• 제목/요약/키워드: laminated finishing

검색결과 17건 처리시간 0.022초

직물 구조인자와 표면 가공특성이 스포츠 의류용 투습직물의 발수/방수/투습특성에 미치는 영향 (Effect of Fabric Structural Parameters and Surface Finishing Characteristics to Water Repellency/Proofing/Vapor Permeability of Breathable Fabrics for Sportswear Clothing)

  • 김현아
    • 한국의류산업학회지
    • /
    • 제22권1호
    • /
    • pp.112-118
    • /
    • 2020
  • This paper examined the water repellency, water proofing and water vapor permeability of twelve types of woven fabrics for sports wear clothing. Their physical properties were compared and discussed with the fabric structural parameters and surface finishing effect. A water repellent property of 100% was obtained in the coated or laminated water repellent finished fabrics; in addition, cotton/nylon breathable composite fabrics treated with a laminated finishing and with low fabric density showed a 90% water repellency. Water proofing fabric above 6,000 mm H2O hydraulic pressure was achieved by coated or laminated finishing; however, high density fabric or medium-level coated fabrics exhibited 100% water repellent and low water proofing characteristics. Superior water vapor permeability characteristics with good water repellency and proofing properties were achieved at the 2.5 layered low density and with 0.7 - 0.9 cover factor nylon fabrics treated with hydrophilic laminated finishing. The regression analysis for examining the effects of fabric structural parameters and surface finishing such as coating and laminating to the water vapor permeability exhibited a high determination coefficient of fabric structural parameters of 63.5%; in addition,, main factors among fabric structural parameters appeared to be cover factor and fabric thickness per weight. Coating and Laminating factors exhibited determination coefficient of water vapor permeability parameters of 36.5%.

VLM-ST 시작품의 적층무늬 제거를 위한 표면처리 방법론 개발 (Development of Surface Finishing Methodology for the Laminated Pattern Removal of VLM-ST Parts)

  • 이상호;김효찬;송민섭;양동열
    • 한국정밀공학회지
    • /
    • 제22권2호
    • /
    • pp.202-209
    • /
    • 2005
  • A new effective thick-layered RP process, Transfer-type Variable Lamination Manufacturing using expandable polystyrene foam (VLM-ST) has been developed with thick layers and sloped surfaces. VLM-ST has the innate advantages by virtue of its working principle: high building speed, low cost for introduction and maintenance of VLM-ST apparatus, little staircase surface irregularities of parts. Despite these advantages in VLM-ST, the surface roughness of VLM-ST parts is still inadequate to be used as RP master patterns for rapid tooling (RT). This paper describes the systematic and effective methodology to remove the laminated pattern and improve the surface roughness for VLM-ST parts. From the results of surface finishing of VLM-ST parts, it can be seen that the laminated pattern is completely removed and the surface characteristics such as surface roughness, surface hardness, and paintability are improved.

Evaluation of Physical, Mechanical Properties and Pollutant Emissions of Wood-Magnesium Laminated Board (WML Board) for Interior Finishing Materials

  • PARK, Hee-Jun;JO, Seok-Un
    • Journal of the Korean Wood Science and Technology
    • /
    • 제48권1호
    • /
    • pp.86-94
    • /
    • 2020
  • This study serves as basic research for the development of a new wood-based building finishing material that improved the weakness of inorganic materials such as gypsum board and magnesium board widely used as interior finishing materials and brought out the strength of the wood. The results of evaluating the physical and mechanical properties and the environmental effect related to hazardous substance discharge having manufactured a wood-magnesium laminated composite are as follows. The thermal conductivity and thermal resistance of WML board was improved by about 28~109 percent over magnesium board due to the low thermal conductivity of wood. The adhesive strength of WML board showed a similar result to that of plywood as it exceeds 0.7N/㎟, the adhesive standard of wood veneer which is presented by KS F 3101. Bending strength and screw holding strength were more improved by manufacturing WML board than magnesium board. The WML board manufactured in this study satisfied the criteria for emissions of hazardous substances prescribed in the Indoor Air Quality Control Act, and confirmed the possibility of development as a new wood-based composite material that can replace existing inorganic materials.

