• Title/Summary/Keyword: glass particles

검색결과 465건 처리시간 0.025초

Magnetization of Ultrafine Cadmium Ferrite Particles

  • Park, Eun-Jung
    • 한국세라믹학회지
    • /
    • 제39권1호
    • /
    • pp.12-15
    • /
    • 2002
  • Ultrafine cadmium ferrite particles have been investigated by X-ray diffractometry, transmission electron microscopy and SQUID magnetometry. All peaks of X-ray diffraction patterns are broad, but correspond to a cubic spinel structure with the lattice constant of 8.65 $\AA$. The average particle size determined by TEM is 9.7 nm and the size distribution of particles is not normal, but lognormal. The maximal magnetization measured at 5 K was 17.7 emu/g. The experimental data show a transi-tion from a disorder ferrimagnetic phase to a spin-glass phase (i.e. reentrant behavior) with a freezing temperature (T$\_$f/) of 30 K. Superparamagnetic behavior of the particles is confirmed by the coincidence of the plots of M vs. H/T for 100 and 300 K.

Cu계 비정질 입자의 가압 성형 (Consolidation of Cu-based amorphous particles)

  • 강은영;정영훈;유호근;박종우
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.273-276
    • /
    • 2005
  • Packing characteristics of amorphous alloy particles were investigated by scanning electron microscopy, compositional analysis, micro-hardness test and finite element method (FEM). Electroless Ni-plating was made on the surface of the Cu-based amorphous particles before consolidation in ambient atmosphere at an intermediate region of glass transition and crystallization temperatures $(T_g\;and\;T_x)$. Some parts of the Ni-layer in the interfaces of the consolidated particles disappeared, while some of them still remained without appreciable change in compositions. No cracks or fractures were found in the particles, which may occur at low temperatures below or near $T_g$ as anticipated by the FEM analysis. Crystallization and change in hardness were not observed after consolidation.

  • PDF

Powder Blasting 을 이용한 유리의 표면부식시 분사각도의 영향 (Effect of Impact Angle on the Etching of Glass by Powder Blasting)

  • 김광현;박경호;박동삼
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2001년도 추계학술대회(한국공작기계학회)
    • /
    • pp.349-354
    • /
    • 2001
  • In this study, we investigated the effect of the impacting ang1e of particles, the scanning times and the stand-off distance on the surface roughness and the weight-loss rate of samples with no mask, and the wall profile and overetching of samples with different mask pattern in powder blasting of soda-lime glass. The varying parameters were the different impact angles between 50$^{\circ}$ and 90$^{\circ}$, scanning times of nozz1e up to 40 and the stand-off distances 70mm and 100mm. The widths of mask pattern were 0.2mm, 0.5mm and 1mm. The powder was alumina sharp particles, WA#600. The mass flow rate of powder during the erosion test was fixed constant at 175g/min and the blasting pressure of powder at 0.2MPa

  • PDF

블록 매칭을 이용한 Granular Flow의 속도 측정 (Velocity Measurement of Granular Flow with Block Matching)

  • 이진걸
    • 공학논문집
    • /
    • 제2권1호
    • /
    • pp.5-11
    • /
    • 1997
  • 입자 물질의 흐름(granular flow)은 일반 산업체의 거의 모든 공정에서 발생한다. 본 논문은 중력 하에서 경사진 슈트 (chute)를 통하여 흐르는 입자들의 속도를 측정하기 위하여 고속 디지털 영상을 이용한 방법을 논한다. 유리 입자 들이 이 실험에서 사용되었다. 유리 입자 들의 평균 속도를 측정하기 위하여 블록 매칭 (block matching)이 사용되었으며 유리입자 들의 평균속도는 변동 정규 상관 함수에 보간법을 적용함으로서 화소 간격보다 적은 단위로 측정하였다.

  • PDF

水性가스 轉換反應觸媒의 流動化에 關하여 (The Fluidization of a Water Gas Shift Conversion Catalyst)

  • 이재성;김영우
    • 대한화학회지
    • /
    • 제6권1호
    • /
    • pp.54-60
    • /
    • 1962
  • The water gas shift conversion catalyst prepared by the American Cyanamide Co. was subjected to fluidization in a 2-in. Pyrex glass tube to obtain the basic fluidization characteristic data. The size of the catalyst charged ranged from 70 to 120 meshes and it was supported on a single layer 300-mesh wire gauze through which the fluidizing medium, the air, was passed. Following are some data and facts found by the authors: (1) The catalyst particles were porous, and their surfaces were trough and irregular. (2) The average effective particle density and the average shape factor of these particles were 152.2 lb/$ft^3$ and 0.865 respectively. (3) As the particle diameter of the catalyst increased, the minimum fluid voidage of the bed decreased slightly. (4) Just before the incipient fluidization, pressure drop suddenly fell and the bed expanded simultaneously. (5) After fluidization set in, the expansion characteristics of the catalyst bed were similar to those of sand and glass beads except intense bubbling in the catalyst bed.

  • PDF

The Thermal Properties of PVC-Ni Composite Materials

  • Moon, Tak-Jin;Kang Chang-Gyun
    • Bulletin of the Korean Chemical Society
    • /
    • 제6권1호
    • /
    • pp.45-50
    • /
    • 1985
  • The glass transition temperature, dynamic shear moduli, and bulk viscosities of PVC, filled with nickel particles, were investigated. The glass temperature of the composite increased with increasing filler concentration. The data were interpreted by assuming that the interaction between filler particles and the polymer matrix reduces molecular mobility and flexibility of the polymer chains in the vicinity of the interfaces. The relative modulus for the PVC/Ni composite system followed the Kerner equation. The relative viscosities were strongly temperature dependent and did not agree with the conventional viscosity predictions for suspensions. It is suggested that the filler has a twofold effect on the viscosity of the composite materials; one is due to its mechanical presence and the other is due to modification of part of the polymer matrix caused by interaction. This phenomenon is approximately bounded by Kerner's predictions for suspensions.

