• 제목/요약/키워드: high temperature steam

검색결과 560건 처리시간 0.034초

고압 고온 수증기에서 지르칼로이-4 산화반응 정량화 및 사고해석에의 응용 (Zricaloy-4 Oxidation Kinetics in High-Pressure High-Temperature Steam and Application to Accident Analysis)

  • 박광헌
    • 한국표면공학회지
    • /
    • 제35권6호
    • /
    • pp.363-370
    • /
    • 2002
  • Empirical equations for the oxide thickness and the weight gain of Zircaloy-4 cladding during the oxidation in high temperature, high pressure steam have been developed. Firstly, the empirical equations for oxide thickness in 1 atm steam in 700~100$0^{\circ}C$ were made, then, the enhancement factor for the steam pressure effects on Zircaloy-4 cladding oxidation in high temperature steam was added. Based on the analysis of the weight fraction of dissolved oxygen in metal layer, empirical equations for the weight gain of Zircaloy-4 in high pressure, high temperature steam were developed. We compare the developed empirical equations with the Baker-Just correlation. The Baker-Just correlation can give a non-conservative estimation of oxidation of Zircaloy-4, depending on the steam pressure. These developed empirical equations can be used for the correct estimation of oxidation of Zircaloy-4 during accident analysis.

인코벨 690 증기발생기 세관의 고온 마모 거동 (High Temperature Wear Behavior of Inconel 690 Steam Generator tube)

  • 홍진기;김인섭;김형남;장기상
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2001년도 제34회 추계학술대회 개최
    • /
    • pp.59-62
    • /
    • 2001
  • Flow induced vibration in steam generators has caused dynamic interactions between tubes and contacting materials resulting in fretting wear . Series of experiments have been performed to examine the wear properties of Inconel 690 steam generator tubes in various environmental conditions. For the present study, the test rig was designed to examine the fretting wear and rolling wear properties in high temperature(room temperature - 290。C) water. The test was performed at constant applied load and sliding distance to investigate the effect of test temperature on wear properties of the steam generator tube materials. To investigate the wear mechanism of material, the worn was observed using scanning electron microscopy. The weight loss increase at higher test temperature was caused by the decrease of water viscosity and the mechanical property change of tube material. The mechanical property changes of steam generator tube material, such as decrease of hardness or yield stress in the high temperature tests. From the SEM observation of worn surfaces, the severe wear scars were observed in specimens tested at the higher temperature.

  • PDF

수소 생산을 위한 동축원통형 수증기 개질기의 성능 및 열유속에 대한 수치해석 연구 (Numerical Study on the Performance and the Heat Flux of a Coaxial Cylindrical Steam Reformer for Hydrogen Production)

  • 박준근;이신구;배중면;김명준
    • 대한기계학회논문집B
    • /
    • 제33권9호
    • /
    • pp.709-717
    • /
    • 2009
  • Heat transfer rate is a very important factor for the performance of a steam reformer because a steam reforming reaction is an endothermic reaction. Coaxial cylindrical reactor is the reactor design which can improve the heat transfer rate. Temperature, fuel conversion and heat flux in the coaxial cylindrical steam reformer are studied in this paper using numerical method under various operating conditions. Langmuir-Hinshelwood model and pseudo-homogeneous model are incorporated for the catalytic surface reaction. Dominant chemical reactions are assumed as a Steam Reforming (SR) reaction, a Water-Gas Shift (WGS) reaction, and a Direct Steam Reforming (DSR) reaction. Although coaxial cylindrical steam reformer uses 33% less amount of catalyst than cylindrical steam reformer, its fuel conversion is increased 10 % more and its temperature is also high as about 30 degree. There is no heat transfer limitation near the inlet area at coaxial-type reactor. However, pressure drop of the coaxial cylindrical reactor is 10 times higher than that of cylindrical reactor. Operating parameters of coaxial cylindrical steam reformer are the wall temperature, the inlet temperature, and the Gas Hourly Space Velocity (GHSV). When the wall temperature is high, the temperature and the fuel conversion are increased due to the high heat transfer rate. The fuel conversion rate is increased with the high inlet temperature. However, temperature drop clearly occurs near the inlet area since an endothermic reaction is active due to the high inlet temperature. When GHSV is increased, the fuel conversion is decreased because of the heat transfer limitation and short residence time.