투습도 측정방법에 따른 스포츠웨어용 투습직물의 투습특성 (Breathability of Breathable Fabrics for Sportswear according to Measuring Method)

  • 김현아;김승진
    • 한국의류산업학회지
    • /
    • 제19권4호
    • /
    • pp.493-503
    • /
    • 2017
  • This study investigated water vapor permeability of the 73 breathable fabrics for sports-wear according to the materials, finishing methods and fabric structural parameters. The water vapor permeability by KS K 0594 method of PET breathable fabric was superior than that of nylon one, in addition, water vapor permeability of coated or laminated breathable fabrics were higher than those of hot melt or dot laminated fabrics. The water vapor permeability of breathable fabric was dependent on the thickness, weight and density, which was consistent with measuring method. However, water vapor permeability according to materials and finishing method showed different results according to measuring method. The correlation coefficient of WVP of PET breathable fabrics between ISO and KS K measuring methods was -0.83 and the correlation coefficient of WVP of coated breathable fabrics was -0.72 and -0.71 for KS K and ASTM and -0.72 for KS K and ISO in hot melt laminated breathable fabrics. According to regression analysis, WVP of PET breathable fabric by both KSK and ISO measuring methods was highly dependent upon on the density and weight. In addition, WVP of hot melt laminated breathable fabric was highly dependent upon thickness, weight and density. Therefore, relevant measuring method for WVP of breathable fabrics has to be adopted to measure precise breathability.

광·열경화형 수지를 이용한 탄소섬유 프리프레그의 물리적 특성 (Mechanical Characteristics of CF Laminated Prepreg with UV-thermal Dual Curable Epoxy Resin)

  • 심지현;김지혜;박성민;구광회;장기욱;배진석
    • 한국염색가공학회지
    • /
    • 제29권1호
    • /
    • pp.37-44
    • /
    • 2017
  • An issue of major concern in the utilization of laminated composites based epoxy resin is associated with the occurrence of delaminations or interlaminar cracks, which may be related to manufacturing defects or are induced in service by low-velocity impacts. A strong interfacial filament/brittle epoxy resin bonding can, however, be combined with the high fracture toughness of weak interfacial bonding, when the filaments are arranged to have alternate sections of shear stress. To improve this drawback of the epoxy resin, UV-thermal dual curable resin were developed. This paper presents UV-thermal dual curable resin which were prepared using epoxy acrylate oligomer, photoinitiators, a thermal-curing agent and thermoset epoxy resin. The UV curing behaviors and characteristics of UV-thermal dual curable epoxy resin were investigated using Photo-DSC, DMA and FTIR-ATR spectroscopy. The mechanical properties of UV-thermal dual curable epoxy resin impregnated CF prepreg by UV curable resin content were measured with Tensile, Flextural, ILSS and Sharpy impact test. The obtained results showed that UV curable resin content improves the epoxy toughness.

CLT 건축물의 외벽 및 지붕 구조체 레이어 구성 유형 분석 (Analysis of the Types of External Wall and Roof Structure Layer Composition of CLT Building)

  • 유동완;이태구
    • 한국농촌건축학회논문집
    • /
    • 제22권4호
    • /
    • pp.71-78
    • /
    • 2020
  • Today, the whole world is going through a big chaos due to the COVID-19, but paradoxically, the emergence of COVID-19 has been leading to the need for sustainable development, such as Green New Deal that can improve global warming and carbon emissions, and the need for sustainable architecture is growing bigger and bigger in the architectural field as well. The level of CLT buildings in Korea is at a very rudimentary stage, while CLT buildings remedying existing wooden buildings are getting the spotlight among European countries for sustainable architecture. This study was conducted to categorize structure layer compositions of overseas CLT buildings and analyze architectural techniques and materials applied by collecting and analyzing information about CLT structure layer compositions of overseas CLT building-related institutions, companies and cases. When classifying structure layer compositions of foreign CLT buildings depending on the roles of layers. it was revealed that exterior wall structure layers were combined and organized within a sequence of external finishing, ventilation, waterproof, board, external insulation, airtightness, structure, airtightness, interior insulation, interior finishing, sloped roof structure layers were external finishing, ventilation, waterproof, board, external insulation, airtightness, structure, airtightness, interior insulation, interior finishing, flat roof structure layers were external finishing, ventilation, waterproof, planking wood, external insulation, waterproof, external insulation, airtightness, structure, airtightness, interior insulation, interior finishing.

프라이머 가공 방법이 열융착 필름 라미네이팅으로 제조한 고충격 대응 에어쿠션 소재의 물성에 미치는 영향 연구 (A Study on the Effect of Primer Processing Method on the Mechanical Properties of Impact Relief Air Cushion Materials Prepared through Thermal Film Laminating)

  • 김지연;김훈민;민문홍
    • 한국염색가공학회지
    • /
    • 제34권3호
    • /
    • pp.173-184
    • /
    • 2022
  • In this study, the TPU film was laminated on an aramid fabric or circular knits in order to implement an air cushion material that can respond to high impact forces in case of a fall and is easy to expand. To increase the bonding strength between the fabric layer and the film layer, a primer layer was formed in two ways: one for thermally bonding and laminating PET film and two for coating and aging hot melt type PUR adhesive. The tensile strength of the aramid air cushion was 2.5 times higher than that of the circular knits, but the tensile elongation of the aramid air cushion was very low compared to that of the circular knits. The tear strength of the aramid air cushion was about twice or more superior to that of the circular knits, the primer treatment method was good at A, and the peel strength was excellent at method A. The aramid air cushion was the lightest in weight. Summarizing the above results, it was best to combine the air cushion material with aramid woven fabric and primer treatment method A to cope with the high impact force applied when falling.

