• 제목/요약/키워드: hard Coating

검색결과 271건 처리시간 0.027초

펄스형 DC PACVD 법에의해 미치는 공정인자의 영향 (The Effect of Processing Parameters on the Mechanical Properties of TiN Films by the Pulsed DC PACVD)

  • 김진관;변응선;백운승;이구현;제창웅;윤재홍;이상로
    • 한국표면공학회지
    • /
    • 제30권5호
    • /
    • pp.298-309
    • /
    • 1997
  • Hard Tin coating on tool steel substrate were prepared using the pulsed PACVE. An orthogonal experimental design was employed to find the best deposition conditions for TiN coating and to systematically understand the effect of processing parameters. The small size Taguchi matrix called the L16 was used for experiment and ANOVA(ANalysis of VAriance) was followed to study the effect of main parameters on hardness and adhesion TiN coatings. In conclusion, pulse on/off time ratio and pulsing frequency were the major deposition parameters to determine hardness and adhesion of TiN coating in the pulsed DC PACVE process. (200) preferred orientation, columnar growth and dome-shaped surface morphology of the TiN films gave rise to a high hardness and a good adhesion to the substrates.

  • PDF

FE ANALYSIS OF INTERFACIAL BEHAVIOR OF COLD FORGING TOOL COATED BY HARD FILM

  • HAYAKAWA Kunio
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 The 8th Asian Symposium on Precision Forging ASPF
    • /
    • pp.18-21
    • /
    • 2003
  • A behavior of interface of cold forging tool coated by hard film is analyzed by FEM. The indentation of a hemispherical tool of SUJ2 in JIS coated by electroplated coating of chromium into a cylindrical workpiece of S25C in JIS is performed. The proposed constitutive equations are implemented by the non-linear springs model at the interface. Calculated results show that the maximum interfacial normal displacement is observed at an immediately forward from the lip of the indentation, whereas maximum interfacial tangential displacement is at the immediately backward of the lip of the indentation.

  • PDF

고속회전 하는 정밀부품을 위한 연질/경질 코팅의 트라이볼로지적 특성에 관한 연구 (Tribological Characteristics of Soft/Hard Coating for High-Speed Rotating Machine Elements)

  • 오진규;정구현;김대은;유제환;김형채
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2003년도 춘계학술대회 논문집
    • /
    • pp.393-397
    • /
    • 2003
  • Recently, rotating elements which use mechanical and electrical systems have been utilized for high speed and accuracy to increase the performance. The most important thing to get a more reliable system is to understand the friction, wear and characteristics which has an effect on various coated surfaces. In this study, the tribologicali characteristics of various soft/hard materials were investigated by using a custom-built pin-on-reciprocator tester From the experimental results, it was found that the friction coefficients of the soft material coated surfaces were lower under various normal loads due to trier self-lubricating ability and material transfer to the counter surface.

  • PDF

Determination of winding diameter based on bending strain analysis for REBCO coated conductor tapes

  • Leon, M.B. De;Dedicatoria, M.J.;Shin, H.S.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제14권2호
    • /
    • pp.8-11
    • /
    • 2012
  • In order to recognize the allowable bending diameter in coils, the strain as function of diameters is evaluated. The irreversible strain limits of $I_c$ in the easy and hard bending modes were measured. Strains were calculated at the coating film in the easy bending and at outer edge or inner edge in the hard bending of the CC tape, respectively. The tape geometry subjected to bending procedures is considered from the current industrial spool winding operation. Through the linear superposition of strain induced in different bending modes regarding the expressions, the appropriate design for critical bending diameter is suggested. Results proved that the existence of buckling resulting from bending in hard direction when applied strain exceeded 0.6% is possible. The depicted results showed that the strain limit as a viable parameter should be considered for future purposes.

수분산 폴리우레탄, 폴리실록산, UHMWPP 분말을 이용하여 제조한 자동차 부품용 코팅제 합성 및 물성 연구 (Synthesis and Properties of Coating Agents for Automobile Parts Using Water-born Polyurethane, Polysiloxane, and UHMWPP Powder)

  • 김용성;박성진;김영환;김혜진;임충선;서봉국
    • 접착 및 계면
    • /
    • 제24권4호
    • /
    • pp.124-130
    • /
    • 2023
  • 외부 온도 변화에 따른 특성변화가 적어야 하는 자동차 부품용 코팅제는 외부 환경 변화에 의한 노이즈 특성 변화가 매우 중요하다. 이에 내한성, 내후성, 내마모성이 우수한 연질의 폴리우레탄과 하이드록시 말단 혹은 곁사슬이 아민으로 변성된 폴리실록산 등이 널리 사용되고 있다. 본 연구에서는 각각의 폴리머 성분들이 노이즈에 미치는 영향을 확인하기 위하여 수분산 폴리우레탄을 합성하였고, 폴리실록산, ultra high molecular polypropylene (UHMWPP) 분말, 카본블랙, 소광제를 첨가하여 코팅제를 제조하였다. 수분산 폴리우레탄의 hard/soft 세그먼트의 함량을 27.1%/72.9%, 아민으로 변성된 폴리실록산과 하이드록시 말단 폴리실록산이 2:7의 비율에서 노이즈의 발생이 가장 적었으며, 마찰자가 고속에서 움직일 때 마찰계수의 차이가 컸다. 또한 SiO2를 UHMWPP 분말로 대체함으로써, 노이즈가 감소하였으며 광택도 또한 감소하였다.

Efficiency enhancement of spray QD solar cells

  • Park, Dasom;Lee, Wonseok;Jang, Jinwoong;Yim, Sanggyu
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.420.1-420.1
    • /
    • 2016
  • Colloidal quantum dot (CQD) is emerging as a promising active material for next-generation solar cell applications because of its inexpensive and solution-processable characteristics as well as unique properties such as a tunable band-gap due to the quantum-size effect and multiple exciton generation. However, the most widely used spin-coating method for the formation of the quantum dot (QD) active layers is generally hard to be adopted for high productivity and large-area process. Instead, the spray-coating technique may potentially be utilized for high-throughput production of the CQD solar cells (CQDSCs) because it can be adapted to continuous process and large-area deposition on various substrates although the cell efficiency is still lower than that of the devices fabricated with spin-coating method. In this work, we observed that the subsequent treatment of two different ligands, halide ion and butanedithiol, on the lead sulfide (PbS) QD layer significantly enhanced the cell efficiency of the spray CQDSCs. The maximum power conversion efficiency was 5.3%, comparable to that of the spin-coating CQDSCs.