화력발전소의 과열기증기의 온도제어 (Temperature Control of Superheater Steam in Thermal Power Plant)

  • 신휘범;이순영
    • 전기학회논문지
    • /
    • 제59권11호
    • /
    • pp.2006-2011
    • /
    • 2010
  • The superheater in the thermal power plant makes the wet steam into the dry steam with high temperature and high pressure by using the boiler heat. The dry steam pressure rotates the turbine-generator system. The efficiency and life time of the boiler heavily depends on the steam temperature regulation. The steam temperature can be deviated from the reference by the MW demand of the power plant. It is therefore required that the PI(proportional-integral) controller should be robust against the disturbance such as the MW demand. In this paper, the PI controller with the integral state predictor is proposed and applied to regulate the steam temperature of the superheater, and it is compared with the conventional PI controller operated in the thermal power plant in view of control performance.

촉진양생에 의한 온도이력이 고강도 모르타르의 강도발현에 미치는 영향 (An Effects of the Strength Development of High Strength Mortar under Temperature History by Steam Curing)

  • 권희성;최응규;임남기;이영도;정상진
    • 한국건축시공학회지
    • /
    • 제8권4호
    • /
    • pp.115-121
    • /
    • 2008
  • The present study performed low-pressure steam curing with mortar specimens in order to examine the temperature profile and strength development of steam curing in high-strength specimens of 100MPa. In addition, as a basic research to utilize PC products, we examined the effects of curing temperature and time in steam curing cycle on strength development resulting from the hydration of cement within the range of high strength by changing four factors affecting the quality of PC displacement time, peak curing temperature, peak temperature duration, and ascending and descending gradient of temperature - in various patterns, and analyzed the optimal strength development characteristic based on the relation between temperature profile and strength development. With regard to the high-temperature curing characteristic of PC, we performed an experiment on the strength characteristic according to the temperature profile of high-strength mortar, and from the results of the experiment according to curing characteristic, displacement time, peak curing temperature, peak temperature duration, and ascending and descending gradient of temperature, we drew conclusions as follows.

Effects of Test Temperature on the Reciprocating Wear of Steam Generator Tubes

  • Hong, J.K.;Kim, I.S.
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.379-380
    • /
    • 2002
  • Steam generators (S/G) of pressurized water reactors are large heat exchangers that use the heat from the primary reactor coolant to make steam in the secondary side for driving turbine generators. Reciprocating sliding wear experiments have been performed to examine the wear properties of Incoloy 800 and Inconel 690 steam generator tubes in high temperature water. In present study, the test rig was designed to examine the reciprocating and rolling wear properties in high temperature (room temperature - $300^{\circ}C$) water. The test was performed at constant applied load and sliding distance to investigate the effect of test temperature on wear properties of steam generator tube materials. To investigate the wear mechanism of material, the worn surfaces were observed using scanning electron microscopy. At $290^{\circ}C$, wear rate of Inconel 690 was higher than that of Incoloy 800. It was assumed to be resulted from the oxide layer property difference due to the a\loy composition difference. Between 25 and $150^{\circ}C$ the wear loss increased with increasing temperature. Beyond $150^{\circ}C$, the wear loss decreased with increasing temperature. The wear loss change with temperature were due to the formation of wear protective oxide layer. From the worn surface observation, texture patterns and wear particle layers were found. As test temperature increased, the proportion of particle layer increased.

