Determination of winding diameter based on bending strain analysis for REBCO coated conductor tapes

  • Leon, M.B. De (Department of Mechanical Engineering, Andong National University) ;
  • Dedicatoria, M.J. (Department of Mechanical Engineering, Andong National University) ;
  • Shin, H.S. (Department of Mechanical Engineering, Andong National University)
  • Received : 2012.03.22
  • Accepted : 2012.04.19
  • Published : 2012.05.31

Abstract

In order to recognize the allowable bending diameter in coils, the strain as function of diameters is evaluated. The irreversible strain limits of $I_c$ in the easy and hard bending modes were measured. Strains were calculated at the coating film in the easy bending and at outer edge or inner edge in the hard bending of the CC tape, respectively. The tape geometry subjected to bending procedures is considered from the current industrial spool winding operation. Through the linear superposition of strain induced in different bending modes regarding the expressions, the appropriate design for critical bending diameter is suggested. Results proved that the existence of buckling resulting from bending in hard direction when applied strain exceeded 0.6% is possible. The depicted results showed that the strain limit as a viable parameter should be considered for future purposes.

Keywords

References

  1. A. Mbaruku, "Electromechanical and fatigue properties of as-manufactured and quench damaged YBCO coated conductor," PhD Thesis, Florida State Univ., 2006.
  2. W. D. Markiewicz, C. A. Swenson, "Winding strain analysis for YBCO coated conductors." Supercond. Sci. Technol, vol. 23, 045017, March 2010. https://doi.org/10.1088/0953-2048/23/4/045017
  3. A. V. Zlobin et al., "Modeling the high-field section of a Muon helical cooling channel," Proceedings of IPAC'10, Kyoto, Japan, pp. 391-393, 2010.
  4. H. C. Jo et al., "Characteristic comparison of various winding methods of HTS magnets", IEEE Trans. Appl. Supercond., 2012, submitted for publication.
  5. H. S. Shin, K. Katagiri, "Critical current degradation behavior in Bi-2223 superconducting tapes under bending and torsion strains". Supercond. Sci. Technol., vol. 16, pp. 1012-1018, 2003. https://doi.org/10.1088/0953-2048/16/9/309
  6. H. S. Shin, M. J. Dedicatoria, N. J. Lee, S. S. Oh, "Effect of bending test procedure on the degradation behavior of critical current in ReBCO coated conductor tapes," KIASC Journal, vol. 11, no. 4, pp. 12-15, 2009
  7. H. S. Shin, J. R. C. Dizon, R. Bonifacio, J. S. Park, "Influence of bending strain on $I_c$ degradation behavior in YBCO coated conductor tapes processed using RABiTs /MOD," KIASC Journal, vol. 9, n0. 2, pp. 11-14, 2007.
  8. H. S. Shin, M. J. Dedicatoria, J. R. C. Dizon, H. S. Ha, S. S. Oh, "Bending strain characteristics of critical current in REBCO CC tapes in different modes," Physica C, vol. 469, pp. 1467-1471, 2009. https://doi.org/10.1016/j.physc.2009.05.067
  9. D. C. van der Laan, J. W. Ekin, C. C. Clickner and T. C. Stauffer, "Delamination strength of YBCO coated conductors under transverse tensile stress," Supercond. Sci. Technol., vol. 20, pp. 765-770, 2007. https://doi.org/10.1088/0953-2048/20/8/007

Cited by

  1. Evaluation of electrical fatigue limits in REBCO coated conductor tapes through static fatigue testing at 77 K vol.35, pp.2, 2012, https://doi.org/10.1088/1361-6668/ac32ac