of Arsenic 1mm Closed-Mine Tailings by Acid-Leaching Process (산침출에 의한 광미중 비소성분의 제거에 관한 연구)

  • 오종기;이화영;김성규;이재령;박재구
    • Journal of Korea Soil Environment Society
    • /
    • v.3 no.3
    • /
    • pp.21-31
    • /
    • 1998
  • A study on the acid leaching and precipitation has been conducted to remove arsenic from the closed-mine tailings. HCI and H$_2$SO$_4$were used as the leach liquor of arsenic and the tailing obtained from the Da-Duck Mine, which was already closed several decades ago, was also used as the source of arsenic. The effect of the concentration of acid, leaching time and the slurry density on the leaching efficiency of arsenic has been examined. In addition, pH controls and the addition of sodium sulfide were also attempted to remove the arsenic compound as the precipitation from the leachate. After 1 hr leaching by HCI, 40 to 86% of arsenic was leached out depending on the concentration of acid or the slurry density while 47 to 77% of it was leached out by $H_2$$SO_4$. The leaching of arsenic by both acids was almost accomplished within 10 min. and after that only a slight increase in leaching efficiency was observed with leaching time. When the leach liquor was used repeatedly for the leaching of arsenic, the concentration of arsenic in the leach liquor was found to increase continuously although the leaching efficiency was diminished. As far as the precipitation of arsenic in the leachate was concerned, more than 99% of arsenic could be precipitated through the addition of sodium sulfide as the precipitator while the pH controls resulted in the precipitation of up to 84%.

  • PDF