  • PDF

Methods and Systems for High-temperature Strain Measurement of the Main Steam Pipe of a Boiler of a Power Plant While in Service

  • Guang, Chen;Qibo, Feng;Keqin, Ding
    • Journal of the Optical Society of Korea
    • /
    • 제20권6호
    • /
    • pp.770-777
    • /
    • 2016
  • It has been a challenge for researchers to accurately measure high temperature creep strain online without damaging the mechanical properties of the pipe surface. To this end, a noncontact method for measuring high temperature strain of a main steam pipe based on digital image correlation was proposed, and a system for monitoring of high temperature strain was designed and developed. Wavelet thresholding was used for denoising measurement data. The sub-pixel displacement search algorithm with curved surface fitting was improved to increase measurement accuracy. A field test was carried out to investigate the designed monitoring system of high temperature strain. The measuring error was less than $0.4ppm/^{\circ}C$, which meets actual measurement requirements for engineering. Our findings provide a new way to monitor creep damage of the main steam pipe of a boiler of an ultra-supercritical power plant in service.

태양열 발전을 위한 고온 축열 물질의 열전달 특성 (Heat Transfer Characteristics of High Temperature molten salt storage for Solar Thermal Power Generation)

  • ;김기만;한귀영;서태범;강용혁
    • 한국태양에너지학회 논문집
    • /
    • 제27권3호
    • /
    • pp.63-69
    • /
    • 2007
  • The heat transfer characteristics of inorganic salt for high temperature heat storage material of solar power system were examined. The inorganic salts employed in this study was a mixture of $NaNO_3$ and $KNO_3$ and the operating temperature range was determined by measuring the melting temperature with DSC and by measuring the thermal decomposition temperature with TGA. The heat transfer characteristics was qualitatively obtained in terms of temperature profiles of salt in the tanks during the heat storage and heat release process as a function of steam flow rates, steam inlet temperature and the inlet position of steam. The effects of steam flow rates and inlet temperature of steam were experimentally determined and the effect of natural convection was observed due to significant density difference with temperature.

고온 증기를 이용한 잎담배의 팽화연구 (Method for expanding tobacco leaves with steam at high temperature and velocity)

  • 김병구;김기환;정한주;유광근;이태호
    • 한국연초학회지
    • /
    • 제17권1호
    • /
    • pp.68-78
    • /
    • 1995
  • A study of expanding tobacco includes the steps of adjusting the moisture content of cut tobacco, without the use of exogenous impregnants by contacting the filler with a high velocity gaseous medium at elevated temperature such that heat is rapidly and substantially uniformly transferred from the medium to the filler for a total contact time sufficient to expand the tobacco leaves. Study is disclosed for drying and expanding cut tobacco by introducing the tobacco into an elongated tubular shaped conduit through which steam high temperature 150-35$0^{\circ}C$ and high velocity above the 18m1sec, super steam is recycled. moisture content of shreded tobacco leaves, immediately before treatment within the range of from 10% to 24% and, most preferably, within the range of from 18% to 21%. Expanding rate showed 70% in NC -82(B.3) and 42% in Burley -21(B.1) which is produced in 1993 under this condition. When expanding tobacco expanded tobacco did not change significally, but they were decreased at 27$0^{\circ}C$ very largely. The curtailment of cost price and physical and chemical properties of various items were improved in cigarettes. Key words : Expanding tobacco, Super steam tobacco expansion, Fast drying tobacco, High temperature treat tobacco, Puffing tobacco.

  • PDF

증기양생 온도조건에 따른 조강시멘트 콘크리트의 강도발현특성 및 내염특성 (The Characteristics of the Strength Development and Chloride Attack Resistance on the Concrete using High Early Strength Cement by Steam Curing Temperature Condition)

  • 이웅종;이원암;엄태선;이종열
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 추계 학술발표회 제17권2호
    • /
    • pp.599-602
    • /
    • 2005
  • In this research, the characteristics of the strength development and chloride attack resistance on the concrete using high early strength cement by steam curing temperature condition were studied. As a result, It is observed that the early strength(16hr) is increasing and the strength of 28 days is decreasing, according as the rising of the steam curing temperature without the kinds of base cement(OPC and high early strength cement). On the other hand, it is observed that the more the contents of the unit binder(base cement + GGBF) is abundant, the more the steam curing temperature can be reduced in case of the high early strength. Also, the chloride attack resistance is improved according as the amount of GGBF is increased with the kinds of base cement(OPC and high early strength cement).

  • PDF