• 제목/요약/키워드: high-volume slag concrete

검색결과 100건 처리시간 0.021초

순환골재 및 소각장 애시를 자극제로 사용한 고로슬래그 미분말 다량치환 콘크리트의 Mock-up 성능평가 (Mockup Test of the High Volume Blast Furnace Slag Concrete Using Recycled Aggregates and Incinerator Ash)

  • 김영희;곽용진;김준호;이향재;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2012년도 추계 학술논문 발표대회
    • /
    • pp.19-21
    • /
    • 2012
  • This paper was to investigate the effect of incinerator ash on engineering properties of the high volume blast furnace slag concrete through Mock-up test. Test results revealed that the use of recycled aggregates resulted in increase of slump compared with the OPC concrete. But, the use of recycled aggregates did not affect the results of air contents and chloride contents. The use of recycled aggregates showed shortening of setting time of high volume blast furnace slag concrete. When the recycled aggregate was used, delay in strength development at early age happened with high volume blast furnace slag concrete compared with that of OPC concrete.

  • PDF

Optimal Mixture Proportion for High Performance Concrete Incorporating Ground Granulated Blast furnace Slag

  • Choi Jae-Jin;Kim Eun-Kyum;Yoo Jung-Hoon
    • 콘크리트학회논문집
    • /
    • 제17권3호
    • /
    • pp.473-480
    • /
    • 2005
  • In this study, a mix design for self compacting concrete was based on Okamura's method and concrete incorporated just a ground granulated blast furnace slag. Replacement ratio of slag is in the range of $20-80\%$ of cement matrix by volume. For the optimal self compactability in mixture incorporating ground granulated blast furnace slag, the paste and mortar tests were first completed. Then the slump flow, elapsed time of 500mm slump flow, V funnel time and filling height by U type box were conducted in concrete. The volume of coarse aggregate in self compacting concrete was in the range of $50-60\%$ to the solid volume percentage of coarse aggregate. Finally, the compressive and splitting tensile strengths were determined in the hardened self compacting concrete incorporating ground granulated blast furnace slag. From the test results, it is desirable for self compacting concrete that the replacement of ground granulated blast furnace slag is in the range of $40-60\%$ of cement matrix by volume and the volume of coarse aggregate to the solid volume percentage of coarse aggregate with a limit of $55\%$.

전기로 산화슬래그 골재를 활용한 중량 콘크리트의 단위 용적 중량 변화에 따른 X-선 차폐 성능 비교 (Comparison of X-ray Shielding Performance according to the Weight of unit volume of Heavy Weight Concrete Utilizing Electric Arc Furnace Oxidizing Slag.)

  • 임희섭;이한승;최재석
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 춘계 학술논문 발표대회
    • /
    • pp.35-36
    • /
    • 2013
  • Electric arc furnace oxidizing slag from massively produced steel slag has been used in road bases and subbases, hot mix asphalt, and landfill. Electric arc furnace oxidizing slag contains iron (15%~30%) and has a high density of 3.0~3.7 ton/m3. Depending on the type and amount of concrete aggregates, the radiation-shielding characteristics can vary. Therefore, aggregates of electric arc furnace oxidizing slag can be considered for the production of radiation-shielding concrete. The experimental design of this study is experiments on Compressive strength experiments, X-ray irradiation experiments, and experiments related to the unit volume weight were carried out on hardened concrete. This experiment compared the performance evaluation of radiation shielding of concrete using electric arc furnace oxidizing slag.

  • PDF

제강 슬래그를 이용한 콘크리트의 동결융해에 대한 실험적 연구 (An Experimental Study on the Freezing and Thawing of Concrete Mixed with Steel Slag)

  • 정원섭;조성현;권기주;박성우;김진만
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.48-53
    • /
    • 2003
  • The steel slag, a by-product which is produced on the process of manufacturing steel by refining pig iron is mainly used as road materials after aging it. It is necessary to age steel slag for long time in air because the reaction with water and free-CaO in steel slag could make the volume expanded. Due to this reason it prevents steel slag from being used as aggregate of concrete. But steel slag used in this study is controled by a air-jet method which rapidly cools substance melted at a high temperature. Rapid cooling prevents from generating of free-CaO in steel slag. In this study, it was investigated that steel slag manufactured by air-jet method affects on concrete in the freezing and thawing. As results of this study, concrete mixed with steel slag was worse in the freezing and thawing than concrete mixed with sand in spite of using air entraining agent. To obtain durability of concrete in the freezing and thawing, it is desirable to mix 50% of steel slag in concrete per unit weight of volume.