프라이머 코팅과 열융착 필름 라미네이팅을 통해 제조한 충격 완화용 고강력 에어쿠션 직물에 관한 연구 (Study on the High-Strength Air-Cushion Fabrics for Impact-Relief Application Prepared through Primer Coating and Thermal Film Laminating)

  • 김지연;김훈민;민문홍
    • 한국염색가공학회지
    • /
    • 제33권4호
    • /
    • pp.269-279
    • /
    • 2021
  • In this study, the laminating of TPU film after coating of primer adhesive on the fabrics was applied in order to secure the strength to withstand a fall from a higher altitude by increasing the adhesion between the fabric and the film layer. It seems that the fineness of the yarn and the weave construction have a greater effect than the type of the laminating films. The order of superiority of the laminated fabrics by film type and thickness was the same for 1000 denier and 210 denier fabrics, and the tendency was consistent with the order of superiority in the film properties and peel strength tests. The tear strength of laminating fabrics increased three to four times for 1000 denier fabrics compared to the fabric alone, but it decreased by 2 times for the 210 denier fabrics. Summarizing the above results, it is most appropriate to combine 1000d fabric with three types of laminating films(100~200㎛ thickness) of A(0.2T) or B(0.15T) or D(0.1T) considering the air pressure resistance, the impact resistance during the fall, and the durability against damage during use.

스포츠웨어용 투습발수직물의 마찰음과 역학적 성질 간의 상관성 (Relationship Between Frictional Sounds and Mechanical Properties of Vapor Permeable Water Repellent Fabrics for Active Wear)

  • 양윤정;박미란;조길수
    • 한국의류산업학회지
    • /
    • 제10권4호
    • /
    • pp.566-571
    • /
    • 2008
  • Frictional sounds of 8 vapor permeable water repellent fabrics by sound generator were recorded and analyzed through FFT fast Fourier transform analysis. The frictional Sounds were quantified by calculating level pressure of total sound(LPT), the level range(${\Delta}L$) and the frequency difference(${\Delta}f$). Mechanical properties were measured by KES-FB. LPT values of specimens finished wet coating were higher than those of other kinds of finishing. ${\Delta}L$ values of specimens laminated were highest. Absolute values of ${\Delta}f$ were high in the cire finished and laminated specimens. Values for bending rigidity, shear stiffness and energy required for the compression of coated specimens increased compared with the cire finished and laminated specimens. Laminated specimens had high values of frictional coefficient and low values of surface roughness. Relationship between frictional sounds and mechanical properties analysed by use of correlation coefficients and stepwise regression. LPT showed significant correlation with elongation, tensile energy, geometrical roughness, weight and thickness. ${\Delta}L$ was highly correlated with tensile linearity, frictional coefficient, and ${\Delta}f$ with tensile linearity, weight and thickness. LPT were revealed to be explained by elongation and weight. ${\Delta}L$were predicted by tensile linearity, and ${\Delta}f$ by tensile linearity and thickness.

신발용 직물의 투습방수 및 내열성 가공 (Water Vapour Permeable/Water Resistant and Heat Resistant Finishing of Footwear Fabric)

  • 이재호;최해욱
    • 접착 및 계면
    • /
    • 제7권3호
    • /
    • pp.16-25
    • /
    • 2006
  • 내열성 및 투습방수기능을 가진 신발용 직물 및 부직포를 제조하기 위하여 스크린 방식으로 공정조건을 검토하고 투습방수 필름을 라미네이팅 한 후, 최종제품의 물성을 평가하였다. 결과는 다음과 같다. 열가소성 핫 멜트와는 달리 반응형 폴리우레탄 핫 멜트는 작업 이후에 적정한 내열성을 보유하는 것으로 나타났다. 최적의 용융접착 공정조건은 다음과 같다 ; 드럼 온도 $95^{\circ}C$, 호스 온도 $97^{\circ}C$, 공급파이프 온도 $100^{\circ}C$, 스크린 온도 $105^{\circ}C$이고, opposite roller의 압력은 $1kgf/cm^2$, laminating roller의 압력은 $3kgf/cm^2$이며, 가공속도는 15 m/min이다. 투습도는 필름의 두께가 증가함에 따라 투습도는 감소하였으나, 내수도는 증가하였고, 공기투과도는 필름의 영향이 지배적이었다.

  • PDF