비수계 테잎성형공정의 유기공정변수의 변화에 따른 티탄산바륨-붕규산염유리계 현탁액의 분산안정성 (Effect of Organic Processing Parameters in Non-aqueous Tape-casting on Dispersion Stability of Barium Titanate-Borosilicate Glass Based Suspensions)

  • 여정구;최성철
    • 한국재료학회지
    • /
    • 제13권11호
    • /
    • pp.725-731
    • /
    • 2003
  • The effect of organic processing parameters on the dispersion stability of the BaTiO$_3$-based dielectric particles and borosilicate glass particulate suspensions was investigated in a system where organic solvents, dispersant, binder and modifier were used as processing additives in a low temperature cofired ceramic fabrication processes. Two- and three-component organic solvents were used to disperse ceramic particles and it was found the better stability in the particulate suspension prepared in a bi-solvent, which was consists of toluene and ethanol in a non-azeotropic composition. The addition amount of organic additives had a great impact on dispersion in the present investigation. The flow curves of the suspensions prepared with binder and modifier were fitted according to the power-law equation, which indicates that the internal structure of the suspension could be disturbed under the applied shear stress. Finally, the LTCC green tapes were successfully tape-cast based upon the optimum formulation of LTCC suspension and its microstructure was compared with that of the hard-agglomerates.

유리 재료의 헬리컬 스캔 연삭 조건 실험 (Experiments on the Grinding Conditions for Helical Scan Grinding of a Glass Material)

  • 이대욱;오창진;이응석;김옥현;김성청
    • 한국정밀공학회지
    • /
    • 제18권9호
    • /
    • pp.165-170
    • /
    • 2001
  • In normal grinding abrasive particles of a grinding wheel rotate on planes parallel to the direction of workpiece fred. which may induce continued scratch lines on ground surface as the workpiece feeds. Instead in helical scan grinding the planes make an angle, called a helical angle, with the feeding direction. Thus scratch lines produced by abrasive particles per one revolution are discontinued which implies that the generation of scratch lines are suppressed by the helical scan grinding. In this study some experimental works have been done on the helical scan grinding of glass to find the effects of grinding conditions on the surface roughness and estimate the optimal grinding conditions. The helical angle, fred rate, material removal rate and the wheel speed are taken as factors for three kinds of grinding wheels i.e., coarse(#140 mesh), medium(#400) and fine(#800) diamond wheels. The experiments are scheduled by Taguchi technique and ANOVA has been carried out for the interpretation of the results. As a result of this study effects of the factors are verified quantitatively showing that the major factors are changed according to the wheel's mesh size and the helical angle is one of the influencing factors on the surface quality.

  • PDF

클린룸 내 롤러 컨베이어 운송장치 주위의 유동해석 (Flow Analysis around the Roller Conveyor in a Clean Room)

  • 전현주;박찬우;임익태
    • 대한설비공학회:학술대회논문집
    • /
    • 대한설비공학회 2009년도 하계학술발표대회 논문집
    • /
    • pp.1507-1512
    • /
    • 2009
  • Flow field in a roller conveyor system, induced from the movement of a cassette in which glasses for flat panel display are loaded, is numerically studied in this paper. Contamination on the glass surface by dust particles produced from mechanical friction between roller and cassette is predicted from the analysis results of flow fields. Results show that a large swirl flow is formed under the moving cassette with constant speed. This swirl flow is confined only under the cassette because two main streams from the backward and the fan filter unit on the top ceiling are sufficiently strong. Therefore, it can be said that possibility of the contamination by the particles originated from the friction is relatively low. It is also revealed that flow direction between glass plates is changed according to the speed of the cassette movement due to the shear force of glass plates.

  • PDF

Cd 입도 크기가 CdS/CdTe 태양전지의 특성에 미치는 영향 (The Effects of Cd particle size on the Properties of Cds/CeTe Solar Cells)

  • 임호빈;노재성
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1987년도 정기총회 및 창립40주년기념 학술대회 학회본부
    • /
    • pp.200-202
    • /
    • 1987
  • Sintered CdS films on glass substrate with low electrical resistivity and high optical transmittance have been prepared by coating and sintering method. All-polycrystalline CdS/CdTe solar cells with different microstructure and properties of CdTe layer were fabricated by coating a number of CdTe slurries, which consisted of Cd and Te powders, an appropriate amount of propylene glycol and 2 or 7.5 w/o $CdC1_2$, on the sintered CdS films and by sintering the glass-CdS-(Cd+Te) composites at various temperature. To explore the dependence of the solar efficiency on the preparation conditions of the CdTe layer, Cd powder with an average particle size of $0.3{\mu}m$ or $5{\mu}m$ was prepared. The use of Cd with finer particles forms more dense or uniform microstructure of the nuclear of CdTe during the heating. Therefore the use of Cd with finer particles improves the efficiency of the sintered CdS/CdTe solar cell by improving the microstructure of sintered CdTe layer. But the difference of solar efficiency by varing a particle size of Cd is decreased with increasing amount of $CdC1_2$ in the (Cd+Te) layer. All-polycrystalline CdS/CdTe solar cells with an efficiency of 10.2% under solar irradiation have been fabricated using a Cd with finer particles.

  • PDF