  • PDF

굵은골재 체적에 따른 고유동콘크리트의 유동특성에 관한 실험적 연구 (The Experience Study on the Floating Properties of High Flow Concrete on volum of Coarse Aggregate used Admixture)

  • 최성우;김호수;백철우;반성수;류득현
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 추계 학술발표회 제16권2호
    • /
    • pp.751-754
    • /
    • 2004
  • There are many factors that affect on the flowing properties of high flowing concrete(HFC), which are fluidity, compactibility, non-segregation ability and fillingability. And because the aggregate which is one of the factors occupies high volume in concrete, it has a much effect on the properties of high flowing concrete according to its size, quality and quantity etc. This is an experimental study to analyze the effect of admixture and volume of coarse aggregate in concrete on the flowing properties of high flowing concrete. For this purpose, the kinds of admixture are fly-ash and blast furnace slag. Also volume of coarse aggregate in concrete are 280, 290, 300, 310, 320 $(\ell/m^3)$. The test of flowablity properties is slump-flow, Air content, V-lot, L-Flow. According to test results, it was found that the compactibility of HFC is more superior to use blast furnace slag than other, and according .to kind of admixture, most compatible volume of coarse are different. Also when used blast furnace slag, the volume of coarse are increased than used fly-ash.

  • PDF

Effect of Powder and Aggregates on Compactability of High Performance Concrete

  • Lee, Seung-Han;Han, Hyung-sub
    • KCI Concrete Journal
    • /
    • 제11권3호
    • /
    • pp.19-28
    • /
    • 1999
  • This study treated self-compacting high Performance concrete as two Phase materials of Paste and aggregates and examined the effect of powder and aggregates on self-compacting high performance, since fluidity and segregation resistance of fresh concrete are changed mainly by paste. To improve the fluidity and self-compactibility of concrete, optimum powder ratio of self-compacting high performance concrete using fly ash and blast-furnace slag as powders were calculated. This study was also designed to provide basic materials for suitable design of mix proportion by evaluating fluidity and compactibility by various volume ratios of fine aggregates, paste, and aggregates. As a result, the more fly ash was replaced, the more confined water ratio was reduced because of higher fluidity. The smallest confined water ratio was determined when 15% blast-furnace slag was replaced. The lowest confined water ratio was acquired when 20% fly ash and 15% blast-furnace slag were replaced together. The optimum fine aggregates ratio with the best compactibility was the fine aggregate ratio with the lowest percentage of void in mixing coarse aggregate and fine aggregate In mixing the high performance concrete. Self-compacting high performance concrete with desirable compactibility required more than minimum of unit volume weight. If the unit volume weight used was less than the minimum, concrete had seriously reduced compactibility.

  • PDF

마이크로버블이 유화처리 정제유지류(ERCO)혼입 고로슬래그 다량 치환 콘크리트의 특성에 미치는 영향 (Effect of Micro Bubble on the High-Voiume Slag Concrete Mixed with Emulsified Refined Cooking Oil)

  • 김민영;박용준;백두환;백병훈;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 춘계 학술논문 발표대회
    • /
    • pp.44-45
    • /
    • 2015
  • Although the carbonation problem of high-volume slag concrete has been solved by the mixed use of emulsified refine cooling oil as the pilot study, there was an instance of securing air quantity and frost resistance followed by the use of Expancel due to the problem of having vulnerability in frost resistance in result as the air quantity has not been secured. But due to the problem of Expancel not being economical, air quantity and frost resistance of high-volume slag concrete mixed with ERCO are attempted to be secured using micro bubble that can remain in the water for a long time as a relatively economical and very microscopic bubble.

  • PDF

분체의 종류에 따른 고유동 콘크리트의 품질성능에 관한 연구 (A study on the quality performances of the high flowing concrete for binder types)

  • 권영호;이현호;하재담
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.567-572
    • /
    • 2002
  • This research investigates experimentally an effect on the quality performances of the high flowing concrete according to binder types. The purpose of this study is to determine the optimum mix proportion of the high flowing concrete having good flowability, viscosity and no-segregation. For this purpose, two types using belite cement+lime stone powder(LSP) and furnace slag cement+lime stone powder are selected and tested by design factors including water cement ratio, fine and coarse aggregate volume ratio. As test results of this study, the optimum mix proportion for binder types is as followings. 1) One type based belite cement ; water cement ratio $51^{\circ}C$, fine aggregate volume ratio $43^{\circ}C$ and coarse aggregate volume ratio $53^{\circ}C$, replacement ratio of LSP $42.7^{\circ}C$. 2) Another type based slag cement : water cement ratio $41^{\circ}C$, fine aggregate volume ratio $47^{\circ}C$ and coarse aggregate volume ratio $53^{\circ}C$, replacement ratio of LSP $13.5^{\circ}C$.

  • PDF

무수석고 함량이 고로슬래그 미분말을 대량 활용한 콘크리트 특성에 미치는 영향 (Effect of Anhydrite on the Mechanical and Durability Properties of High Volume Slag Concrete)

  • 문규돈;김주형;조영근;최영철
    • 한국건설순환자원학회논문집
    • /
    • 제2권3호
    • /
    • pp.239-246
    • /
    • 2014
  • 온실가스 저감 및 자원활용 목적으로 고로슬래그 미분말을 다량으로 활용한 콘크리트에 대한 연구가 활발히 진행되고 있으나, 조기강도 및 내구성능 확보에 어려움이 있다. 따라서, 본 연구에서는 무수석고 함량(0%, 4%, 6%, 8%, 10%)에 따라 고로슬래그 미분말을 대량 활용한 콘크리트의 수화, 강도발현, 크리프, 탄산화, 건조수축 특성을 분석하였다. 무수석고를 바인더의 4~6% 수준으로 치환할 경우 고로슬래그 미분말 대량 활용 콘크리트의 가장 취약점인 초기강도 발현을 보완할 수 있으며, 내구성 측면에서도 보통 포틀랜드 시멘트를 사용한 콘크리트와 유사한 성능을 발현하는 것을 알 수 있었다. 반면, 무수석고를 8% 이상 활용할 경우 초기강도 증진 효과가 미흡한 결과를 나타냈다.

슬래그를 다량 치환한 콘크리트의 동결융해 저항성능에 미치는 미세공극의 영향 (Effects of Micropores on the Freezing-Thawing Resistance of High Volume Slag Concrete)

  • 김래환;김규용;이보경;신경수;송권용
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제19권4호
    • /
    • pp.67-74
    • /
    • 2015
  • 본 연구에서는 슬래그를 다량 치환한 콘크리트의 동결융해 저항성능에 미치는 미세공극의 영향을 검토하였다. 콘크리트는 용선예비처리 슬래그가 포함된 고로슬래그 미분말을 0, 40, 70 % 치환하여 제조하였으며 압축강도 특성 및 동결융해 저항성능과 미세공극을 검토하였다. 또한 설계기준강도와 목표공기량을 설정하고, 동결융해 작용에 따른 열화를 확인하기 위하여 재령 14일의 낮은 압축강도로 인한 내력저하를 유도하였다. 실험결과, 설계기준강도를 유사하게 설정하고 목표공기량을 확보하였음에도 불구하고 콘크리트의 미세공극 분포가 상이한 결과를 나타내었다. GGBS70 시험체는 동결융해를 받지 않은 초기 0사이클에서 10~100 nm 크기의 공극량이 가장 적어 공극 내 동결할 수 있는 물의 양이 적을 것으로 판단된다. 이러한 이유로 다른 시험체에 비해 동결팽창압력이 상대적으로 작기 때문에 동결융해 저항성능이 우수한 것으로 판단된다.